Resource utilization method of epoxy resin waste liquid

Through wet catalytic oxidation and targeted adsorption systems, combined with catalyst recovery processing, the resource utilization of NaCl and catalysts in epoxy resin waste liquid is solved, efficient wastewater treatment and resource recycling are achieved, and environmental pollution and resource waste are reduced.

CN118724310AInactive Publication Date: 2024-10-01BEIJING BIOTECHINA ENVIRONMENT CORP

Patent Information

Application Number
CN202310335946.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The high-salt and high-organic waste liquid produced by the industrial production of epoxy resin is difficult to process, leading to environmental pollution and resource waste. It is difficult to achieve effective resource and energy recycling with existing technology.

Method used

Wet catalytic oxidation, reaction tank treatment, inclined tube precipitation/ultrafiltration, targeted adsorption system and catalyst recovery treatment are adopted. The pH is adjusted through CuCl2 catalyst and sodium hydroxide, NaCl and catalyst are separated and recovered, and the resource utilization of waste liquid is realized.

Benefits of technology

It achieves effective treatment of high-salt wastewater, saves resources and energy, avoids environmental pollution, and improves the clean production level and resource utilization efficiency of the epoxy resin industry.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118724310A_ABST
    Figure CN118724310A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of industrial production waste liquid treatment, and particularly provides a resource utilization method of epoxy resin waste liquid. The main process or process comprises wet catalytic oxidation (CWO), reaction tank treatment, inclined tube precipitation / ultrafiltration, targeted adsorption I and targeted adsorption II, and is provided with catalyst recovery treatment. The method is simple and effective, salt and organic matter can be separated, and a solution is provided for treatment of high-salt and high-organic matter waste liquid. The purified and recycled salt can be returned to the front-end production process, so that resources and energy can be saved, higher benefits can be created, resource utilization can be realized, and the problems of environmental pollution and the like can be avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of industrial production waste liquid treatment, and specifically provides a resource utilization method for epoxy resin waste liquid. Background Art

[0002] There are many ways to produce epoxy resins in the industry. The main differences lie in the order of the main chemical reactions, the time of adding catalysts, the recovery of raw materials, etc. Currently, the most widely used epoxy resin in industry is bisphenol A. The production of 1 ton of epoxy resin will produce 10 to 16 tons of waste liquid, and its total organic carbon is as high as 4000 to 6000 mg / L. There are three main types of pollutants in the waste liquid: the first is organic matter, which comes from aged resins (macromolecular waste polymers) generated by additional reactions, organic hydrolysis products, organic solvents and extracts, such as phenol, acetone, toluene, butanol, glycerol, etc.; the second is inorganic matter, such as NaCl, NaOH, Na2CO3, Na2HPO4, etc.; the third is the catalyst added during the production process, such as Cu 2+ wait.

[0003] Therefore, as the production capacity of epoxy resin increases rapidly, a large amount of high-salt and high-organic waste liquid is generated, which is difficult to treat. Direct discharge not only pollutes the environment, but also harms human health. In addition, aged resin is extremely difficult to degrade in the natural environment. Inorganic salts and acid-base inorganic substances will change the pH of water and soil. Organic pollution will cause damage to the ecosystem and directly threaten human survival. If environmental protection measures based on governance are adopted, due to the high salt and high-difficult-to-degrade organic matter in the waste liquid, conventional methods are not only difficult to treat, but also require a lot of manpower, material and financial resources, and are prone to produce a large amount of secondary pollution, resulting in a great waste of resources and energy.

[0004] Therefore, it is urgent to improve the level of environmental protection and clean production through technological innovation and technological transformation, realize the multiple utilization of resources such as NaCl and catalysts, and implement closed-loop circulation of resources and energy, so as to optimize the integration and utilization of resources, make the product structure more reasonable, be more environmentally friendly, and make the benefits more obvious. The problem of epoxy resin waste liquid can be solved at the source, which will safeguard the large-scale development of epoxy resin.

[0005] In view of this, the present invention is proposed. Summary of the invention

[0006] The purpose of the present invention is to provide a method for resource utilization of epoxy resin waste liquid, which can recycle NaCl in high-salt wastewater generated in the production process of the epoxy resin industry, thereby solving the problem of high-salt wastewater treatment and saving treatment costs, and creating benefits and value, thereby achieving the goals of clean production and energy conservation and emission reduction.

[0007] In order to achieve the above object, the present invention adopts the following technical solution:

[0008] A method for recycling epoxy resin waste liquid comprises the following steps:

[0009] (1) Wet catalytic oxidation: After adding hydrochloric acid to adjust the pH of the waste liquid to 2-4, a wet catalytic oxidation reaction is carried out. The catalyst is CuCl2. After the reaction, the effluent enters the reaction tank system.

