Band-aid type concrete crack vacuum repairing method
Through the Band-aid concrete crack vacuum repair method, the expansion agent and vacuum channel technology are used to solve the problem of differentiation and flatness of concrete crack repair in the existing technology, achieving efficient and beautiful repair results, and reducing repair costs and time.
Patent Information
- Application Number
- CN202411121587.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-05
AI Technical Summary
The existing concrete crack repair method has the problems of large differences from the parent body after forming, difficult to guarantee flatness, requiring regular maintenance and high cost, and cannot be applied to repair structures with high overall aesthetic requirements.
Using the Band-Aid concrete crack vacuum repair method, by opening a multi-section linear groove body at the crack, adding expansion agent repair material after pretreatment, and using the Band-Aid and vacuum channel for airtight vacuum maintenance, ensuring that the repair area is flush and compact with the parent body. , reduce the need for subsequent polishing.
The matching of the mechanical properties and chromaticity of the repair material with the parent body is achieved, the bonding strength and aesthetics are enhanced, the repair time is shortened, the repair efficiency is improved, and the occurrence of secondary cracks is avoided.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of building construction, and in particular to a Band-Aid type vacuum repair method for concrete cracks. Background Art
[0002] At present, there are fewer and fewer new construction projects. As a large number of construction projects built during the period of port construction in the 1970s and 1980s have gradually entered the repair and maintenance period, crack repair is a method for buildings to quickly restore their use functions in a short period of time with relatively small investment.
[0003] Concrete cracks are a problem that is prone to occur in the early stage of structural parts. If not repaired in time, concrete cracks will develop into through cracks and deep cracks, which will cause internal steel corrosion, resulting in local or even overall structural damage to the structure. Therefore, concrete crack repair is a daily maintenance and maintenance item for wharf structures. For cast-in-place concrete cracks, the surface crack sealing repair method is usually adopted. The construction method includes grooving along the seam, pressing and applying filling materials, and covering and curing. This construction method has the following disadvantages:
[0004] ① After forming, the repair area is quite different from the parent body, including strength, color, roughness, etc.;
[0005] ② Artificial control of leveling, no support formwork, flatness after forming cannot be guaranteed, and it is impossible to control the repair area to be flush with the parent body on both sides of the groove;
[0006] ③It requires regular maintenance, which is time-consuming and labor-intensive;
[0007] ④There is an obvious shrinkage joint between the repair area and the parent body;
[0008] ⑤After forming, the whole part needs to be polished or trimmed.
[0009] As can be seen from the above, the crack repair method in the prior art is labor-intensive, time-consuming and costly, and the appearance effect after molding is significantly different from the parent body, and cannot be applied to the repair of structures with high requirements for overall aesthetics. Summary of the invention
[0010] The purpose of the present invention is to overcome the defects in the prior art and provide a Band-Aid type concrete crack vacuum repair method to overcome one or more problems caused by the limitations and defects of the relevant technology to a certain extent.
[0011] In order to achieve the above object, the technical solution of the present invention is as follows:
[0012] A Band-Aid type concrete crack vacuum repair method comprises the following steps:
[0013] S1. Grooving: A repair groove is opened along the concrete crack, and the groove depth is 2-6 cm. The repair groove is a multi-segment linear groove splicing structure, and the groove depth at each location is kept consistent;
[0014] S2. Pretreatment of the repair groove: Use a brush to clean the particles and dust in the repair groove, and spray high-pressure fresh water to rinse and wet the repair groove and the mother body on both sides;
[0015] S3. Preparation of repair materials: Use the pouring order, test data and other traceable materials to find the batch of concrete to be repaired. According to the technical parameters of the batch, the crushed stones need to be ground into fine particles, and the repair material base is made and configured. The repair material base is transported to the site, and the original proportion of water is added. At the same time, 8%-12% of the expansion agent is added according to the volume fraction, stirred to a uniform state, and allowed to stand until the concrete slump is 10-40mm to obtain the repair material;
[0016] S4, height marking; calculate the expansion height according to the expansion rate of the expansion agent dosage and the structural dimensions of the repair groove, mark the filling height of the repair groove, and reserve the expansion height in the repair groove;
[0017] S5, repair and filling; repair and fill the repair groove in sections, first use a small spatula to press and fill the repair material to the bottom of the repair groove, press and smear repeatedly, so as to press and smear the repair material layer by layer along the groove body section of the repair groove until the filling height mark is reached, scrape off the excess repair material, and smooth the repair material filling plane in the groove body section of the repair groove along the filling height mark; repair each groove body section in sequence;
[0018] S6, making a wound patch; the wound patch includes a template patch and a plastic tape, the template patch is cut according to the length of each section of the groove, the width of the template patch is greater than the width of the repair groove, the adjacent ends of adjacent template patches are cut into matching splicing structures, and the template patches are arranged in sequence according to the path of the repair groove and bonded to the plastic tape;
[0019] S7, constructing a closed vacuum channel; cutting and gluing a plastic tape with a template patch, the template patch is located in the middle of the plastic tape, and the single-side width of the plastic tape is at least 4 cm greater than the template patch, applying adhesive on the parent concrete plane on both sides of the template patch at least 2 cm away from the side of the template patch, the plastic tape is initially bonded to the parent concrete by the adhesive, and at least one closed vacuum channel is formed between the parent concrete plane and the plastic tape;
[0020] S8, vacuum maintenance; vacuum the closed vacuum channels of traceable materials respectively, each of which can be connected with a pluggable hose, apply adhesive to the inner end surface of the traceable material hose, and connect the inner end to the vacuum channel, start the vacuum equipment connected to the outer end of the hose to vacuumize, and stop vacuuming when the vacuum degree reaches 0.09MPa;
[0021] S9. After the negative pressure vacuum self-maintenance is completed, the concrete repair is completed by removing the bandage.
