Coffee residue sludge aerobic fermentation auxiliary material as well as preparation method and application thereof

By modifying the aerobic fermentation auxiliary materials of coffee ground sludge with a combination of coffee ground gel microspheres and ceramic particles, the existing conditioning agents have solved the problem of large area and high cost, and improved the aerobic fermentation efficiency of sludge and the adsorption of phosphorus The ability to realize the recycling and environmental protection of coffee grounds.

CN118930004AInactive Publication Date: 2024-11-12GUANGZHOU WATER ENVIRONMENTAL PROTECTION TECH CO LTD

Patent Information

Application Number
CN202411118513.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing sludge aerobic fermentation conditioner has problems such as large storage area, high cost, difficulty in improving the stack structure and not in line with the concept of sustainable development. The direct landfill of coffee grounds will produce methane, which will harm the environment.

Method used

Aerobic fermentation auxiliary materials for coffee ground sludge made in proportion with modified coffee ground gel microspheres, porous ceramic particles, fly ash, bacterial agents and binders, are combined with modified coffee ground biochar and ceramic particles. Form a three-dimensional network structure to improve microbial activity and oxygen transmission, and promote aerobic fermentation of sludge.

Benefits of technology

It improves the aerobic fermentation efficiency of sludge, reduces the fermentation cost, realizes the recycling of coffee grounds, enhances the adsorption capacity of phosphorus, promotes microbial activity, and has good recycling potential and physical structural stability of auxiliary materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004994341160000121
    Figure BDA0004994341160000121
  • Figure BDA0004994341160000131
    Figure BDA0004994341160000131
  • Figure BDA0004994341160000132
    Figure BDA0004994341160000132
Patent Text Reader

Abstract

The invention provides an auxiliary material for aerobic fermentation of coffee residue sludge. The auxiliary material is prepared from the following raw material components in parts by mass: 100 parts of modified coffee residue gel microspheres, 5-10 parts of porous ceramic particles, 30-40 parts of fly ash, 10-20 parts of a microbial agent, 20-30 parts of an adhesive and 5-15 parts of water, the modified coffee residue gel microspheres are prepared from modified coffee residue biochar, and the modified coffee residue biochar is prepared by modifying coffee residue, magnesium chloride hexahydrate and lanthanum nitrate hexahydrate according to a mass ratio of 1: 3: 1; the adhesive comprises bisphenol A epoxy resin, polyvinyl alcohol and sodium alginate, and the mass ratio of the bisphenol A epoxy resin to the polyvinyl alcohol to the sodium alginate to the water is 1: 4: 1: 0.5. The auxiliary material for aerobic fermentation of the coffee residue sludge is large in specific surface and rich in pores, can provide an enough living environment for microorganisms and increase the activity of the microorganisms, has the effect of improving aerobic fermentation of the sludge, further solves the difficulty of reutilization of the coffee residue by taking the coffee residue as a main raw material, and is beneficial to environmental protection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of solid waste resource utilization, and in particular to a coffee grounds sludge aerobic fermentation auxiliary material and a preparation method and application thereof. Background Art

[0002] Sludge is a by-product of sewage treatment, which has both pollution and resource properties. Urban sludge is a waste rich in organic matter. Its effective treatment and resource utilization have always been an important issue in environmental protection. Aerobic fermentation technology can achieve the degradation and stabilization of pollutants in sludge, and convert sludge into resource materials such as soil conditioners or organic fertilizers. It is one of the mainstream technologies for sludge treatment and disposal. Aerobic fermentation refers to the fact that under the condition of sufficient oxygen supply, organic solid waste produces a high temperature under the action of aerobic microorganisms, so that organic matter is biodegraded and harmless, and finally produces stable humification products. The aerobic fermentation process requires the addition of conditioners. Currently, commonly used conditioners include wood chips, sawdust, straw, etc. The above conditioners can adjust the moisture content and C / N ratio of the pile, and can also provide certain nutrients. However, the above conditioners are easily restricted by seasonality and regionality, and there are problems such as large storage area, high addition cost, difficulty in improving the physical structure of the pile, inability to recycle, and non-compliance with the concept of sustainable development, which limits the large-scale promotion of composting technology.