[0010] (2) Reaction tank treatment: Add sodium hydroxide to adjust the pH of the wet catalytic oxidation effluent to 7-10, and remove Cu 2+ Cu(OH)2 precipitate is formed and stirred to mix well, and the effluent enters the inclined tube precipitation / ultrafiltration system.

[0011] (3) Inclined tube sedimentation or ultrafiltration: After sufficient sedimentation in the inclined tube, the bottom precipitate enters the catalyst recovery system, and the supernatant enters the targeted adsorption system I, or the concentrated water enters the catalyst recovery system after being intercepted by the ultrafiltration membrane, and the produced water enters the targeted adsorption system I.

[0012] (4) Targeted adsorption I: After the supernatant of the inclined tube sedimentation or the ultrafiltration water is adsorbed by the targeted adsorption I system, Cu 2+ The liquid remains on the adsorption column and enters the targeted adsorption II system. After the targeted adsorption I system is saturated with adsorption, the adsorption column is regenerated and the regenerated liquid returns to the front-end reaction tank system.

[0013] (5) Targeted Adsorption II: The targeted adsorption II system directionally adsorbs TOC in water, and the effluent is a NaCl solution with a TOC below 10 mg / L, which can be returned to the epoxy resin production line for resource utilization. After the targeted adsorption II system reaches saturation, the adsorbent is regenerated, and the regenerated liquid is returned to the front-end wet catalytic oxidation system.

[0014] Furthermore, the resource utilization method includes catalyst recovery processing, and the catalyst recovery system includes candle filtration and hydrochloric acid dissolution processes. The bottom sediment of the inclined tube sedimentation or the ultrafiltration concentrated water first enters the candle filter, and is separated by candle filtration to obtain filtrate and Cu(OH)2 solid. Then, the Cu(OH)2 solid is dissolved with hydrochloric acid to form a CuCl2 solution, which is returned to the front-end wet catalytic oxidation system as its catalyst, and the filtrate returns to the reaction tank system.

[0015] Furthermore, the candle filter includes a central tube, a filter medium, a collection chamber, and a filter tube.

[0016] Preferably, the outer ring of the central tube surrounds 6 filter tubes, and the outer layer of the 6 filter tubes is wrapped with a layer of filter medium. The diameter of the central tube and the filter tube is 10-25 mm, and the length is 500 mm-3000 mm. Holes with a diameter of 1-2 mm are arranged at intervals on each central tube and filter tube.

[0017] Preferably, the filter medium is a radially woven felt cloth or a membrane with a pore diameter of less than 1 μm.

[0018] Preferably, the collecting chamber is at the port of the filter tube, and is used to connect the central tube and the filter tube.

[0019] Preferably, the working pressure of the candle filtration is 0.1-0.5 MPa, the liquid-solid content after filtration is ≤5 ppm, and the filter cake thickness can reach 3-50 mm.

[0020] Preferably, hydrochloric acid with a mass percentage concentration of 5% to 10% is used to dissolve Cu(OH)2, and the pH is controlled below 4.7.

[0021] Furthermore, in step (1), hydrochloric acid with a mass percentage concentration of 5% to 10% is added to adjust the pH of the waste liquid to 2 to 4.

[0022] Furthermore, in step (1), the oxidant is air or oxygen, the reaction temperature is 200°C to 300°C, the reaction pressure is 3 to 10 MPa, the catalyst dosage is 1% to 5%, and the catalytic oxidation time is 2 to 4 hours.

[0023] Preferably, a fixed bed is provided in the wet catalytic oxidation device, and a metal oxidant filler with a diameter of 4 to 10 mm is filled as a reinforced disperser, and a filling density of 1.0 to 1.5 g / mL is used. The metal oxidant is preferably a Ti8 alloy.

[0024] Furthermore, in step (2), a sodium hydroxide solution with a mass percentage concentration of 5% to 10% is added to adjust the pH of the waste liquid.

[0025] Preferably, the stirring speed is 40 to 50 rpm, and the stirring time is 20 to 30 min.

[0026] Furthermore, in step (3), in the inclined tube sedimentation, the diameter of the inclined tube is 50 mm to 100 mm, the thickness is not less than 1 mm, the material is PP material, and the sedimentation time is 0.5 to 1.5 h.

[0027] Preferably, the ultrafiltration adopts tubular ultrafiltration, the inner diameter of the membrane tube is 5-8 mm, the length of the membrane tube is 3-4 m, the membrane pore diameter is 20-50 nm, and the membrane material is PVDF material.

[0028] Furthermore, in step (4), the adsorbent model filled in the targeted adsorption I is CH-90Na, the pH of the waste liquid is adjusted to 3-5 before adsorption, the working flow rate is 10BV / H, and the saturated adsorption capacity is about 50g / L.

[0029] Preferably, when the adsorption is saturated, it is first analyzed with a hydrochloric acid solution, then backwashed with pure water or soft water, and finally transformed with sodium hydroxide.