[0022] Furthermore, during the concrete pouring operation, the concrete mixing station retains samples of the raw materials used for mixing concrete for each batch and marks them. The repair material base uses the retained materials. Except for the crushed stone that needs to be processed into fine particles, the remaining retained materials are processed into the material particle size specifications of the current batch, and the repair material base is configured according to the material ratio of the current batch.
[0023] Furthermore, a side of the template patch facing the repair groove is a buckling surface, and a rough surface with a roughness close to that of the parent body is prefabricated on the buckling surface.
[0024] Furthermore, a roughness comparison atlas of the template samples is prepared. Before the repair construction, a template sample with a roughness close to that of the matrix is selected according to the roughness comparison atlas, and a trial forming test is carried out using the retained raw materials of the current batch of concrete matrix to determine the roughness of the buckling surface.
[0025] Compared with the prior art, the Band-Aid type concrete crack vacuum repair method of the present invention has the following beneficial effects:
[0026] 1. The repair material is made and configured according to the technical parameters of the matrix, and an expansion agent is added to obtain mechanical properties and color similar to the matrix, enhance the bonding strength, effect and aesthetics of the repair material, and improve the density, impermeability, crack resistance and compression resistance of the concrete in the repair area;
[0027] 2. Use a band-aid structure for support and build a vacuum curing environment. The template patch of the band-aid is set on the repair groove by negative pressure to avoid damaging the surface of the parent concrete and provide a flattening force during the concrete forming process of the repair area. The repair area is located in a vacuum curing environment. Due to its small thickness, the gas inside the repair filling layer is emptied under a vacuum state, and the material is more compact after forming. In addition, the free moisture in the repair filling layer can be effectively discharged, which strengthens the bonding between the repair concrete and the parent concrete, and it is not easy to have secondary cracks in the repair area. In addition, due to the strong self-moisture retention ability in the vacuum curing environment, the curing effect of the repair concrete is better.
[0028] 3. After the concrete in the repair area is hardened and formed, due to the reserved expansion amount and the negative pressure of the formwork patch, the forming plane of the repair area is basically flush with the plane of the parent concrete, and the flatness of the concrete in the repair area can be guaranteed. No manual grinding or trimming is required later, and vacuum curing shortens the curing time. As a result, the overall repair efficiency is significantly improved. DETAILED DESCRIPTION
[0029] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only the best embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] A Band-Aid type vacuum repair method for concrete cracks in this embodiment can be used to repair concrete cracks, and can also be used to repair concrete surface damage that is difficult to support formwork and maintain, comprising the following steps:
[0031] S1. Grooving: The concrete cracks are repaired by the digging and patching method to ensure the overall mechanical properties after the repair. First, the repair groove is arranged. The width of the repair groove is 4-18cm. The groove width is determined according to the maximum repair bifurcation spacing in each repair path or the maximum offset of a single irregular crack. The crack is located in the groove area, and the average spacing between the two sides of the groove area and the crack is 2-8cm. For the repair area with complex crack shapes and wide crack dispersion, several parallel groove areas need to be set at intervals. If the maximum offset of the crack is too large, the groove area is set by segmented offset splicing; if it is a repair of local surface damage, the shape and width of the repair groove are adapted to the pre-damage The structure can be opened flexibly, but the distance between the side of the groove area and the nearest damaged edge should be no less than 2cm; the groove form of the repair groove can be V-shaped or concave groove, the groove depth is 2-6cm, which should be greater than the thickness of the protective layer, and the repair groove should be composed of multiple linear grooves. If it is a V-shaped groove, the V-shaped angle and groove depth of the repair groove should be consistent at all places, and the groove width should be of uniform specifications as much as possible. For concrete with extremely irregular cracks, a small number of groove widths of several specifications can be allowed, but the same groove width should be used in the same repair section; if it is a regular concave groove, the groove depth of the repair groove should be consistent at all places, and the groove width can be flexibly determined according to the cracks, but the same groove width should be used in the same repair section;
[0032] S2. Pretreatment of the repair groove: After the excavation of all the repair grooves in the repair area is completed, use a brush to clean the particles and dust in and on both sides of the repair groove, and spray high-pressure fresh water to rinse and wet the repair groove and the matrix on both sides to prevent impurities from affecting the later repair effect;
