Method for manufacturing flash memory

By using hard mask layers and self-alignment technology in flash memory manufacturing to form word line polysilicon gates, the problem of high process costs caused by multiple photomask layers in existing flash memory manufacturing is solved and a more efficient manufacturing process is achieved.

CN113782437BActive Publication Date: 2024-10-29SHANGHAI HUALI INTEGRATED CIRCUIT CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202110928065.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-08-12
Publication Date
2024-10-29
Estimated Expiration
2041-08-12

AI Technical Summary

Technical Problem

In the existing flash memory manufacturing method, there are many layers of masks used to form the word line polysilicon gate, resulting in high process costs.

Method used

By forming a first gate dielectric layer and a polysilicon layer on a semiconductor substrate, using a hard mask layer for photolithography definition, self-aligning to form source line openings and word line polysilicon gates, reducing mask levels, and erasing the gate After formation, the second side surface is further etched to achieve self-alignment to form a word line polysilicon gate.

Benefits of technology

The mask level is reduced, the process cost is reduced, and the manufacturing efficiency is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113782437B_ABST
    Figure CN113782437B_ABST
Patent Text Reader

Abstract

The present invention discloses a method for manufacturing a flash memory, comprising: step 1, forming a first gate dielectric layer and a first polysilicon layer; step 2, forming a hard mask layer; step 3, photolithographically defining a source line forming region and performing a first etching to form a source line opening, and forming a first side surface of a word line polysilicon gate in the first etching; step 4, forming a source region; step 5, forming a first inter-gate dielectric layer and a floating gate on the side surface of the source line opening; step 6, forming a second inter-gate dielectric layer and a control gate in the source line opening; step 7, forming a third inter-gate dielectric layer and a conductive material layer of an erase gate, performing photolithographic definition and etching to form an erase gate; step 8, removing the hard mask layer to form a first sidewall; step 9, using the first sidewall as a self-alignment condition, performing a second etching on the first polysilicon layer and the first gate dielectric layer to form a second side surface of the word line polysilicon gate. The present invention can self-align to form a word line polysilicon gate, can reduce the mask level and can reduce the process cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for manufacturing a semiconductor integrated circuit, and in particular to a method for manufacturing a flash memory. Background Art

[0002] like Figure 1 FIG. 1 is a schematic diagram of the structure of an existing 38 super flash memory (SF); the existing 38 super flash memory includes:

[0003] A first gate dielectric layer (not shown) and a word line (WL) polysilicon gate 102 are formed on the semiconductor substrate 101 .

[0004] The floating gate (FG) 104 is composed of a TiN layer. An inter-gate dielectric layer 103 is provided to separate the floating gate 104 from the word line polysilicon gate 102 .

[0005] A control gate (CG) 106 is formed above the source region 109 , and the control gate 106 also serves as a source line (SL).

[0006] An inter-gate dielectric layer 105 is provided between the control gate 106 and the floating gate 104 .

[0007] The erase gate 108 covers the top of the control gate 106 and the floating gate 104 , and an inter-gate dielectric layer 107 is provided between the erase gate 108 and the bottom control gate 106 and the floating gate 104 .

[0008] A lightly doped drain region 110 a and a drain region 110 are also formed in the semiconductor substrate 101 on the side of the word line polysilicon gate 102 in a self-aligned manner.

[0009] Compared with the third generation SF structure in the industry, 38SF uses horizontal electric field write operation and cutting-edge TiN no voltage coupling erase operation, which greatly improves erase efficiency and reduces operating voltage. This structure increases the nesting window of EG to FG and better cutting-edge control, and has better endurance performance. Summary of the invention

[0010] The technical problem to be solved by the present invention is to provide a method for manufacturing a flash memory, which can form a word line polysilicon gate by self-alignment, reduce the number of mask layers and thus reduce the process cost.

[0011] In order to solve the above technical problems, the present invention provides a method for manufacturing a flash memory, comprising the following steps:

[0012] Step 1: forming a first gate dielectric layer and a first polysilicon layer on a semiconductor substrate.

[0013] Step 2: forming a hard mask layer on top of the first polysilicon layer.

