Method for preparing monosaccharide from lignocellulose raw materials

By adopting low-strength pretreatment, preenzyme decomposition and grinding methods in lignocellulose raw materials, the problems of high enzyme usage and large energy consumption in the existing processes are solved, the production efficiency of monosaccharides and raw material utilization are improved, and the utilization rate of raw materials is reduced. production costs.

CN114574531BActive Publication Date: 2024-11-05GUOTOU BIO TECH INVESTMENT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011387999.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-01
Publication Date
2024-11-05
Estimated Expiration
2040-12-01

AI Technical Summary

Technical Problem

In the existing process for preparing monosaccharides for lignocellulose raw materials, the high enzyme usage and high energy consumption lead to high production costs, and the uneven pretreatment strength leads to low enzymatic lysis efficiency and low raw material utilization.

Method used

Preenzymatic decomposition is performed after low-intensity pretreatment, so that the material is degraded into soluble glycans, reducing viscosity, and processing the harder-degraded parts through grinding, and then enzymatic decomposition is performed to reduce grinding energy consumption and enzyme consumption.

Benefits of technology

It improves the production efficiency of monosaccharides, reduces the amount and energy consumption of enzymes, shortens the enzymatic lysis time, improves the utilization rate of raw materials, and is suitable for enzymatic lysis conditions at high dry substance concentrations.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to the field of monosaccharide production, and discloses a method for preparing monosaccharides from lignocellulose raw materials, the method comprising: sequentially pretreating, pre-enzymatically hydrolyzing, grinding and enzymatically hydrolyzing the lignocellulose raw materials to prepare monosaccharides. The method of the present invention can reduce the amount of enzymes used, accelerate the enzymatic hydrolysis rate and improve the monosaccharide yield under the condition of high dry matter concentration (up to 40 weight %).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for preparing monosaccharide, and in particular to a method for preparing monosaccharide from lignocellulose raw materials. Background Art

[0002] Monosaccharides such as glucose and xylose are important raw materials for modern biotechnology. Glucose is an indispensable nutrient for metabolism in organisms and is widely used in the pharmaceutical industry. In the field of industrial production, glucose is an important raw material for the food and fermentation industries. Many industrial products, such as ethanol, butanol, organic acids, amino acids, enzyme preparations, etc., can be produced by fermentation of microorganisms using glucose as a raw material; it can also be used in the printing and dyeing leather industry and the mirror industry. Xylose can be used as a food additive to replace some dietary fiber; it can also be used to produce xylitol through hydrogenation reactions, which is a widely used non-caloric sweetener.

[0003] The existing glucose production process mainly uses starch as raw materials, and xylose is mainly produced from raw materials rich in hemicellulose such as corn cobs. The source of lignocellulose raw materials is very wide, and it is a good substitute for starch raw materials. The main components of lignocellulose include cellulose, hemicellulose and lignin. Among them, cellulose is degraded to produce glucose, and hemicellulose is degraded to mainly produce xylose. The two account for 55-70% of lignocellulose raw materials, and their content varies with the type of raw materials. Because the structure of lignocellulose is very dense, it needs to be pretreated, such as steam explosion, cooking, puffing, etc., to destroy its crystalline structure, and then enzymatically hydrolyzed by cellulase. The enzymatic hydrolysis process of cellulose and hemicellulose is the result of the synergistic action of multiple enzymes. Usually, under the action of endo-enzymes, most of the fibers are degraded to produce soluble polysaccharides, so that the system presents a rapid liquefaction state, has good fluidity, and the viscosity is significantly reduced. Then the soluble polysaccharides are generated under the action of exo-enzymes, and finally glucose or xylose is generated under the action of glycosidases.

[0004] In the existing biorefining process using lignocellulose as raw material, the amount of cellulase used is often large, resulting in high enzyme costs. Taking the cellulose ethanol process as an example, the cost of cellulase is generally 1,000-3,000 yuan / ton of ethanol, accounting for about 20% of the total production cost. The corresponding total production cost is high, usually higher than 7,000 yuan / ton of ethanol. In the traditional starch alcohol process, the enzyme cost is only about 100 yuan / ton of ethanol, and the total production cost is about 5,000 yuan / ton of ethanol. In comparison, the difference between the two is very large. Therefore, how to improve the efficiency of enzymatic hydrolysis and reduce the cost of cellulase is an important direction for the development of high-value conversion technology for lignocellulose.

