JBS silicon carbide diode device structure and manufacturing method for enhancing reliability
By adopting a double-layer silicon carbide epitaxial structure with a barrier buffer layer and a multi-layer epitaxial layer design in JBS diode devices, the reliability problems caused by substrate defects and interface instability are solved, and higher device reliability is achieved and packaging resistance.
Patent Information
- Application Number
- CN202111052349.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-08
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2041-09-08
AI Technical Summary
Existing JBS diode devices are susceptible to substrate defects and interface instability, resulting in poor reliability, especially when reverse operation under high temperature conditions, leakage problems are prone to occur.
Using a double-layer silicon carbide epitaxial structure with a barrier buffer layer, combined with multi-layer epitaxial layer, N-type cutoff ring, P-type voltage divider ring, composite terminal passivation layer, etc., a multi-layer structure is formed through a deposition process to reduce lining Bottom defects and leakage currents improve device reliability.
It effectively reduces the leakage of the device edge, reduces forward conduction loss, improves the product yield and reliability, enhances the anti-packaging capability, and reduces the core breakage rate.
Smart Images

Figure CN113658922B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of JBS silicon carbide diode structure design, and in particular to a JBS silicon carbide diode device structure and a manufacturing method for enhancing reliability. Background Art
[0002] SiC (Silicon Carbide) is also called wide bandgap semiconductor material because of its bandgap width which is three times that of silicon atom, high breakdown field strength (0.8E16~3E16V / cm), which is 10 times that of Si, and high thermal conductivity (4.9W / cmK), which is about 3.2 times that of Si. In the industry, it is called third-generation semiconductor material, which can perform device performance normally under high temperature, high power and high frequency operating environment. Therefore, the third-generation semiconductor-SIC (Silicon Carbide) has become an ideal semiconductor material for making high temperature, high frequency, radiation-resistant and high-power power electronic devices due to its high bandgap width, high blocking voltage and high thermal conductivity.
[0003] At present, there are ordinary planar diodes and JBS diodes on the market. Ordinary planar diodes have been widely used in the field of low-voltage and high-current DC due to their low forward voltage drop, low power, and high switching speed. However, the low voltage drop and low power consumption of traditional planar diodes are based on low potential barriers. A lower potential barrier height will increase the reverse leakage current of the device and reduce the maximum operating temperature.
[0004] The difference between JBS diodes and ordinary planar diodes is that JBS integrates multiple comb-shaped P-type diffusion regions in the N-drift region of ordinary planar diodes. The current channel between adjacent P-type regions is designed to ensure that it is not pinched off when zero bias and forward bias, allowing the forward current to flow from the anode to the cathode of the device through the inter-gate current channel. In reverse bias, when the reverse bias voltage exceeds a certain voltage, the adjacent junction depletion regions overlap, causing the depletion layer to punch through. After the depletion layer punches through, a potential barrier will be formed in the channel, and the depletion layer will expand toward the N-substrate. Therefore, the barrier layer shields the influence of the applied voltage on the barrier, prevents the barrier from lowering, reduces reverse leakage, and improves the device withstand voltage.
[0005] The existing Chinese patent with publication number CN112289848A discloses a low-power, high-performance super junction JBS diode and its manufacturing method. A low-power, high-performance super junction JBS diode is manufactured using traditional silicon-based process technology, with low manufacturing cost; the large-area, high-concentration, deep junction characteristics of the P heavily doped columnar region and the N columnar drift region are used to reduce the forward on-resistance; a super junction is formed, and good reverse blocking characteristics are achieved by optimizing the electric field distribution; by optimizing the super junction parameters, a higher blocking withstand voltage can be achieved, and the on-state and off-state power consumption of the device can be reduced.
[0006] The inventors believe that the JBS diode in the prior art is easily affected by substrate defects and interface instability, resulting in poor reliability of the device. In addition, when the silicon carbide device works in reverse, especially under high temperature conditions, when the surface charge on the oxide layer is sufficient to cause a large leakage channel in the n-type semiconductor, large leakage is likely to occur at the edge of the device, and there is room for improvement. Summary of the invention
[0007] In view of the defects in the prior art, an object of the present invention is to provide a JBS silicon carbide diode device structure and a manufacturing method for enhancing reliability.