[0014] Step three, photolithography defines the source line formation area, and according to the photolithography definition, the hard mask layer, the first polysilicon layer and the first gate dielectric layer are sequentially etched for the first time to form a source line opening, and the bottom of the source line opening exposes the surface of the semiconductor substrate; the side of the first polysilicon layer formed by the first etching is the first side of the word line polysilicon gate.

[0015] Step 4: forming a source region in the semiconductor substrate at the bottom of the source line opening.

[0016] Step 5: forming a first inter-gate dielectric layer and a floating gate composed of a TiN layer on the side of the source line opening; the first inter-gate dielectric layer realizes isolation between the floating gate and the word line polysilicon gate, and the first inter-gate dielectric layer is also located on the surface of the semiconductor substrate at the bottom of the floating gate to realize isolation between the floating gate and the source region.

[0017] Step six: forming a second inter-gate dielectric layer and a control gate composed of a conductive material layer in the source line opening formed with the first inter-gate dielectric layer and the floating gate; the second inter-gate dielectric layer realizes isolation between the control gate and the floating gate.

[0018] Step seven, forming a third inter-gate dielectric layer and a conductive material layer of an erase gate, photolithographically defining a formation area of ​​the erase gate and etching the third inter-gate dielectric layer and the conductive material layer of the erase gate to form the erase gate; the erase gate is located on top of the floating gate and the control gate and the coverage area of ​​the erase gate is larger than the formation area of ​​the source line opening.

[0019] Step eight: remove the hard mask layer to form a first sidewall spacer, wherein the first sidewall spacer is formed on a side surface of the erase gate and a side surface of the first inter-gate dielectric layer at the bottom of the erase gate.

[0020] Step nine: performing a second etching on the first polysilicon layer and the first gate dielectric layer with the first sidewall as a self-alignment condition, wherein the side surface of the first polysilicon layer formed by the second etching serves as the second side surface of the word line polysilicon gate.

[0021] A further improvement is that the semiconductor substrate comprises a silicon substrate.

[0022] A further improvement is that the first gate dielectric layer includes an oxide layer.

[0023] A further improvement is that the hard mask layer is formed by stacking a first nitride layer and a second oxide layer.

[0024] A further improvement is that the first etching in step 3 includes the following sub-steps:

[0025] The hard mask layer is etched sequentially according to the photolithography definition.

[0026] A second sidewall spacer is formed on the side of the hard mask layer.

[0027] The first polysilicon layer and the first gate dielectric layer are etched under the self-alignment condition of the second sidewall to form the source line opening.

[0028] A further improvement is that, in the first etching, after the etching of the first gate dielectric layer is completed, a step of over-etching the semiconductor substrate is also included.

[0029] A further improvement is that, before the over-etching of the first etching, a step of forming a third sidewall is included on the side of the second sidewall and the first side of the word line polysilicon gate, and then the over-etching of the first etching is performed with the third sidewall as a self-alignment condition.

[0030] A further improvement is that the top surface of the floating gate is higher than the top surface of the control gate, and the floating gate forms a tip structure above the top surface of the control gate.

[0031] A further improvement is that the conductive material layer of the control gate is made of tungsten.

[0032] A further improvement is that a plurality of unit structures of the flash memory are formed on the semiconductor substrate, and one source region is shared by two adjacent unit structures.

[0033] A further improvement is that step nine also includes:

[0034] The second side surface of the word line polysilicon gate is used as a self-alignment condition to perform N+ implantation to form a drain region.

[0035] A further improvement is that the flash memory is 38 super flash memory.

[0036] A further improvement is that the material of the first spacer includes an oxide layer.

[0037] A further improvement is that the material of the second spacer includes an oxide layer.

[0038] A further improvement is that the material of the third spacer includes an oxide layer.

[0039] A further improvement is that the material of the first inter-gate dielectric layer includes an oxide layer;

[0040] The material of the second inter-gate dielectric layer includes an oxide layer;

[0041] The material of the third inter-gate dielectric layer includes an oxide layer.

