A method for treating lithium-containing mother liquor of fludioxonil intermediate
Through the adsorption of macroporous resin and the recycling and treatment of potassium hydroxide and potassium carbonate, the problem of lithium-containing mother liquor in the production process of rosinoxin intermediates is solved, the product yield is improved and the environmentally friendly recycling of wastewater is achieved, and the Economic and environmental benefits.
Patent Information
- Application Number
- CN202311237211.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-25
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2043-09-25
AI Technical Summary
In the prior art, the lithium-containing mother liquor produced during the production of rosinoxin intermediate cannot be recovered, resulting in economic losses and environmental pollution.
Using primary and secondary adsorption of macroporous resins, combined with the recovery treatment of potassium hydroxide and potassium carbonate, 2,2-difluorobenzo[1,3] m-dioxolene is recovered through the elution and precipitation steps- 4-Formaldehyde and lithium elements form an efficient wastewater recycling process.
It improves product yield, significantly reduces production costs, and realizes environmentally friendly recycling of wastewater, with significant economic and environmental benefits.
Smart Images

Figure SMS_3
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of fludioxonil intermediate processing, and particularly relates to a method for processing a fludioxonil intermediate lithium-containing mother liquor. Background Art
[0002] Fludioxonil is a new type of non-systemic fungicide with epoch-making significance. It is used for foliar treatment of wheat, barley, corn, peas, rapeseed, rice, vegetables, grapes, lawns, and ornamental crops to control Fusarium spp., wheat net black rot, and damping-off fungi. It is particularly effective against gray mold. It is currently one of the world's largest-selling seed treatment agents with advantages such as low dosage, extremely low toxicity, and long lasting effect. Its structural formula is as follows:
[0003] .
[0004] 2,2-Difluorobenzo[1,3]dioxole-4-carboxaldehyde, molecular formula C 12 H6F2N2O2, with a relative molecular mass of 248.2, is a key intermediate in the synthesis of fludioxonil. Currently, the method of synthesizing 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde from 2,2-difluoro[1,3]benzodioxole has been well used in industrial production. The reaction equation is as follows:
[0005] ,
[0006] The reaction uses n-hexane as solvent, and 2,2-difluoro[1,3]benzodioxole reacts with dimethylformamide under the action of n-butyl lithium and tetramethylethylenediamine to undergo electrophilic substitution reaction. After the reaction is completed, the reactant is added dropwise to dilute hydrochloric acid to quench, and the liquid is allowed to stand for separation. The organic phase is taken and the solvent is removed by reduced pressure distillation to obtain the product. The mother liquor refers to the aqueous phase obtained after standing. In the current prior art, the product in the mother liquor of the above production process cannot be recovered. The mother liquor is directly treated as lithium-containing wastewater, which causes serious economic losses and environmental pollution. Summary of the invention
[0007] The object of the present invention is to provide a mild, low-cost and industrially valuable method for treating the lithium-containing mother liquor of fludioxonil intermediate. The quenched and layered mother liquor of the obtained 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is subjected to secondary adsorption by a macroporous resin, and then eluted to obtain a high-content 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde. The tetramethylethylenediamine in the mother liquor is freed and recovered by potassium hydroxide, and the crude lithium carbonate is precipitated and recovered by potassium carbonate. The crude lithium carbonate is then purified to obtain refined lithium carbonate. The potassium hydroxide and potassium carbonate used in the mother liquor treatment process are recovered in the form of potassium chloride to achieve the purpose of material recovery in wastewater.
