A welding equipment for gas boiler production

By designing welding equipment for components such as arc bases and annular grinding shells, the burr problem in gas boiler welding is solved, efficient grinding and debris removal is achieved, and the welding quality and stability are improved.

CN118143652BActive Publication Date: 2024-10-01JIANGSU NUOERXIN THERMAL ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410331198.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-03-22
Publication Date
2024-10-01
Estimated Expiration
2044-03-22

AI Technical Summary

Technical Problem

Existing gas boiler welding equipment cannot effectively remove burrs on the inner wall of the heat conduction chamber, causing air gaps and excessive weld seams to easily occur during welding, affecting the welding quality.

Method used

A welding equipment including an arc base, an annular base ring, a movable arm and a movable block is designed. It is equipped with a boiler inner ring grinding unit and a boiler inner wall debris removal unit. Through annular grinding shells, suction boxes and other components, , to achieve the grinding and debris removal of the inner wall of the heat conduction chamber and improve the welding quality.

Benefits of technology

Effectively remove burrs and debris on the inner wall of the heat conduction chamber, improve welding quality, reduce the problem of excessive air gaps and weld seams, and improve welding effects and equipment stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118143652B_ABST
    Figure CN118143652B_ABST
Patent Text Reader

Abstract

The invention discloses a welding device for gas boiler production, comprising an arc-shaped base, an annular base ring, a movable arm and a movable block. During use of the invention, the electric rotating shaft rotating end will drive the grinding block to perform cyclic grinding on the grinding part when rotating forward and reversely, so that the welding position is roughened, thereby improving the adhesion effect of the flux in the grinding area, and the air suction boxes on both sides of the top of the movable block will absorb the scattered debris, and the debris will enter the air suction cavity through the air intake grille, and the debris falling into the bottom of the air suction cavity will flow into the filter box under the guidance of the guide inclined plate, so that the scattered debris is further absorbed, and the debris collection effect is further improved, and the ejected hot gas will blow off the metal debris attached to the grinding area, and the hot gas will heat the ejected area by heat conduction, and after the inner wall of the heat conduction chamber cavity is preheated, the adhesion capacity of the flux and the solder will be further improved, thereby further improving the welding and assembly effect of the heat conduction chamber.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of boiler welding, in particular to welding equipment for producing gas boilers. Background Art

[0002] Gas boilers include gas-fired water boilers, gas-fired hot water boilers, gas-fired steam boilers, etc. Among them, gas-fired hot water boilers are also called gas-fired heating boilers and gas-fired bathing boilers. As the name suggests, gas-fired boilers refer to boilers whose fuel is gas. Gas boilers can be divided into natural gas boilers, city gas boilers, coke oven gas boilers, liquefied petroleum gas boilers and biogas boilers according to fuel; according to function, they can be divided into KS-Q gas-fired water boilers, CLHS / CWNS gas-fired hot water boilers (including gas-fired heating boilers and gas-fired bathing boilers), LHS / WNS gas-fired steam boilers, etc.; according to structure, they can be divided into vertical gas-fired boilers and horizontal gas-fired boilers; according to the flue gas flow, they can be divided into single-pass gas-fired boilers and three-pass gas-fired boilers. During the assembly process of the boiler, the heat transfer chamber is spliced, welded and installed. During the welding process, it is necessary to avoid excessive machining burrs on the inner wall of the heat transfer chamber, which will cause air gaps in the welding or excessive welds, resulting in poor air tightness of the heat transfer chamber.

[0003] In the prior art, a gas boiler inner wall welding device disclosed in publication number "CN209886933U" includes a box shell, a wiring pipe and a welding gun, wheel seats are arranged at the four corners of the lower end of the box shell, a universal wheel is arranged at the lower end of the wheel seat, a wheel lock is arranged on one side of the universal wheel, cooling fans are arranged on the two side walls of the box shell, a lifting rod is arranged in the middle of the upper end of the box shell, a transformer is arranged in the box shell, and a rectifier is arranged on one side of the transformer. The beneficial effect is that: the utility model can make the welding gun fit better with the inner wall of the boiler by arranging a supporting slide plate, so that the welding gun can better move along the weld to be welded, and the convenience of using the device is increased. By arranging a flaw detector and a flaw detection head, the device can detect the welding quality of the weld, so that the staff can adjust the operation mode according to the detection result, so as to better complete the welding work.