[0003] Coffee grounds are produced during the production and use of coffee. Studies have shown that coffee is one of the most popular drinks in the world. According to the 2021-2022 annual report of the International Coffee Organization (ICO), a total of 170.3 million bags of coffee, about 10 million tons, are consumed worldwide. It is estimated that 1 ton of raw coffee can produce about 650 kilograms of coffee grounds, and the global production of grounds in that year alone is as much as 6.5 million tons. Coffee grounds are mainly composed of cellulose, hemicellulose, lignin, lipids and proteins, etc., and can become potential biodegradable materials. They are valuable raw materials for a variety of bio-based products. If a large amount of coffee grounds are directly landfilled, they will produce methane, a gas related to the greenhouse effect, which will lead to the continuous deterioration of the global climate and even endanger human life. To this end, coffee grounds are reused as the main material of sludge aerobic fermentation conditioner, and a coffee ground sludge aerobic fermentation auxiliary material is developed, which effectively improves the efficiency of sludge fermentation while reducing the cost of sludge fermentation, which is of great significance for resource regeneration and environmental protection. Summary of the invention

[0004] The present invention aims to provide a coffee grounds sludge aerobic fermentation auxiliary material and a preparation method and application thereof. Coffee grounds are used as the main material for preparing the fermentation auxiliary material. The preparation method is simple and easy to implement, and recycling can be achieved to reduce the fermentation cost.

[0005] To achieve the above-mentioned purpose, the present invention provides a coffee ground sludge aerobic fermentation auxiliary material, which includes the following raw material components by mass: 100 parts of modified coffee ground gel microspheres, 5-10 parts of porous ceramic particles, 30-40 parts of fly ash, 10-20 parts of bacterial agent, 20-30 parts of adhesive and 5-15 parts of water. The modified coffee ground gel microspheres are made of modified coffee ground biochar, which is modified by coffee grounds, magnesium chloride hexahydrate and lanthanum nitrate hexahydrate in a mass ratio of 1:3:1. The adhesive includes bisphenol A epoxy resin, polyvinyl alcohol and sodium alginate, and the mass ratio of bisphenol A epoxy resin, polyvinyl alcohol, sodium alginate and water is 1:4:1:0.5. The porous ceramic particles are divided into first-grade ceramic particles and second-grade ceramic particles, and the particle size of the second-grade ceramic particles is larger than that of the first-grade ceramic particles.

[0006] Preferably, the particle size of the first-grade ceramic particles is 2-4 mm, the particle size of the second-grade ceramic particles is 5-8 mm, and the volume ratio of the first-grade ceramic particles to the second-grade ceramic particles is 2:1.

[0007] Preferably, the bacterial agent is an EM bacterial agent.

[0008] The present invention also provides a method for preparing a coffee grounds sludge aerobic fermentation auxiliary material, which is used to prepare the coffee grounds sludge aerobic fermentation auxiliary material. The steps for preparing the coffee grounds sludge aerobic fermentation auxiliary material are as follows:

[0009] S1: uniformly mixing the modified coffee grounds gel microspheres, second-grade ceramic particles, fly ash, a binder and water to obtain a blank;

[0010] S2: evenly spread the first-grade ceramic particles on the inner surface of the mold, then fill the blank into the mold, press-form and demold to obtain spherical particles with a diameter of 15-25 mm, dry the spherical particles, and naturally cure for 7-14 days to obtain the prepared auxiliary material;

[0011] S3: The prepared auxiliary material is evenly sprayed with the bacterial agent to obtain coffee ground sludge aerobic fermentation auxiliary material.

