Gallium nitride power device structure and manufacturing method thereof
By introducing a graphene heat dissipation layer and microstructure design into gallium nitride power devices, the electric field distribution is optimized, solving the problems of interface damage and insufficient heat dissipation in HEMT devices, and improving the reliability and stability of the devices.
Patent Information
- Application Number
- CN202010519988.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-06-10
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2040-06-10
AI Technical Summary
Existing gallium nitride high electron mobility transistor (HEMT) devices are prone to interface damage and cracks under high-intensity electric field stress, leading to performance degradation and insufficient heat dissipation, which affects reliability.
A gallium nitride power device structure was designed, using graphene as a heat dissipation layer, and setting a recess and a gate insertion layer protrusion on the AlGaN barrier layer. Combined with microstructure design, the electric field distribution and heat dissipation performance were optimized.
It improves the heat dissipation performance and electric field uniformity of the device, reduces the leakage current collapse effect, enhances the reliability and stability of the device, and is compatible with existing chip manufacturing processes.
Smart Images

Figure CN111584629B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of power semiconductor devices, and in particular to a gallium nitride power device structure and a manufacturing method thereof. Background Art
[0002] High electron mobility transistors (HEMTs) based on gallium nitride materials have the advantages of high breakdown voltage, high electron mobility, fast switching speed, and simple process steps, and have broad application prospects in the field of power semiconductor devices. However, HEMT devices are subject to high-intensity electric field stress in the working state, which causes interface damage during the long-term operation of the device, resulting in a decrease in device performance or even damage. Therefore, improving device reliability through design is an important issue that device designers are concerned about.
[0003] In terms of epitaxial material growth, due to the huge lattice mismatch and thermal expansion coefficient mismatch between the heterogeneous substrate and GaN, such as: Si-based GaN usually faces crack problems caused by tensile stress relaxation during the epitaxial process and when cooling down after the growth, so the epitaxial growth of high-quality Si-based GaN materials is very challenging. The lattice mismatch of epitaxial GaN film on Si substrate is as high as 17%, and the lattice mismatch during the growth process will introduce a large number of dislocations. Secondly, the large difference in thermal expansion coefficient between Si substrate and GaN leads to a large thermal mismatch. The thermal expansion coefficient of Si is 3.59×10 -6 K -1 , while the thermal expansion coefficient of GaN is 5.59×10 -6 K -1 The difference between the two is very large, resulting in the epitaxial layer to be subjected to a large tensile stress during the cooling process after high-temperature growth, and because the thickness of the epitaxial layer is much smaller than the thickness of the substrate, cracks will appear in the epitaxial layer. Therefore, how to achieve high-quality HEMT epitaxial materials is one of the key factors restricting device performance.
[0004] At the same time, existing studies have shown that when HEMT devices are working, there is a large electric field peak at the gate end of the device. When the device is in operation, the strong electric field at the gate end will cause a large number of interface states to be generated in this area, resulting in a decrease in device performance and reliability issues. At the same time, the heat of HEMT devices is usually accumulated in the active area. In order to improve the overall heat dissipation capacity of HEMT devices, high thermal conductivity materials are used to improve the heat dissipation capacity of HEMT devices. Graphene materials, which are currently a research hotspot, have even stronger heat dissipation capabilities, and their thermal conductivity is about 5000W / m·K. Such a high heat dissipation rate material will greatly help solve the problem of thermal conduction of HEMT devices and further improve the reliability of HEMT devices. Summary of the invention
[0005] One of the purposes of the present invention is to overcome the deficiencies in the prior art and provide a gallium nitride power device structure with low leakage and better heat dissipation performance.
[0006] Another object of the present invention is to provide a method for preparing a gallium nitride power device structure.