[0004] However, the existing technology still has major deficiencies, such as:

[0005] In the above-mentioned device and the prior art, when the heat transfer chamber is assembled and welded, it is impossible to perform annular grinding on the welding position, resulting in excessive excess burrs on the inner wall of the heat transfer chamber, affecting the welding effect. If the burrs on the inner wall of the heat transfer chamber can be removed by setting a grinding structure, burrs and debris will be generated during the grinding process. The burrs and debris will adhere to the inner wall of the heat transfer chamber in large quantities, especially accumulate in the bottom area of ​​the inner wall of the heat transfer chamber, resulting in the problem of too many air gaps and welds in the welding of this area. Summary of the invention

[0006] The object of the present invention is to provide a welding device for gas boiler production to solve the problems raised in the above background technology.

[0007] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: A welding device for gas boiler production, comprising an arc-shaped base, an annular base ring, a movable arm and a movable block, wherein the annular base ring is installed on the top surface of the arc-shaped base, an annular guide rail is installed on the inner wall of the annular base ring, an annular movable block is installed on the movable end of the annular guide rail, the movable arm is arranged on one side of the annular movable block, the movable block is arranged on the top of the movable arm, a welding gun head is installed in the central area of ​​the end of the movable block, an installation groove is arranged inside the movable block, a receiving groove is arranged at the end of the movable arm, a movable guide rail is installed in the receiving groove, and the movable block is installed on the movable end of the movable guide rail;

[0008] A boiler inner ring grinding unit, which is arranged on the outer surface of the welding gun head and is used to remove impurities and grind the surface of the welding position of the boiler inner wall before welding, so as to improve the adhesion of the flux and the flux material;

[0009] The boiler inner wall debris removal unit is arranged on one side of the movable block and is used to remove the metal debris remaining on the boiler inner wall after the grinding debris is removed, thereby reducing the adhesion of a large amount of metal debris caused by grinding and improving the welding and fixing effect between the boiler liner and the boiler inner wall.

[0010] Preferably, the boiler inner ring grinding unit comprises an annular grinding shell, a collecting groove is provided on the surface of the annular grinding shell, a grinding block is installed on the surface of the collecting groove, a grinding pattern is provided on the surface of the grinding block, the grinding blocks are annularly installed in several groups, a rotating shaft is rotatably installed inside the installation groove, a transmission arm is fixedly sleeved on the surface of the rotating shaft, one end of the transmission arm is fixed to the inner ring of the annular grinding shell, a driving arm is also sleeved on the surface of the rotating shaft, a first fixed seat is installed on one end of the driving arm, a torsion spring is sleeved on one end of the rotating shaft, two ends of the torsion spring are respectively fixed to one side of the inner wall of the collecting groove and one side of the transmission arm, a motor fixing frame is installed on one side of the outer side of the movable block, an electric winding roller is installed on the motor fixing frame, a linkage steel cable is sleeved on the electric winding roller, and one end of the linkage steel cable is fixed to one side of the first fixed seat.

[0011] Preferably, the boiler inner wall debris removal unit includes an air suction box, the air suction boxes are symmetrically installed on both sides of the top of the movable block, an air suction cavity is arranged in the air suction box, a guide inclined plate is installed at the bottom of the air suction cavity, an electromagnetic heating rod is installed in the air suction cavity, and the electromagnetic heating rods are arranged in several groups at intervals, an air intake grille is installed outside the air suction cavity, an air intake groove is arranged on the surface of the air intake grille, an exhaust groove is arranged on one side of the air suction box, a filter box is installed outside the exhaust groove, an injection unit is connected between two groups of the filter boxes, and injection ducts are installed on the surface of the injection unit at intervals, an air storage box is installed on the inner wall of the annular polishing shell, the air storage boxes are symmetrically arranged in two groups, and the two groups of the air storage boxes are connected by an air guide pipe, wherein the air guide pipe is installed on the inner wall of the annular polishing shell through a duct rack, and an air supply hose is connected to one side of the air suction box, and the air supply hose is connected to one of the air suction boxes.

[0012] Preferably, the inner bottom of the installation groove is configured to be a concave arc shape.

[0013] Preferably, a fixed clamping plate is installed on the inner wall of the annular base ring, an electric rotating shaft is installed in the central area of ​​the fixed clamping plate, the rotating end on one side of the electric rotating shaft is fixed to one side of the movable arm, a strip pressure plate is installed on the rotating end on the other side of the electric rotating shaft, and an arc-shaped limiting plate is installed at the bottom of the strip pressure plate.

[0014] Preferably, an arc-shaped placement plate is installed on one side of the fixed clamping plate, a partition plate is installed in the central area of ​​the arc-shaped placement plate, a through groove is provided on the surface of the partition plate, the arc-shaped limit plate slides through the inside of the through groove, and a first telescopic airbag and a second telescopic airbag are provided on both sides of the partition plate.