[0005] In the lignocellulose degradation technology, pulping is one of the commonly used pretreatment methods. Generally, a pulping machine is used to grind the lignocellulose raw materials after crushing or further pretreatment to reduce the particle size of the material and improve the efficiency of enzymatic hydrolysis. During the pulping process, a large amount of heat is generated due to the strong friction. The material temperature usually rises to more than 100°C. It is necessary to use additional equipment to cool down before the next step of enzymatic hydrolysis can be carried out, which increases the energy consumption and process complexity of the process (Liu Gang. Process simulation and process deduction of dry biorefining technology on Aspen Plus platform [D]. East China University of Science and Technology, 2017.). The pulping process usually consumes a lot of energy. Xiaowen Chen et al. boiled and dehydrated corn stalks with sodium hydroxide solution, then used a disc mill for pulping, and then added cellulase for degradation. When a high sugar yield is achieved, the power consumption per ton of raw material dry matter is about 300kwh. According to this process, the energy consumption of the pulping part alone requires about 2000kwh / ton of ethanol, which significantly increases the production cost. (Xiaowen Chen, etc. A highly efficient dilutealkali deacetylation and mechanical (disc) refining process for the conversion of renewable biomass to lower cost sugars [J]. Biotechnology for Biofuels, 2014, 7: 98.) To avoid the above problems, some processes use a lower dry matter concentration for refining. For example, CN102203271A uses a colloid mill to refine corn stalks that have been pre-crushed by a hammer mill, and the enzymatic hydrolysis efficiency is increased by 10%. However, the substrate concentration is only 10% by weight, the water consumption is large, and the sugar concentration produced by enzymatic hydrolysis is very low, which makes it difficult to apply it industrially.

[0006] Generally speaking, since the distribution of various components of lignocellulosic raw materials is not very uniform, the degree of tissue damage in different parts is also different during the pretreatment process. Taking corn stalks as an example, the outer skin of corn stalks is relatively hard, while the core part is relatively loose. When the pretreatment intensity is not high, some materials, mainly the outer skin part, still show obvious fiber state, which is difficult to degrade, while the core part becomes loose and easy to degrade. After adding cellulase, most of the raw materials can be quickly degraded under the action of fiber endonucleases, the viscosity decreases rapidly, and the fluidity is good. The more difficult to degrade part is difficult to be completely degraded until the end of enzymolysis, resulting in low total enzymolysis conversion rate and low raw material utilization. If the pretreatment intensity is increased (high temperature, high pressure, high acid / alkali, etc.), the outer skin of corn stalks can also be turned into finer particles, which are easy to be degraded by cellulase. However, due to the high pretreatment intensity, part of the cellulose and hemicellulose are directly degraded to generate monosaccharides such as glucose and xylose, and further react under high temperature and high pressure to generate inhibitors such as aldehydes and acids, which affect the efficiency of enzymolysis and subsequent fermentation reactions. This ultimately leads to an increase in raw material consumption and high overall production costs. Summary of the invention

[0007] The purpose of the present invention is to overcome the problem of difficulty in balancing production efficiency and energy consumption when preparing monosaccharides using lignocellulose raw materials in the prior art, and to provide a method for preparing monosaccharides from lignocellulose raw materials, which can improve the production efficiency of monosaccharides while reducing the amount of enzyme used.

[0008] In order to achieve the above object, the present invention provides a method for preparing monosaccharides from lignocellulose raw materials, the method comprising: sequentially pretreating, pre-enzymatically hydrolyzing, grinding and enzymatically hydrolyzing the lignocellulose raw materials to prepare monosaccharides.

[0009] Preferably, the concentration of the pretreated material is 10-40% by weight based on dry matter.

[0010] Preferably, the viscosity of the material after pre-enzymatic hydrolysis is below 6000 mPa·s.

[0011] Preferably, the grinding conditions are such that at least 90% of the particles in the ground material have a particle size of 100-500 μm.

[0012] The present invention is to pre-treat the lignocellulose raw material at a relatively low intensity, and then add enzymes for pre-enzymatic hydrolysis. Most of the solids are degraded into soluble polysaccharides and part of monosaccharides under the action of the enzyme, the viscosity is reduced, and the material is in a better flow state, and can be pumped in a pipeline. The material is subjected to pulping treatment to grind the fibers that are difficult to degrade, and then the enzymatic hydrolysis is continued.

[0013] Its main feature is that cellulase is first used to convert most of the materials into soluble polysaccharides. On the one hand, it reduces the viscosity and increases the fluidity of the system, which can be transported by a pump and is easy to grind. On the other hand, it reduces the total amount of solids in the grinding process, avoids the generation of a large amount of heat during the grinding process, and significantly reduces the energy consumption and processing costs of the grinding process.

[0014] The method of the present invention can achieve a good enzymatic hydrolysis effect even under the condition of low pretreatment intensity, shorten the enzymatic hydrolysis time, and improve the utilization rate of raw materials. The method is particularly suitable for enzymatic hydrolysis conditions with high dry matter concentration, and can achieve a high enzymatic hydrolysis efficiency even under the condition of less free water, thus exploring an effective way for high-value conversion of lignocellulose raw materials. DETAILED DESCRIPTION

[0015] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0016] The invention provides a method for preparing monosaccharides from lignocellulose raw materials. The method comprises: sequentially performing pretreatment, preenzymatic hydrolysis, grinding and enzymatic hydrolysis on the lignocellulose raw materials to prepare monosaccharides.

[0017] In the present invention, the type of lignocellulosic raw material is any lignocellulosic raw material available in the art, as long as it contains lignocellulose, and the lignocellulosic raw material includes but is not limited to at least one of corn stalks, corn husks, corn cobs, wheat straws, rice straws, bagasse, bean stalks, cotton stalks, banana stalks, coconut shells, bamboo, switchgrass, reed, branches, wood chips and sawdust. It is understood that the stalks include stems and leaves of plants and optionally roots.