[0008] The chemical reaction equation involved in the present invention is as follows:
[0009]
[0010] A method for treating a lithium-containing mother liquor of a fludioxonil intermediate comprises the following steps:
[0011] 1) Pre-load the macroporous adsorption resin into the first resin adsorption column and the second resin adsorption column respectively, pass the quenched and layered mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde into the first resin adsorption column for primary resin adsorption, and then continue to pass through the second resin adsorption column for secondary resin adsorption, collect the adsorption liquid, and when 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is detected in the discharge, it is considered that the adsorption is saturated;
[0012] 2) The first resin adsorption column is subjected to primary elution with anhydrous methanol, and the primary eluate is continuously fed into the second resin adsorption column for secondary elution. When no 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is detected in the discharge, the elution is considered complete, and the secondary eluate is concentrated to obtain 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde, which is then recycled to regenerate the macroporous adsorption resin for reuse;
[0013] 3) Potassium hydroxide is added to the adsorption liquid in step 1) to release tetramethylethylenediamine, and a mixture of water and tetramethylethylenediamine is distilled off. The lithium-containing mother liquor remaining in the kettle is added with potassium hydroxide to the mixture of water and tetramethylethylenediamine, stirred, and then allowed to stand for separation. The upper layer of liquid is further refluxed with potassium hydroxide for dehydration, and distilled under reduced pressure to obtain tetramethyldiethylamine. The potassium hydroxide residue remaining in the kettle is used in the next batch;
[0014] 4) The lithium-containing mother liquor in step 3) is evaporated to precipitate potassium chloride, which is filtered to obtain potassium chloride solid and filtrate, potassium carbonate is added to the filtrate for precipitation, and crude lithium carbonate is obtained by filtering, deionized water is added to the crude lithium carbonate to prepare a suspension, CO2 is introduced to convert it into a lithium bicarbonate solution, and then refined lithium carbonate is obtained through filtering, heating decomposition, and rinsing steps.
[0015] Furthermore, the macroporous adsorption resin in step 1) is XDA-1, XDA-2, XDA-6 or XDA-8, and the mass concentration of the quenched and layered mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is 1.00-1.50%.
[0016] Furthermore, in step 1), the flow rate of the quenched and layered mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde passing through the first resin adsorption column and the second resin adsorption column is 10-30 g / min.
[0017] Furthermore, in step 2), the flow rate of anhydrous methanol is 10-25 g / min, the elution temperature of anhydrous methanol is 25-65°C, and the concentration temperature is 80-85°C.
[0018] Furthermore, in step 3), the mass concentration of tetramethylethylenediamine dihydrochloride in the adsorption solution is 10.00-15.00%.
[0019] Furthermore, in step 3), potassium hydroxide is added for neutralization at a temperature of 25-50°C, the pH after neutralization is 12-14, and the distillation temperature is 95-130°C.
[0020] Furthermore, in step 4), the mass concentration of lithium chloride in the filtrate is 2.00-5.00%.
[0021] Furthermore, in step 4), the precipitation temperature is 70-90°C, the CO2 introduction temperature is 15-40°C, and the heating decomposition temperature is 80-95°C.
[0022] Furthermore, in step 4), the mass ratio of crude lithium carbonate to deionized water is 1:15-30, and the CO2 flow rate is 50-80 g / h.
[0023] The beneficial effects of the present invention are:
[0024] During the synthesis of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde, a certain amount of the product cannot be precipitated in the aqueous phase, resulting in a low product yield. The mother liquor can be adsorbed and desorbed by a resin to recover 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde, thereby increasing the product yield. The tetramethylethylenediamine and lithium element (recovered in the form of lithium carbonate) in the mother liquor can be further recovered, and the potassium hydroxide and potassium carbonate used in the mother liquor treatment process can be recovered in the form of potassium chloride, which has significant economic benefits and good environmental benefits. DETAILED DESCRIPTION
[0025] The present invention is further described below in conjunction with embodiments, but the protection scope of the present invention is not limited thereto.