[0015] Preferably, a first air supply box is installed on one side of the arc base, and a second air supply box is installed on the other side of the arc base. A first air supply pipe is connected to one side of the first telescopic airbag, and a second air supply pipe is connected to one side of the second telescopic airbag. The first air supply pipe is connected to the first air supply box, and the second air supply pipe is connected to the second air supply box.

[0016] Preferably, a first pneumatic telescopic rod is installed on one side of the first air supply box, the first pneumatic telescopic rod is installed on one side of the arc base, a first arc support block is installed on the output end of the first pneumatic telescopic rod, and an adsorption unit is embedded in the bottom of the arc base.

[0017] Preferably, a second pneumatic telescopic rod is installed on one side of the second air supply box, the second pneumatic telescopic rod is installed on one side of the arc-shaped base, and a second arc-shaped support block is installed on the output end of the second pneumatic telescopic rod.

[0018] Preferably, the bottom of the second arc-shaped support block and the first arc-shaped support block are also rollingly inlaid with supporting balls, and the bottom of the arc-shaped base is rollingly inlaid with moving balls.

[0019] Compared with the prior art, the present invention has the following beneficial effects:

[0020] 1. The arc base can smoothly reciprocate on the inner wall of the heat transfer chamber cavity through the provided moving ball. During the movement, the first arc support block and the second arc support block on both sides of the arc base will provide support for both sides of the arc base during the movement of the arc base. When the arc base moves to the welding position, the operator can fix the arc base on the inner wall of the heat transfer chamber cavity by magnetic attraction through the provided adsorption unit, and then start the moving guide rail to move the movable block out of the storage groove. The movable block will push the annular grinding shell close to the inner wall of the heat transfer chamber cavity until the grinding block is attached thereto, and then start the electric shaft to perform intermittent forward and reverse rotation. When the electric shaft rotates forward and reversely, it will drive the grinding block to perform cyclic grinding on the grinding part, so that the welding position is roughened, thereby improving the flux adhesion effect in the grinding area, so as to improve the welding assembly effect of the heat transfer chamber;

[0021] 2. During the grinding process, the grinding block continuously contacts and roughens the inner wall of the heat conduction chamber cavity. Part of the debris generated by the roughening will fall into the collection groove on the surface of the annular grinding shell. When the annular grinding shell is oscillating in a cycle, the metal debris in the collection groove will fall into the deep part of the collection groove along the inner wall of the collection groove, and part of the debris will be scattered from the outside of the annular grinding shell. The suction boxes on both sides of the top of the movable block will absorb the scattered debris, and the debris will enter the suction cavity through the air intake grille. The debris that falls into the bottom of the suction cavity will flow into the filter box under the guidance of the guide ramp, so that the scattered debris is further absorbed, further improving the debris collection effect;

[0022] 3. The electromagnetic heating rod in the air intake cavity will heat the incoming gas, and the gas will be injected into the jet unit through the filter box. The jet unit will spray toward the grinding area of ​​the inner wall of the heat transfer chamber through the air guide pipe. The ejected hot gas will blow off the metal debris attached to the grinding area. At the same time, the hot gas will conduct heat conduction to the spraying area. After the inner wall of the heat transfer chamber cavity is preheated, the adhesion of the flux and solder will be further improved, thereby further improving the welding and assembly effect of the heat transfer chamber;

[0023] 4. During the grinding process, the strip pressure plate will rotate with the rotation end of the electric shaft. When the strip pressure plate rotates in the forward direction, the strip pressure plate will squeeze the first telescopic airbag to contract and discharge gas outward during the rotation process. The gas in the first telescopic airbag will be injected into the first air supply box through the first air supply pipe. The first air supply box injects the gas into the first pneumatic telescopic rod, so that the output end of the first pneumatic telescopic rod will expand outward. The output end of the first pneumatic telescopic rod will push the first arc-shaped support block to expand outward, thereby improving the stability of the inner wall of the heat transfer chamber during the forward grinding process. When the strip pressure plate rotates reversely, the strip pressure plate will squeeze the second telescopic airbag to contract and discharge gas outward during the rotation process, and the gas in the second telescopic airbag will be injected into the second air supply box through the second air supply pipe, and the second air supply box will inject the gas into the second pneumatic telescopic rod, so that the output end of the second pneumatic telescopic rod will expand outward, and the output end of the second pneumatic telescopic rod will push the second arc-shaped support block to expand outward, thereby improving the stability during the reverse grinding of the inner wall of the heat transfer chamber cavity, while improving the stability of the device during welding, and further improving the welding effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is an overall schematic diagram of the device of the present invention;