[0007] According to the technical solution provided by the present invention, the gallium nitride power device structure includes a substrate, a nucleation layer, a first GaN epitaxial layer, an insertion layer, a second GaN epitaxial layer and an AlGaN barrier layer arranged in sequence from bottom to top, a barrier layer recess is opened in the middle of the upper surface of the AlGaN barrier layer, a gate insertion layer is arranged just above the barrier layer recess, a gate insertion layer protrusion is arranged on the lower surface of the gate insertion layer, the gate insertion layer protrusion is embedded in the barrier layer groove and fills the barrier layer recess, a P-type GaN gate is arranged on the upper surface of the gate insertion layer, a protective layer is arranged on the upper surfaces of the AlGaN barrier layer and the P-type GaN gate, a heat dissipation layer is arranged on the upper surface of the protective layer, a protective layer recess is opened on the upper surface of the protective layer, a heat dissipation layer protrusion is arranged on the lower surface of the heat dissipation layer, the heat dissipation layer protrusion is embedded in the protective layer recess and fills the protective layer recess;
[0008] A source metal window and a drain metal window are provided on the protective layer and the heat dissipation layer, the source metal window is provided with a source metal connected to the AlGaN barrier layer, the drain metal window is provided with a drain metal connected to the AlGaN barrier layer, a gate metal window is also provided on the protective layer and the heat dissipation layer, the gate metal window is provided with a gate metal connected to the P-type GaN gate.
[0009] Preferably, the maximum depth of the depression of the barrier layer is located above the upper surface of the second GaN epitaxial layer; and the maximum depth of the depression of the protection layer is located above the upper surface of the AlGaN barrier layer.
[0010] Preferably, the material of the insertion layer is any one of GaN, AlGaN, AlInN, and AlInGaN, or any one or more of a multi-period superlattice structure material composed of any combination of GaN, AlN, InN, AlGaN, AlInN, InGaN, and AlInGaN. When the insertion layer is a multi-period superlattice structure, the number of periods is 1 to 5, and the thickness of the insertion layer is 50 nm to 500 nm.
[0011] Preferably, the material of the gate insertion layer is any one of single-layer AlN, AlGaN, AlInN, AlInGaN, or any one or more of a multi-period superlattice structure material composed of any combination of AlN, AlGaN, AlInN, AlInGaN. When the gate insertion layer is a multi-period superlattice structure, the number of periods is 1 to 100, and the thickness of the gate insertion layer is 50 nm to 500 nm.
[0012] Preferably, the material of the protective layer is SiO 2 、Si 3 N 4 、SiC、TiO 2 、Al 2 O 3 , any one or more of phosphosilicate glass, and the thickness of the protective layer is 500nm ~ 3000nm.
[0013] Preferably, the gate insertion layer is P-type doped, and the doping concentration is: 1×10 16 cm -3 ~ 5×10 21 cm -3 The doping concentration of the P-type GaN gate is: 1×10 16 cm -3 ~ 5×10 21 cm -3 , thickness is 20 nm ~ 200nm.
[0014] Preferably, the substrate is made of any one of sapphire, silicon, silicon carbide, gallium nitride, aluminum nitride, boron nitride, gallium oxide, zinc oxide, and diamond;
[0015] The material of the nucleation layer is any one of GaN, AlN and InN, and the thickness is 5 nm to 30 nm;
[0016] The thickness of the first GaN epitaxial layer is 500 nm to 3500 nm;
[0017] The thickness of the second GaN epitaxial layer is 800 nm to 3500 nm;
[0018] The thickness of the AlGaN barrier layer is 5 nm to 60 nm;
[0019] The heat dissipation layer is made of graphene material, and has a thickness of 0.335 nm to 10 nm;
[0020] The source metal, gate metal, and drain metal are made of any one or more of titanium, aluminum, gold, nickel, silver, copper, and platinum.
[0021] Preferably, the barrier layer is recessed in an inverted triangular pyramid or a rectangular parallelepiped shape, and the gate insertion layer protrusion is inverted triangular pyramid or a rectangular parallelepiped shape.
[0022] Preferably, the protective layer is concave in a hemispherical shape or an inverted tetrahedron shape, and the heat dissipation layer is convex in a hemispherical shape or an inverted tetrahedron shape.