[0026] Example 1
[0027] The macroporous adsorption resin was pre-loaded into the first resin adsorption column and the second resin adsorption column, respectively. The resin used was XDA-1, the temperature was controlled at 25°C, the mass concentration of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde in the quenched and layered mother liquor was 1.12%, tetramethylethylenediamine dihydrochloride was 11.57%, and lithium chloride was 2.40%. 1200 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde lithium-containing mother liquor was taken into the first resin adsorption column for primary adsorption, and then continued to enter the second resin adsorption column for secondary adsorption. The primary adsorption and secondary adsorption flow rates were both controlled at 20 g / min. When 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was detected in the discharge, the adsorption was considered to be saturated. The temperature was controlled at 40°C, and 159 g of potassium hydroxide was slowly added to the adsorption liquid with stirring. The pH value was 13 when neutralization was completed. The temperature was raised to 110°C, and 304 g of a mixture of water and tetramethylethylenediamine was obtained by atmospheric distillation. The lithium-containing mother liquor (1) remained in the kettle. 159 g of potassium hydroxide was slowly added to the mixture of water and tetramethylethylenediamine with stirring. g potassium hydroxide, continue stirring for 0.5 h after the addition is completed, let stand and separate the liquids. The upper liquid is aqueous tetramethylethylenediamine (0.82% water content), and the lower layer is potassium hydroxide aqueous solution (2). Slowly add 59 g potassium hydroxide to the aqueous tetramethylethylenediamine while stirring, heat and reflux for 2 h, cool to room temperature, and dehydrate by vacuum distillation to obtain 69.8 g of finished tetramethylethylenediamine (0.07% water content). Potassium hydroxide residue (3) remains in the kettle.
[0028] The first resin adsorption column was subjected to primary elution with anhydrous methanol, and the primary eluent continued to enter the second resin adsorption column for secondary elution. The eluent flow rate was controlled at 20 g / min, and the elution temperature was 30°C. When no 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was detected in the discharge material, the elution was considered complete. The secondary eluent was concentrated at 80°C, and the concentrated condensate was methanol, which was used for the next batch of elution. After concentration, 13.2 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was obtained, and the regenerated macroporous adsorption resin was recycled.
[0029] Distill about 390 g of lithium-containing mother liquor (1), filter out 112.8 g of precipitated potassium chloride (wet), heat the filtrate to 50°C, add 50.2 g of potassium carbonate under stirring, and keep at 85°C for 1 h for precipitation. Wash the filter cake obtained by filtration with 60 g of water, filter out 31.3 g of filter cake (wet), dry to obtain 20.5 g of crude lithium carbonate, add concentrated hydrochloric acid dropwise to the filtrate, adjust the pH to 3, distill about 405 g of water under normal pressure, filter out 122.3 g of potassium chloride (wet), combine and dry to obtain 194.9 g of potassium chloride, and the filtrate is 269.6 g of lithium-containing residual liquid (4). Put 20.5 g of crude lithium carbonate into 410 g of deionized water, control the temperature at 25°C, and introduce CO2 under stirring (300 r / min) until the solution is clear (a small amount of floccules floats), with a CO2 flow rate of 60 g / h. Filter out the filter residue, and heat the filtrate to 90°C for 2 h for decomposition. The filtrate obtained by filtration was 407 g of purified mother liquor (5). The filter cake was rinsed with 3×30 g of deionized water, and 19.4 g of filter cake (wet) was obtained by filtration. After drying, 15.3 g of refined lithium carbonate was obtained.
[0030] Conclusion: 69.8 g of tetramethylethylenediamine was obtained, with a content of 99.5% and a yield of 81.8%; 13.2 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was obtained, with a content of 99.8% and a yield of 98.0%; 15.3 g of refined lithium carbonate was obtained, with a content of 99.2% and a yield of 61.0%; 194.9 g of potassium chloride was obtained, with a content of 98.2% and a yield of 72.1%.