[0025] Figure 2 It is an overall exploded view of the device of the present invention;

[0026] Figure 3 It is a schematic diagram of the arc-shaped placement plate in the present invention;

[0027] Figure 4 It is a partial schematic diagram of the movable arm and movable block in the present invention;

[0028] Figure 5 It is a partial schematic diagram of the jet unit in the present invention;

[0029] Figure 6 It is a partial exploded view of the movable block in the present invention;

[0030] Figure 7 It is a partial schematic diagram of the first telescopic airbag and the second telescopic airbag in the present invention;

[0031] Figure 8 It is a schematic diagram of the adsorption unit and the supporting ball part in the present invention;

[0032] Fig. 9 It is a schematic diagram of the air supply hose part of the present invention;

[0033] Fig.10 It is a partial schematic diagram of the gas storage box in the present invention.

[0034] In the figure: 1, arc base; 11, moving ball; 2, annular base ring; 21, annular guide rail; 22, annular moving block; 23, fixed card plate; 24, electric shaft; 25, strip pressure plate; 26, arc limit plate; 3, movable arm; 31, storage slot; 32, moving guide rail; 4, movable block; 41, installation slot; 411, shaft; 412, transmission arm; 413, torsion spring; 414, driving arm; 415, first fixed seat; 42, annular grinding shell; 421, collecting tank; 43, grinding block; 44, jet unit; 441, filter box; 442, jet duct; 45, suction box; 451, suction cavity; 452, air intake grille; 453, electromagnetic heating Hot rod; 454, guide ramp; 455, exhaust groove; 456, air inlet groove; 46, motor fixing bracket; 461, electric winding roller; 462, linkage steel cable; 47, air storage box; 471, air guide tube; 472, catheter rack; 48, air supply hose; 5, first arc-shaped support block; 51, first pneumatic telescopic rod; 52, first air supply box; 6, second arc-shaped support block; 61, second pneumatic telescopic rod; 62, second air supply box; 7, arc-shaped placement plate; 71, partition plate; 711, through groove; 72, first telescopic air bag; 721, first air supply pipe; 73, second telescopic air bag; 731, second air supply pipe; 8, welding gun head; 9, adsorption unit; 91, support ball. DETAILED DESCRIPTION

[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0036] See also Figure 1-10 , the present invention provides a technical solution:

[0037] Embodiment 1: A welding device for gas boiler production: comprising an arc-shaped base 1, an annular base ring 2, a movable arm 3 and a movable block 4, the annular base ring 2 is installed on the top surface of the arc-shaped base 1, an annular guide rail 21 is installed on the inner wall of the annular base ring 2, an annular movable block 22 is installed on the movable end of the annular guide rail 21, the movable arm 3 is arranged on one side of the annular movable block 22, the movable block 4 is arranged on the top of the movable arm 3, a welding gun head 8 is installed in the central area of ​​the end of the movable block 4, an installation groove 41 is arranged inside the movable block 4, a receiving groove 31 is arranged at the end of the movable arm 3, a movable guide rail 32 is installed in the receiving groove 31, and the movable block 4 is installed on the movable end of the movable guide rail 32;

[0038] A fixed clamping plate 23 is installed on the inner wall of the annular base ring 2, and an electric shaft 24 is installed in the central area of ​​the fixed clamping plate 23. The rotating end of one side of the electric shaft 24 is fixed to one side of the movable arm 3, and a strip pressure plate 25 is installed on the rotating end of the other side of the electric shaft 24. An arc-shaped limit plate 26 is installed at the bottom of the strip pressure plate 25;

[0039] In this embodiment, the arc base 1 can smoothly reciprocate on the inner wall of the heat transfer chamber cavity through the provided moving ball 11. During the movement, the first arc support block 5 and the second arc support block 6 on both sides of the arc base 1 will provide support for both sides of the arc base 1 during the movement of the arc base 1. When the arc base 1 moves to the welding position, the operator can magnetically fix the arc base 1 on the inner wall of the heat transfer chamber cavity through the provided adsorption unit 9, and then start the moving guide rail 32 to move the movable block 4 out of the storage groove 31. The movable block 4 will push the annular grinding shell 42 close to the inner wall of the heat transfer chamber cavity until the grinding block 43 is attached thereto, and then start the electric shaft 24 for intermittent forward and reverse rotation. When the rotating end of the electric shaft 24 is forward and reversed, it will drive the grinding block 43 to cyclically grind the grinding part, so that the welding position is roughened, thereby improving the flux adhesion effect in the grinding area, so as to improve the welding assembly effect of the heat transfer chamber.