[0030] Preferably, first use 5% hydrochloric acid solution for analysis at a flow rate of 4-5BV / H for 30-45min, then use pure water or soft water for backwashing at a backwash flow rate of 5-10BV / H for 30min, and finally use 5% sodium hydroxide solution for transformation at a transformation flow rate of 4-5BV / H for 30min.

[0031] Furthermore, in step (5), the targeted adsorption II is filled with microcrystalline material, the liquid flow rate is 0.5 to 1 BV / H, and the adsorption temperature is 20 to 35°C.

[0032] Compared with the prior art, the technical effects of the present invention are:

[0033] The resource utilization method of epoxy resin waste liquid provided by the present invention realizes the recovery and utilization of salt in the waste liquid. The method is simple and effective, can realize the separation of salt and organic matter, and provides a solution for the treatment of high-salt and high-organic waste liquid. The purified and recovered salt can be returned to the front-end production process, which can not only save resources and energy, create higher profits, realize resource utilization, but also avoid environmental pollution and other problems.

[0034] Furthermore, the present invention also provides a method for recovering catalysts in the epoxy resin industry. The catalyst recovery method of the present invention has a short process and strong practicality. The recovered catalyst can be used as a catalyst for front-end wet catalytic oxidation, thereby avoiding the catalyst from entering the environment to cause catalyst pollution and waste of resources. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] The various technical features of the present invention and the relationship between them are further explained below with reference to the accompanying drawings. The accompanying drawings are exemplary, and some technical features are not shown in actual proportion. In addition, some drawings may omit technical features that are commonly used in the technical field to which the present invention belongs and are not essential for understanding and implementing the present invention, or additionally show technical features that are not essential for understanding and implementing the present invention. In other words, the combination of the various technical features shown in the accompanying drawings is not used to limit the present invention. In addition, in the full text of the present invention, the same figure numerals refer to the same content. The specific description of the drawings is as follows:

[0036] Figure 1 This is a process flow chart for resource utilization of epoxy resin waste liquid of the present invention;

[0037] Figure 2 It is a schematic diagram of a candle filter device used in the process of recycling epoxy resin waste liquid according to the present invention. DETAILED DESCRIPTION

[0038] Hereinafter, specific embodiments of the present invention will be described in detail with reference to the accompanying drawings.

[0039] Suspended solids (SS) refers to solid matter suspended in water, including organic and inorganic particles, such as inorganic and organic matter that is difficult to dissolve in water, mud, clay, microorganisms, etc. The content of suspended solids in water is one of the indicators to measure the degree of water pollution.

[0040] Catalytic Wet Oxidation Process (CWO) is a deep treatment technology for wastewater. Under certain temperature and pressure conditions, in a reactor filled with a special fixed catalyst, the wastewater is kept in a liquid state. Under the action of oxygen (air), the principle of catalytic oxidation is used to perform deep treatment (contact time 10min-2.0h) of pollutants such as COD (chemical oxygen demand), TOC (total organic carbon), ammonia, and cyanide in high-concentration industrial organic wastewater at one time, converting them into harmless components such as CO2, N2, and water, and at the same time deodorizing, decolorizing, and sterilizing, thereby achieving the purpose of purifying and treating wastewater.

[0041] The present invention provides a method for recycling epoxy resin waste liquid, which is applicable to waste liquid with high salt content and high organic matter content generated in the production process of epoxy resin industry, and is particularly applicable to the process of treating such waste liquid by wet catalytic oxidation. Such waste liquid is extremely difficult to treat by conventional methods, and is also hazardous waste, and the disposal cost is extremely high.

[0042] The present invention provides a method for resource utilization of epoxy resin waste liquid, the main process or procedure includes "wet catalytic oxidation (CWO) + reaction tank treatment + inclined tube precipitation / ultrafiltration + targeted adsorption I + targeted adsorption II", and is provided with catalyst recovery treatment. This method can recover NaCl in high-salt wastewater generated in the production process of the epoxy resin industry, so that both salt and catalyst can be utilized as resources, which not only solves the problem of high-salt wastewater treatment, but also achieves the purpose of clean production and energy conservation and emission reduction, not only saves resources, but also creates revenue, and the whole process flow is simple, stable in operation, and highly practical. In addition, the present invention can recover catalysts such as copper introduced in the production and wastewater treatment process of the epoxy resin industry, not only with high purity, but also as a catalyst for the wet catalytic oxidation system in the water treatment process, to achieve the purpose of resource recovery and utilization.

[0043] The method of the present invention is applicable to the treatment of NaCl-containing wastewater generated in the production process of the epoxy resin industry, but is not limited to this type of wastewater. For example, if the wastewater contains NaCl, the acid and alkali for adjusting pH and dissolving Cu(OH)2 in the method may be hydrochloric acid and sodium hydroxide; if the wastewater contains Na2SO4, the acid and alkali for adjusting pH and dissolving Cu(OH)2 in the method may be sulfuric acid and sodium hydroxide.