[0012] Preferably, the preparation steps of the modified coffee grounds gel microspheres are: 1) crushing the coffee grounds to remove impurities, washing, air-drying and sieving to obtain coffee grounds powder, preparing magnesium chloride hexahydrate and lanthanum nitrate hexahydrate into a solution in proportion and pouring it into a container containing coffee grounds powder, stirring and soaking for 12 hours, and then vacuum filtering, adding pure water for washing 3-5 times during the filtration process, placing the separated solid in an oven at 100°C for drying, and then pyrolyzing it at 600°C for 2 hours under oxygen-limited conditions, and cooling it to room temperature to obtain modified coffee grounds biochar. 2) Prepare a mixed solution with a NaOH mass fraction of 6.7% and a urea mass fraction of 12%, add cellulose and sodium alginate while stirring to obtain a cellulose-sodium alginate composite gel, then add the modified coffee grounds biochar under continuous stirring, stir evenly at room temperature to obtain a suspension, the mass ratio of the cellulose, sodium alginate and modified coffee grounds biochar added is 2:2:0.9, add the suspension dropwise into a mixed solution containing 5% mass fraction of CaCl2 and 5% HCl, solidify for 20 hours, filter and separate the solid, rinse with pure water until the solid surface is neutral, and freeze-dry to obtain the modified coffee grounds gel microspheres.

[0013] Preferably, the preparation steps of the adhesive are: adding polyvinyl alcohol, sodium alginate and water into a container and placing it in a 70°C water bath, stirring at 500 r / min for 1 hour to obtain a polyvinyl alcohol-sodium alginate solution; adding bisphenol A type epoxy resin dropwise to the polyvinyl alcohol-sodium alginate solution under a constant temperature state, stirring while adding until the mixture is evenly mixed to obtain the adhesive.

[0014] The invention also provides an application of a coffee grounds sludge aerobic fermentation auxiliary material, wherein the coffee grounds sludge aerobic fermentation auxiliary material is used for aerobic fermentation of municipal sludge.

[0015] Preferably, the method comprises the following steps: fully mixing the sludge and the coffee grounds sludge aerobic fermentation auxiliary material to obtain a mixed pile, adjusting the moisture content of the mixed pile to 55% to 65%, and then placing the mixed pile in an aerobic fermentation reaction tank for aerobic fermentation for 30-40 days to obtain an aerobic fermentation product, and turning the mixed pile for multiple times during the aerobic fermentation process; after the aerobic fermentation is completed, using a sifter to sieve the coffee grounds sludge aerobic fermentation auxiliary material from the aerobic fermentation product for recovery.

[0016] Preferably, the coffee grounds sludge aerobic fermentation auxiliary material to be recycled is soaked and rinsed until there is no obvious solid cover on the surface, and then dried and soaked in an ethanol solution for 6 to 12 hours, and then naturally air-dried and sprayed with a bacterial agent again for reuse.

[0017] Preferably, the mass ratio of the sludge to the coffee grounds sludge aerobic fermentation auxiliary material is 10:3-6.

[0018] Beneficial effects of the invention: The invention provides a coffee grounds sludge aerobic fermentation auxiliary material, which is made of modified coffee grounds gel microspheres, porous ceramic particles, fly ash, bacterial agent, adhesive and water in proportion. The coffee grounds sludge aerobic fermentation auxiliary material has a large specific surface area and rich pores, can provide a sufficient living environment for microorganisms, increase the activity of microorganisms, and has the effect of improving the aerobic fermentation of sludge. At the same time, using coffee grounds as the main raw material further solves the difficulty of reusing coffee grounds, which is beneficial to environmental protection. The coffee ground sludge aerobic fermentation auxiliary material modifies coffee grounds by co-loading magnesium and lanthanum, and prepares magnesium-lanthanum-coffee ground biochar by a one-step pyrolysis process. The surface chemical properties and physical structure characteristics of the coffee ground biochar before and after loading are changed, so that its adsorption capacity for phosphorus is enhanced, and the specific surface area of ​​the coffee grounds can be increased by more than 10 times, and modified coffee ground gel microspheres with a three-dimensional network structure are further made. The larger specific surface area provides more active sites, and the developed pore structure provides more residence space, which can enhance the transmission of oxygen, increase the activity of microorganisms, promote the process of aerobic fermentation of municipal sludge, and thus improve the conversion of insoluble phosphates. Different grades of ceramic particles are used, and ceramic particles of different particle sizes are combined. Large-particle ceramic particles are mainly used as aggregates to fill the interior of early fermentation auxiliary material particles, which can play a good supporting effect. Small-particle ceramic particles are mainly distributed on the outside of the fermentation auxiliary material particles to enhance the wear resistance of the fermentation auxiliary material particles and increase the living space of microorganisms. Further, bacterial agents are sprayed on the outside of the fermentation auxiliary material particles, and the bacterial agents are carried by ceramic particle aggregates. Since ceramic particles are porous expanded clay particles, they are relatively independent and will not be absorbed by sludge. Fermentation auxiliary materials and sludge can be evenly distributed through mixing to achieve uniform distribution of bacteria, avoid adding bacterial agents separately, and avoid uneven mixing of bacterial agents, which will cause waste and reduce fermentation efficiency. At the same time, an adhesive is obtained by compounding bisphenol A epoxy resin, polyvinyl alcohol and sodium alginate. The adhesive can bind the modified coffee grounds biochar, porous ceramic particles and fly ash into a whole. The fly ash can be filled in the gaps formed by the porous ceramic particles and the modified coffee grounds biochar to enhance the strength of the porous ceramic particles and the modified coffee grounds biochar without destroying the microporous structure between the two, so that the fermentation auxiliary material particles have a stable physical structure and good porosity. The stable physical structure makes the fermentation auxiliary material particles less lost in the subsequent fermentation process and have excellent recycling potential.