[0040] The boiler inner ring grinding unit is arranged on the outer surface of the welding gun head 8, and is used to remove impurities and grind the surface of the welding position of the inner wall of the boiler before welding, so as to improve the adhesion ability of the flux and the flux material;

[0041] The boiler inner ring grinding unit comprises an annular grinding shell 42, a collecting groove 421 is arranged on the surface of the annular grinding shell 42, a grinding block 43 is installed on the surface of the collecting groove 421, and a grinding pattern is arranged on the surface of the grinding block 43. The grinding blocks 43 are annularly installed in a plurality of groups, and a rotating shaft 411 is rotatably installed inside the installation groove 41. A transmission arm 412 is fixedly sleeved on the surface of the rotating shaft 411. One end of the transmission arm 412 is fixed to the inner ring of the annular grinding shell 42, and a driving arm 412 is also sleeved on the surface of the rotating shaft 411. 14, a first fixed seat 415 is installed at one end of the driving arm 414, a torsion spring 413 is sleeved at one end of the rotating shaft 411, and two ends of the torsion spring 413 are respectively fixed to one side of the inner wall of the collecting tank 421 and one side of the transmission arm 412, a motor fixing frame 46 is installed at one side of the outer side of the movable block 4, an electric winding roller 461 is installed on the motor fixing frame 46, and a linkage steel cable 462 is sleeved on the electric winding roller 461, and one end of the linkage steel cable 462 is fixed to one side of the first fixed seat 415.

[0042] The inner bottom of the installation groove 41 is configured to be a concave arc shape.

[0043] In this embodiment, during the grinding process, the grinding block 43 continuously contacts and roughens the inner wall of the heat conduction chamber cavity, and a portion of the debris generated by the grinding will fall into the collecting groove 421 on the surface of the annular grinding shell 42. When the annular grinding shell 42 is oscillating in a cycle, the metal debris in the collecting groove 421 will fall into the deep part of the collecting groove 421 along the inner wall of the collecting groove 421, and a portion of the debris will be scattered from the outside of the annular grinding shell 42. The air suction boxes 45 on both sides of the top of the movable block 4 will absorb the scattered debris, and the debris will enter the air suction chamber 451 through the air intake grille 452. The debris that falls into the bottom of the air suction chamber 451 will flow into the filter box 441 under the guidance of the guide ramp 454, so that the scattered debris is further absorbed, further improving the debris collection effect.

[0044] The boiler inner wall debris removal unit is arranged on one side of the movable block 4 and is used to remove the metal debris remaining on the boiler inner wall after the grinding debris is removed, thereby reducing the adhesion of a large amount of metal debris caused by grinding and improving the welding and fixing effect between the boiler liner and the boiler inner wall.

[0045] The boiler inner wall debris removal unit includes an air suction box 45, which is symmetrically installed on both sides of the top of the movable block 4, and an air suction chamber 451 is arranged in the air suction box 45, and a guide inclined plate 454 is installed at the bottom of the air suction chamber 451, and an electromagnetic heating rod 453 is installed in the air suction chamber 451, and the electromagnetic heating rod 453 is arranged in a plurality of groups at intervals, and an air intake grille 452 is installed outside the air suction chamber 451, and an air intake groove 456 is arranged on the surface of the air intake grille 452, and an exhaust groove 455 is arranged on one side of the air suction box 45, and the exhaust groove 45 A filter box 441 is installed on the outside, and an air jet unit 44 is connected between two groups of filter boxes 441. Air jet ducts 442 are installed on the surface of the air jet unit 44 at intervals. An air storage box 47 is installed on the inner wall of the annular polishing shell 42. The air storage boxes 47 are symmetrically arranged in two groups. The two groups of air storage boxes 47 are connected through an air guide pipe 471, wherein the air guide pipe 471 is installed on the inner wall of the annular polishing shell 42 through a duct frame 472. One side of an air suction box 45 is connected to an air supply hose 48, and the air supply hose 48 is connected to an air suction box 45.

[0046] In this embodiment, the jet unit 44 may be composed of an air pump and a jet chamber. This technology is well known to those skilled in the art and will not be described in detail herein.

[0047] The electromagnetic heating rod 453 in the air intake cavity 451 will heat the incoming gas, and the gas will be injected into the jet unit 44 through the filter box 441. The jet unit 44 will spray toward the grinding area of ​​the inner wall of the heat transfer chamber cavity through the air guide pipe 471. The ejected hot gas will blow off the metal debris attached to the grinding area. At the same time, the hot gas will heat the spraying area by heat conduction. After the inner wall of the heat transfer chamber cavity is preheated, the adhesion ability of the flux and solder will be further improved, thereby further improving the welding and assembly effect of the heat transfer chamber. Embodiment 2:

[0048] This embodiment is based on the first embodiment and takes into account that the entire device will vibrate during grinding, causing the device to shake during grinding, and causing the flux and solder to separate during the welding process. Therefore, an auxiliary support structure is provided in this embodiment to ensure that the auxiliary support structure is unfolded during the grinding process, reduce the vibration frequency of the device during forward and reverse grinding, and prevent the flux and solder from separating due to vibration.