[0023] A method for manufacturing a gallium nitride power device structure comprises the following steps:
[0024] Step 1: growing a nucleation layer on a substrate;
[0025] Step 2: growing a first GaN epitaxial layer on the nucleation layer;
[0026] Step 3, growing an insertion layer on the first GaN epitaxial layer;
[0027] Step 4: growing a second GaN epitaxial layer on the insertion layer;
[0028] Step 5: growing an AlGaN barrier layer on the second GaN epitaxial layer;
[0029] Step 6: Make a mask on the upper surface of the AlGaN barrier layer, and selectively etch part of the epitaxial layer by wet or dry method to form periodic or non-periodic barrier layer depressions, and control the maximum depth of the barrier layer depressions to be above the upper surface of the second GaN epitaxial layer;
[0030] Step 7: growing a gate insertion layer just above the corresponding barrier layer recessed region, and forming a gate insertion layer protrusion on the lower surface of the gate insertion layer that matches the barrier layer recessed region;
[0031] Step 8: growing a P-type GaN gate on the gate insertion layer;
[0032] Step nine, growing a protective layer on the upper surface of the entire epitaxial layer;
[0033] Step 10, etching the protective layer located on both sides of the P-type GaN gate to form periodic or non-periodic protective layer depressions, and controlling the maximum etching depth of the protective layer depressions to be located above the upper surface of the AlGaN barrier layer;
[0034] Step 11: growing a heat dissipation layer on the upper surface of the etched protective layer, and forming a heat dissipation layer protrusion on the lower surface of the heat dissipation layer to match the protective layer concave;
[0035] Step 12: Make a mask on the upper surface of the heat dissipation layer, and selectively photolithography to open windows corresponding to the source metal, the gate metal, and the drain metal respectively;
[0036] Step 13: Make a mask on the upper surface of the heat dissipation layer, perform selective photolithography, and etch the covering layer of part or all of the upper surface of the P-type GaN gate until the upper surface of the P-type GaN gate is exposed to form a recessed area, and then evaporate the gate metal in the recessed area, and anneal the electrode;
[0037] Step 14: Make a mask on the upper surface of the heat dissipation layer, perform selective photolithography, and etch the epitaxial layer until the AlGaN barrier layer is exposed to form a recessed area, then evaporate the source metal in the recessed area, and anneal the electrode;
[0038] Step 15: Make a mask on the upper surface of the heat dissipation layer, perform selective photolithography, and etch the epitaxial layer until the AlGaN barrier layer is exposed to form a recessed area. Then, evaporate the drain metal in the recessed area and anneal the electrode.
[0039] The device of the present invention has a smaller peak electric field at the gate end in the withstand voltage state, has smaller leakage, and effectively avoids the current collapse effect. At the same time, the graphene heat dissipation layer design is adopted, combined with the microstructure design, which greatly increases the heat dissipation area and channel, improves the heat dissipation performance of the device, and thus the reliability of the device is further improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 is a cross-sectional view of the device of the present invention. DETAILED DESCRIPTION
[0041] The present invention will be further described below in conjunction with specific embodiments.
