An oxidant for sample graphitization pretreatment and its preparation method and application
By using a combination of oxidant of persulfate, metal oxide and carbon-free abrasive additive, the problems of low carbon dioxide conversion efficiency and complex equipment in the prior art are solved, and the effect of efficient graphitization and simplification of operation at low temperatures is achieved.
Patent Information
- Application Number
- CN202011158876.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-26
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2040-10-26
AI Technical Summary
In the prior art In the sample graphitization pretreatment, the carbon dioxide conversion efficiency of the oxidant is low, requires high-temperature operation, and the equipment is complex, making it difficult to achieve efficient carbon element conversion.
Provided an oxidant combination, including persulfate 20-40 wt%, metal oxide 40-80 wt%, and carbon-free abrasive additive 1-20 wt%, prepared by uniform mixing and drying for the polyolefin at lower temperatures The carbon element in the sample is converted into carbon dioxide, simplifying the operation process.
实现了在较低温度下高效转化二氧化碳,简化了设备需求,避免了碳污染,适用于处理少量或贵重样品,提高了石墨化过程的效率和可靠性。
Smart Images

Figure BDA0002743673000000091
Abstract
Description
Technical Field
[0001] The present invention relates to 14 The field of C detection technology, more specifically, relates to an oxidant for sample pre-graphitization treatment and a preparation method and application thereof. Background Art
[0002] Bio-based materials refer to materials that are partially or completely made from renewable biomass raw materials. Unlike traditional materials that rely on petrochemical raw materials, bio-based materials use abundant natural materials such as plant straw and starch as raw materials, which can reduce the consumption of petroleum resources and reduce carbon dioxide emissions during the material production process. They are also biodegradable, which greatly reduces or avoids environmental pollution.
[0003] Due to technical and cost issues, most bio-based material products at home and abroad are mixed products of bio-based and petroleum-based materials. Having more bio-based content means having more low-carbon and environmentally friendly biological components. Based on the overall industrial policies of their own countries and the current status of the bio-based industry, different countries have made different classification regulations on the bio-based content in bio-based materials.
[0004] The biobased content of a biobased material refers to the proportion of biobased raw materials in the material. 14 The percentage of C in the total carbon content is expressed as the bio-based carbon content. 14 C content refers to the 14 C and modern carbon-containing standard substances 14 The principle of this measurement is that due to the interaction between cosmic rays and the atmosphere 14 The continuous action of N produces 14 C, so the atmosphere 14 The C content will always remain relatively stable, which means that any bio-based raw material from living organisms 14 C and 12 The ratio of C in the atmosphere will be 14 C and 12 Once an organism dies, it stops exchanging carbon with the atmosphere and the biosphere, and the remaining carbon in its body 14 C decays with a half-life of 5730 years, so petroleum-based raw materials that have been buried underground for tens or even hundreds of millions of years contain almost no C. 14 C. Therefore, it is only necessary to compare the 14 C and pure bio-based raw materials 14 The proportion of C to the total number of carbon atoms, that is, comparing the percentage of modern carbon in the sample with the percentage of modern carbon in pure bio-based raw materials, can determine the bio-based carbon content. Among them, X Bis the biobased content in the sample, pMC is the percentage of modern carbon in the sample, and pMC B It is the percentage of modern carbon in pure bio-based feedstock.
[0005] Existing products can be used to determine 14 The methods for measuring C content include proportional scintillation method (PSM), β ionization (BI) or accelerated mass spectrometry (AMS). Among them, the proportional scintillation method requires the C in the sample to be converted into benzene series before detection. The sample volume required is large, and the converted benzene series form secondary pollution. In addition, the sensitivity is low and the time is long. It takes several hours to test the decay value. The β ionization method takes several days to complete the measurement. Among the above methods, the accelerator mass spectrometry AMS method has the highest sensitivity and accuracy, and has high automation. The sample measurement speed is very fast. It is the first recommended method in relevant international standards.