[0018] In the present invention, the enzymatic hydrolysis of lignocellulose raw materials is used to prepare monosaccharides containing xylose and glucose.

[0019] The pretreatment method of the lignocellulose raw material can be any method conventionally used in the art for pretreatment of the lignocellulose raw material, and can also be adjusted according to the type of material.

[0020] Generally speaking, the lignocellulose raw material may contain impurities, which may be pre-treated to remove impurities. The impurity removal method may be a conventional technical means in the art, as long as the impurities in the lignocellulose raw material can be removed. For example, a dust collector may be used to remove dust impurities, a dust remover may be used to remove sand and stone impurities, and a magnetic adsorption method may be used to remove iron impurities. Those skilled in the art may perform impurity removal operations in combination with the above methods as needed.

[0021] In the present invention, preferably, the method further comprises: before pre-treating the lignocellulose raw material, pulverizing it.

[0022] In the present invention, the pulverization method can be a conventional method in the art, for example, a pulverizer can be used to pulverize the lignocellulosic raw material. Preferably, the pulverization process makes the particle size of the particles in the material after the pulverization process be 1-3 cm. It should be understood that when the material after the pulverization process is in the shape of strips or filaments and the like, its particle size refers to its length.

[0023] It should be understood that setting the crushing parameters of the crusher to control the particle size of the crushed material to 1-3 cm does not mean that the particle size of all particles is 1-3 cm, but that the particle size of most particles is 1-3 cm, for example, more than 90% by weight is 1-3 cm.

[0024] The pulverizer may be a conventional pulverizer in the art, such as a hammer pulverizer, a roller pulverizer, a shear pulverizer, and the like.

[0025] In the present invention, the pretreatment method may be a pretreatment method conventionally used in the art, and the pretreatment method includes but is not limited to at least one of steam explosion, cooking and puffing.

[0026] In the present invention, the steam explosion method may be a conventional steam explosion method in the art, preferably including at least one of neutral steam explosion, dilute acid steam explosion and alkaline steam explosion.

[0027] The steam explosion method preferably comprises mixing the lignocellulosic raw material with water or dilute acid or alkaline substance, maintaining the mixture at 150-210°C (e.g., 150, 160, 170, 180, 190, 200, 210, and any range between any two values) for 1-120 min (e.g., 1, 5, 10, 20, 30, 40, 50, 60, 70, 80, 90, 100, 110, 120 min, and any range between any two values), and then releasing the mixture under reduced pressure instantly. It should be understood that when the lignocellulosic raw material is mixed with water, it is a neutral steam explosion; when it is mixed with dilute acid, it is a dilute acid steam explosion; when it is mixed with alkaline substance, it is an alkaline steam explosion.

[0028] In the present invention, preferably, the amount of water or dilute acid or alkali used is such that the content of lignocellulosic raw material in the mixture of lignocellulosic raw material and water or dilute acid or alkaline substance is 30-60% by weight (for example, it can be 30, 35, 40, 45, 50, 55, 60% by weight and any range between any two values).

[0029] In the present invention, the content of the lignocellulosic raw material is based on dry matter.

[0030] In the present invention, the water may be water commonly used in the art, such as tap water and industrial water.

[0031] In the present invention, the dilute acid is a dilute acid conventionally used in the art, for example, an acid solution with a concentration of 0.1-3 wt % (for example, 0.1, 0.2, 0.4, 0.6, 0.8, 1, 1.2, 1.4, 1.6, 1.8, 2, 2.5, 3 wt % and any range between any two values), and the acid includes but is not limited to phosphoric acid and sulfuric acid.

[0032] In the present invention, the alkaline substance is an alkaline substance conventionally used in the art, for example, it can be an alkaline solution with a concentration of 1-20% by weight (for example, it can be 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20% by weight and any range between any two values), and the alkaline substance includes but is not limited to sodium hydroxide, potassium hydroxide, sodium sulfite, potassium sulfite and ammonium sulfite.

[0033] In the present invention, the cooking method may be a conventional cooking method in the art, such as mixing the lignocellulosic raw material with water, heating and cooking, and then performing solid-liquid separation to obtain the cooked material.

[0034] Preferably, the amount of water used is such that the dry matter content of the lignocellulosic raw material in the material used for cooking is 10-30% by weight.

[0035] In a preferred embodiment of the present invention, the material used for cooking further contains sulfite and / or bisulfite, such as sodium sulfite, ammonium sulfite, magnesium sulfite or ammonium bisulfite, and the content of sulfite or bisulfite in the material used for cooking is 3-20% by weight.

[0036] The cooking described in the present invention can be achieved by a digester, and the digester is a stirred tank reactor or a non-stirred tank reactor (for example, a vertical or horizontal reactor).

[0037] Preferably, the cooking is carried out under closed conditions.

[0038] Preferably, the cooking conditions include: a temperature of 140-200° C. and a time of 5-120 min.

[0039] In the present invention, the solid-liquid separation method includes but is not limited to extrusion, and a centrifugal method may also be used.

[0040] It should be understood that the material after the solid-liquid separation can also be washed with water, for example, water (such as 70-95° C.) can be added to the material after the solid-liquid separation and mixed evenly before the solid-liquid separation is performed again.