[0008] According to the present invention, a JBS silicon carbide diode device structure for enhancing reliability includes a silicon carbide substrate, a multi-layer epitaxial layer, a front electrode, a barrier layer, an N-type silicon atomic layer, a P-type diffusion region, a P-type voltage divider ring, an N-type cut-off ring, a composite terminal passivation layer, an ohmic contact layer, and a back electrode; the back electrode, the ohmic contact layer, and the silicon carbide substrate are stacked in sequence from bottom to top, the multi-layer epitaxial layer is arranged above the silicon carbide substrate, and the P-type diffusion region, the P-type voltage divider ring, and the N-type cut-off ring are all arranged at a position located at In the top epitaxial layer, the P-type diffusion region is arranged in the middle of the top epitaxial layer, the P-type voltage divider ring is arranged on the outside of the P-type diffusion region, and one or more groups of N-type cut-off rings are respectively arranged on the inner and outer sides of the P-type voltage divider ring; the barrier layer and the front electrode are stacked in sequence from bottom to top on the multi-layer epitaxial layer, the N-type silicon atomic layer is arranged in the barrier layer, the composite terminal passivation layer is arranged on the multi-layer epitaxial layer, and the composite terminal passivation layer semi-surrounds the front electrode and leaves the upper surface of the front electrode partially exposed.
[0009] Preferably, the composite terminal passivation layer comprises a silicon dioxide layer, a silicon nitride layer and a polyimide layer, and the silicon dioxide layer, the silicon nitride layer and the polyimide layer are sequentially stacked from bottom to top on the multi-layer epitaxial layer, and the silicon dioxide layer is located below the front electrode.
[0010] Preferably, both the silicon nitride layer and the polyimide layer cover the edge of the upper surface of the front electrode.
[0011] Preferably, the multi-layer epitaxial layer comprises an isolation buffer layer, a first epitaxial layer and a second epitaxial layer, and the isolation buffer layer, the first epitaxial layer and the second epitaxial layer are sequentially stacked from bottom to top on the silicon carbide substrate.
[0012] Preferably, the isolation buffer layer comprises an N-type silicon carbide conductive material with a thickness between 0.5um and 1.5um and a resistivity between 10 16 -10 17 between.
[0013] Preferably, both the first epitaxial layer and the second epitaxial layer include N-type silicon carbide conductive material; the thickness of the first epitaxial layer is between 0.5um and 5um, and the resistivity of the first epitaxial layer is between 10 16 -10 17 The thickness of the second epitaxial layer is between 2um and 50um, and the resistivity of the second epitaxial layer is between 10 15 -10 16 between.