[0049] An arc-shaped placement plate 7 is installed on one side of the fixed clamping plate 23, and a partition plate 71 is installed in the central area of ​​the arc-shaped placement plate 7. A through groove 711 is arranged on the surface of the partition plate 71. The arc-shaped limiting plate 26 slides through the inside of the through groove 711. A first telescopic airbag 72 and a second telescopic airbag 73 are arranged on both sides of the partition plate 71.

[0050] A first air supply box 52 is installed on one side of the arc base 1, and a second air supply box 62 is installed on the other side of the arc base 1. A first air supply pipe 721 is connected to one side of the first telescopic air bag 72, and a second air supply pipe 731 is connected to one side of the second telescopic air bag 73. The first air supply pipe 721 is connected to the first air supply box 52, and the second air supply pipe 731 is connected to the second air supply box 62.

[0051] A first pneumatic telescopic rod 51 is installed on one side of the first air supply box 52 . The first pneumatic telescopic rod 51 is installed on one side of the arc-shaped base 1 . A first arc-shaped support block 5 is installed on the output end of the first pneumatic telescopic rod 51 . An adsorption unit 9 is embedded in the bottom of the arc-shaped base 1 .

[0052] A second pneumatic telescopic rod 61 is installed on one side of the second air supply box 62 . The second pneumatic telescopic rod 61 is installed on one side of the arc-shaped base 1 . A second arc-shaped support block 6 is installed on the output end of the second pneumatic telescopic rod 61 .

[0053] Support balls 91 are rollingly embedded in the bottom of the second arc-shaped support block 6 and the first arc-shaped support block 5 , and moving balls 11 are rollingly embedded in the bottom of the arc-shaped base 1 .

[0054] In this embodiment, during the grinding process, the strip pressure plate 25 will rotate along with the rotation end of the electric shaft 24. When the strip pressure plate 25 rotates forward, the strip pressure plate 25 will squeeze the first telescopic airbag 72 to contract and discharge gas outward during the rotation process. The gas in the first telescopic airbag 72 will be injected into the first air supply box 52 through the first air supply pipe 721. The first air supply box 52 injects the gas into the first pneumatic telescopic rod 51, so that the output end of the first pneumatic telescopic rod 51 is expanded outward. The output end of the first pneumatic telescopic rod 51 will push the first arc-shaped support block 5 to expand outward, thereby improving the forward grinding process of the inner wall of the heat transfer chamber cavity. In order to improve the stability of the heat transfer chamber, when the strip pressure plate 25 rotates in the reverse direction, the strip pressure plate 25 will squeeze the second telescopic airbag 73 to contract and discharge the gas outward during the rotation process, and the gas in the second telescopic airbag 73 will be injected into the second gas supply box 62 through the second gas supply pipe 731, and the second gas supply box 62 will inject the gas into the second pneumatic telescopic rod 61, so that the output end of the second pneumatic telescopic rod 61 will expand outward, and the output end of the second pneumatic telescopic rod 61 will push the second arc-shaped support block 6 to expand outward, thereby improving the stability during the reverse grinding of the inner wall of the heat transfer chamber cavity, and at the same time improving the stability of the device during welding, and further improving the welding effect.