[0006] Since most AMS instruments require the use of graphite carbon as the ion source of the accelerator, 14 Before C determination, the sample to be tested needs to be graphitized. After the treatment, the carbon element in the sample is converted into graphite, and then it can be pressed into the aluminum cathode target of AMS for testing. The steps of graphitization of general carbon-containing (except carbonate) samples include surface cleaning, sealed tube oxidation, carbon dioxide purification, catalytic reduction and other steps. It can be briefly summarized as follows: first, the pollutants on the surface of the sample are washed off, all the air in the sample container is extracted, the tube is sealed, and the sample is heated to react with the pre-mixed oxidant and converted into carbon dioxide gas; after the reaction is completed, all the carbon dioxide gas is transferred to another container pre-filled with a reducing agent, and is reduced to graphite powder under the action of the reducing agent. This process can be completed by manual step-by-step operation or by automated equipment. In addition to being determined by the carbon content in the sample, the output of graphite powder is also affected by the performance of the oxidant. Due to the different oxidation difficulties of the materials, high temperature or other harsh operating conditions are often required in the actual preparation of samples, and it is difficult to achieve the ideal carbon dioxide conversion efficiency.
[0007] At present, the oxidants used for sample graphitization pretreatment in AMS measurement mainly include copper oxide, high-purity oxygen, etc. When using oxidizing gases such as oxygen as oxidants, the system needs to add an oxygen gas line, and the pumping and ventilation operations are relatively cumbersome; solid oxidants represented by copper oxide have the advantages of no pollution to the sample and easy operation. However, the efficiency of various solid oxidants reported in the literature to oxidize carbon in the sample into carbon dioxide is not ideal, the temperature required for processing polyolefin samples is very high, and the carbon dioxide conversion efficiency is low. Summary of the invention
[0008] The purpose of the present invention is to overcome the defects of the prior art and provide an oxidant used for sample graphitization pretreatment in the determination of bio-based content of polyolefins and a preparation method thereof. The oxidant can convert carbon elements in polyolefin samples into carbon dioxide, requires a low heating temperature, has a high carbon dioxide conversion rate, does not require an additional gas path for the sample processing device, and is easy to operate. This provides a more efficient and reliable option for sample graphitization pretreatment in the determination of bio-based content of polyolefins.
[0009] In order to achieve the above-mentioned purpose, the first aspect of the present invention provides an oxidant for sample graphitization pretreatment, which comprises, based on the total weight of the oxidant, 20-40wt% persulfate, 40-80wt% metal oxide and 1-20wt% carbon-free grinding aid, wherein the sum of the weight percentages of each component is 100wt%.
[0010] The second aspect of the present invention provides a method for preparing the above-mentioned oxidant for sample pre-graphitization treatment, the preparation method comprising:
[0011] (1) uniformly mixing persulfate and water to obtain a persulfate aqueous solution;
[0012] (2) mixing the persulfate aqueous solution, the metal oxide and the carbon-free grinding aid to obtain a mixture;
[0013] (3) removing water from the mixture and then drying it to obtain the oxidant.
[0014] The third aspect of the present invention provides the use of the above oxidant as an oxidant for pre-graphitization treatment of samples for determination of bio-based content in polyolefin materials.
[0015] The technical solution of the present invention has the following advantages:
[0016] 1) The oxidant of the present invention can treat polyolefin samples at a relatively low temperature, without the need for high temperatures of more than 800°C as in conventional oxidants;
[0017] 2) The oxidant carbon dioxide of the present invention has a high yield and can be used to treat samples with a small total amount or relatively precious samples;
[0018] 3) The oxidant of the present invention does not contain any form of carbon element and will not pollute the generated carbon dioxide gas product;
[0019] 4) The oxidant of the present invention is a solid oxidant, which is easy to handle and requires simple equipment. There is no need to add a gas path to the sample processing equipment, and no volatile vapor is generated during the entire sample processing process;
[0020] 5) The oxidant of the present invention is easy to use and can be packaged and vacuumed for oxidation treatment after being ground together with the sample.
[0021] Other features and advantages of the present invention will be described in detail in the following detailed description. DETAILED DESCRIPTION
[0022] The preferred embodiments of the present invention will be described in more detail below. Although the preferred embodiments of the present invention are described below, it should be understood that the present invention can be implemented in various forms and should not be limited to the embodiments set forth herein.
[0023] The first aspect of the present invention provides an oxidant for sample graphitization pretreatment, which comprises, based on the total weight of the oxidant, 20-40wt% persulfate, 40-80wt% metal oxide and 1-20wt% carbon-free grinding aid, wherein the sum of the weight percentages of the components is 100wt%.
[0024] According to the present invention, preferably, the persulfate is at least one of sodium persulfate, potassium persulfate, ammonium persulfate, barium persulfate and calcium persulfate; the persulfate is preferably sodium persulfate and / or potassium persulfate.