[0044] For the wet catalytic oxidation system (CWO system), hydrochloric acid is added to adjust the pH of the waste liquid to 2-4, and then the wet catalytic oxidation reaction is carried out. The catalyst is CuCl2, and the effluent after the reaction enters the reaction tank system. The working conditions can be: temperature 200℃-300℃, pressure 3-10MPa, the catalyst is mainly CuCl2, the catalyst dosage is 1%-5%, the oxidant is air or oxygen (the oxygen concentration under oxygen-rich conditions can reach 40%-90%), the catalytic oxidation time is 2-4h, and the refractory organic matter and ammonia are oxidized and decomposed. The wet catalytic oxidation device is equipped with a fixed bed, filled with φ4-10mm metal oxidant fillers as a reinforced disperser, and the filling density is 1.0-1.5g / mL to increase the contact area between oxygen and water, reduce the amount of catalyst used, and ensure that the wet catalytic oxidation can efficiently remove organic matter and play a catalytic role at the same time.

[0045] For the reaction tank system, sodium hydroxide is added to adjust the pH of the wet catalytic oxidation effluent to 7-10, and Cu 2+ Cu(OH)2 precipitate is formed and stirred and mixed, and the effluent enters the inclined tube precipitation / ultrafiltration system. Further, 5% to 10% sodium hydroxide solution is added to adjust the pH of the waste liquid to 7 to 10, preferably 8 to 10, the reaction stirring speed is 40 to 50 rpm, and the reaction time is 20 to 30 minutes.

[0046] For the inclined tube sedimentation or ultrafiltration system, after sufficient sedimentation in the inclined tube, the bottom sediment enters the catalyst recovery system, and the supernatant enters the targeted adsorption I system, or the concentrated water enters the catalyst recovery system after being intercepted by the ultrafiltration membrane, and the produced water enters the targeted adsorption I system. If an inclined tube sedimentation tank is used, the diameter of the inclined tube is 50mm~100mm, the thickness is not less than 1mm, and the material is PP material. The sedimentation time is 0.5~1.5h, preferably 1h, and a sedimentation collection tank is set in the sedimentation area to facilitate the collection and discharge of solids. If ultrafiltration is used, the ultrafiltration adopts tubular ultrafiltration, the inner diameter of the membrane tube is 5~8mm, preferably 8mm, the membrane tube length is 3~4m, the membrane pore size is 20~50nm, and the membrane material is PVDF material. The inclined tube sedimentation treatment effect is significant and cost-effective. It is particularly suitable for the precipitation of inorganic insoluble matter when the treatment volume is small, and the wastewater treatment volume exceeds 50m 3 / h, the precipitate can be concentrated using an ultrafiltration membrane first.

[0047] For the targeted adsorption I system, the supernatant of the inclined tube sedimentation or the ultrafiltration water was adsorbed by the targeted adsorption I system. 2+Stay on the adsorption column, and the column liquid enters the targeted adsorption II system; the targeted adsorption I system regenerates the adsorption column after adsorption saturation, and the regenerated liquid returns to the front-end reaction tank system. Preferably, the adsorbent model filled with targeted adsorption I is CH-90Na. Before adsorption, the pH of the supernatant of the inclined tube sedimentation or the ultrafiltration water is adjusted to 3-5, the working flow rate is 10BV / H, and the saturated adsorption capacity is about 50g / L. When the adsorption is saturated, first use 5% hydrochloric acid solution for analysis, the flow rate is 4-5BV / H, and the time is 30-45min. Then use pure water or soft water for backwashing, the backwash flow rate is 5-10BV / H, and the backwash time is 30min. Finally, use 5% sodium hydroxide solution for transformation, the transformation flow rate is 4-5BV / H, and the time is 30min. Acid and alkali are recycled, and when the acidity of the analytical solution is less than 1%, it is discharged to the reaction tank to recover the copper therein. When the sodium hydroxide concentration is lower than 1%, sodium hydroxide is supplemented for continued use.

[0048] For the targeted adsorption II system, the targeted adsorption II system directionally adsorbs TOC in the water, and the effluent is a NaCl solution with a TOC below 10 mg / L, which can be returned to the epoxy resin production line for resource utilization. After the targeted adsorption II system is saturated with adsorption, the adsorbent is regenerated, and the regenerated liquid is returned to the front-end wet catalytic oxidation system. Preferably, the targeted adsorption II is filled with microcrystalline materials, which are artificial hydrothermally synthesized aluminosilicate crystals, and the air velocity of the adsorbent is 0.05-0.15 m 3 / (m 3 ·h), the liquid flow rate is 0.5~1BV / H, and the adsorption temperature is 20~35℃. When the TOC of the NaCl solution after adsorption is below 10mg / L, it can be directly returned to the production line of epoxy resin to realize the resource utilization of NaCl. When the TOC of the NaCl solution after adsorption exceeds 10mg / L, the microcrystalline material needs to be alkali washed, and the alkali is 5% sodium hydroxide solution, the alkali washing rate is 0.5~1BV / H, and the alkali washing water returns to the front-end CWO system.