[0042] Example 1
[0043] A gallium nitride power device structure comprises, from bottom to top, a silicon substrate 101, an AlN nucleation layer 102 with a thickness of 5 nm, a first GaN epitaxial layer 103 with a thickness of 500 nm, an AlInGaN insertion layer 104 with a thickness of 50 nm, a second GaN epitaxial layer 105 with a thickness of 800 nm, and an AlGaN barrier layer 106 with a thickness of 5 nm, wherein an inverted triangular pyramid barrier layer depression with a maximum depth of 25 nm is provided in the middle of the upper surface of the AlGaN barrier layer 106, and a P-type doping concentration of 1×10 16 cm -3 , a GaN / AlInGaN superlattice gate insertion layer 107 with a period number of 1 and a thickness of 50 nm, a gate insertion layer protrusion is provided on the lower surface of the gate insertion layer 107, the gate insertion layer protrusion is embedded in the barrier layer groove and fills the barrier layer recess, and a doping concentration of 1×10 16 cm-3 The P-type GaN gate 108 has a thickness of 20 nm, and a SiO layer with a thickness of 500 nm is provided on the upper surface of the AlGaN barrier layer 106 and the P-type GaN gate 108. 2 A protective layer 109, a heat dissipation layer 110 made of graphene material and having a thickness of 0.335 nm is provided on the upper surface of the protective layer 109, a hemispherical protective layer depression with a maximum depth of 250 nm is opened on the upper surface of the protective layer 109, and a heat dissipation layer protrusion is provided on the lower surface of the heat dissipation layer 110, and the heat dissipation layer protrusion is embedded in the protective layer depression and fills the protective layer depression;
[0044] A source metal window and a drain metal window are provided on the protective layer 109 and the heat dissipation layer 110, which are deep to the upper surface of the AlGaN barrier layer 106; a titanium / aluminum / nickel / gold source metal 111 connected to the AlGaN barrier layer 106 is provided in the source metal window; a titanium / aluminum / nickel / gold drain metal 113 connected to the AlGaN barrier layer 106 is provided in the drain metal window; a gate metal window is also provided on the protective layer 109 and the heat dissipation layer 110, which is deep to the upper surface of the P-type GaN gate 108; a titanium / aluminum / nickel / gold gate metal 112 connected to the P-type GaN gate 108 is provided in the gate metal window.
[0045] The method for manufacturing the above-mentioned gallium nitride power device structure comprises the following steps:
[0046] Step 1: growing a nucleation layer 102 on the substrate 101;
[0047] Step 2: growing a first GaN epitaxial layer 103 on the nucleation layer 102;
[0048] Step 3: growing an insertion layer 104 on the first GaN epitaxial layer 103;
[0049] Step 4: growing a second GaN epitaxial layer 105 on the insertion layer 104;
[0050] Step 5: growing an AlGaN barrier layer 106 on the second GaN epitaxial layer 105;
[0051] Step 6: Make a mask on the upper surface of the AlGaN barrier layer 106, and selectively etch part of the epitaxial layer by wet or dry method to form periodic or non-periodic barrier layer depressions, and control the maximum depth of the barrier layer depressions to be located above the upper surface of the second GaN epitaxial layer 105;
[0052] Step 7: growing a gate insertion layer 107 directly above the corresponding barrier layer recessed region, and forming a gate insertion layer protrusion on the lower surface of the gate insertion layer 107 that matches the barrier layer recessed region;
[0053] Step 8: growing a P-type GaN gate 108 on the gate insertion layer 107;
[0054] Step nine, growing a protective layer 109 on the upper surface of the entire epitaxial layer;
[0055] Step 10: etching the protective layer 109 on both sides of the P-type GaN gate 108 to form periodic or non-periodic protective layer depressions, and controlling the maximum etching depth of the protective layer depressions to be located above the upper surface of the AlGaN barrier layer 106;
[0056] Step 11: growing a heat dissipation layer 110 on the upper surface of the etched protection layer 109, and forming a heat dissipation layer protrusion on the lower surface of the heat dissipation layer 110 to match the protection layer depression;
[0057] Step 12: Make a mask on the upper surface of the heat dissipation layer 110, and selectively perform photolithography to open windows corresponding to the source metal 111, the gate metal 112, and the drain metal 113 respectively;
[0058] Step 13: Make a mask on the upper surface of the heat dissipation layer 110, perform selective photolithography, and etch the covering layer of part or all of the upper surface of the P-type GaN gate 108 until the upper surface of the P-type GaN gate 108 is exposed to form a recessed area, and then evaporate the gate metal 112 in the recessed area, and anneal the electrode;
[0059] Step 14: Make a mask on the upper surface of the heat dissipation layer 110, perform selective photolithography, and etch the epitaxial layer until the AlGaN barrier layer 106 is exposed to form a recessed area, then evaporate the source metal 111 in the recessed area, and anneal the electrode;
[0060] Step 15: Make a mask on the upper surface of the heat dissipation layer 110, perform selective photolithography, and etch the epitaxial layer until the AlGaN barrier layer 106 is exposed to form a recessed area, then evaporate the drain metal 113 in the recessed area, and anneal the electrode.