[0019] The present invention also proposes a method for preparing a coffee ground sludge aerobic fermentation auxiliary material. The preparation process is simple. Combined with modified coffee ground gel microspheres and the properties of various materials, they are added in batches. Second-level ceramic particles and modified coffee ground gel microspheres, fly ash, adhesive, etc. are first made into blanks to achieve the aggregate support effect of the second-level ceramic particles. First-level ceramic particles are laid on the inner surface of the mold and then the blanks are filled, thereby achieving the effect of evenly distributing the second-level ceramic particles on the outer surface of the auxiliary material particles. The first-level ceramic particles and the second-level ceramic particles are distributed inside and outside, and promote each other to greatly enhance the strength of the fermentation auxiliary material particles, laying a foundation for the subsequent recycling of coffee ground sludge aerobic fermentation auxiliary materials.

[0020] The present invention also proposes to apply coffee grounds sludge aerobic fermentation auxiliary material to municipal sludge aerobic fermentation. The coffee grounds sludge aerobic fermentation auxiliary material can be directly mixed with sludge to achieve a fermentation-promoting effect, is easy to use, and can be recycled and reused after fermentation, thereby greatly reducing the cost of sludge fermentation. DETAILED DESCRIPTION

[0021] The embodiments described below are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] The invention provides a coffee ground sludge aerobic fermentation auxiliary material, which comprises the following raw material components in mass fractions: 100 parts of modified coffee ground gel microspheres, 5-10 parts of porous ceramic particles, 30-40 parts of fly ash, 10-20 parts of bacterial agent, 20-30 parts of adhesive and 5-15 parts of water. The modified coffee ground gel microspheres are made of modified coffee ground biochar, which is modified by coffee grounds, magnesium chloride hexahydrate and lanthanum nitrate hexahydrate in a mass ratio of 1:3:1. The adhesive comprises bisphenol A epoxy resin, polyvinyl alcohol and sodium alginate, and the mass ratio of bisphenol A epoxy resin, polyvinyl alcohol, sodium alginate and water is 1:4:1:0.5. The porous ceramic particles are divided into first-grade ceramic particles and second-grade ceramic particles, and the particle size of the second-grade ceramic particles is larger than that of the first-grade ceramic particles.

[0023] The particle size of the first-grade ceramic particles is 2-4 mm, the particle size of the second-grade ceramic particles is 5-8 mm, and the volume ratio of the first-grade ceramic particles to the second-grade ceramic particles is 2:1.

[0024] The bacterial agent is an EM bacterial agent. The EM bacterial agent was purchased from Heilongjiang Lvsen Toner Technology Co., Ltd. and Nongfukang Co., Ltd. (Henan, China). Its specific composition includes: Proteobacteria 55.9±1.05%, Firmicutes 40.0±0.96%, Actinobacteria 3.63±0.16%; Ascomycota 96.5±3.71%, Basidiomycota 3.41±3.69%, etc.