[0055] Working principle: When the device is in use, the operator first places the device into the heat transfer chamber, and adjusts the position of the arc base 1 on the inner wall of the heat transfer chamber cavity by means of the movable ball 11 and the support ball 91. During the movement, the first arc support block 5 and the second arc support block 6 on both sides of the arc base 1 will provide support for both sides of the arc base 1 during the movement of the arc base 1. When the arc base 1 moves to the welding position, the operator can magnetically fix the arc base 1 on the inner wall of the heat transfer chamber cavity by means of the adsorption unit 9, and then start the movable guide rail 32 to move the movable block 4 out of the storage groove 31. The movable block 4 will push the annular grinding shell 42 close to the inner wall of the heat transfer chamber cavity until the grinding block 43 fits on it, and then start the electric The rotating shaft 24 rotates intermittently in forward and reverse directions. When the rotating end of the electric rotating shaft 24 rotates forward and reversely, it will drive the grinding block 43 to perform cyclic grinding on the grinding part, so that the welding position is roughened, thereby improving the flux adhesion effect in the grinding area, so as to improve the welding and assembly effect of the heat conduction chamber. The grinding block 43 continuously contacts and roughens the inner wall of the heat conduction chamber cavity. A part of the debris generated by the roughening will fall into the collecting groove 421 on the surface of the annular grinding shell 42. When the annular grinding shell 42 is cyclically swung, the metal debris in the collecting groove 421 will fall into the deep part of the collecting groove 421 along the inner wall of the collecting groove 421, and a part of the debris will be scattered from the outside of the annular grinding shell 42. The suction boxes 45 on both sides of the top of the movable block 4 will absorb the scattered debris, and the debris will pass through the air intake grille 4 52 enters the suction chamber 451, and the debris falling into the bottom of the suction chamber 451 will flow into the filter box 441 under the guidance of the guide inclined plate 454, so that the scattered debris will be further adsorbed, further improving the debris collection effect, and the strip pressure plate 25 will follow the rotation driven by the rotating end of the electric shaft 24. When the strip pressure plate 25 rotates forward, the strip pressure plate 25 will squeeze the first telescopic airbag 72 to contract and discharge gas outward during the rotation process, and the gas in the first telescopic airbag 72 will be injected into the first air supply box 52 through the first air supply pipe 721. The first air supply box 52 injects the gas into the first pneumatic telescopic rod 51, so that the output end of the first pneumatic telescopic rod 51 is expanded outward, and the output end of the first pneumatic telescopic rod 51 pushes the first arc-shaped support block 5 outward The second air supply box 62 is used to inject gas into the second pneumatic telescopic rod 61, so that the output end of the second pneumatic telescopic rod 61 is expanded outward, and the output end of the second pneumatic telescopic rod 61 pushes the second arc-shaped support block 6 to expand outward, thereby improving the stability of the inner wall of the heat conduction chamber cavity during the reverse grinding process, and at the same time improving the stability of the device during welding, and further improving the welding effect. The electromagnetic heating rod 453 in the air suction chamber 451 heats the incoming gas.The gas is injected into the jet unit 44 through the filter box 441, and the jet unit 44 sprays toward the grinding area of ​​the inner wall of the heat transfer chamber through the air guide pipe 471. The ejected hot gas will blow off the metal debris attached to the grinding area, and the hot gas will heat the spray area by heat conduction. After the inner wall of the heat transfer chamber cavity is preheated, the adhesion of the flux and solder will be further improved, thereby further improving the welding and assembly effect of the heat transfer chamber.

[0056] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A welding device for gas boiler production, characterized in that: The invention comprises an arc-shaped base (1), an annular base ring (2), a movable arm (3) and a movable block (4), wherein the annular base ring (2) is mounted on the top surface of the arc-shaped base (1), an annular guide rail (21) is mounted on the inner wall of the annular base ring (2), an annular movable block (22) is mounted on the movable end of the annular guide rail (21), the movable arm (3) is arranged on one side of the annular movable block (22), the movable block (4) is arranged on the top of the movable arm (3), a welding gun head (8) is mounted in the central area of ​​the end of the movable block (4), a mounting groove (41) is arranged inside the movable block (4), a receiving groove (31) is arranged at the end of the movable arm (3), a movable guide rail (32) is mounted in the receiving groove (31), and the movable block (4) is mounted on the movable end of the movable guide rail (32); A boiler inner ring grinding unit, the boiler inner ring grinding unit being arranged on the outer surface of the welding gun head (8) and being used for removing impurities and grinding the surface of the welding position of the boiler inner wall before welding, so as to improve the adhesion of the soldering flux and the soldering material; The boiler inner ring grinding unit comprises an annular grinding shell (42), a collecting groove (421) is arranged on the surface of the annular grinding shell (42), a grinding block (43) is installed on the surface of the collecting groove (421), a grinding pattern is arranged on the surface of the grinding block (43), the grinding blocks (43) are annularly installed in a plurality of groups, a rotating shaft (411) is rotatably installed inside the installation groove (41), a transmission arm (412) is fixedly sleeved on the surface of the rotating shaft (411), one end of the transmission arm (412) is fixed to the inner ring of the annular grinding shell (42), and a driving arm (412) is also sleeved on the surface of the rotating shaft (411). 4), a first fixed seat (415) is installed at one end of the driving arm (414), a torsion spring (413) is sleeved at one end of the rotating shaft (411), two ends of the torsion spring (413) are respectively fixed to one side of the inner wall of the collecting tank (421) and one side of the transmission arm (412), a motor fixing frame (46) is installed at one side of the outer side of the movable block (4), an electric winding roller (461) is installed on the motor fixing frame (46), a linkage steel cable (462) is sleeved on the electric winding roller (461), and one end of the linkage steel cable (462) is fixed to one side of the first fixed seat (415); A boiler inner wall debris removal unit, the boiler inner wall debris removal unit being arranged on one side of the movable block (4) and being used to remove metal debris remaining on the boiler inner wall after the grinding debris is removed, thereby reducing the adhesion of a large amount of metal debris generated by grinding and improving the welding and fixing effect between the boiler liner and the boiler inner wall; The boiler inner wall debris removal unit comprises an air suction box (45), the air suction box (45) being symmetrically mounted on both sides of the top of the movable block (4), an air suction chamber (451) being arranged in the air suction box (455), a guide inclined plate (454) being mounted at the bottom of the air suction chamber (451), an electromagnetic heating rod (453) being mounted in the air suction chamber (451), the electromagnetic heating rods (453) being arranged in a plurality of groups at intervals, an air intake grille (452) being mounted outside the air suction chamber (451), an air intake groove (456) being mounted on the surface of the air intake grille (452), an exhaust groove (455) being mounted on one side of the air suction box (45), the exhaust groove (455) being mounted on the inner side of the air suction chamber (451), and the exhaust groove (456) being mounted on the inner side of the air suction chamber (451). 5) A filter box (441) is installed on the outside, and an air jet unit (44) is connected between two groups of the filter boxes (441). Air jet ducts (442) are installed on the surface of the air jet unit (44) at intervals. An air storage box (47) is installed on the inner wall of the annular polishing shell (42). The air storage boxes (47) are symmetrically arranged in two groups. The two groups of air storage boxes (47) are connected through an air guide tube (471), wherein the air guide tube (471) is installed on the inner wall of the annular polishing shell (42) through a duct frame (472). One side of one of the air suction boxes (45) is connected to an air supply hose (48), and the air supply hose (48) is connected to one of the air suction boxes (45).