[0014] According to a manufacturing method of a JBS silicon carbide diode device for enhancing reliability provided by the present invention, the manufacturing method comprises the following steps: S1, preparing the silicon carbide substrate, and growing an isolation buffer layer on the upper surface of the silicon carbide substrate; S2, depositing a plurality of epitaxial layers twice or multiple times on the upper surface of the isolation buffer layer; S3, depositing a silicon dioxide protective layer on the outer surface of the plurality of epitaxial layers located at the top layer, and then etching the N-type region window by a photoresist coating, exposure and development process, and then forming an N-type cutoff ring by multiple N ion implantations. ; S4, remove the silicon dioxide protective layer and dry it; S5, generate a silicon dioxide protective layer on the outer surface of the silicon carbide epitaxial layer located at the top layer by deposition, and then perform etching treatment by photoresist coating, exposure and development process to form a P-type voltage divider ring window and a P-type diffusion area window in the active area, and then form a P-type voltage divider ring and a P-type diffusion area by multiple P ion implantation; S6, remove the silicon dioxide protective layer and dry it; S7, deposit a carbon film by sputtering or coating PR glue, and then perform high-temperature annealing to activate it, and then remove the carbon film; S8, A silicon dioxide layer is grown on the epitaxial layer by thermal oxidation, S9, etching is performed on the silicon dioxide layer by a coating, exposure and development process of a photoresist to form an electrode window; S10, Si material is deposited on the multi-layer epitaxial layer by an atomic layer deposition process or a molecular beam epitaxy process to form an N-type silicon atomic layer; S11, etching is performed by a coating, exposure and development process of a photoresist so that the N-type silicon atomic layer covers the active area and avoids the P-type diffusion area; S12, metal is deposited at the electrode window to form the barrier layer; S13, metal or composite metal is deposited on the barrier layer, and The front electrode is formed by etching through the coating, exposure and development process of photoresist; S14, a silicon nitride layer and a polyimide layer are deposited in sequence on top of the silicon dioxide layer, and a part of the top area of the front electrode is exposed by etching through the coating, exposure and development process of photoresist; S15, the thickness of the silicon carbide substrate is reduced to 100um-300um by grinding; S16, metal nickel is deposited on the back side of the silicon carbide substrate to form the ohmic contact layer, and laser annealing is performed; S17, metal or composite metal is deposited on the back side of the ohmic contact layer to form a back electrode.
[0015] Preferably, for step S3, the N-type ions implanted are nitrogen ions, the implantation temperature is 300-700 degrees, and the implantation energy is 300-600kev.
[0016] Preferably, for step S5, the P-type ions implanted are Al ions or boron ions, the implantation temperature is 300-700 degrees, and the implantation energy is 30-800kev.
[0017] Preferably, for step S8, the thermal oxidation temperature is between 1300-2000 degrees, and the oxidation thickness is 10-1000 angstroms.
[0018] Compared with the prior art, the present invention has the following beneficial effects:
[0019] 1. The present invention reduces the extension of defects of the silicon carbide substrate into the silicon carbide epitaxy during homogeneous epitaxy through double-layer silicon carbide epitaxy with a blocking buffer layer, thereby reducing the defects of the silicon carbide substrate, thereby helping to improve the yield and reliability of the product; and through the N-type cut-off ring, the leakage current generated by the leakage channel can be effectively cut off, thereby helping to reduce the occurrence of large leakage at the edge of the device;
[0020] 2. The present invention deposits a thin layer of N-type silicon atomic layer on the surface of the second epitaxial layer, so that the N-type silicon atomic layer and the metal form a silicon-based barrier alloy layer, thereby avoiding the high barrier caused by the silicon carbide alloy layer, and can effectively reduce the barrier height during forward conduction, thereby greatly reducing the forward turn-on voltage VF of the JBS silicon carbide diode, reducing the turn-on loss of the diode and improving the system reliability;
[0021] 3. The present invention forms a multi-layer composite terminal passivation layer structure through a silicon dioxide layer, a silicon nitride layer and a polyimide layer, which helps to improve the overall protection effect of the terminal; and solves the problem of high stress between different films and the problem of mismatch in expansion coefficient with the metal layer material, reduces the internal stress between the films, improves the product's anti-packaging ability, reduces the core breakage rate during wafer processing and packaging, and enhances the reliability of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Other features, objects and advantages of the present invention will become more apparent from the detailed description of non-limiting embodiments made with reference to the following drawings:
[0023] Figure 1 The present invention mainly embodies the layer structure schematic diagram of the overall cross section of the JBS silicon carbide diode;
[0024] Figure 2 The present invention mainly embodies a flow chart of a method for manufacturing a JBS silicon carbide diode.
[0025] As shown in the figure:
[0026] DETAILED DESCRIPTION
[0027] The present invention is described in detail below in conjunction with specific embodiments. The following embodiments will help those skilled in the art to further understand the present invention, but are not intended to limit the present invention in any form. It should be noted that, for those of ordinary skill in the art, several changes and improvements can also be made without departing from the concept of the present invention. These all belong to the protection scope of the present invention.