[0041] In the present invention, the puffing method may be a conventional puffing method in the art, for example, the lignocellulose raw material may be mixed with water and then puffed to obtain a puffed material.

[0042] Preferably, the amount of water used is such that the content of lignocellulosic raw material in the material used for puffing is 20-60 wt % (for example, it can be 20, 25, 30, 35, 40, 45, 50, 55, 60 wt % and any range between any two values).

[0043] The puffing can be performed in a puffing machine.

[0044] Preferably, the puffing conditions include: a temperature of 120-180° C. and a screw speed of 50-80 rpm.

[0045] In the present invention, the pre-enzymatic hydrolysis method may be a conventional enzymatic hydrolysis method in the art. Preferably, the pre-enzymatic hydrolysis method comprises: contacting the pretreated material with a first enzyme preparation to perform pre-enzymatic hydrolysis to obtain a pre-enzymatically hydrolyzed material.

[0046] In the present invention, the pretreated material can be directly used for enzymolysis, or the pretreated material can be mixed with water and adjusted to a suitable concentration for enzymolysis.

[0047] Preferably, the concentration of the pretreated material is 10-40 wt % (e.g., 10, 15, 20, 25, 30, 35, 40 wt % and any range between any two values) based on dry matter. It should be understood that when the dry matter concentration of the pretreated material is within the aforementioned range, it can be used directly, and when its dry matter concentration exceeds the aforementioned range, the pretreated material can be diluted or concentrated to be within the aforementioned range.

[0048] Preferably, the first enzyme preparation comprises cellulase, and optionally further comprises hemicellulase and / or β-glucosidase.

[0049] In the first enzyme preparation, the weight ratio of cellulase, hemicellulase and β-glucosidase can be 1:0-0.3:0-0.2.

[0050] The first enzyme preparation can be obtained in various ways, for example, it can be purchased commercially.

[0051] In the present invention, the amount of the first enzyme preparation can be selected in a wide range, as long as it can degrade the lignocellulosic raw material to prepare monosaccharides, and those skilled in the art can add it as needed. For example, the amount of the first enzyme preparation is 1-20% by weight of the dry matter weight of the pretreated material, more preferably 2-15% by weight (for example, it can be 2, 4, 6, 8, 10, 12, 14, 15% by weight and any range between any two values).

[0052] The pre-enzymatic hydrolysis conditions may be such that the enzyme can work normally. Preferably, the pre-enzymatic hydrolysis conditions include: a temperature of 40-60° C. and a pH of 4.5-5.5.

[0053] In the present invention, the pre-enzymatic hydrolysis time can be selected within a wide range, and the enzymatic hydrolysis time will also vary depending on the type of material and the substrate concentration. Generally speaking, the material after pre-enzymatic hydrolysis can be transported by pumping, that is, it is in a pumpable state. Preferably, the viscosity of the material after pre-enzymatic hydrolysis is below 6000mPa·s, more preferably 200-6000mPa·s.

[0054] The viscosity of the enzymatic hydrolysis system can be measured by the NDJ-5S digital viscometer produced by Shanghai Sunny Hengping Scientific Instrument Co., Ltd. The viscosity value will vary depending on the selected rotor model and speed. Depending on the substrate concentration of the enzymatic hydrolysis system, you can choose 2# or 3# rotor, and adjust it according to the actual situation within the corresponding measurement range of the instrument to ensure that the system is in a pumpable flow state.

[0055] The pump may be a pump commonly used in the art, such as a centrifugal pump, a reciprocating pump, etc.

[0056] In the present invention, the pre-enzymatically hydrolyzed material is ground. The grinding method may be a conventional grinding method in the art, as long as the pre-enzymatically hydrolyzed material can be further crushed.

[0057] The equipment used for grinding can be an existing grinding equipment that can be used to grind the pre-enzymatically hydrolyzed material. Preferably, the grinding is carried out in a high shearing device.

[0058] The high shearing device includes but is not limited to a disc mill, a colloid mill, a convex tooth mill, and other devices that generate high-intensity shearing force through shearing components. Preferably, the high shearing device comprises relatively rotating shearing components. Within the preferred range, the time for preparing monosaccharides can be further shortened, and the output and yield of monosaccharides can be increased.

[0059] Preferably, the high shear device comprises two counter-rotating shearing members having a gap between the shearing members of 0.1-1.8 mm, such as 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1, 1.1, 1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8 mm and any range between any two values, more preferably 0.2-0.6 mm.

[0060] Preferably, the grinding conditions are such that at least 90% of the particles in the ground material have a particle size of 100-500 μm. Within the preferred range, the time for preparing monosaccharides can be further shortened, and the output and yield of monosaccharides can be increased.

[0061] The particle size distribution can be measured by a particle size analyzer.

[0062] In the present invention, the ground material is further subjected to enzymolysis. Preferably, the enzymolysis method comprises: contacting the ground material with an optional second enzyme preparation, performing enzymolysis, and obtaining monosaccharides. During the enzymolysis, the second enzyme preparation may be added to further accelerate the enzymolysis, or the enzymolysis of the lignocellulosic raw material may be continued by the first enzyme preparation without adding an enzyme preparation.