[0049] For the catalyst recovery system, the catalyst recovery treatment includes candle filtration and hydrochloric acid dissolution process. The bottom sediment of the inclined tube sedimentation or the ultrafiltration concentrated water first enters the candle filter, and the filtrate and Cu(OH)2 solid are separated by candle filtration. Then the Cu(OH)2 solid is dissolved with hydrochloric acid to form a CuCl2 solution, which is returned to the front wet catalytic oxidation system as its catalyst, and the filtrate is returned to the reaction tank system. The diameter of the candle filtration center tube and the filter tube is 10-25mm, and the length is 500mm-3000mm, preferably 630mm-2500mm. Each center tube and filter tube is spaced with holes with a diameter of 1-2mm. The filter medium uses radially woven felt cloth or a membrane with a micropore diameter of less than 1μm. The working pressure of candle filtration is 0.1-0.5MPa, preferably 0.3-0.5MPa. The liquid-solid content after filtration is ≤5ppm, the filter cake thickness can reach 3-50mm, the dryness of the filter cake is adjustable, and it can be dried to a residual moisture content of less than 50% by cold or hot air or steam. The entire filtration, drying, filter cake shedding, backwashing and other processes are fully automatic. The candle filtration process has a short process, is simple and easy to operate, and is stable and reliable.

[0050] It is further preferred that the acid for dissolving the Cu(OH)2 precipitate is 5% to 10% dilute hydrochloric acid, the pH is controlled below 4.7, the dissolution process is fully stirred, and the stirring speed is 50 to 150 rpm to ensure that the Cu(OH)2 precipitate is completely dissolved and the dissolved liquid returns to the front-end CWO system.

[0051] The present invention improves the clean production and environmental protection level of the epoxy resin industry, realizes closed-loop circulation of resources and energy, optimizes resource integration and utilization, makes product structure more reasonable, is more environmentally friendly, and has more obvious benefits.

[0052] The embodiments of the present invention will be described in detail below in conjunction with examples, but those skilled in the art will appreciate that the following examples are only used to illustrate the present invention and should not be considered to limit the scope of the present invention. If no specific conditions are specified in the examples, they are carried out according to conventional conditions or conditions recommended by the manufacturer.

[0053] Example 1

[0054] The waste liquid produced by an epoxy resin industry has a water volume of 40t / h, a measured pH of 6-8, a TOC of 5600mg / L, and a NaCl content of 20%-22%.

[0055] Wet catalytic oxidation: Use 10% dilute hydrochloric acid to adjust the pH of the wet catalytic oxidation water from the wastewater storage tank to 2-4. Control the wet catalytic oxidation temperature to 270°C, the pressure to 8MPa, the copper catalyst to 10000mg / L, and use φ4-10mm Ti8 alloy as fixed bed filler with a packing density of 1.5g / mL. Continue to introduce air and catalytically oxidize for 2h. After wet catalytic oxidation, the waste liquid is light blue, the pH is 6, the TOC is about 280mg / L, and the NaCl content is 18%-20%.

[0056] Reaction tank treatment + inclined tube sedimentation: 5.4m 3 / h 10% NaOH solution to the reaction tank, adjust the pH of the solution in the reaction tank to about 8, and stir and precipitate. The reaction precipitation system produces about 36t / h of sludge, about 20g / L of SS, and about 51t / h of supernatant, Cu 2+ The concentration is about 110mg / L.

[0057] Candle filtration: A candle filter is used to filter the solid-liquid mixture at the bottom of the inclined tube sedimentation, producing 1.44t / h of Cu(OH)2 solid with a water content of about 50%, which is fully dissolved by adding 10% dilute hydrochloric acid and then returned to the front-end wet catalytic oxidation system. About 34.56t / h of filtrate is produced and returned to the front-end reaction tank.

[0058] Targeted adsorption I: Two tanks are used, with a single tank inner diameter of 1.6m and a height of 2.6m. The liquid contact part is made of duplex stainless steel. Use 10% dilute hydrochloric acid to adjust the pH of the supernatant to 3-5 in the inclined tube precipitation. No copper ions are detected in the column liquid, and TOC is 257mg / L. Targeted adsorption I adsorbs 80BV of waste liquid to reach saturation. 4BV of dilute hydrochloric acid is required for analysis, and the copper-containing solution is blue-green. The regenerated liquid of targeted adsorption I returns to the front end for reaction precipitation. When the adsorption is saturated, first use 5% hydrochloric acid solution for analysis, with a flow rate of 4-5BV / H and a time of 30-45min. Then use pure water or soft water for backwashing, with a backwash flow rate of 5-10BV / H and a backwash time of 30min. Finally, use 5% sodium hydroxide solution for transformation, with a transformation flow rate of 4-5BV / H and a time of 30min.