[0025] In the present invention, the oxidation reaction of polyolefin is a free radical chain reaction. In order to prevent the polyolefin product from aging and deteriorating too quickly, a certain amount of antioxidants and other additives are usually added. These additives make it difficult for free radicals to be generated in the polyolefin. The addition of persulfate can provide sulfate free radicals (SO4 - ·) to improve the conditions for thermal initiation of the chain reaction and promote the oxidation of polyolefins. Polyolefins preliminarily treated with sulfate free radicals can react more completely with transition metal oxides at lower temperatures to generate carbon dioxide products.
[0026] According to the present invention, preferably, the metal oxide is at least one of Fe2O3, Fe3O4, Cu2O, CuO, MnO2, Ag2O, PbO2, SnO2, GeO2 and V2O5.
[0027] According to the present invention, preferably, the carbon-free grinding aid is at least one of silicon dioxide, hydrotalcite, boron nitride and silicon nitride.
[0028] In the present invention, the carbon-free grinding aid can improve the degree of mixing between the components of the present invention without introducing contaminated carbon. At the same time, in the process of co-grinding the present invention with the sample to be oxidized, the carbon-free grinding aid can also improve the uniformity of grinding mixing and promote the contact between the sample and the oxidant, thereby optimizing the use effect of the oxidant.
[0029] According to the present invention, preferably, the average particle size of the carbon-free grinding aid is 80-100 meshes.
[0030] The second aspect of the present invention provides a method for preparing the above-mentioned oxidant for sample pre-graphitization treatment, the preparation method comprising:
[0031] (1) uniformly mixing persulfate and water to obtain a persulfate aqueous solution;
[0032] (2) mixing the persulfate aqueous solution, the metal oxide and the carbon-free grinding aid to obtain a mixture;
[0033] (3) removing water from the mixture and then drying it to obtain the oxidant.
[0034] The oxidant of the present invention should be stored away from direct sunlight or heat.
[0035] According to the present invention, preferably, step (2) is to mix the persulfate aqueous solution and the metal oxide uniformly to obtain a mixed system; then add a carbon-free grinding aid to the mixed system, mix uniformly, and obtain the mixture.
[0036] According to the present invention, preferably, in step (3), the mixture is subjected to rotary evaporation in a water bath to remove water;
[0037] Wherein, the temperature of the water bath is no more than 40°C.
[0038] According to the present invention, preferably, in step (3), the drying is vacuum drying;
[0039] The vacuum drying is carried out at a temperature of 20-40°C and for a time of 10-15 hours.
[0040] The third aspect of the present invention provides the use of the above oxidant as an oxidant for pre-graphitization treatment of samples for determination of bio-based content in polyolefin materials.
[0041] The present invention is further described below by examples:
[0042] 1. Oxidation experimental methods and instruments used:
[0043] a. Oxidation test method: After mixing the sample to be oxidized with the oxidant of the present invention, the sample is fully frozen and ground, and then placed in a quartz reactor; after evacuating the interior of the reactor, the reactor is sealed, and the reactor is placed in a box-type electric furnace, and the oxidation treatment is performed under the conditions of specified temperature and heating time. (See the following examples and comparative examples for details)
[0044] b. The instruments used in the experiment are:
[0045] Cryo grinder, Peian SPEX 6875
[0046] Box-type electric furnace, Tianjin Zhonghuan Electric Furnace SX-G07123 energy-saving box-type electric furnace.
[0047] The sealed quartz reactor can be vacuumed inside and has good sealing performance at room temperature to 900℃.
[0048] 2. Oxidation effect evaluation method and instruments used:
[0049] a. Oxidation effect evaluation method: After the oxidation treatment is completed, the solid residue is collected and the residual carbon content in the residue is analyzed using an element analyzer; the carbon content in the residue is compared with that in the mixture before the heating treatment (i.e., oxidation treatment) to evaluate the oxidation effect.
[0050] b. The instrument used for the test is: element analyzer, vario EL element analyzer from Elementar Analysensysteme GmbH, Germany.
[0051] Example 1
[0052] 1) Weigh 4 g of sodium persulfate and add it into 50 mL of deionized water, stirring to dissolve it completely;
[0053] 2) Weigh 15 g of copper oxide (CuO, analytical grade) and mix it thoroughly with the solution obtained in step 1) to obtain a mixed system;
[0054] 3) adding 1 g of silica abrasive (average particle size of 80-100 mesh) to the mixed system obtained in step 2), and performing ultrasound to uniformly disperse the suspension system;
[0055] 4) adjusting the water bath temperature to 40° C., slowly evaporating the mixed suspension system obtained in step 3) on a rotary evaporator, collecting the solid mixture remaining after evaporation, and drying it in a vacuum drying oven without heating (i.e., at room temperature 25° C.) for 12 h; and obtaining the oxidant.