[0063] Preferably, the second enzyme preparation comprises cellulase, and optionally further comprises hemicellulase and / or beta-glucosidase. The second enzyme preparation and the first enzyme preparation may be the same or different. Within the preferred range, the time for preparing monosaccharides can be further shortened, and the output and yield of monosaccharides can be increased.

[0064] In a preferred embodiment of the present invention, the dosage ratio of the first enzyme preparation to the second enzyme preparation is 1:0-0.5, more preferably 1:0.1-0.3, such as 1:0.1, 1:0.15, 1:0.2, 1:0.25, 1:0.3 and any range between any two values. When the dosage of the second enzyme preparation is too high, although the enzymolysis process can be further accelerated, the benefits brought are lower than the loss of enzyme preparation consumption.

[0065] The enzymolysis conditions may be such that the enzyme can work normally. Preferably, the enzymolysis conditions include: a temperature of 40-60° C., a pH of 4.5-5.5, and an enzymolysis time of 48-120 h.

[0066] In a preferred embodiment of the present invention, the method comprises: pre-treating, pre-enzymolysis, grinding and enzymolysis of lignocellulosic raw materials in sequence to prepare monosaccharides. The pre-treated material is contacted with a first enzyme preparation for pre-enzymolysis to obtain a pre-enzymolyzed material, and the concentration of the pre-treated material is 10-40% by weight based on dry matter. The first enzyme preparation contains cellulase, and optionally also contains hemicellulase and / or β-glucosidase. The dosage of the first enzyme preparation is 2-15% by weight of the dry matter weight of the pre-treated material. The viscosity of the pre-enzymolyzed material is 200-6000mPa·s. The pre-enzymolyzed material is ground, and the grinding conditions make at least 90% of the particles in the ground material have a particle size of 100-500μm. The ground material is contacted with a second enzyme preparation for enzymolysis to obtain monosaccharides. The second enzyme preparation contains cellulase, and optionally also contains hemicellulase and / or β-glucosidase. The dosage ratio of the first enzyme preparation to the second enzyme preparation is 1:0.1-0.3. Under the preferred conditions, the time for preparing monosaccharides can be further shortened, and the output and yield of monosaccharides can be increased.

[0067] Monosaccharides are obtained by enzymatic hydrolysis, and the monomers include glucose and xylose. The contents of glucose and xylose can be determined by HPLC.

[0068] In the following examples and comparative examples, cellulase was purchased from Novozymes with a brand name of CTec2;

[0069] Xylanase was purchased from Xiasheng Company, brand FDY-3001;

[0070] β-Glucosidase was purchased from Xiasheng Company with the brand name SPE-007A.

[0071] In the following examples and comparative examples, the lignocellulosic raw materials were crushed into small pieces of 1-3 cm by a hammer mill before pretreatment.

[0072] The conditions for pre-enzymatic hydrolysis and enzymatic hydrolysis are: temperature of 50±2°C and pH of 5±0.5.

[0073] In the following examples and comparative examples, the substrate concentration is calculated based on the dry weight of the pretreated material as the weight of the substrate.

[0074] Glucose yield = glucose production / amount of glucose that can be produced by total degradation of raw materials.

[0075] Xylose yield = xylose production / the amount of xylose that can be produced by the complete degradation of raw materials.

[0076] In the following examples and comparative examples, the glucose and xylose contents were determined using the HPLC method, and the specific conditions were:

[0077] Chromatographic column: BIO-RAD analytical column HPX-87H

[0078] Injection volume: 20 μL

[0079] Mobile phase: 0.005M sulfuric acid, filtered through a 0.2μm filter membrane and degassed

[0080] Flow rate: 0.5mL / min

[0081] Column temperature: 55-65℃

[0082] Detector temperature: as close to column temperature as possible

[0083] Detector: Differential detector

[0084] Running time: 30min.

[0085] The particle size of the particles was measured using a Malvern Mastersizer 300 particle size analyzer.

[0086] The viscosity of the enzymatic hydrolysis system was measured using a NDJ-5S digital viscometer produced by Shanghai Sunny Hengping Scientific Instrument Co., Ltd., using rotor #3. In the following examples, the viscosity of the product after pre-enzymatic hydrolysis was in the range of 200-6000 mPa·s.

[0087] Example 1-1

[0088] This example is used to illustrate the method for preparing monosaccharides from wheat straw.

[0089] (1) The wheat straw was subjected to neutral steam explosion pretreatment, with a substrate concentration of 50% by weight, a temperature of 165° C., and a holding time of 30 min.

[0090] (2) Adding water and an enzyme preparation to the pretreated material for pre-enzymatic hydrolysis, wherein the substrate concentration is 10% by weight and the amount of the enzyme preparation added is 3% by weight of the substrate dry matter weight. After 2 hours of pre-enzymatic hydrolysis, the material is liquefied to obtain a pre-enzymatically hydrolyzed material. The enzyme preparation is cellulase.