[0033] S3, preparation of repair materials; in order to obtain mechanical properties and color similar to those of the parent material, traceable materials such as casting orders and test data are used to find the batch of concrete to be repaired, and the technical parameters such as the composition, material specifications and component ratio of the parent material of the batch are obtained. According to the technical parameters of the parent batch, the repair material base is made and configured. It should be noted that the crushed stone in the original component should not use the original particle size, but should be processed into fine particles; due to the great influence of material collection time and origin differences on material properties and final color, in this embodiment, the retained materials of the batch at that time are directly selected for configuration. Therefore, it can be understood that during the concrete pouring operation period, a raw material retention process should be added, requiring the concrete mixing station to retain and store samples of the raw materials used for mixing concrete for each batch, and to make casting order marks for each batch of pouring sections. The marks should record various technical parameters of the corresponding batch of concrete pouring to ensure traceability;
[0034] Except for crushed stone, the retained materials are processed separately according to the particle size specifications of the batch at that time, and after being mixed according to the original component ratio, they are transported to the site in a loose and dry state, and water in the original mix ratio is added to obtain a repair material base that is basically the same as the parent material. In order to enhance the interface bonding force between the parent concrete and the repair area concrete, and at the same time improve the mechanical properties of the crack repair area, an expansive agent is mixed into the repair material base. In order to obtain a filling expansive concrete with a self-stress value of σ = 0.5 ~ 1Mpa, 8% - 15% of the expansive agent is added into the repair material base according to the volume fraction. It should be noted that the amount of the expansive agent should be adjusted according to the The retention period of the materials is appropriately increased to ensure the performance of the repaired concrete. Specifically, the amount of the expansive agent should be determined by experiment before repairing. The mechanical properties, expansion rate, expansion speed and other parameters of the repaired concrete under different dosages are comprehensively considered to determine the optimal amount of the expansive agent and the subsequent construction period. If the construction period cannot be guaranteed, a certain amount of retarder can be added to the repair material to meet the construction period requirements. There are many types of expansive agents. In order to meet the high impermeability and durability requirements of the port, the concrete prepared with the expansive agent can adopt the structural self-waterproofing technology. In this embodiment, HEA expansive agent is preferably used;
[0035] After mixing the above materials, add an equal amount of water of the current batch, stir the repair material until it is uniform, and let it stand until the concrete slump is 10-40mm to obtain a repair material that can be constructed;
[0036] S4, height marking; during the preparation of the repair material, the repair height is marked at the same time. In order to form a natural surface roughness similar to that of the matrix, the repair concrete of this embodiment is not polished after forming. Therefore, the height of the repair material in the repair groove after solidification and forming should be limited. The expansion height is calculated according to the expansion rate of the expansion agent dosage and the structural dimensions of the repair groove to obtain a filling height slightly lower than the groove surface of the repair groove, and a linear marking device is used to mark the filling height of the repair material, and the expansion height is reserved in the repair groove;
[0037] S5. Repair and filling: When the repair groove and the matrix on both sides are fully moistened and there is no water accumulation or visible water, fill the repair material and repair the cracks in sections. First, use a small spatula to press the repair material to the bottom of the repair groove, compact and smooth it repeatedly, and then press and smooth the repair material layer by layer along the groove section until the filling height mark of the repair groove is reached. Scrape off the excess repair material and smooth the repair material filling plane in the repair groove along the filling height mark; use the same method to repair and fill each section of the groove in sequence; it should be noted that if the repair and filling period is long, the preparation and construction of the repair material should be carried out in batches;
[0038] S6. After filling, a bandage structure is used to cover the repair groove for protection and maintenance. The bandage includes a template patch and a plastic tape. The template patch should be made of a lightweight plate with a certain rigidity, such as an aluminum sheet, a wood sheet or a hard plastic sheet. The template patch can also keep the expansion height of each part the same during the expansion of the repair material to obtain a flat repair surface. First, the template patch is cut according to the length of each section of the groove body. The width of the template patch is greater than the width of the repair groove. Each section of the template patch is cut in turn. At the joints of adjacent sections of template patches, matching joint structures should be cut out on the connecting end faces. For joints with special shapes such as folded corners, the end faces of the template patches should be cut to form joint slopes that match each other and overlap. The sections of template patches in the area are arranged on the plastic tape in sequence according to the repair path in the slotted area. The four corners of the template patches are smeared with adhesive and then glued to the plastic tape to form an integrated structure. Thus, a bandage for repairing the slot is obtained. If the repair area is too large, the plastic tape is made of multiple pieces of plastic.