[0025] The present invention also provides a method for preparing a coffee grounds sludge aerobic fermentation auxiliary material, which is used to prepare the coffee grounds sludge aerobic fermentation auxiliary material. The steps for preparing the coffee grounds sludge aerobic fermentation auxiliary material are as follows:

[0026] S1: uniformly mixing the modified coffee grounds gel microspheres, second-grade ceramic particles, fly ash, a binder and water to obtain a blank;

[0027] S2: evenly spread the first-grade ceramic particles on the inner surface of the mold, then fill the blank into the mold, press-form and demold to obtain spherical particles with a diameter of 15-25 mm, dry the spherical particles, and naturally cure for 7-14 days to obtain the prepared auxiliary material;

[0028] S3: The prepared auxiliary material is evenly sprayed with the bacterial agent to obtain coffee ground sludge aerobic fermentation auxiliary material.

[0029] It should be noted that a layer of release agent can be applied in advance on the inner surface of the mold to facilitate the subsequent demolding of the fermentation auxiliary material particles. The release agent is an oily release agent for concrete conversion, which is a milky yellow liquid in appearance, non-corrosive to the steel mold, and pH neutral. Other existing release agents can be used as long as the demolding effect can be achieved without causing damage to the fermentation auxiliary material particles. Furthermore, the inner surface of the mold can be provided with a plurality of pits, the diameter of which matches the size of the first-level ceramic particles, so as to facilitate the uniform dispersion of the first-level ceramic particles on the inner surface of the mold.

[0030] The preparation steps of the modified coffee grounds gel microspheres are as follows: 1) crushing coffee grounds to remove impurities, washing, air-drying and sieving to obtain coffee grounds powder, preparing magnesium chloride hexahydrate and lanthanum nitrate hexahydrate into a solution in proportion, pouring the solution into a container containing coffee grounds powder, stirring and soaking for 12 hours, and then vacuum filtering, adding pure water for washing 3-5 times during the filtration process, placing the separated solid in an oven for drying at 100°C, and then pyrolyzing at 600°C for 2 hours with limited oxygen, and cooling to room temperature to obtain modified coffee grounds biochar. 2) Prepare a mixed solution with a NaOH mass fraction of 6.7% and a urea mass fraction of 12%, add cellulose and sodium alginate while stirring to obtain a cellulose-sodium alginate composite gel, then add the modified coffee grounds biochar under continuous stirring, stir evenly at room temperature to obtain a suspension, the mass ratio of the cellulose, sodium alginate and modified coffee grounds biochar added is 2:2:0.9, add the suspension dropwise into a mixed solution containing 5% mass fraction of CaCl2 and 5% HCl, solidify for 20 hours, filter and separate the solid, rinse with pure water until the solid surface is neutral, and freeze-dry to obtain the modified coffee grounds gel microspheres.

[0031] The preparation steps of the adhesive are as follows: polyvinyl alcohol, sodium alginate and water are added into a container and placed in a 70° C. water bath, and stirred at 500 r / min for 1 hour to obtain a polyvinyl alcohol-sodium alginate solution; bisphenol A type epoxy resin is added dropwise into the polyvinyl alcohol-sodium alginate solution under a constant temperature state, and stirred while adding until the mixture is evenly mixed to obtain the adhesive.

[0032] The invention also provides an application of a coffee grounds sludge aerobic fermentation auxiliary material, wherein the coffee grounds sludge aerobic fermentation auxiliary material is used for aerobic fermentation of municipal sludge.

[0033] The method comprises the following steps: fully mixing sludge and coffee ground sludge aerobic fermentation auxiliary material to obtain a mixed pile, adjusting the moisture content of the mixed pile to 55%-65%, then placing the mixed pile in an aerobic fermentation reaction tank for aerobic fermentation for 30-40 days to obtain an aerobic fermentation product, and turning the mixed pile for multiple times during the aerobic fermentation process; and after the aerobic fermentation is completed, using a sifter to sieve the coffee ground sludge aerobic fermentation auxiliary material from the aerobic fermentation product for recovery.

[0034] The coffee grounds sludge aerobic fermentation auxiliary material to be recycled is soaked and rinsed until there is no obvious solid cover on the surface. After drying, the coffee grounds sludge aerobic fermentation auxiliary material to be recycled is placed in an ethanol solution and soaked for 6 to 12 hours. After natural air drying, it is sprayed with a bacterial agent again and can be used again.