[0059] Targeted adsorption II: The TOC of the adsorbed effluent is 7.7 mg / L, copper ions are not detected, the NaCl content is 17% to 19%, and the effluent is colorless and transparent, which can reach the purity for reuse.

[0060] Figure 1 The present invention shows the treatment process of epoxy resin production waste liquid in a chemical industry.

[0061] Example 2

[0062] The waste liquid from epoxy resin production in a chemical industry has a water volume of 60t / h, a measured pH of 10-12, a TOC of 4000mg / L, a NaCl content of 21%-22%, glycerol of 3.3%, and toluene of 50mg / L.

[0063] This waste liquid is difficult to treat by conventional biochemical, electrochemical and other methods due to its high organic and salt content, and NaCl is easily discharged as miscellaneous salts during the treatment process, resulting in high disposal costs. The salt recycling and catalyst recovery method provided by the present invention is not only applicable to the epoxy resin industry, but also to such high-salt and high-organic waste liquid.

[0064] Wet catalytic oxidation: Use 10% dilute hydrochloric acid to adjust the pH of the wet catalytic oxidation influent to 2-4. The wet catalytic oxidation temperature is 265°C, the pressure is 7MPa, the copper catalyst is 10000mg / L, and the Ti8 alloy with a diameter of φ4-10mm is used as the fixed bed filler with a packing density of 1.5g / mL. Air is continuously introduced, and the wet catalytic oxidation time is 4h. After wet catalytic oxidation, the waste liquid is light blue, the pH is 4, the TOC is about 200mg / L, and the NaCl content is 20%-21%.

[0065] Reaction tank treatment + ultrafiltration: 8.1m 3 / h 10% NaOH solution is added to the reaction tank, the pH of the solution in the reaction tank is adjusted to about 8, and the precipitation is fully stirred. The ultrafiltration concentrated water flow is 27t / h, SS is 40g / L, the ultrafiltration water production is 76.6t / h, and the copper concentration is about 120mg / L.

[0066] Candle filtration: The ultrafiltration concentrated water is filtered by candle filters to produce 2.16t / h of Cu(OH)2 solid with a water content of about 50%. After being fully dissolved by adding 10% dilute hydrochloric acid, it returns to the front-end wet catalytic oxidation system. The filtrate produced is 24.84t / h, which is returned to the front-end reaction precipitation.

[0067] Targeted adsorption I: Two tanks are used, with a single tank inner diameter of 1.8m and a height of 3m. The liquid contact part is made of duplex stainless steel. Use 10% dilute hydrochloric acid to adjust the ultrafiltration water pH to 3-5. No copper ions are detected in the column liquid, and the TOC is about 183.7mg / L. Targeted adsorption I adsorbs 40BV of waste liquid to reach saturation. 4BV of dilute hydrochloric acid is required for analysis. The copper-containing solution is blue-green, and the regenerated liquid adsorbed by the resin returns to the front end for reaction precipitation. When the adsorption is saturated, first use 5% hydrochloric acid solution for analysis, with a flow rate of 4-5BV / H and a time of 30-45min. Then use pure water or soft water for backwashing, with a backwash flow rate of 5-10BV / H and a backwash time of 30min. Finally, use 5% sodium hydroxide solution for transformation, with a transformation flow rate of 4-5BV / H and a time of 30min.

[0068] Targeted adsorption II: The TOC of the adsorbed effluent is 5.5 mg / L, copper ions are not detected, the NaCl content is 19% to 20%, and the effluent is colorless and transparent, which can reach the purity for reuse.

[0069] Example 3

[0070] The waste liquid from epichlorohydrin production in a chemical industry has a water volume of 52t / h, a measured pH of more than 12, a TOC of 8800mg / L, a NaCl content of 25%, sodium hydroxide 1-5g / L, glycerol 1-1.3%, glycidol 0.2-1%, epichlorohydrin 0.01%, dichloropropane 0.06%, and sodium acetate ≤0.5%.

[0071] The waste liquid in Example 3 is the same as that in Example 2, and is difficult to treat using conventional methods. In addition, NaCl is easily discharged as impurity salts during the treatment process, resulting in high disposal costs.

[0072] Wet catalytic oxidation: Use 10% dilute hydrochloric acid to adjust the pH of the wet catalytic oxidation influent to 2-4. The wet catalytic oxidation temperature is 265°C, the pressure is 7MPa, the copper catalyst is 20000mg / L, and the Ti8 alloy with a diameter of φ4-10mm is used as the fixed bed filler with a packing density of 1.5g / mL. Air is continuously introduced, and the wet catalytic oxidation time is 3h. After wet catalytic oxidation, the waste liquid is light blue, the pH is 6, the TOC is 352mg / L, and the NaCl content is 21%-22%.