[0042] In the present invention, the first side of the word line polysilicon gate is formed by self-alignment of a mask with a source line opening, and there is no need to use a mask to define the first side of the word line polysilicon gate separately. The second side of the word line polysilicon gate is defined by self-alignment of the first side wall formed on the side of the erase gate after the erase gate is formed. Therefore, the present invention can form the word line polysilicon gate by self-alignment, reduce the mask level and thus reduce the process cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] The present invention is further described in detail below with reference to the accompanying drawings and specific embodiments:

[0044] Figure 1 It is a schematic diagram of the structure of the existing 38 super flash memory;

[0045] Figure 2 is a flow chart of a method for manufacturing a flash memory according to an embodiment of the present invention;

[0046] Figure 3A-Figure 3F It is a schematic diagram of the device structure in each step of the flash memory manufacturing method according to an embodiment of the present invention. DETAILED DESCRIPTION

[0047] like Figure 2 FIG. 1 is a flow chart of a method for manufacturing a flash memory according to an embodiment of the present invention; FIG. 3A to FIG. 3F FIG. 1 is a schematic diagram of the device structure in each step of the method for manufacturing a flash memory according to an embodiment of the present invention; the flash memory according to the embodiment of the present invention is a 38 super flash memory, and the method for manufacturing a flash memory according to the embodiment of the present invention includes the following steps:

[0048] Step 1: Figure 3A As shown, a first gate dielectric layer (not shown) and a first polysilicon layer 202 are formed on a semiconductor substrate 201 .

[0049] In the embodiment of the present invention, the semiconductor substrate 201 includes a silicon substrate.

[0050] The first gate dielectric layer includes an oxide layer.

[0051] Step 2: Figure 3A As shown, a hard mask layer is formed on top of the first polysilicon layer 202 .

[0052] In the embodiment of the present invention, the hard mask layer is formed by stacking a first nitride layer 203 and a second oxide layer 204 .

[0053] Step three, photolithography defines the source line formation area, and according to the photolithography definition, the hard mask layer, the first polysilicon layer 202 and the first gate dielectric layer are etched for the first time in sequence to form a source line opening, and the bottom of the source line opening exposes the surface of the semiconductor substrate 201; the side of the first polysilicon layer 202 formed by the first etching is the first side of the word line polysilicon gate 202a.

[0054] In the embodiment of the present invention, the first etching comprises the following steps:

[0055] The hard mask layer is etched sequentially according to the photolithography definition.

[0056] A second spacer 205 is formed on the side of the hard mask layer.

[0057] The first polysilicon layer 202 and the first gate dielectric layer are etched under the self-alignment condition of the second sidewall 205 to form the source line opening.

[0058] Before the over-etching of the first etching, a step of forming a third sidewall 206 on the side of the second sidewall 205 and the first side of the word line polysilicon gate 202a is also included, and then the over-etching of the first etching is performed with the third sidewall 206 as a self-alignment condition.

[0059] In the first etching, after the etching of the first gate dielectric layer is completed, a step of over-etching the semiconductor substrate 201 is also included.

[0060] The material of the second sidewall spacer 205 is an oxide layer. The material of the third sidewall spacer 206 is an oxide layer. Figure 3A In the embodiment, the second sidewall spacer 205, the third sidewall spacer 206 and the second oxide layer 204 are an integral structure.

[0061] Step 4: Figure 3B As shown, a source region 207 is formed in the semiconductor substrate 201 at the bottom of the source line opening.

[0062] In the embodiment of the present invention, a plurality of unit structures of the flash memory are formed on the semiconductor substrate 201 , and one source region 207 is shared by two adjacent unit structures.

[0063] Step 5: Figure 3BAs shown, a first inter-gate dielectric layer 208 and a floating gate 209 composed of a TiN layer are formed on the side of the source line opening; the first inter-gate dielectric layer 208 realizes isolation between the floating gate 209 and the word line polysilicon gate 202a, and the first inter-gate dielectric layer 208 is also located on the surface of the semiconductor substrate 201 at the bottom of the floating gate 209 to realize isolation between the floating gate 209 and the source region 207.

[0064] In the embodiment of the present invention, the material of the first inter-gate dielectric layer 208 is an oxide layer, and the second sidewall spacer 205 and the third sidewall spacer 206 , which are also oxide layers, and the first inter-gate dielectric layer 208 are in an integrated structure.