2. A welding device for gas boiler production according to claim 1, characterized in that: The inner bottom of the installation groove (41) is configured to be an inwardly concave arc shape.

3. A welding device for gas boiler production according to claim 1, characterized in that: A fixed clamping plate (23) is installed on the inner wall of the annular base ring (2), an electric rotating shaft (24) is installed in the central area of ​​the fixed clamping plate (23), a rotating end on one side of the electric rotating shaft (24) is fixed to one side of the movable arm (3), a strip-shaped pressing plate (25) is installed on the rotating end on the other side of the electric rotating shaft (24), and an arc-shaped limiting plate (26) is installed at the bottom of the strip-shaped pressing plate (25).

4. A welding device for gas boiler production according to claim 3, characterized in that: An arc-shaped placement plate (7) is installed on one side of the fixed clamping plate (23), a partition plate (71) is installed in the central area of ​​the arc-shaped placement plate (7), a through groove (711) is provided on the surface of the partition plate (71), the arc-shaped limit plate (26) slides through the inside of the through groove (711), and a first telescopic airbag (72) and a second telescopic airbag (73) are provided on both sides of the partition plate (71).

5. A welding device for gas boiler production according to claim 4, characterized in that: A first air supply box (52) is mounted on one side of the arc-shaped base (1), and a second air supply box (62) is mounted on the other side of the arc-shaped base (1); a first air supply pipe (721) is connected to one side of the first telescopic airbag (72), and a second air supply pipe (731) is connected to one side of the second telescopic airbag (73); the first air supply pipe (721) is connected to the first air supply box (52), and the second air supply pipe (731) is connected to the second air supply box (62).

6. A welding device for gas boiler production according to claim 5, characterized in that: A first pneumatic telescopic rod (51) is connected to one side of the first air supply box (52), the first pneumatic telescopic rod (51) is installed on one side of the arc-shaped base (1), a first arc-shaped support block (5) is installed on the output end of the first pneumatic telescopic rod (51), and an adsorption unit (9) is embedded in the bottom of the arc-shaped base (1).

7. A welding device for gas boiler production according to claim 6, characterized in that: A second pneumatic telescopic rod (61) is connected to one side of the second air supply box (62), the second pneumatic telescopic rod (61) is installed on one side of the arc-shaped base (1), and a second arc-shaped support block (6) is installed on the output end of the second pneumatic telescopic rod (61).

8. A welding device for gas boiler production according to claim 7, characterized in that: The bottom of the second arc-shaped support block (6) and the first arc-shaped support block (5) are also rollingly inlaid with support balls (91), and the bottom of the arc-shaped base (1) is rollingly inlaid with moving balls (11).