[0031] Example 2
[0032] The macroporous adsorption resin is pre-loaded into the first resin adsorption column and the second resin adsorption column respectively. The resin used is XDA-2, the temperature is controlled at 25°C, the mass concentration of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde in the quenching and layering mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is 1.12%, tetramethylethylenediamine dihydrochloride is 11.57%, and lithium chloride is 2.40%. 1200 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde lithium-containing mother liquor was taken into the first resin adsorption column for primary adsorption, and then continued to enter the second resin adsorption column for secondary adsorption. The primary adsorption and secondary adsorption flow rates were both controlled at 20 g / min. When 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was detected in the discharge, it was considered that the adsorption was saturated. The temperature was controlled at 40° C., and the potassium hydroxide aqueous solution (2) in Example 1 was slowly added to the adsorption liquid with stirring. When the neutralization was completed, the pH was 13. The temperature was raised to 110° C., and 306 g of a mixture of water and tetramethylethylenediamine was obtained by atmospheric distillation. The lithium-containing mother liquor (6) remained in the kettle. The potassium hydroxide residue (3) in Example 1 and 100 g of potassium hydroxide were slowly added to the mixture of water and tetramethylethylenediamine under stirring. After the addition was completed, stirring was continued for 0.5 h, and allowed to stand for separation. The upper liquid was aqueous tetramethylethylenediamine (water content 0.84%), and the lower liquid was potassium hydroxide aqueous solution (7). 59 g of potassium hydroxide was slowly added to the aqueous tetramethylethylenediamine under stirring, and the mixture was heated under reflux for 2 h. The mixture was cooled to room temperature and distilled under reduced pressure to obtain 80.2 g of finished tetramethylethylenediamine (water content 0.07%). Potassium hydroxide residue (8) remained in the kettle.
[0033] The first resin adsorption column was subjected to primary elution with anhydrous methanol, and the primary eluent continued to enter the second resin adsorption column for secondary elution. The eluent flow rate was controlled at 15 g / min, and the elution temperature was 30°C. When no 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was detected in the discharge material, the elution was considered complete. The secondary eluent was concentrated at 80°C, and the concentrated condensate was methanol, which was used for the next batch of elution. After concentration, 12.9 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was obtained, and the regenerated macroporous adsorption resin was recycled.
[0034] About 610 g of water was distilled from the lithium-containing mother liquor (6), and 116.5 g of potassium chloride (wet) precipitated was removed by filtration. The filtrate was combined with the lithium-containing residual liquor (4) in Example 1, heated to 50°C, and 65 g of potassium carbonate was added under stirring. The mixture was kept at 85°C for 1 h for precipitation. The filter cake obtained by filtration was washed with 60 g of water, and 36.6 g of filter cake (wet) was obtained by filtration. The filter cake was dried to obtain 24.4 g of crude lithium carbonate. Concentrated hydrochloric acid was added dropwise to the filtrate to adjust the pH to 3. About 570 g of water was distilled under normal pressure, and 198.3 g of potassium chloride (wet) was removed by filtration. The mixture was combined and dried to obtain 261.1 g of potassium chloride. The filtrate was the lithium-containing residual liquor (9), totaling 356.3 g. 24.4 g of crude lithium carbonate was added to the purified mother liquor (5) in Example 1, and 80 g of deionized water was added. The temperature was controlled at 25°C, and CO2 was introduced under stirring (300 r / min) until the solution was clarified (a small amount of flocs floated). The CO2 flow rate was 65 g / h. The residue was removed by filtration, and the filtrate was heated to 90°C and decomposed for 2 h. The filtrate obtained by filtration was 482 g of purified mother liquor (10). The filter cake was rinsed with 3×30 g of deionized water, and 28.4 g of filter cake (wet) was obtained by filtration. After drying, 22.8 g of refined lithium carbonate was obtained.
[0035] Conclusion: 80.2 g of tetramethylethylenediamine was obtained, with a content of 99.5% and a yield of 94.0%; 12.9 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was obtained, with a content of 99.8% and a yield of 95.8%; 22.8 g of refined lithium carbonate was obtained, with a content of 99.2% and a yield of 90.8%; 261.1 g of potassium chloride was obtained, with a content of 98.2% and a yield of 91.1%.