[0035] The mass ratio of the sludge to the coffee grounds sludge aerobic fermentation auxiliary material is 10:3-6.

[0036] Example 1

[0037] The present embodiment provides a coffee ground sludge aerobic fermentation auxiliary material, which includes the following raw material components by weight: 100 parts of modified coffee ground gel microspheres, 8 parts of porous ceramic particles, 30 parts of fly ash, 12 parts of EM bacterial agent, 20 parts of binder and 10 parts of water. The porous ceramic particles are divided into first-grade ceramic particles and second-grade ceramic particles, the particle size of the first-grade ceramic particles is 3 mm, the particle size of the second-grade ceramic particles is 6 mm, and the volume ratio of the first-grade ceramic particles to the second-grade ceramic particles is 2:1.

[0038] The steps for preparing the coffee ground sludge aerobic fermentation auxiliary material are as follows: S1: uniformly mixing the modified coffee ground gel microspheres, the second-grade ceramic particles, fly ash, a binder and water to obtain a blank;

[0039] S2: evenly spread the first-grade ceramic particles on the inner surface of the mold, then fill the blank into the mold, press-form and demold to obtain spherical particles with a diameter of 20±1 mm, dry the spherical particles, and naturally cure for 7 days to obtain the prepared auxiliary material;

[0040] S3: The prepared auxiliary material is evenly sprayed with the EM bacterial agent to obtain a coffee ground sludge aerobic fermentation auxiliary material.

[0041] The preparation steps of the modified coffee grounds gel microspheres are as follows: 1) crushing coffee grounds to remove impurities, washing, air-drying and sieving to obtain coffee grounds powder, preparing magnesium chloride hexahydrate and lanthanum nitrate hexahydrate into a solution at a mass ratio of 1:3:1, pouring the solution into a container containing coffee grounds powder, stirring and soaking for 12 hours, and then vacuum filtering, adding pure water for washing 3-5 times during the filtration process, placing the separated solid in an oven for drying at 100°C, and then pyrolyzing at 600°C for 2 hours with limited oxygen, and cooling to room temperature to obtain modified coffee grounds biochar. 2) Prepare a mixed solution with a NaOH mass fraction of 6.7% and a urea mass fraction of 12%, add cellulose and sodium alginate while stirring to obtain a cellulose-sodium alginate composite gel, then add the modified coffee grounds biochar under continuous stirring, stir evenly at room temperature to obtain a suspension, the mass ratio of the cellulose, sodium alginate and modified coffee grounds biochar added is 2:2:0.9, add the suspension dropwise into a mixed solution containing 5% mass fraction of CaCl2 and 5% HCl, solidify for 20 hours, filter and separate the solid, rinse with pure water until the solid surface is neutral, and freeze-dry to obtain the modified coffee grounds gel microspheres.

[0042] The preparation steps of the adhesive are as follows: adding polyvinyl alcohol, sodium alginate and water into a container and placing it in a water bath at 70°C, stirring at 500r / min for 1h to obtain a polyvinyl alcohol-sodium alginate solution; adding bisphenol A epoxy resin dropwise to the polyvinyl alcohol-sodium alginate solution under a constant temperature state, stirring while adding until the mixture is uniform to obtain the adhesive. The mass ratio of bisphenol A epoxy resin, polyvinyl alcohol, sodium alginate and water is 1:4:1:0.5.

[0043] Example 2

[0044] The present embodiment provides a coffee ground sludge aerobic fermentation auxiliary material, which includes the following raw material components by weight: 100 parts of modified coffee ground gel microspheres, 5 parts of porous ceramic particles, 35 parts of fly ash, 17 parts of EM bacterial agent, 25 parts of binder and 10 parts of water. The porous ceramic particles are divided into first-grade ceramic particles and second-grade ceramic particles, the particle size of the first-grade ceramic particles is 3 mm, the particle size of the second-grade ceramic particles is 6 mm, and the volume ratio of the first-grade ceramic particles to the second-grade ceramic particles is 2:1.