[0028] like Figure 1 As shown, a JBS silicon carbide diode device structure for enhancing reliability provided according to the present invention includes a silicon carbide substrate 1, a multi-layer epitaxial layer 98, a front electrode 70, a barrier layer 40, an N-type silicon atomic layer 90, a P-type diffusion region 10, a P-type voltage divider ring 20, an N-type cut-off ring 30, a composite terminal passivation layer 99, an ohmic contact layer 100 and a back electrode 110.
[0029] like Figure 1 As shown, the back electrode 110, the ohmic contact layer 100 and the silicon carbide substrate 1 are stacked in sequence from bottom to top. The silicon carbide substrate 1 is a layer structure made of an N-type conductive material, and the thickness of the silicon carbide substrate 1 is 200-400um, preferably 200um. The ohmic contact layer 100 is formed by depositing metal nickel on the back of the silicon carbide substrate 1, and the thickness of the ohmic contact layer 100 is between 50nm and 1000nm, preferably 1000nm. The back electrode 110 is formed by depositing a metal or a composite metal on the back of the ohmic contact layer 100, and the back electrode 110 includes but is not limited to a titanium metal layer, a nickel metal layer, a silver metal layer, and an alloy layer composed of a continuous multi-layer metal combination, and the thickness of the back electrode 110 is between 1-10um, preferably 5um.
[0030] like Figure 1 As shown, the multi-layer epitaxial layer 98 includes an isolation buffer layer 11, a first epitaxial layer 12 and a second epitaxial layer 13. The isolation buffer layer 11 is grown on the upper surface of the silicon carbide substrate 1. The isolation buffer layer 11 is an N-type silicon carbide conductive material layer. The thickness of the isolation buffer layer 11 is between 0.5um and 1.5um, preferably 1um; the resistivity is between 10 16 -10 17 The first epitaxial layer 12 and the second epitaxial layer 13 are sequentially grown from bottom to top on the upper surface of the isolation buffer layer 11, and both the first epitaxial layer 12 and the second epitaxial layer 13 are made of N-type silicon carbide conductive material.
[0031] The thickness of the first epitaxial layer 12 is between 0.5um and 5um, preferably 5um, and the resistivity of the first epitaxial layer 12 is between 10 16 -10 17The thickness of the second epitaxial layer 13 is between 2um and 50um, preferably 20um, and the resistivity of the second epitaxial layer 13 is between 10 15 -10 16 The use of the multilayer epitaxial layer 98 with the isolation buffer layer 11, the first epitaxial layer 12 and the second epitaxial layer 13 can reduce the defects of the silicon carbide substrate 1 extending into the silicon carbide epitaxial layer during homoepitaxial growth, thereby reducing the defects of the silicon carbide substrate 1 and improving the yield and reliability of the product.
[0032] The P-type diffusion region 10, the P-type voltage divider ring 20 and the N-type cut-off ring 30 are all installed on the upper side of the second epitaxial layer 13. Six groups of P-type diffusion regions 10 are symmetrically embedded and installed at equal intervals in the middle of the second epitaxial layer 13. Five P-type voltage divider rings 20 are installed concentrically in the second epitaxial layer 13 by ion implantation, and the five P-type voltage divider rings 20 are all located on the outside of the P-type diffusion region 10. Two N-type cut-off rings 30 are embedded and installed on the second epitaxial layer 13 by ion implantation. The two N-type cut-offs are respectively located on the inside and outside of the five P-type voltage divider rings 20, and the two N-type cut-off rings 30 are concentric with the five P-type voltage divider rings 20. The N-type cut-off ring 30 on the outermost side of the second epitaxial layer 13 can act as a leakage channel cut-off at the edge of the oxide layer outside the depletion layer, can effectively cut off the leakage current generated by the leakage channel, and can effectively reduce the damage of the P-type voltage divider ring 20 caused by various situations.