[0036] Example 3
[0037] The macroporous adsorption resin is pre-loaded into the first resin adsorption column and the second resin adsorption column respectively. The resin used is XDA-6, the temperature is controlled at 25°C, the mass concentration of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde in the quenching and layering mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is 1.12%, tetramethylethylenediamine dihydrochloride is 11.57%, and lithium chloride is 2.40%. 1200 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde lithium-containing mother liquor was taken into the first resin adsorption column for primary adsorption, and then continued to enter the second resin adsorption column for secondary adsorption. The primary adsorption and secondary adsorption flow rates were both controlled at 25 g / min. When 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was detected in the discharge, it was considered that the adsorption was saturated. The temperature was controlled at 40° C., and the potassium hydroxide aqueous solution (7) in Example 2 was slowly added to the adsorption liquid with stirring. When the neutralization was completed, the pH was 13. The temperature was raised to 110° C., and 308 g of a mixture of water and tetramethylethylenediamine was obtained by atmospheric distillation. The lithium-containing mother liquor (11) remained in the kettle. The potassium hydroxide residue (8) in Example 2 and 100 g of potassium hydroxide were slowly added to the mixture of water and tetramethylethylenediamine under stirring. After the addition was completed, stirring was continued for 0.5 h, and allowed to stand for separation. The upper liquid was aqueous tetramethylethylenediamine (water content 0.85%), and the lower liquid was potassium hydroxide aqueous solution (12). 59 g of potassium hydroxide was slowly added to the aqueous tetramethylethylenediamine under stirring, and the mixture was heated to reflux for 2 h. The mixture was cooled to room temperature and distilled under reduced pressure to obtain 81.3 g of finished tetramethylethylenediamine (water content 0.07%). Potassium hydroxide residue (13) remained in the kettle.
[0038] The first resin adsorption column was subjected to primary elution with anhydrous methanol, and the primary eluent continued to enter the second resin adsorption column for secondary elution. The eluent flow rate was controlled at 20 g / min, and the elution temperature was 30°C. When no 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was detected in the discharge material, the elution was considered complete. The secondary eluent was concentrated at 80°C, and the concentrated condensate was methanol, which was used for the next batch of elution. After concentration, 13.3 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was obtained, and the regenerated macroporous adsorption resin was used in a circular manner.
[0039] About 610 g of water was distilled from the lithium-containing mother liquor (11), and 115.3 g of potassium chloride (wet) precipitated was removed by filtration. The filtrate was combined with the lithium-containing residual liquor (9) in Example 2, heated to 50°C, and 65 g of potassium carbonate was added under stirring. The mixture was kept at 85°C for 1 h for precipitation. The filter cake obtained by filtration was washed with 60 g of water, and 37.5 g of filter cake (wet) was obtained by filtration. After drying, 24.6 g of crude lithium carbonate was obtained. Concentrated hydrochloric acid was added dropwise to the filtrate to adjust the pH to 3. About 745 g of water was distilled under normal pressure, and 202.5 g of potassium chloride (wet) was removed by filtration. The mixture was combined and dried to obtain 263.6 g of potassium chloride. The filtrate was 277.1 g of lithium-containing residual liquor (14). 24.6 g of crude lithium carbonate was added to the purified mother liquor (10) in Example 2, and the temperature was controlled at 25°C. CO2 was introduced under stirring (300 r / min) until the solution was clear (a small amount of flocs floated). The CO2 flow rate was 60 g / h. The residue was removed by filtration, and the filtrate was heated to 90°C for 2 h for decomposition. The filtrate obtained by filtration was 475 g of purified mother liquor (10). The filter cake was rinsed with 3×30 g of deionized water, and 29.1 g of filter cake (wet) was obtained by filtration. After drying, 22.9 g of refined lithium carbonate was obtained.
[0040] Conclusion: 81.3 g of tetramethylethylenediamine was obtained, with a content of 99.5% and a yield of 95.3%; 13.3 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was obtained, with a content of 99.8% and a yield of 98.8%; 22.9 g of refined lithium carbonate was obtained, with a content of 99.2% and a yield of 91.2%; 263.6 g of potassium chloride was obtained, with a content of 98.2% and a yield of 92.0%.