[0061] Example 2
[0062] A gallium nitride power device structure is provided, which comprises, from bottom to top, a silicon carbide substrate 101, an AlN nucleation layer 102 with a thickness of 30 nm, a first GaN epitaxial layer 103 with a thickness of 3500 nm, a GaN / AlInGaN superlattice insertion layer 104 with a period number of 5 and a thickness of 500 nm, a second GaN epitaxial layer 105 with a thickness of 3500 nm, and an AlGaN barrier layer 106 with a thickness of 60 nm, wherein a barrier layer depression with a rectangular shape and a maximum depth of 30 nm is provided in the middle of the upper surface of the AlGaN barrier layer 106, and a p-type doping concentration of 5×1021 cm -3 , a GaN / AlInGaN superlattice gate insertion layer 107 with a thickness of 500 nm, a gate insertion layer protrusion is provided on the lower surface of the gate insertion layer 107, the gate insertion layer protrusion is embedded in the barrier layer groove and fills the barrier layer recess, and a doping concentration of 5×10 21 cm -3 The P-type GaN gate 108 has a thickness of 200 nm, and a Si layer with a thickness of 3000 nm is provided on the upper surface of the AlGaN barrier layer 106 and the P-type GaN gate 108. 3 N 4 A protective layer 109, a heat dissipation layer 110 made of graphene material and having a thickness of 10 nm is provided on the upper surface of the protective layer 109, a protective layer depression with an inverted tetrahedron shape and a maximum depth of 1500 nm is opened on the upper surface of the protective layer 109, and a heat dissipation layer protrusion is provided on the lower surface of the heat dissipation layer 110, and the heat dissipation layer protrusion is embedded in the protective layer depression and fills the protective layer depression;
[0063] A source metal window and a drain metal window are provided on the protective layer 109 and the heat dissipation layer 110, which are deep to the upper surface of the AlGaN barrier layer 106; a titanium / aluminum / titanium / nickel / gold source metal 111 connected to the AlGaN barrier layer 106 is provided in the source metal window; a titanium / aluminum / titanium / nickel / gold drain metal 113 connected to the AlGaN barrier layer 106 is provided in the drain metal window; a gate metal window is also provided on the protective layer 109 and the heat dissipation layer 110, which is deep to the upper surface of the P-type GaN gate 108; a titanium / aluminum / titanium / nickel / gold gate metal 112 connected to the P-type GaN gate 108 is provided in the gate metal window.