[0039] S7, constructing a closed vacuum channel; cutting and pasting the plastic tape with the template patch, ensuring that the distance between the edge of the plastic tape and the side of the nearest template patch is not less than 4cm, applying adhesive on the parent concrete plane at least 2cm away from the side and end of the template patch, the plastic tape is initially adhered to the parent concrete by the adhesive, and at least one closed vacuum channel that sequentially connects the repair sections is formed between the parent concrete plane and the plastic tape, the vacuum channel can be several parallel channels in the same direction, or channels that cross each other vertically and horizontally, and the template patch is covered in the vacuum channel; the plastic tape for constructing the closed vacuum channel is a PET+PE vacuum film with a thickness of 0.08-0.1mm, which has high tensile strength, is soft and transparent, can be deformed to a certain extent after vacuuming, and has a certain adsorption retention force;
[0040] S8. Vacuum maintenance: When the adhesive is still fluid, the above-mentioned closed vacuum channel is evacuated to form a closed negative pressure curing environment. Negative pressure curing can not only fix the template patch without destroying the concrete matrix, but also provide a certain leveling force during the expansion of the repair material, which is conducive to obtaining a repair surface with relatively uniform flatness; each closed vacuum channel can be connected to a hose for vacuuming, and each hose is connected to a vacuuming device. Sufficient adhesive should be applied to the inner end surface of each hose, and the inner end is inserted into any end of each vacuum channel of the plastic tape, and the inner end port extends into the adhesive area. Each vacuuming channel is connected to a vacuuming device, and the vacuuming device is turned on to vacuum the inside of each vacuuming channel until the plastic tape is tightly attached to the concrete matrix and the vacuum degree reaches 0.09MPa, then the vacuuming is stopped; at this time, the air in the gap of the repair groove is basically exhausted, and the pores or holes of the concrete matrix inside the band-aid are emptied of the air therein. Due to the small thickness of the repair filling layer, the gas therein is emptied in the vacuum state, making the material more compact. In addition, the free moisture in the repair filling layer can be effectively discharged, and the bonding between the repair concrete and the matrix concrete is strengthened, and secondary cracks are not easy to appear in the repair area;
[0041] Press the inner end of the hose by hand through the plastic tape, and slowly pull out the hose while ensuring airtightness. When the adhesive area of the inner end of the hose is straightened, continue to pull out and tidy up the adhesive under the plastic tape, so that the adhesive on the inner side of the inner end of the hose gradually surrounds and seals the vacuum channel, and the hose is disassembled;
[0042] S9. Self-maintenance of repaired concrete is carried out in a negative pressure vacuum environment. Since most of the free moisture is separated, the curing time of the repaired concrete is significantly shortened. In addition, since it is in a vacuum state, it has a strong self-moisture retention ability and a better curing effect. The curing is completed according to the curing time of the concrete curing specification, the bandage is removed, the colloid is removed, and the concrete repair is completed.
[0043] In this embodiment, during the expansion and hardening molding process of the repair material, it is flattened by the pressing surface of the template patch (i.e., the side of the template patch facing the repair groove), and its roughness depends on the roughness of the pressing surface. As a technical solution to further reduce the difference in roughness between the concrete in the repair area and the parent concrete, a rough surface consistent with the surface roughness of the parent is prefabricated on the pressing surface; in order to quickly produce a template patch with a high degree of profiling, according to the roughness of the concrete surface formed by the conventional concrete construction specifications, template samples with various roughness specifications are processed by profiling, and a roughness comparison atlas is made, and the corresponding roughness processing mold is kept for rapid selection during the repair construction. In order to facilitate batch processing of surface roughness, the template patch is preferably an aluminum sheet or a hard plastic sheet; before the repair construction, template samples with similar roughness specifications are selected according to the roughness comparison atlas, and trial molding tests are carried out using the retained raw materials of the batch of concrete parent at that time, and the molding effects of several similar template samples are tested respectively, and the template sample with the highest similarity is selected. After determining the roughness of the pressing surface, the surface roughness of the template patch is processed.