[0056] Oxidation experiment:
[0057] 1) Weigh 1 g of the oxidant prepared in this example and weigh 0.05 g of the shredded HDPE sample, mix them and grind them evenly using a cryo-grinder, load them into a quartz reactor, then evacuate the interior of the quartz reactor and seal it.
[0058] 2) Place the sealed quartz reactor containing the sample in a box-type electric furnace and heat it at 100°C for 1 hour, then heat it to 500°C for 2 hours. The oxidation effect is evaluated according to the above-mentioned oxidation effect evaluation method (the oxidation effect evaluation results are shown in Table 1).
[0059] Example 2
[0060] 1) Weigh 8 g of potassium persulfate and add it into 50 mL of deionized water, stirring until it is completely dissolved;
[0061] 2) Weigh 10 g of iron oxide (Fe2O3, analytical grade) and mix it thoroughly with the solution obtained in step 1) to obtain a mixed system;
[0062] 3) adding 2 g of boron nitride abrasive (average particle size of 80-100 mesh) to the mixed system obtained in step 2), and performing ultrasound to uniformly disperse the suspension system;
[0063] 4) adjusting the water bath temperature to 40° C., slowly evaporating the mixed suspension system obtained in step 3) on a rotary evaporator, collecting the solid mixture remaining after evaporation, and drying it in a vacuum drying oven without heating (i.e., at room temperature 25° C.) for 12 h; and obtaining the oxidant.
[0064] Oxidation experiment:
[0065] 1) Weigh 1 g of the oxidant prepared in this example and weigh 0.05 g of the shredded HDPE sample, mix them and grind them evenly using a cryo-grinder, load them into a quartz reactor, then evacuate the interior of the quartz reactor and seal it.
[0066] 2) The sealed quartz reactor containing the sample was placed in a box-type electric furnace and heated at 100°C for 1 hour, and then heated to 700°C for 2 hours. The oxidation effect was evaluated according to the above-mentioned oxidation effect evaluation method (the oxidation effect evaluation results are shown in Table 1).
[0067] Example 3
[0068] 1) Weigh 6 g of barium persulfate and add it into 50 mL of deionized water, stirring to dissolve it completely;
[0069] 2) Weigh 13 g of tin oxide (SnO2, analytical grade) and mix it thoroughly with the solution obtained in step 1) to obtain a mixed system;
[0070] 3) adding 1 g of silicon nitride abrasive (average particle size of 80-100 mesh) to the mixed system obtained in step 2), and performing ultrasound to uniformly disperse the suspension system;
[0071] 4) adjusting the water bath temperature to 40° C., slowly evaporating the mixed suspension system obtained in step 3) on a rotary evaporator, collecting the solid mixture remaining after evaporation, and drying it in a vacuum drying oven without heating (i.e., at room temperature 25° C.) for 12 h; and obtaining the oxidant.
[0072] Oxidation experiment:
[0073] 1) Weigh 1 g of the oxidant prepared in this example and weigh 0.05 g of the shredded HDPE sample, mix them and grind them evenly using a cryo-grinder, load them into a quartz reactor, then evacuate the interior of the quartz reactor and seal it.
[0074] 2) The sealed quartz reactor containing the sample was placed in a box-type electric furnace and heated at 100°C for 1 hour, and then heated to 700°C for 2 hours. The oxidation effect was evaluated according to the above-mentioned oxidation effect evaluation method (the oxidation effect evaluation results are shown in Table 1).
[0075] Comparative Example 1
[0076] Copper oxide (CuO, analytical grade), oxidation treatment temperature 850°C.
[0077] Oxidation experiment:
[0078] 1) Weigh 1 g of copper oxide powder (analytical grade) and 0.05 g of shredded HDPE sample, mix them and grind them evenly using a cryo-grinder, load them into a quartz reactor, then evacuate the inside of the quartz reactor and seal it.
[0079] 2) The sealed quartz reactor containing the sample was placed in a box-type electric furnace and heated at 850° C. for 3 h, and the oxidation effect was evaluated according to the aforementioned oxidation effect evaluation method (the oxidation effect evaluation results are shown in Table 1).