[0073] Reaction tank treatment + ultrafiltration: 16.9m 3 / h 10% NaOH solution is added to the reaction tank, the pH of the solution in the reaction tank is adjusted to about 8, and the precipitation is fully stirred. The ultrafiltration concentrated water flow is 56.48t / h, SS is 40g / L, ultrafiltration water production is 86.5t / h, and the copper concentration is about 200mg / L.

[0074] Candle filtration: The ultrafiltration concentrated water is filtered by candle filters to produce 4.52t / h of Cu(OH)2 solid with a water content of about 50%. After adding 10% dilute hydrochloric acid to fully dissolve it, it returns to the front-end wet catalytic oxidation system. The filtrate produced is 51.96t / h, which is returned to the front-end reaction precipitation.

[0075] Targeted adsorption I: Two tanks are used, with a single tank inner diameter of 1.8m and a height of 3m. The liquid contact part is made of duplex stainless steel. Use 10% dilute hydrochloric acid to adjust the pH of the supernatant to 3-5 in the inclined tube precipitation. No copper ions are detected in the column liquid, and the TOC is 300mg / L. Targeted adsorption I adsorbs 40BV of waste liquid to reach saturation. 5BV of dilute hydrochloric acid is required for analysis, and the copper-containing solution is blue-green. The regenerated liquid of targeted adsorption I returns to the front end for reaction precipitation. When the adsorption is saturated, first use 5% hydrochloric acid solution for analysis, with a flow rate of 4-5BV / H and a time of 30-45min. Then use pure water or soft water for backwashing, with a backwash flow rate of 5-10BV / H and a backwash time of 30min. Finally, use 5% sodium hydroxide solution for transformation, with a transformation flow rate of 4-5BV / H and a time of 30min.

[0076] Targeted adsorption II: The TOC of the adsorbed effluent is 9 mg / L, copper ions are not detected, the NaCl content is 18% to 20%, and the effluent is colorless and transparent, which can reach the purity for reuse.

[0077] In this specification, the numerical range expressed using "a numerical value A to a numerical value B" means a range including the endpoints A and B.

[0078] In this specification, unless otherwise specified, the word "multiple" in "multiple", "multiple", "plurality", etc. means a numerical value of 2 or more.

[0079] In this specification, unless otherwise specified, "%" means mass percentage.

[0080] In this specification, the word "may" includes both performing a certain process and not performing a certain process.

[0081] In the present specification, "optional" or "optionally" means that the event or situation described below may or may not occur, and the description includes cases where the event occurs and cases where it does not occur.

[0082] In this specification, the references to "some specific / preferred embodiments", "other specific / preferred embodiments", "embodiments", etc., mean that the specific elements (e.g., features, structures, properties and / or characteristics) described in connection with the embodiments are included in at least one embodiment described herein, and may or may not exist in other embodiments. In addition, it should be understood that the elements may be combined in various embodiments in any suitable manner.

[0083] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may also include more other equivalent embodiments without departing from the technical concept of the present invention, all of which belong to the protection scope of the present invention.

Claims

1. A method for recycling epoxy resin waste liquid, characterized in that: The steps include: (1) Wet catalytic oxidation: After adding hydrochloric acid to adjust the pH of the waste liquid to 2-4, a wet catalytic oxidation reaction is carried out. The catalyst is CuCl2. After the reaction, the effluent enters the reaction tank system; (2) Reaction tank treatment: Add sodium hydroxide to adjust the pH of the wet catalytic oxidation effluent to 7-10, and remove Cu 2+ Cu(OH)2 precipitate is formed and stirred and mixed, and the effluent enters the inclined tube precipitation / ultrafiltration system; (3) Inclined tube sedimentation or ultrafiltration: After sufficient sedimentation in the inclined tube, the bottom sediment enters the catalyst recovery system, and the supernatant enters the targeted adsorption system I, or the concentrated water enters the catalyst recovery system after being intercepted by the ultrafiltration membrane, and the produced water enters the targeted adsorption system I; (4) Targeted adsorption I: After the supernatant of the inclined tube sedimentation or the ultrafiltration water is adsorbed by the targeted adsorption I system, Cu 2+ The liquid remains on the adsorption column, and the column liquid enters the targeted adsorption system II. After the targeted adsorption system I is saturated with adsorption, the adsorption column is regenerated, and the regenerated liquid returns to the front-end reaction tank system. (5) Targeted Adsorption II: The targeted adsorption II system directionally adsorbs TOC in water, and the effluent is a NaCl solution with a TOC below 10 mg / L, which can be returned to the epoxy resin production line for resource utilization. After the targeted adsorption II system reaches saturation, the adsorbent is regenerated, and the regenerated liquid is returned to the front-end wet catalytic oxidation system.