[0091] (3) The pre-enzymatically hydrolyzed material is refined by a disc mill, wherein the gap between the shearing components is 0.6 mm, and the grinding conditions are such that at least 90% by weight of the particles in the ground material have a particle size of 100-500 μm.

[0092] (4) After adding the enzyme preparation to the ground material, the enzymatic hydrolysis is continued for 48 hours, and the weight ratio of the amount of the enzyme preparation added in step (2) to the amount of the enzyme preparation added in this step is 1:0.25, that is, 0.75% by weight of the dry matter weight of the substrate, to obtain a material after enzymatic hydrolysis. Among them, the results of glucose yield, xylose yield, glucose concentration and xylose concentration in the material after enzymatic hydrolysis are shown in Table 1.

[0093] Example 1-2

[0094] This example is used to illustrate the method for preparing monosaccharides from wheat straw.

[0095] The method described in Example 1-1 was followed, with the same total enzyme preparation amount, except that the weight ratio of the enzyme preparation amount added in step (2) to the enzyme preparation amount added in step (4) was 1:0.1.

[0096] The results of the conversion rate of the lignocellulose raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 1.

[0097] Examples 1-3

[0098] This example is used to illustrate the method for preparing monosaccharides from wheat straw.

[0099] The operation was carried out according to the method described in Example 1-1, with the same total reaction time and total enzyme preparation dosage, except that the weight ratio of the enzyme preparation dosage in step (2) to the enzyme preparation dosage in step (4) was 1:0.3. Results After 3 hours of pre-enzymatic hydrolysis, the material was liquefied, and the subsequent reaction was the same as in Example 1-1.

[0100] The results of the conversion rate of the lignocellulose raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 1.

[0101] Examples 1-4

[0102] This example is used to illustrate the method for preparing monosaccharides from wheat straw.

[0103] The operation was carried out according to the method described in Example 1-1, with the same total reaction time and total enzyme preparation dosage, except that the ratio of the amount of enzyme preparation added in step (2) to the amount of enzyme preparation added in step (4) was 1:0.5. Results After 5 hours of pre-enzymatic hydrolysis, the material was liquefied, and the subsequent reaction was the same as in Example 1-1.

[0104] The results of the conversion rate of the lignocellulose raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 1.

[0105] Examples 1-5

[0106] This example is used to illustrate the method for preparing monosaccharides from wheat straw.

[0107] The method described in Example 1-1 was followed, except that no enzyme preparation was added in step (4), and the amount of enzyme preparation added in step (2) was 3.75% by weight of the dry matter of the pretreated material.

[0108] The results of the conversion rate of the lignocellulose raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 1.

[0109] Comparative Example 1

[0110] This comparative example is used to illustrate the method for preparing monosaccharides using wheat straw as a reference.

[0111] The method described in Example 1-1 was followed, except that the grinding operation was not performed, that is, water and enzyme preparation were added to the pretreated material for enzymolysis, wherein the substrate concentration was 10% by weight, and the amount of enzyme preparation added was 3.75% by weight of the substrate dry matter weight. After 50 hours of enzymolysis, the enzymolyzed material was obtained.

[0112] The results of the conversion rate of the lignocellulose raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 1.

[0113] Table 1

[0114] serial number Glucose yield (%) Xylose yield (%) Glucose concentration (g / L) Xylose concentration (g / L) Example 1-1 80.8 83.6 41.3 14.8 Example 1-2 78.5 80.1 40.2 14.2 Examples 1-3 75.1 77.1 38.5 13.7 Examples 1-4 67.3 69.8 34.6 12.4 Examples 1-5 69.1 71.0 35.4 12.6 Comparative Example 1 61.6 67.9 31.6 12.1

[0115] Example 2

[0116] This example is used to illustrate the method for preparing monosaccharides from corn stalks.

[0117] (1) Sodium sulfite is added to corn stalks for cooking, with a substrate concentration of 20% by weight and a sodium sulfite concentration of 2% by weight. The mixture is fully mixed, sealed, and heated for cooking at 160°C for 90 minutes. After the cooking is completed, the material is squeezed for solid-liquid separation. Hot water at 80°C is added to the solid, and after sufficient stirring and mixing, a second solid-liquid separation is performed.

[0118] (2) Adding water and enzyme preparation to the pretreated material for pre-enzymatic hydrolysis, wherein the substrate concentration is 22% by weight, and the amount of enzyme preparation added is 7% by weight of the substrate dry matter weight. After 15 hours of pre-enzymatic hydrolysis, the material is liquefied to obtain a pre-enzymatically hydrolyzed material. The enzyme preparation is cellulase.

[0119] (3) The pre-enzymatically hydrolyzed material is refined by a disc mill, wherein the gap between the shearing components is 0.2 mm, and the grinding conditions are such that at least 90% by weight of the particles in the ground material have a particle size of 100-500 μm.

[0120] (4) The ground material was further enzymatically hydrolyzed for 60 hours to obtain an enzymatically hydrolyzed material. The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0121] Comparative Example 2

[0122] This comparative example is used to illustrate the method of preparing monosaccharides using corn stalks as a reference.