[0064] The method for manufacturing the above-mentioned gallium nitride power device structure comprises the following steps:
[0065] Step 1: growing a nucleation layer 102 on the substrate 101;
[0066] Step 2: growing a first GaN epitaxial layer 103 on the nucleation layer 102;
[0067] Step 3: growing an insertion layer 104 on the first GaN epitaxial layer 103;
[0068] Step 4: growing a second GaN epitaxial layer 105 on the insertion layer 104;
[0069] Step 5: growing an AlGaN barrier layer 106 on the second GaN epitaxial layer 105;
[0070] Step 6: Make a mask on the upper surface of the AlGaN barrier layer 106, and selectively etch part of the epitaxial layer by wet or dry method to form periodic or non-periodic barrier layer depressions, and control the maximum depth of the barrier layer depressions to be located above the upper surface of the second GaN epitaxial layer 105;
[0071] Step 7: growing a gate insertion layer 107 directly above the corresponding barrier layer recessed region, and forming a gate insertion layer protrusion on the lower surface of the gate insertion layer 107 that matches the barrier layer recessed region;
[0072] Step 8: growing a P-type GaN gate 108 on the gate insertion layer 107;
[0073] Step nine, growing a protective layer 109 on the upper surface of the entire epitaxial layer;
[0074] Step 10: etching the protective layer 109 on both sides of the P-type GaN gate 108 to form periodic or non-periodic protective layer depressions, and controlling the maximum etching depth of the protective layer depressions to be located above the upper surface of the AlGaN barrier layer 106;
[0075] Step 11: growing a heat dissipation layer 110 on the upper surface of the etched protection layer 109, and forming a heat dissipation layer protrusion on the lower surface of the heat dissipation layer 110 to match the protection layer depression;
[0076] Step 12: Make a mask on the upper surface of the heat dissipation layer 110, and selectively perform photolithography to open windows corresponding to the source metal 111, the gate metal 112, and the drain metal 113 respectively;
[0077] Step 13: Make a mask on the upper surface of the heat dissipation layer 110, perform selective photolithography, and etch the covering layer of part or all of the upper surface of the P-type GaN gate 108 until the upper surface of the P-type GaN gate 108 is exposed to form a recessed area, and then evaporate the gate metal 112 in the recessed area, and anneal the electrode;
[0078] Step 14: Make a mask on the upper surface of the heat dissipation layer 110, perform selective photolithography, and etch the epitaxial layer until the AlGaN barrier layer 106 is exposed to form a recessed area, then evaporate the source metal 111 in the recessed area, and anneal the electrode;
[0079] Step 15: Make a mask on the upper surface of the heat dissipation layer 110, perform selective photolithography, and etch the epitaxial layer until the AlGaN barrier layer 106 is exposed to form a recessed area, then evaporate the drain metal 113 in the recessed area, and anneal the electrode.
[0080] Compared with the conventional solution, the present invention does not need to set a field plate, but only needs to add an insertion layer 104 below the gate, set a barrier layer depression on the upper surface of the AlGaN barrier layer 106, and set a gate insertion layer protrusion on the lower surface of the gate insertion layer 107, so as to improve the gate electric field distribution of the device. The electric field distribution is more uniform, and the withstand voltage capability of the device is further enhanced, so that the gallium nitride power device structure proposed by the present invention has higher reliability.
[0081] The technical solution of adding a gate insertion layer 104 under the P-type GaN gate of the present invention can effectively improve the gate turn-on voltage and gate voltage stability of the device while improving the crystal quality of the P-type GaN gate material, further improving the stability and reliability of the device.
[0082] The present invention adopts a technical solution of adding an insertion layer 104 between the first GaN epitaxial layer 103 and the second GaN epitaxial layer 105, which can greatly improve the crystal quality of the epitaxial GaN material on the heterogeneous substrate, effectively block the upward extension of dislocations, effectively reduce the device leakage caused by dislocations, and improve the reliability of the device.
[0083] The present invention uses graphene material as the heat dissipation layer 110 on the device surface, taking advantage of the large thermal conductivity and excellent thermal conductivity of graphene material, and adopts a structure in which a protective layer depression is provided on the upper surface of the protective layer 109 and a heat dissipation layer protrusion is provided on the lower surface of the heat dissipation layer to further improve the heat dissipation performance of the GaN power device. While improving the heat dissipation performance, the reliability of the device working at a higher temperature is also improved.
[0084] The gallium nitride power device structure and the manufacturing method thereof disclosed in the present invention can be implemented in a compatible manner with existing chip processing technology and are compatible with traditional processes, thereby reducing the preparation cost of the gallium nitride power device structure.