2. The resource utilization method according to claim 1, characterized in that: The resource utilization method includes catalyst recovery processing, and the catalyst recovery system includes candle filtration and hydrochloric acid dissolution process. The bottom sediment of the inclined tube sedimentation or the ultrafiltration concentrated water first enters the candle filter, and the filtrate and Cu(OH)2 solid are separated by candle filtration. Then, the Cu(OH)2 solid is dissolved with hydrochloric acid to form a CuCl2 solution, which is returned to the front-end wet catalytic oxidation system as its catalyst, and the filtrate is returned to the reaction tank system.

3. The resource utilization method according to claim 2, characterized in that: The candle filter comprises a central tube, a filter medium, a collection chamber, and a filter tube; Preferably, the outer ring of the central tube surrounds 6 filter tubes, the outer layer of the 6 filter tubes is wrapped with a layer of filter medium, the diameter of the central tube and the filter tube is 10-25 mm, the length is 500 mm-3000 mm, and holes with a diameter of 1-2 mm are arranged at intervals on each central tube and filter tube; Preferably, the filter medium is a radially woven felt cloth or a membrane with a pore diameter of less than 1 μm; Preferably, the collecting chamber is at the port of the filter tube, and is used to connect the central tube and the filter tube; Preferably, the working pressure of the candle filtration is 0.1-0.5 MPa, the liquid-solid content after filtration is ≤5 ppm, and the filter cake thickness can reach 3-50 mm; Preferably, hydrochloric acid with a mass percentage concentration of 5% to 10% is used to dissolve Cu(OH)2, and the pH is controlled below 4.

7.

4. The resource utilization method according to claim 1, characterized in that: In step (1), hydrochloric acid with a mass percentage concentration of 5% to 10% is added to adjust the pH of the waste liquid to 2 to 4.

5. The resource utilization method according to claim 1, characterized in that: In step (1), the oxidant is air or oxygen, the reaction temperature is 200°C to 300°C, the reaction pressure is 3 to 10 MPa, the catalyst dosage is 1% to 5%, and the catalytic oxidation time is 2 to 4 hours; Preferably, a fixed bed is provided in the wet catalytic oxidation device, and a metal oxidant filler with a diameter of 4 to 10 mm is filled as a reinforced disperser, and a filling density of 1.0 to 1.5 g / mL is used. The metal oxidant is preferably Ti8 alloy.

6. The resource utilization method according to claim 1, characterized in that: In step (2), a sodium hydroxide solution having a mass percentage concentration of 5% to 10% is added to adjust the pH of the waste liquid; Preferably, the stirring speed is 40 to 50 rpm, and the stirring time is 20 to 30 min.

7. The resource utilization method according to claim 1, characterized in that: In step (3), in the inclined tube sedimentation, the diameter of the inclined tube is 50 mm to 100 mm, the thickness is not less than 1 mm, the material is PP material, and the sedimentation time is 0.5 to 1.5 h; Preferably, the ultrafiltration adopts tubular ultrafiltration, the inner diameter of the membrane tube is 5-8 mm, the length of the membrane tube is 3-4 m, the membrane pore diameter is 20-50 nm, and the membrane material is PVDF material.

8. The resource utilization method according to claim 1, characterized in that: In step (4), the adsorbent model filled in the targeted adsorption I is CH-90Na, the pH of the waste liquid is adjusted to 3-5 before adsorption, the working flow rate is 10BV / H, and the saturated adsorption capacity is about 50g / L; Preferably, when the adsorption is saturated, it is first analyzed with a hydrochloric acid solution, then backwashed with pure water or soft water, and finally transformed with sodium hydroxide; Preferably, first use 5% hydrochloric acid solution for analysis at a flow rate of 4-5BV / H for 30-45min, then use pure water or soft water for backwashing at a backwash flow rate of 5-10BV / H for 30min, and finally use 5% sodium hydroxide solution for transformation at a transformation flow rate of 4-5BV / H for 30min.

9. The resource utilization method according to claim 1, characterized in that: In step (5), the targeted adsorption II is filled with microcrystalline material, the liquid flow rate is 0.5 to 1 BV / H, and the adsorption temperature is 20 to 35°C.

Citation Information

Patent Citations

  • Method for treating high-concentration organic copper-containing wastewater and recycling copper

    CN104876380A

  • Resourceful treatment method for high salinity waste water with reusable catalyst

    CN104925997A

  • Treatment method of epoxy resin synthesis wastewater

    CN105645634A

Cited By

  • Method for treating POSM production wastewater

    CN119912125A

  • Method for treating and recycling MTO (Methanol To Olefins) production wastewater

    CN120058176A

  • Method for treating and recycling MTO production wastewater

    CN120058176B

  • Resource utilization method of calcium chloride high-salt water containing high-concentration organic matters

    CN120271179A