[0123] The method described in Example 2 was followed, except that the grinding operation was not performed. That is, water and enzyme preparation were added to the pretreated material for enzymolysis, wherein the substrate concentration was 22% by weight and the amount of enzyme preparation added was 7% by weight of the substrate dry matter weight. After 75 hours of enzymolysis, the enzymolyzed material was obtained.

[0124] The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0125] Example 3

[0126] This example is used to illustrate the method for preparing monosaccharides from bagasse.

[0127] (1) Bagasse was mixed with 2 wt % dilute sulfuric acid, the substrate concentration was 40 wt %, and the steam explosion treatment conditions were a temperature of 165° C. and a holding time of 8 min.

[0128] (2) Adding water and enzyme preparation to the pretreated material for pre-enzymatic hydrolysis, wherein the substrate concentration is 30% by weight, and the amount of enzyme preparation added is 10% by weight of the substrate dry matter weight. After 36 hours of pre-enzymatic hydrolysis, the material is liquefied to obtain a pre-enzymatically hydrolyzed material. The enzyme preparation is cellulase.

[0129] (3) The pre-enzymatically hydrolyzed material is ground using a colloid mill, wherein the gap between the shearing components is 0.1 mm, and the grinding conditions are such that at least 90% by weight of the particles in the ground material have a particle size of 100-500 μm.

[0130] (4) The ground material was further enzymatically hydrolyzed for 60 hours to obtain an enzymatically hydrolyzed material. The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0131] Comparative Example 3

[0132] This comparative example is used to illustrate the method for preparing monosaccharides using reference bagasse.

[0133] The method described in Example 3 was followed, except that the grinding operation was not performed, that is, water and enzyme preparation were added to the pretreated material for enzymolysis, wherein the substrate concentration was 30% by weight, and the amount of enzyme preparation added was 10% by weight of the substrate dry matter weight. After 96 hours of enzymolysis, the enzymolyzed material was obtained.

[0134] The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0135] Example 4

[0136] This example is used to illustrate the method for preparing monosaccharides from cotton stalks.

[0137] (1) Add ammonium sulfite to cotton stalks for steaming, with a substrate concentration of 20% by weight and an ammonium sulfite concentration of 6% by weight. Mix thoroughly, seal and heat to steam at 165°C for 70 minutes. After steaming, the material is ejected in the form of steam explosion, and then extruded for solid-liquid separation. Add 90°C hot water to the solid, stir and mix thoroughly, and then perform a second solid-liquid separation.

[0138] (2) adding water and enzyme preparation to the pretreated material for pre-enzymatic hydrolysis, wherein the substrate concentration is 15% by weight, and the amount of enzyme preparation added is 5% by weight of the substrate dry matter weight. After 8 hours of pre-enzymatic hydrolysis, the material is liquefied to obtain a pre-enzymatically hydrolyzed material. The enzyme preparation is cellulase.

[0139] (3) The pre-enzymatically hydrolyzed material is ground using a convex tooth mill, wherein the gap between the shearing components is 1.8 mm, and the grinding conditions are such that at least 90% by weight of the particles in the ground material have a particle size of 100-500 μm.

[0140] (4) The ground material was further enzymatically hydrolyzed for 60 hours to obtain an enzymatically hydrolyzed material. The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0141] Comparative Example 4

[0142] This comparative example is used to illustrate the method for preparing monosaccharides from cotton stalks.

[0143] The method described in Example 4 was followed, except that the grinding operation was not performed, that is, water and enzyme preparation were added to the pretreated material for enzymolysis, wherein the substrate concentration was 15% by weight, and the amount of enzyme preparation added was 5% by weight of the substrate dry matter weight. After enzymolysis for 68 hours, the enzymolyzed material was obtained.

[0144] The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0145] Example 5

[0146] This example is used to illustrate the method for preparing monosaccharides from corn stalks.

[0147] (1) Corn stalks were mixed with water and then pre-expanded. The barrel temperature was 160°C and the screw speed was 65 r / min. -1 , the dry matter content is 50% by weight.

[0148] (2) Adding water and enzyme preparation to the pretreated material for pre-enzymatic hydrolysis, wherein the substrate concentration is 25% by weight and the amount of the composite enzyme preparation added is 8% by weight of the substrate dry matter weight. After 30 hours of pre-enzymatic hydrolysis, the material is liquefied to obtain a pre-enzymatically hydrolyzed material. The enzyme preparation is a composite enzyme preparation (cellulase: xylanase: β-glucosidase = 1:0.2:0.1).

[0149] (3) The pre-enzymatically hydrolyzed material is ground with a convex tooth mill, the gap between the shearing parts of which is 0.5 mm, and the grinding conditions are such that at least 90% by weight of the particles in the ground material have a particle size of 100-500 μm.

[0150] (4) The ground material was further enzymatically hydrolyzed for 50 hours to obtain an enzymatically hydrolyzed material. The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0151] Comparative Example 5

[0152] This comparative example is used to illustrate the method of preparing monosaccharides using corn stalks as a reference.

[0153] The method described in Example 5 was followed, except that the grinding operation was not performed, that is, water and enzyme preparation were added to the pretreated material for enzymolysis, wherein the substrate concentration was 25% by weight, and the amount of the composite enzyme preparation added was 10% by weight of the substrate dry matter weight. After 80 hours of enzymolysis, the enzymolyzed material was obtained.