[0033] The barrier layer 40 is a Schottky barrier layer, which is grown by deposition in the middle of the top wall of the second epitaxial layer 13. The barrier layer 40 includes but is not limited to a titanium layer, a nickel layer, a molybdenum layer, a platinum layer, a chromium layer and an alloy layer. The front electrode 70 is grown by deposition on the Schottky barrier layer 40. The front electrode 70 includes but is not limited to a titanium layer, a nickel layer, a molybdenum layer, a platinum layer, a chromium layer and an alloy layer. The thickness of the front electrode 70 is between 1-10um, preferably 5um. The thickness of the N-type silicon atomic layer 90 is within 50-300nm, and the resistivity is 10 17 -10 18 Seven N-type silicon atomic layers 90 are embedded and installed in the barrier layer 40 , and the seven N-type silicon atomic layers 90 are all in contact with the second epitaxial layer 13 , and the seven N-type silicon atomic layers 90 are all away from the P-type diffusion region 10 .
[0034] By depositing a thin N-type silicon atomic layer 90 on the surface of the second epitaxial layer 13, the N-type silicon atomic layer 90 and the metal form a silicon-based barrier alloy layer, thereby avoiding the high barrier caused by the silicon carbide alloy layer, and effectively reducing the barrier height during forward conduction, thereby greatly reducing the forward turn-on voltage VF of the JBS silicon carbide diode, reducing the turn-on loss of the diode and improving the system reliability.
[0035] The composite terminal passivation layer 99 includes a silicon dioxide layer 50, a silicon nitride layer 60 and a polyimide layer 80, which are stacked on the upper surface of the second epitaxial layer 13 from bottom to top, and the composite terminal passivation layer 99 half surrounds the front electrode 70 and partially exposes the upper surface of the front electrode 70. The thickness of the silicon dioxide layer 50 is between 10-1000 angstroms, preferably 1000 angstroms. Both the silicon nitride layer 60 and the polyimide layer 80 cover the edge portion of the front electrode 70, and the thickness of the silicon nitride layer 60 is between 1000-10000 angstroms, preferably 5000 angstroms; the thickness of the polyimide layer 80 is between 1um-5um, preferably 3um.
[0036] The composite terminal passivation layer 99 composed of a silicon dioxide layer 50, a silicon nitride layer 60 and a polyimide layer 80 surrounds the front electrode 70, thereby improving the overall protection of the terminal, solving the problem of high stress between different thin film layers and the problem of mismatch in expansion coefficient with the metal layer material, reducing the internal stress between the thin film layers, improving the product's anti-packaging ability, reducing the core breakage rate during wafer processing and packaging, and enhancing the reliability of the device.
[0037] like Figure 2 As shown, a manufacturing method of a JBS silicon carbide diode device for enhancing reliability provided by the present invention includes the above-mentioned JBS silicon carbide diode device structure for enhancing reliability, and the manufacturing method includes the following steps:
[0038] S1 . Generating an isolation buffer layer 11 : preparing a silicon carbide substrate 1 , and growing an isolation buffer layer 11 on the upper surface of the silicon carbide substrate 1 . The thickness of the isolation buffer layer 11 is 1 um.
[0039] S2, generating a silicon carbide epitaxial layer: depositing a first epitaxial layer 12 and a second epitaxial layer 13 twice on the upper surface of the isolation buffer layer 11; the thickness of the first epitaxial layer 12 is 5 um, and the thickness of the second epitaxial layer 13 is 20 um.
[0040] S3, forming an N-type cut-off ring 30: a silicon dioxide protective layer is deposited on the outer surface of the second epitaxial layer 13, and the thickness of the silicon dioxide protective layer is between 1-2um. Then, an N-type region window is formed by etching through a photoresist coating, exposure and development process, and then an N-type cut-off ring 30 is formed by multiple N-ion implantations; the N-type ion implantation is nitrogen ion, the implantation temperature is 300-700 degrees, and the implantation energy is 300-600kev.
[0041] S4. Removing the silicon dioxide protective layer: removing the silicon dioxide protective layer and drying it. After removing the silicon dioxide protective layer, it can be cleaned with a cleaning solution, and repeatedly cleaned with deionized water, dried with nitrogen, and dried.