[0041] Example 4
[0042] The macroporous adsorption resin is pre-loaded into the first resin adsorption column and the second resin adsorption column respectively. The resin used is XDA-6, the temperature is controlled at 25°C, the mass concentration of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde in the quenching and layering mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is 1.12%, tetramethylethylenediamine dihydrochloride is 11.57%, and lithium chloride is 2.40%. 1200 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde lithium-containing mother liquor was taken into the first resin adsorption column for primary adsorption, and then continued to enter the second resin adsorption column for secondary adsorption. The primary adsorption and secondary adsorption flow rates were both controlled at 20 g / min. When 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was detected in the discharge, it was considered that the adsorption was saturated. The temperature was controlled at 40° C., and the potassium hydroxide aqueous solution (12) in Example 3 was slowly added to the adsorption liquid with stirring. When the neutralization was completed, the pH was 13. The temperature was raised to 110° C., and 307 g of a mixture of water and tetramethylethylenediamine was obtained by atmospheric distillation. The lithium-containing mother liquor (16) remained in the kettle. The potassium hydroxide residue (13) in Example 3 and 100 g of potassium hydroxide were slowly added to the mixture of water and tetramethylethylenediamine under stirring. After the addition was completed, stirring was continued for 0.5 h, and allowed to stand for separation. The upper liquid was aqueous tetramethylethylenediamine (water content 0.84%), and the lower liquid was potassium hydroxide aqueous solution (17). 59 g of potassium hydroxide was slowly added to the aqueous tetramethylethylenediamine under stirring, and the mixture was heated to reflux for 2 h. The mixture was cooled to room temperature and distilled under reduced pressure to obtain 81.1 g of finished tetramethylethylenediamine (water content 0.07%). Potassium hydroxide residue (18) remained in the kettle.
[0043] The first resin adsorption column was subjected to primary elution with anhydrous methanol, and the primary eluent continued to enter the second resin adsorption column for secondary elution. The eluent flow rate was controlled at 20 g / min, and the elution temperature was 30°C. When no 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was detected in the discharge material, the elution was considered complete. The secondary eluent was concentrated at 80°C, and the concentrated condensate was methanol, which was used for the next batch of elution. After concentration, 13.2 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was obtained, and the regenerated macroporous adsorption resin was recycled.
[0044] About 610 g of water was distilled from the lithium-containing mother liquor (16), and 119.3 g of potassium chloride (wet) precipitated was removed by filtration. The filtrate was combined with the lithium-containing residual liquor (14) in Example 3, heated to 50°C, and 65 g of potassium carbonate was added under stirring. The mixture was kept at 85°C for 1 h for precipitation. The filter cake obtained by filtration was washed with 60 g of water, and 37.2 g of filter cake (wet) was obtained by filtration. The filter cake was dried to obtain 24.5 g of crude lithium carbonate. Concentrated hydrochloric acid was added dropwise to the filtrate to adjust the pH to 3. About 575 g of water was distilled under normal pressure, and 194.3 g of potassium chloride (wet) was removed by filtration. The mixture was combined and dried to obtain 259.9 g of potassium chloride. The filtrate was the lithium-containing residual liquor (14), totaling 362.3 g. 24.5 g of crude lithium carbonate was added to the purified mother liquor (15) in Example 3, and 10 g of deionized water was added. The temperature was controlled at 25°C, and CO2 was introduced under stirring (300 r / min) until the solution was clarified (a small amount of flocs floated). The CO2 flow rate was 65 g / h. The residue was removed by filtration, and the filtrate was heated to 90°C and decomposed for 2 h. The filtrate obtained by filtration was 481 g of purified mother liquor (10). The filter cake was rinsed with 3×30 g of deionized water, and 29.4 g of filter cake (wet) was obtained by filtration. 22.8 g of refined lithium carbonate was obtained by drying.