[0045] The steps for preparing the coffee ground sludge aerobic fermentation auxiliary material are as follows: S1: uniformly mixing the modified coffee ground gel microspheres, the second-grade ceramic particles, fly ash, a binder and water to obtain a blank;

[0046] S2: evenly spread the first-grade ceramic particles on the inner surface of the mold, then fill the blank into the mold, press-form and demold to obtain spherical particles with a diameter of 20±1 mm, dry the spherical particles, and naturally cure for 7 days to obtain the prepared auxiliary material;

[0047] S3: The prepared auxiliary material is evenly sprayed with the EM bacterial agent to obtain a coffee ground sludge aerobic fermentation auxiliary material.

[0048] The preparation steps of the modified coffee grounds gel microspheres and the preparation steps of the binder are the same as those in Example 1.

[0049] Example 3

[0050] The present embodiment provides a coffee ground sludge aerobic fermentation auxiliary material, which includes the following raw material components by weight: 100 parts of modified coffee ground gel microspheres, 10 parts of porous ceramic particles, 40 parts of fly ash, 20 parts of EM bacterial agent, 30 parts of binder and 10 parts of water. The porous ceramic particles are divided into first-grade ceramic particles and second-grade ceramic particles, the particle size of the first-grade ceramic particles is 3 mm, the particle size of the second-grade ceramic particles is 6 mm, and the volume ratio of the first-grade ceramic particles to the second-grade ceramic particles is 2:1.

[0051] The steps for preparing the coffee ground sludge aerobic fermentation auxiliary material are as follows: S1: uniformly mixing the modified coffee ground gel microspheres, the second-grade ceramic particles, fly ash, a binder and water to obtain a blank;

[0052] S2: evenly spread the first-grade ceramic particles on the inner surface of the mold, then fill the blank into the mold, press-form and demold to obtain spherical particles with a diameter of 20±1 mm, dry the spherical particles, and naturally cure for 7 days to obtain the prepared auxiliary material;

[0053] S3: The prepared auxiliary material is evenly sprayed with the EM bacterial agent to obtain a coffee ground sludge aerobic fermentation auxiliary material.

[0054] The preparation steps of the modified coffee grounds gel microspheres and the preparation steps of the binder are the same as those in Example 1.

[0055] Comparative Example

[0056] The present comparative example provides a coffee ground sludge aerobic fermentation auxiliary material, which includes the following raw material components in parts by weight: 100 parts of coffee ground biochar, 50 parts of fly ash, 20 parts of EM bacterial agent, 30 parts of adhesive and 20 parts of water.

[0057] The steps for preparing the coffee ground sludge aerobic fermentation auxiliary material are as follows: S1: mixing coffee ground biochar, fly ash, a binder and water evenly to obtain a blank;

[0058] S2: The blank is filled into a mold, press-formed, and then demolded to obtain spherical particles with a diameter of 20±1 mm, and the spherical particles are dried and naturally cured for 7 days to obtain a prepared auxiliary material;

[0059] S3: The prepared auxiliary material is evenly sprayed with the EM bacterial agent to obtain a coffee ground sludge aerobic fermentation auxiliary material.

[0060] The preparation steps of the coffee grounds biochar are as follows: crushing the coffee grounds to remove impurities, washing, air-drying and sieving to obtain coffee grounds powder, then subjecting the coffee grounds powder to oxygen-limited pyrolysis at 600° C. for 2 hours, and cooling to room temperature to obtain coffee grounds biochar.

[0061] The coffee grounds sludge aerobic fermentation auxiliary materials of Examples 1-3 and Comparative Example 1 were subjected to sludge fermentation test.

[0062] The ingredients are as follows:

[0063] Group A: sludge (from Guangzhou Datansha Sewage Treatment Plant, with a water content of 65%) + coffee grounds sludge aerobic fermentation auxiliary material in Example 1, the mass ratio of sludge to auxiliary material is 10:4;

[0064] Group B: sludge (from Guangzhou Datansha Sewage Treatment Plant, with a water content of 65%) + coffee grounds sludge aerobic fermentation auxiliary material in Example 2, the mass ratio of sludge to auxiliary material was 10:4;

[0065] Group C: sludge (from Guangzhou Datansha Sewage Treatment Plant, with a water content of 65%) + coffee grounds sludge aerobic fermentation auxiliary material in Example 3, the mass ratio of sludge to auxiliary material is 10:4;