[0042] S5, forming a P-type voltage divider ring 20 and a P-type diffusion region 10: a silicon dioxide protective layer is deposited on the outer surface of the second epitaxial layer 13, and the thickness of the silicon dioxide protective layer is between 1-2um. Then, etching is performed through the coating, exposure and development process of the photoresist to form a P-type voltage divider ring window and a P-type diffusion region 10 window in the active area, and then multiple P ion implantations are performed to form a P-type voltage divider ring 20 and a P-type diffusion region 10; the P-type ion implantation is Al ions or boron ions, the implantation temperature is 300-700 degrees, and the implantation energy is 30-800kev.
[0043] S6. Removing the silicon dioxide protective layer: removing the silicon dioxide protective layer and drying it. After removing the silicon dioxide protective layer, it can be cleaned with a cleaning solution, and repeatedly cleaned with deionized water, blown dry with nitrogen, and dried.
[0044] S7, high temperature annealing activation: deposit a carbon film by sputtering or coating PR glue, the thickness of the carbon film is 10-500nm, and then perform high temperature annealing activation, the temperature of high temperature annealing activation is between 1300-2000 degrees, and use inert gas as protective gas, and then remove the carbon film;
[0045] S8. Growth of silicon dioxide layer 50: thermal oxidation growth of silicon dioxide layer 50 is performed on the uppermost silicon carbide epitaxial layer, the thermal oxidation temperature is between 1300-2000 degrees, and the oxidation thickness is 10-1000 angstroms.
[0046] S9, forming an electrode window: etching the silicon dioxide layer 50 through a photoresist coating, exposure and development process to form an electrode window.
[0047] S10 , forming an N-type silicon atomic layer 90 : depositing Si material on the multi-layer epitaxial layer 98 by using an atomic layer deposition process or a molecular beam epitaxy process to form an N-type silicon atomic layer 90 .
[0048] S11 , etching is performed through a photoresist coating, exposure and development process, so that the N-type silicon atomic layer 90 covers the active area and avoids the P-type diffusion area 10 .
[0049] S12, growing a barrier layer 40: depositing metal at the electrode window to form a barrier layer 40, the alloy temperature of the deposited metal and the N-type silicon atomic layer 90 is 500-600 degrees.
[0050] S13, growing the front electrode 70: depositing metal or composite metal on the Schottky barrier layer 40, and etching to form the front electrode 70 through a photoresist coating, exposure and development process; the thickness of the front electrode 70 is between 1-10 um.
[0051] S14, growing a silicon nitride layer 60 and a polyimide layer 80: depositing a silicon nitride layer 60 and a polyimide layer 80 in sequence on the silicon dioxide layer 50, and performing etching through a photoresist coating, exposure and development process to expose a portion of the top area of the front electrode 70; the thickness of the silicon nitride layer 60 is between 1000-10000 angstroms, and the thickness of the polyimide layer 80 is between 1um-5um.
[0052] S15, grinding the silicon carbide substrate 1: reducing the thickness of the silicon carbide substrate 1 to 100 um-300 um by grinding.
[0053] S16, forming an ohmic contact layer 100: depositing metal nickel on the back side of the silicon carbide substrate 1 to form the ohmic contact layer 100, wherein the thickness of the ohmic contact layer 100 is between 50 nm and 1000 nm, and laser annealing is performed.
[0054] S17, forming a back electrode 110: depositing metal or composite metal on the back side of the ohmic contact layer 100 to form a back electrode 110, the thickness of the back electrode 110 is between 1-10 um.