[0045] Conclusion: 81.1 g of tetramethylethylenediamine was obtained, with a content of 99.5% and a yield of 95.1%; 13.2 g of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde was obtained, with a content of 99.8% and a yield of 98.0%; 22.8 g of refined lithium carbonate was obtained, with a content of 99.2% and a yield of 90.8%; 259.9 g of potassium chloride was obtained, with a content of 98.2% and a yield of 90.7%.
Claims
1. A method for treating a lithium-containing mother liquor of a fludioxonil intermediate, characterized in that: The steps include: 1) Pre-load the macroporous adsorption resin into the first resin adsorption column and the second resin adsorption column respectively, pass the quenched and layered mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde into the first resin adsorption column for primary resin adsorption, and then continue to pass through the second resin adsorption column for secondary resin adsorption, collect the adsorption liquid, and when 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is detected in the discharge, it is considered that the adsorption is saturated; 2) The first resin adsorption column is subjected to primary elution with anhydrous methanol, and the primary eluate is continuously fed into the second resin adsorption column for secondary elution. When no 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is detected in the discharge, the elution is considered complete, and the secondary eluate is concentrated to obtain 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde, which is then recycled to regenerate the macroporous adsorption resin for reuse; 3) Potassium hydroxide is added to the adsorption liquid in step 1) to release tetramethylethylenediamine, and a mixture of water and tetramethylethylenediamine is distilled off. The lithium-containing mother liquor remaining in the kettle is added with potassium hydroxide to the mixture of water and tetramethylethylenediamine, stirred, and then allowed to stand for separation. The upper layer of liquid is further refluxed with potassium hydroxide for dehydration, and distilled under reduced pressure to obtain tetramethyldiethylamine. The potassium hydroxide residue remaining in the kettle is used in the next batch; 4) The lithium-containing mother liquor in step 3) is evaporated to precipitate potassium chloride, which is filtered to obtain potassium chloride solid and filtrate, potassium carbonate is added to the filtrate for precipitation, and crude lithium carbonate is obtained by filtering, deionized water is added to the crude lithium carbonate to prepare a suspension, CO2 is introduced to convert it into a lithium bicarbonate solution, and then refined lithium carbonate is obtained through filtering, heating decomposition, and rinsing steps.
2. The processing method according to claim 1, characterized in that The macroporous adsorption resin described in step 1) is XDA-1, XDA-2, XDA-6 or XDA-8, and the mass concentration of the quenched and layered mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde is 1.00-1.50%.
3. The processing method according to claim 1, characterized in that: In step 1), the flow rate of the quenched and layered mother liquor of 2,2-difluorobenzo[1,3]dioxole-4-carboxaldehyde passing through the first resin adsorption column and the second resin adsorption column is 10-30 g / min.
4. The processing method according to claim 1, characterized in that In step 2), the flow rate of anhydrous methanol is 10-25 g / min, the elution temperature of anhydrous methanol is 25-65°C, and the concentration temperature is 80-85°C.
5. The processing method according to claim 1, characterized in that: Step 3) The mass concentration of tetramethylethylenediamine dihydrochloride in the adsorption solution is 10.00-15.00%.
6. The processing method according to claim 1, characterized in that: Step 3) Add potassium hydroxide for neutralization at a temperature of 25-50°C. After neutralization, the pH is 12-14 and the distillation temperature is 95-130°C.
7. The processing method according to claim 1, characterized in that: Step 4) The mass concentration of lithium chloride in the filtrate is 2.00-5.00%.
8. The processing method according to claim 1, characterized in that: In step 4), the precipitation temperature is 70-90°C, the CO2 introduction temperature is 15-40°C, and the heating decomposition temperature is 80-95°C.
9. The processing method according to claim 1, characterized in that: In step 4), the mass ratio of crude lithium carbonate to deionized water is 1:15-30, and the CO2 flow rate is 50-80 g / h.