[0085] It must be pointed out that the above are only preferred embodiments of the present invention and the technical principles used. The present invention is not limited to the specific embodiments described herein, and it is possible for those skilled in the art to make various obvious changes, readjustments and substitutions without departing from the scope of protection of the present invention. Therefore, although the present invention is described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A gallium nitride power device structure, comprising, arranged in order from bottom to top, a substrate (101), a nucleation layer (102), a first GaN epitaxial layer (103), an insertion layer (104), a second GaN epitaxial layer (105) and an AlGaN barrier layer (106), Its characteristics are: A barrier layer recess is provided in the middle of the upper surface of the AlGaN barrier layer (106); a gate insertion layer (107) is provided directly above the barrier layer recess; a gate insertion layer protrusion is provided on the lower surface of the gate insertion layer (107); the gate insertion layer protrusion is embedded in the barrier layer groove and fills the barrier layer recess; a P-type GaN gate (108) is provided on the upper surface of the gate insertion layer (107); a protective layer (109) is provided on the upper surfaces of the AlGaN barrier layer (106) and the P-type GaN gate (108); a heat dissipation layer (110) is provided on the upper surface of the protective layer (109); a protective layer recess is provided on the upper surface of the protective layer (109); a heat dissipation layer protrusion is provided on the lower surface of the heat dissipation layer (110); the heat dissipation layer protrusion is embedded in the protective layer recess and fills the protective layer recess; A source metal window and a drain metal window are provided on the protective layer (109) and the heat dissipation layer (110) and are as deep as the upper surface of the AlGaN barrier layer (106); a source metal (111) connected to the AlGaN barrier layer (106) is provided in the source metal window; a drain metal (113) connected to the AlGaN barrier layer (106) is provided in the drain metal window; a gate metal window is also provided on the protective layer (109) and the heat dissipation layer (110) and is as deep as the upper surface of the P-type GaN gate (108); a gate metal (112) connected to the P-type GaN gate (108) is provided in the gate metal window.
2. The gallium nitride power device structure according to claim 1, Its characteristics are: The maximum depth of the depression of the barrier layer is located above the upper surface of the second GaN epitaxial layer (105); and the maximum depth of the depression of the protective layer is located above the upper surface of the AlGaN barrier layer (106).
3. The gallium nitride power device structure according to claim 1, Its characteristics are: The material of the insertion layer (104) is any one of GaN, AlGaN, AlInN, and AlInGaN, or any one or more of a multi-period superlattice structure material formed by any combination of GaN, AlN, InN, AlGaN, AlInN, InGaN, and AlInGaN. When the insertion layer (104) is a multi-period superlattice structure, the number of periods is 1 to 5, and the thickness of the insertion layer (104) is 50 nm to 500 nm.
4. The gallium nitride power device structure according to claim 1, Its characteristics are: The material of the gate insertion layer (107) is any one of single-layer AlN, AlGaN, AlInN, and AlInGaN, or any one or more of multi-period superlattice structure materials formed by any combination of AlN, AlGaN, AlInN, and AlInGaN. When the gate insertion layer (107) is a multi-period superlattice structure, the number of periods is 1 to 100, and the thickness of the gate insertion layer (107) is 50 nm to 500 nm.
5. The gallium nitride power device structure according to claim 1, Its characteristics are: The material of the protective layer (109) is SiO 2 、Si 3 N 4 、SiC、TiO 2 、Al 2 O 3 , phosphosilicate glass, and the thickness of the protective layer (109) is 500nm ~ 3000nm.
6. The gallium nitride power device structure according to claim 1, Its characteristics are: The gate insertion layer (107) is P-type doped, and the doping concentration is: 1×10 16 cm -3 ~ 5×10 21 cm -3 The doping concentration of the P-type GaN gate (108) is: 1×10 16 cm -3 ~ 5×10 21 cm -3 , thickness is 20 nm ~ 200 nm.
7. The gallium nitride power device structure according to claim 1, Its characteristics are: The material of the substrate (101) is any one of sapphire, silicon, silicon carbide, gallium nitride, aluminum nitride, boron nitride, gallium oxide, zinc oxide, and diamond; The material of the nucleation layer (102) is any one of GaN, AlN and InN, and has a thickness of 5 nm to 30 nm; The thickness of the first GaN epitaxial layer (103) is 500 nm to 3500 nm; The thickness of the second GaN epitaxial layer (105) is 800 nm to 3500 nm; The thickness of the AlGaN barrier layer (106) is 5 nm to 60 nm; The heat dissipation layer (110) is made of graphene material and has a thickness of 0.335 nm to 10 nm; The source metal (111), the gate metal (112), and the drain metal (113) are made of any one or more of titanium, aluminum, gold, nickel, silver, copper, and platinum.