[0055] How it works
[0056] During work, the staff sequentially produces a double-layer silicon carbide epitaxial layer with an isolation buffer layer 11 by generating an isolation buffer layer 11, a first epitaxial layer 12, a second epitaxial layer 13, forming an N-type cutoff ring 30, removing a silicon dioxide protective layer, forming a P-type protection ring and a P-type diffusion region 10, removing a silicon dioxide protective layer, high-temperature annealing activation, growing a silicon dioxide layer 50, forming an electrode window, forming an N-type silicon atomic layer 90, etching, growing a barrier layer 40, growing a front electrode 70, growing a silicon nitride layer 60 and a polyimide layer 80, grinding a silicon carbide substrate 1, forming an ohmic contact layer 100, and forming a back electrode 110. The N-type cutoff ring 30 is arranged in the second epitaxial layer 13, thereby reducing the defects of the silicon carbide substrate 1, improving the yield and reliability of the product, and can effectively cut off the leakage current generated by the leakage channel, and can effectively prevent the damage of the P-type voltage divider ring 20 caused by various situations.
[0057] In the description of the present application, it should be understood that the terms "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0058] The above describes the specific embodiments of the present invention. It should be understood that the present invention is not limited to the above specific embodiments, and those skilled in the art can make various changes or modifications within the scope of the claims, which does not affect the essence of the present invention. In the absence of conflict, the embodiments of the present application and the features in the embodiments can be combined with each other arbitrarily.
Claims
1. A JBS silicon carbide diode device structure for enhancing reliability, characterized in that: It comprises a silicon carbide substrate (1), a multi-layer epitaxial layer (98), a front electrode (70), a barrier layer (40), an N-type silicon atomic layer (90), a P-type diffusion region (10), a P-type voltage divider ring (20), an N-type cut-off ring (30), a composite terminal passivation layer (99), an ohmic contact layer (100) and a back electrode (110); The back electrode (110), the ohmic contact layer (100) and the silicon carbide substrate (1) are stacked in sequence from bottom to top; the multiple epitaxial layers (98) are arranged above the silicon carbide substrate (1); the P-type diffusion region (10), the P-type voltage divider ring (20) and the N-type cut-off ring (30) are all arranged in the epitaxial layer located at the top layer; the P-type diffusion region (10) is arranged in the middle of the epitaxial layer located at the top layer; the P-type voltage divider ring (20) is arranged outside the P-type diffusion region (10); The N-type cut-off ring (30) is provided with one or more groups on both sides of the inner and outer sides of the P-type voltage divider ring (20); the barrier layer (40) and the front electrode (70) are stacked in sequence from bottom to top on the multi-layer epitaxial layer (98); the N-type silicon atomic layer (90) is provided in the barrier layer (40); the composite terminal passivation layer (99) is provided on the multi-layer epitaxial layer (98); and the composite terminal passivation layer (99) semi-encloses the front electrode (70) and partially exposes the upper surface of the front electrode (70).
2. The JBS silicon carbide diode device structure for enhancing reliability according to claim 1, characterized in that: The composite terminal passivation layer (99) comprises a silicon dioxide layer (50), a silicon nitride layer (60) and a polyimide layer (80), wherein the silicon dioxide layer (50), the silicon nitride layer (60) and the polyimide layer (80) are sequentially stacked from bottom to top on the multi-layer epitaxial layer (98), and the silicon dioxide layer (50) is located below the front electrode (70).
3. The JBS silicon carbide diode device structure for enhancing reliability according to claim 2, characterized in that: Both the silicon nitride layer (60) and the polyimide layer (80) cover the edge of the upper surface of the front electrode (70).
4. The JBS silicon carbide diode device structure for enhancing reliability according to claim 1, characterized in that: The multi-layer epitaxial layer (98) comprises an isolation buffer layer (11), a first epitaxial layer (12) and a second epitaxial layer (13), wherein the isolation buffer layer (11), the first epitaxial layer (12) and the second epitaxial layer (13) are stacked in sequence from bottom to top on the silicon carbide substrate (1).
5. The JBS silicon carbide diode device structure for enhancing reliability according to claim 4, characterized in that: The isolation buffer layer (11) comprises an N-type silicon carbide conductive material with a thickness between 0.5 um and 1.5 um and a resistivity between 10 16 -10 17 between.