[0065] Step 6: Figure 3B As shown, a second inter-gate dielectric layer 210 and a control gate 211 composed of a conductive material layer are formed in the source line opening formed with the first inter-gate dielectric layer 208 and the floating gate 209 ; the second inter-gate dielectric layer 210 realizes isolation between the control gate 211 and the floating gate 209 .

[0066] In the embodiment of the present invention, the top surface of the floating gate 209 is higher than the top surface of the control gate 211 , and the floating gate 209 forms a tip structure above the top surface of the control gate 211 .

[0067] The conductive material layer of the control gate 211 is made of tungsten.

[0068] The material of the second inter-gate dielectric layer 210 includes an oxide layer.

[0069] Step 7: Figure 3B As shown, a third inter-gate dielectric layer 212 and a conductive material layer of an erase gate 213 are formed, the formation area of ​​the erase gate 213 is defined by photolithography, and the third inter-gate dielectric layer 212 and the conductive material layer of the erase gate 213 are etched to form the erase gate 213; the erase gate 213 is located on top of the floating gate 209 and the control gate 211 and the coverage area of ​​the erase gate 213 is larger than the formation area of ​​the source line opening.

[0070] In the embodiment of the present invention, the material of the third inter-gate dielectric layer 212 includes an oxide layer.

[0071] A top oxide layer 214 is also formed on the top of the conductive material layer of the erase gate 213. The photolithography process forms a pattern structure of the photoresist 215. When etching is performed, the top oxide layer 214 is etched first, and then the conductive material layer of the erase gate 213 at the bottom is etched. The second oxide layer 204 of the hard mask layer will be basically removed.

[0072] Step 8: Figure 3CAs shown, the hard mask layer is removed. Since the second oxide layer 204 has been substantially removed, the first nitride layer 203 is mainly removed at this time. Thereafter, the photoresist 215 is removed.

[0073] like Figure 3D As shown, a first spacer 216 is formed. The first spacer 216 is formed on the side of the erase gate 213 and the side of the first inter-gate dielectric layer 208 at the bottom of the erase gate 213 .

[0074] The material of the first spacer 216 includes an oxide layer.

[0075] Step 9: Figure 3E As shown, the first polysilicon layer 202 and the first gate dielectric layer are etched for the second time with the first sidewall 216 as a self-alignment condition, and the side surface of the first polysilicon layer 202 formed by the second etching is the second side surface of the word line polysilicon gate 202a.

[0076] Step 9 and beyond also include:

[0077] The second side of the word line polysilicon gate 202a is used as a self-aligned condition to perform N+ implantation to form a drain region 219. Generally, before forming the drain region 219, a step of forming a lightly doped drain region (LDD) 218 ​​is also included.

[0078] In the embodiment of the present invention, the first side of the word line polysilicon gate 202a is formed by self-alignment of a mask with a source line opening, and there is no need to use a separate mask to define the first side of the word line polysilicon gate 202a. The second side of the word line polysilicon gate 202a is self-aligned and defined by the first side wall 216 formed on the side of the erase gate 213 after the erase gate 213 is formed. Therefore, the embodiment of the present invention can form the word line polysilicon gate 202a by self-alignment, which can reduce the number of mask layers and thus reduce the process cost.

[0079] The present invention has been described in detail above through specific embodiments, but these do not constitute limitations of the present invention. Without departing from the principle of the present invention, those skilled in the art may also make many variations and improvements, which should also be considered as the protection scope of the present invention.