8. The gallium nitride power device structure according to claim 1, Its characteristics are: The barrier layer is concave in an inverted triangular pyramid or a rectangular parallelepiped shape, and the gate insertion layer is convex in an inverted triangular pyramid or a rectangular parallelepiped shape.
9. The gallium nitride power device structure according to claim 1, Its characteristics are: The protective layer is concave in a hemispherical shape or an inverted tetrahedron shape, and the heat dissipation layer is convex in a hemispherical shape or an inverted tetrahedron shape.
10. A method for manufacturing a gallium nitride power device structure The following steps are involved: Step 1: growing a nucleation layer (102) on a substrate (101); Step 2: growing a first GaN epitaxial layer (103) on the nucleation layer (102); Step 3: growing an insertion layer (104) on the first GaN epitaxial layer (103); Step 4: growing a second GaN epitaxial layer (105) on the insertion layer (104); Step 5: growing an AlGaN barrier layer (106) on the second GaN epitaxial layer (105); Step 6: Make a mask on the upper surface of the AlGaN barrier layer (106), and selectively etch part of the epitaxial layer by wet or dry method to form a periodic or non-periodic barrier layer depression, and control the maximum depth of the barrier layer depression to be located above the upper surface of the second GaN epitaxial layer (105); Step 7: growing a gate insertion layer (107) directly above the corresponding barrier layer recessed region, and forming a gate insertion layer protrusion on the lower surface of the gate insertion layer (107) that matches the barrier layer recessed region; Step 8: growing a P-type GaN gate (108) on the gate insertion layer (107); Step nine, growing a protective layer (109) on the upper surface of the entire epitaxial layer; Step 10: etching the protective layer (109) located on both sides of the P-type GaN gate (108) to form periodic or non-periodic protective layer depressions, and controlling the maximum etching depth of the protective layer depressions to be located above the upper surface of the AlGaN barrier layer (106); Step 11: growing a heat dissipation layer (110) on the upper surface of the etched protection layer (109), and forming a heat dissipation layer protrusion on the lower surface of the heat dissipation layer (110) that matches the protection layer concave; Step 12: prepare a mask on the upper surface of the heat dissipation layer (110), and selectively perform photolithography to open windows corresponding to the source metal (111), the gate metal (112), and the drain metal (113); Step 13: prepare a mask on the upper surface of the heat dissipation layer (110), selectively perform photolithography, and etch the covering layer of part or all of the upper surface of the P-type GaN gate (108) until the upper surface of the P-type GaN gate (108) is exposed to form a recessed area, and then evaporate the gate metal (112) in the recessed area, and perform annealing on the electrode; Step 14: prepare a mask on the upper surface of the heat dissipation layer (110), selectively perform photolithography, and etch the epitaxial layer until the AlGaN barrier layer (106) is exposed to form a recessed area, then evaporate the source metal (111) in the recessed area, and perform annealing on the electrode; Step 15: prepare a mask on the upper surface of the heat dissipation layer (110), perform selective photolithography, and etch the epitaxial layer until the AlGaN barrier layer (106) is exposed to form a recessed area, then evaporate the drain metal (113) in the recessed area, and anneal the electrode.
Citation Information
Patent Citations
Semiconductor device
CN104409431A
Enhanced type HEMT (high electron mobility transistor) device based on AlGaN / GaN (aluminium gallium nitride / gallium nitride) heterojunction of Si (silicon) substrate and manufacturing method thereof
CN106711212A
An enhanced high electron mobility transistor HEMT and a preparation method thereof
CN108987474A
Gallium nitride power device with high reliability and preparation method thereof
CN111261714A
Gallium nitride power device structure
CN212257404U