6. The JBS silicon carbide diode device structure for enhancing reliability according to claim 4, characterized in that: Both the first epitaxial layer (12) and the second epitaxial layer (13) comprise N-type silicon carbide conductive material; The thickness of the first epitaxial layer (12) is between 0.5um and 5um, and the resistivity of the first epitaxial layer (12) is between 10 16 -10 17 between; The thickness of the second epitaxial layer (13) is between 2um and 50um, and the resistivity of the second epitaxial layer (13) is between 10 15 -10 16 between.
7. A method for manufacturing a JBS silicon carbide diode device for enhancing reliability, characterized in that: A JBS silicon carbide diode device structure for enhancing reliability comprising any one of claims 1 to 6, wherein the manufacturing method comprises the following steps: S1, preparing the silicon carbide substrate (1), and growing an isolation buffer layer (11) on the upper surface of the silicon carbide substrate (1); S2, depositing a multi-layer epitaxial layer (98) on the upper surface of the isolation buffer layer (11) twice or more times; S3, forming a silicon dioxide protective layer on the outer surface of the multi-layer epitaxial layer (98) located at the top by deposition, then etching it through a photoresist coating, exposure and development process to form an N-type region window, and then forming an N-type cut-off ring (30) by multiple N ion implantations; S4, removing the silicon dioxide protective layer and drying; S5, forming a silicon dioxide protective layer by deposition on the outer surface of the multi-layer epitaxial layer (98) located at the top layer, and then etching by a photoresist coating, exposure and development process to form a P-type voltage dividing ring window and a P-type diffusion region (10) window in the active region, and then forming a P-type voltage dividing ring (20) and a P-type diffusion region (10) by multiple P ion implantation; S6, removing the silicon dioxide protective layer and drying; S7, depositing a carbon film by sputtering or coating a PR glue, then performing high temperature annealing to activate it, and then removing the carbon film; S8, performing thermal oxygen growth of a silicon dioxide layer (50) on the uppermost silicon carbide epitaxial layer, S9, etching the silicon dioxide layer (50) by a photoresist coating, exposure and development process to form an electrode window; S10, depositing Si material on the multi-layer epitaxial layer (98) by using an atomic layer deposition process or a molecular beam epitaxy process to form an N-type silicon atomic layer (90); S11, performing etching through a photoresist coating, exposure and development process, so that the N-type silicon atomic layer (90) covers the active area and avoids the P-type diffusion area (10); S12, depositing metal at the electrode window to form the barrier layer (40); S13, depositing a metal or a composite metal on the barrier layer (40), and etching through a photoresist coating, exposure and development process to form the front electrode (70); S14, depositing a silicon nitride layer (60) and a polyimide layer (80) in sequence on the silicon dioxide layer (50), and performing etching through a photoresist coating, exposure and development process to expose a portion of the top of the front electrode (70); S15, reducing the thickness of the silicon carbide substrate (1) to 100 um-300 um by grinding; S16, depositing metal nickel on the back side of the silicon carbide substrate (1) to form the ohmic contact layer (100), and performing laser annealing; S17, depositing metal or composite metal on the back side of the ohmic contact layer (100) to form a back side electrode (110).
8. The method for manufacturing a JBS silicon carbide diode device for enhancing reliability according to claim 7, characterized in that: For step S3, the N-type ions implanted are nitrogen ions, the implantation temperature is 300-700 degrees, and the implantation energy is 300-600kev.
9. The method for manufacturing a JBS silicon carbide diode device for enhancing reliability according to claim 7, characterized in that: For step S5, the P-type ion implantation is Al ion or boron ion, the implantation temperature is 300-700 degrees, and the implantation energy is 30-800kev.
10. The method for manufacturing a JBS silicon carbide diode device for enhancing reliability according to claim 7, characterized in that: For step S8, the thermal oxidation temperature is between 1300-2000 degrees, and the oxidation thickness is 10-1000 angstroms.
Citation Information
Patent Citations
Low-power-consumption high-performance super-junction JBS diode and manufacturing method thereof
CN112289848A
JBS silicon carbide diode device structure for enhancing reliability
CN216528860U