[0154] The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0155] Example 6

[0156] This example is used to illustrate the method for preparing monosaccharides from rice straw.

[0157] (1) Rice straw was mixed with 1.5 wt % dilute sulfuric acid, the substrate concentration was 50 wt %, and the steam explosion treatment conditions were a temperature of 160° C. and a heat preservation time of 10 min.

[0158] (2) Adding water and enzyme preparation to the pretreated material for pre-enzymatic hydrolysis, wherein the substrate concentration is 40% by weight and the amount of the composite enzyme preparation added is 15% by weight of the substrate dry matter weight. After 45 hours of pre-enzymatic hydrolysis, the material is liquefied to obtain a pre-enzymatically hydrolyzed material. The enzyme preparation is a composite enzyme preparation (cellulase: xylanase = 1:0.3).

[0159] (3) The pre-enzymatically hydrolyzed material is ground using a colloid mill, wherein the gap between the shearing components is 0.3 mm, and the grinding conditions are such that at least 90% by weight of the particles in the ground material have a particle size of 100-500 μm.

[0160] (4) The ground material was further enzymatically hydrolyzed for 75 hours to obtain an enzymatically hydrolyzed material. The results of the conversion rate of the lignocellulosic raw material, the concentration of glucose and the concentration of xylose in the enzymatically hydrolyzed material are shown in Table 2.

[0161] Comparative Example 6

[0162] This comparative example is used to illustrate the method for preparing monosaccharides using rice straw as a reference.

[0163] The method described in Example 6 was followed, except that the grinding operation was not performed, that is, water and enzyme preparation were added to the pretreated material for enzymolysis, wherein the substrate concentration was 40% by weight, and the amount of the composite enzyme preparation added was 15% by weight of the substrate dry matter weight. After enzymolysis for 120 hours, the enzymolyzed material was obtained.

[0164] The results of the glucose concentration and xylose concentration in the obtained enzymatically hydrolyzed material are shown in Table 2.

[0165] Table 2

[0166] serial number Glucose concentration (g / L) Xylose concentration (g / L) Example 2 90.2 33.7 Comparative Example 2 76.4 29.4 Example 3 120.6 39.5 Comparative Example 3 105.7 33.6 Example 4 64.8 17.8 Comparative Example 4 55.2 15.4 Example 5 95.6 36.7 Comparative Example 5 82.7 30.4 Example 6 160.2 54.7 Comparative Example 6 141.3 46.7

[0167] It can be seen from the results in Table 1 and Table 2 that the technical solution in the embodiment of the present invention, especially the preferred enzyme addition method, has the effect of promoting enzymatic hydrolysis of raw materials and significantly improving sugar yield.

[0168] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A method for preparing monosaccharides from lignocellulose raw materials, characterized in that: The method comprises: sequentially pretreating, pre-enzymatically hydrolyzing, grinding and enzymatically hydrolyzing lignocellulose raw materials to prepare monosaccharides; Wherein, the concentration of the pretreated material is 25-40% by weight based on dry matter; The pre-enzymatic hydrolysis method comprises: contacting the pre-treated material with a first enzyme preparation to perform pre-enzymatic hydrolysis to obtain a pre-enzymatic hydrolyzed material; the first enzyme preparation comprises cellulase; the amount of the first enzyme preparation is 1-20% by weight of the dry matter weight of the pre-treated material; The enzymatic hydrolysis method comprises: contacting the ground material with an optional second enzyme preparation; the second enzyme preparation comprises cellulase; the dosage ratio of the first enzyme preparation to the second enzyme preparation is 1:0.1-0.3; The grinding conditions are such that at least 90% of the particles in the ground material have a particle size of 100-500 μm; The pretreatment method includes at least one of steam explosion, cooking and puffing; The viscosity of the material after pre-enzymatic hydrolysis is less than 6000 mPa•s; Wherein, the pre-enzymatic hydrolysis conditions include: temperature of 40-60°C and pH of 4.5-5.

5.

2. The method according to claim 1, wherein: The first enzyme preparation optionally further comprises hemicellulase and / or β-glucosidase.

3. The method according to claim 1, wherein: The grinding is carried out in a high shear device.

4. The method according to claim 3, wherein: The high shear device comprises two relatively rotating shearing components, and the gap between the shearing components is 0.1-1.8 mm.

5. The method according to claim 4, wherein: The gap of the shearing component is 0.2-0.6 mm.

6. The method according to claim 1, wherein: The second enzyme preparation optionally further comprises hemicellulase and / or beta-glucosidase.

7. The method according to claim 1, wherein: The lignocellulosic raw material comprises at least one of corn stalks, corn husks, corn cobs, wheat straw, rice straw, bagasse, bean stalks, cotton stalks, banana stalks, coconut shells, bamboo, switchgrass, reed, branches, wood chips and sawdust.

8. The method according to claim 1, wherein: The method further comprises: before pre-treating the lignocellulose raw material, pulverizing it.

9. The method according to claim 8, wherein: The pulverization process makes the particle size of the particles in the pulverized material be 1-3 cm.