[0080] Comparative Example 2
[0081] Copper oxide (CuO, analytical grade), oxidation treatment temperature 500°C.
[0082] Oxidation experiment:
[0083] 1) Weigh 1 g of copper oxide powder (analytical grade) and 0.05 g of shredded HDPE sample, mix them and grind them evenly using a cryo-grinder, load them into a quartz reactor, then evacuate the inside of the quartz reactor and seal it.
[0084] 2) The sealed quartz reactor containing the sample was placed in a box-type electric furnace and heated at 500° C. for 3 h, and the oxidation effect was evaluated according to the aforementioned oxidation effect evaluation method (the oxidation effect evaluation results are shown in Table 1).
[0085] Table 1 Evaluation results of oxidation effects of comparative examples and examples
[0086]
[0087] It can be seen from the oxidation effect evaluation results in Table 1 that the oxidant used for sample graphitization pretreatment in the determination of polyolefin bio-based content in the present invention requires a lower temperature for oxidizing the sample than the traditional oxidant, has less remaining carbon elements after oxidation treatment, and has a higher carbon dioxide conversion efficiency.
[0088] The present invention provides an oxidant with good performance for sample graphitization pre-treatment in the determination of bio-based content of polyolefins. The oxidant has the advantages of lower temperature required for treating polyolefin samples, less residual carbon elements after oxidation treatment, higher carbon dioxide conversion efficiency, etc. The oxidant itself does not contain any form of carbon elements, will not pollute the generated graphite product, and will not affect the determination results.
[0089] The embodiments of the present invention have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those skilled in the art without departing from the scope and spirit of the described embodiments.
Claims
1. An oxidizing agent for sample pre-graphitization treatment for determination of bio-based content in polyolefin materials, It is characterized in that Based on the total weight of the oxidant, the oxidant comprises: 20-40wt% of persulfate, 40-80wt% of metal oxide and 1-20wt% of carbon-free grinding aid, wherein the sum of the weight percentages of the components is 100wt%.
2. The oxidizing agent according to claim 1, in, The persulfate is at least one of sodium persulfate, potassium persulfate, ammonium persulfate, barium persulfate and calcium persulfate.
3. The oxidizing agent according to claim 2, in, The persulfate is sodium persulfate and / or potassium persulfate.
4. The oxidizing agent according to claim 1, in, The metal oxide is Fe 2 O 3 , Fe 3 O 4 , Cu 2 O, CuO, MnO 2 、Ag 2 O, PbO 2 SnO 2 ,GeO 2 and V 2 O 5 At least one of .
5. The oxidizing agent according to claim 1, in, The carbon-free grinding aid is at least one of silicon dioxide, hydrotalcite, boron nitride and silicon nitride.
6. The oxidizing agent according to claim 1, in, The average particle size of the carbon-free grinding aid is 80-100 meshes.
7. A method for preparing an oxidant for sample graphitization pretreatment for determining bio-based content in polyolefin materials according to any one of claims 1 to 6, It is characterized in that The preparation method comprises: (1) uniformly mixing persulfate and water to obtain a persulfate aqueous solution; (2) uniformly mixing the persulfate aqueous solution, the metal oxide and the carbon-free grinding aid to obtain a mixture; (3) removing moisture from the mixture and then drying it to obtain the oxidant.
8. The preparation method according to claim 7, in, Step (2) is to mix the persulfate aqueous solution and the metal oxide evenly to obtain a mixed system; then add a carbon-free grinding aid to the mixed system and mix evenly to obtain the mixture.
9. The preparation method according to claim 7, in, In step (3), the mixture is subjected to rotary evaporation in a water bath to remove water; Wherein, the temperature of the water bath is no more than 40°C.
10. The preparation method according to claim 7, in, In step (3), the drying is vacuum drying; The vacuum drying is carried out at a temperature of 20-40°C and for a time of 10-15 hours.
11. Use of the oxidant according to any one of claims 1 to 6 as an oxidant for pre-graphitization treatment of samples for determination of bio-based content in polyolefin materials.
Citation Information
Patent Citations
Seawater total organic carbon automatic on-line monitoring instrument
CN101672775A
Treatment method for organic wastewater containing alkylphenol
CN108892280A
Solid oxidant and preparation method and application thereof
CN109696337A
Heavy metal hyperaccumulation biomass charcoal catalyst as well as preparation method and application thereof
CN110898825A
Solid catalyst and preparation method and application thereof
CN111097473A