Claims

1. A method for manufacturing a flash memory, characterized in that: The steps include: Step 1: forming a first gate dielectric layer and a first polysilicon layer on a semiconductor substrate; Step 2: forming a hard mask layer on top of the first polysilicon layer; Step 3: photolithography defines a source line formation area, and according to the photolithography definition, the hard mask layer, the first polysilicon layer and the first gate dielectric layer are sequentially etched for the first time to form a source line opening, wherein the bottom of the source line opening exposes the surface of the semiconductor substrate; the side surface of the first polysilicon layer formed by the first etching is the first side surface of the word line polysilicon gate; The first etching of step 3 includes the following sub-steps: etching the hard mask layer in sequence according to the photolithography definition; forming a second sidewall spacer on the side of the hard mask layer; Etching the first polysilicon layer and the first gate dielectric layer under the condition of self-alignment of the second sidewall to form the source line opening; Step 4: forming a source region in the semiconductor substrate at the bottom of the source line opening; Step 5, forming a first inter-gate dielectric layer and a floating gate composed of a TiN layer on the side of the source line opening; the first inter-gate dielectric layer realizes isolation between the floating gate and the word line polysilicon gate, and the first inter-gate dielectric layer is also located on the surface of the semiconductor substrate at the bottom of the floating gate to realize isolation between the floating gate and the source region; Step 6: forming a second inter-gate dielectric layer and a control gate composed of a conductive material layer in the source line opening formed with the first inter-gate dielectric layer and the floating gate; the second inter-gate dielectric layer realizes isolation between the control gate and the floating gate; Step 7: forming a third inter-gate dielectric layer and a conductive material layer of an erase gate, photolithographically defining a formation region of the erase gate, and etching the third inter-gate dielectric layer and the conductive material layer of the erase gate to form the erase gate; The erase gate is located on top of the floating gate and the control gate, and the coverage area of ​​the erase gate is larger than the formation area of ​​the source line opening; Step eight, removing the hard mask layer to form a first sidewall spacer, wherein the first sidewall spacer is formed on a side surface of the erase gate and a side surface of the first inter-gate dielectric layer at the bottom of the erase gate; Step nine: performing a second etching on the first polysilicon layer and the first gate dielectric layer with the first sidewall as a self-alignment condition, wherein the side surface of the first polysilicon layer formed by the second etching serves as the second side surface of the word line polysilicon gate.

2. The method for manufacturing a flash memory according to claim 1, wherein: The semiconductor substrate includes a silicon substrate.

3. The method for manufacturing a flash memory according to claim 1, wherein: The first gate dielectric layer includes an oxide layer.

4. The method for manufacturing a flash memory according to claim 1, wherein: The hard mask layer is formed by stacking a first nitride layer and a second oxide layer.

5. The method for manufacturing a flash memory according to claim 4, wherein: In the first etching, after the etching of the first gate dielectric layer is completed, a step of over-etching the semiconductor substrate is also included.

6. The method for manufacturing a flash memory according to claim 5, wherein: Before the over-etching of the first etching, the step of forming a third sidewall on the side of the second sidewall and the first side of the word line polysilicon gate is also included, and then the over-etching of the first etching is performed with the third sidewall as a self-alignment condition.

7. The method for manufacturing a flash memory according to claim 5, wherein: A top surface of the floating gate is higher than a top surface of the control gate, and the floating gate forms a tip structure above the top surface of the control gate.

8. The method for manufacturing a flash memory according to claim 7, wherein: The conductive material layer of the control gate is made of tungsten.

9. The method for manufacturing a flash memory according to claim 1, wherein: A plurality of unit structures of the flash memory are formed on the semiconductor substrate, and one source region is shared by two adjacent unit structures.

10. The method for manufacturing a flash memory according to claim 9, wherein: Step 9 and beyond also include: The second side surface of the word line polysilicon gate is used as a self-alignment condition to perform N+ implantation to form a drain region.

11. The method for manufacturing a flash memory according to claim 1, wherein: The material of the first spacer includes an oxide layer.

12. The method for manufacturing a flash memory according to claim 5, wherein: The material of the second spacer includes an oxide layer.

13. The method for manufacturing a flash memory according to claim 6, wherein: The material of the third spacer includes an oxide layer.

14. The method for manufacturing a flash memory according to claim 1, wherein: The material of the first inter-gate dielectric layer includes an oxide layer; The material of the second inter-gate dielectric layer includes an oxide layer; The material of the third inter-gate dielectric layer includes an oxide layer.

Citation Information

Patent Citations

  • Split gate flash memory and forming method thereof

    CN103021952A

  • Process for Manufacturing NOR Memory Cell with Vertical Floating Gate

    US20200303387A1