[0044] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A Band-Aid type concrete crack vacuum repair method, characterized in that: The following steps are involved: S1, slotting; a repair groove is opened along the concrete crack, and the groove depth is 2-6 cm. The repair groove is a multi-segment linear groove splicing structure, and the groove depth at each location is kept consistent; S2, pretreatment of the repair groove: using a brush to clean the particles and dust in the repair groove, and spraying high-pressure fresh water to rinse and wet the repair groove and the mother bodies on both sides; S3, preparation of repair materials: using the casting order, test data and other traceable materials to find the batch of the parent concrete at that time, processing materials according to the technical parameters of the batch at that time, wherein the crushed stone needs to be ground into fine particles, and making and configuring the repair material base, the repair material base is transported to the site, adding the original proportion of water, and at the same time adding 8%-12% of the expansion agent according to the volume fraction, stirring to a uniform state, and standing until the concrete slump is 10-40mm, to obtain the repair material; S4, height marking; calculating the expansion height according to the expansion rate of the expansion agent dosage and the structural dimensions of the repair groove, marking the filling height of the repair groove, and reserving the expansion height in the repair groove; S5, repair and filling; repair and fill the repair groove in sections, first use a small spatula to press and fill the repair material to the bottom of the repair groove, repeatedly press and spread the repair material layer by layer along the groove section of the repair groove until the filling height mark is reached, scrape off the excess repair material, and smooth the repair material filling plane in the repair groove along the filling height mark; repair the groove sections of each section of the repair groove in sequence; S6, making a wound patch; the wound patch includes a template patch and a plastic tape, the template patch is cut according to the length of each section of the groove body, the width of the template patch is greater than the width of the repair groove, the adjacent ends of the adjacent template patches are cut into matching splicing structures, and the template patches are arranged in sequence according to the path of the repair groove and bonded to the plastic tape; S7, constructing a closed vacuum channel; cutting and gluing the plastic tape with the template patch, wherein the template patch is located in the middle of the plastic tape, and the single-side width of the plastic tape is at least 4 cm greater than the template patch, applying adhesive on the parent concrete plane on both sides of the template patch at a distance of at least 2 cm from the template patch, and the plastic tape is initially glued to the parent concrete by the adhesive, and at least one closed vacuum channel is formed between the parent concrete plane and the plastic tape; S8, vacuum maintenance; vacuuming the closed vacuum channels respectively, each of which is connected with a pluggable hose, the inner end surface of the hose is coated with adhesive, and the inner end is connected to the vacuum channel, and the vacuum equipment connected to the outer end of the hose is started to vacuumize, and the vacuuming is stopped when the vacuum degree reaches 0.09MPa; S9. After the negative pressure vacuum self-maintenance is completed, the concrete repair is completed by removing the bandage.
2. The Band-Aid type concrete crack vacuum repair method according to claim 1, characterized in that: During the concrete pouring operation, the concrete mixing station retains samples of the raw materials used for mixing concrete for each batch and marks them. The repair material base adopts the retained materials. Except for the crushed stone which needs to be processed into fine particles, the remaining retained materials are processed into the material particle size specifications of the current batch, and the repair material base is configured according to the material ratio of the current batch.
3. The Band-Aid type concrete crack vacuum repair method according to claim 2, characterized in that: The side of the template patch facing the repair groove is a pressing surface, and a rough surface with a roughness close to that of the parent body is prefabricated on the pressing surface.
4. The Band-Aid type concrete crack vacuum repair method according to claim 3, characterized in that: A roughness comparison atlas of the template samples is prepared. Before the repair construction, the template samples with a roughness close to that of the matrix are selected according to the roughness comparison atlas, and a trial molding test is carried out using the retained raw materials of the current batch of the matrix to determine the roughness of the buckling surface.
Citation Information
Patent Citations
Concrete crack surface cut groove sealing and blocking structure and method
CN103437432A
Cement concrete pavement crack damage grooving type repair method
CN108797292A
Mass concrete internal bleeding water vacuum pumping discharge removal and structural anti-cracking method
CN110565958A
Construction device and method for repairing concrete cracks
CN110821205A
Concrete crack repairing method
CN113027160A