[0066] Group D: sludge (from Guangzhou Datansha Sewage Treatment Plant, with a water content of 65%) + coffee grounds sludge aerobic fermentation auxiliary material in Comparative Example 1, the mass ratio of sludge to auxiliary material is 10:4;

[0067] The sludge fermentation treatment steps are as follows: the materials of groups A, B, C and D are mixed evenly and adjusted to a moisture content of 60±2%, and then placed in an aerobic fermentation tank for aerobic fermentation treatment. The bottom of the aerobic fermentation tank is provided with aeration holes, and ventilation is performed once per hour for 2 minutes each time. The sludge is turned over once on the second, eighth and 21st days of fermentation, and the initial fermentation is terminated on the 35th day. Samples are taken on days 0, 3, 7, 11, 16, 21, 28 and 35. All samples are sampled in the middle and around the pile using the five-point method and averaged. A part of the sample is air-dried under natural conditions to remove large impurities such as stones and plastics. After being crushed by a crusher, the samples are passed through 16 mesh, 60 mesh and 100 mesh sieves respectively. After that, the samples are packed in sealed bags, marked and stored in a desiccator for the detection of organic matter (OM) and available phosphorus (AP). The other part is stored in a refrigerator at 4°C for the detection of germination index (GI).

[0068] Determination of organic matter: Weigh 0.5g of naturally air-dried sample, put it into a crucible of known weight, place it in a 105℃ oven to dry to constant weight, take it out and put it in a desiccator to cool to room temperature, weigh it and record it, then put the crucible in a muffle furnace and heat it to 550℃ and burn it for 5h, take it out and cool it in a desiccator and weigh it. Make 3 parallels for each sample. The organic matter content is the mass loss of the sample before and after burning.

[0069] Determination of available phosphorus: weigh 2.5g of air-dried sample (passed through a 20-mesh sieve) in a 100mL conical flask, add 0.5mol / L sodium bicarbonate extractant, oscillate in a constant temperature oscillator at 25°C at an oscillation frequency of 200r / min for 30min, filter, draw 5mL of filtrate in a 50mL stoppered colorimetric tube, add 10mL of 0.5mol / L NaHCO3 solution, dilute to 30mL with deionized water, add 2 drops of dinitrophenol indicator, add 5mL of molybdenum antimony reagent to the volume and shake well, and use a UV spectrophotometer to compare colors at 880nm after 30min. The available phosphorus of the sample is determined according to HJ 704-2014 "Determination of Available Phosphorus in Soil by Sodium Bicarbonate Extraction-Molybdenum Antimony Antispectrophotometry".

[0070] Determination of seed germination rate: Weigh 5.0g of fresh samples at the end of aerobic fermentation in each experimental group, put them into a 100mL conical flask, add deionized water at a solid-liquid ratio of 1:10, shake at room temperature for 12 hours, and centrifuge. Spread a piece of filter paper on the bottom of the culture dish, take 20 rapeseeds and evenly disperse them in the culture dish, absorb 5mL of the extract into the culture dish, use deionized water as a blank control, and then place it in a 30℃ constant temperature incubator for 48 hours. After the culture is completed, the germination rate and the length of the germinated root are counted. Each sample is paralleled for 3 times, and the seed germination rate is finally calculated by the following formula.

[0071]

[0072] The test data of aerobic fermentation process of AD group are shown in Table 1, Table 2 and Table 3.

[0073] Table 1 is the test data of organic matter% in aerobic fermentation process of AD group

[0074] project 0d 3d 7d 11d 16d 21d 28d 35d Group A 58.34% 55.27% 50.16% 47.26% 45.17% 41.24% 39.18% 36.62% Group B 58.23% 55.38% 51.28% 48.98% 45.37% 42.36% 40.68% 39.07% Group C 58.29% 55.21% 50.98% 46.24% 45.39% 42.28% 39.26% 37.86% Group D 56.97% 53.87% 49.87% 48.46% 47.56% 46.86% 43.38% 42.26%

[0075] Table 2 shows the test data of available phosphorus in the aerobic fermentation process of the AD group

[0076]

[0077] Table 3 shows the test data of seed germination rate in aerobic fermentation process of AD group

[0078]

[0079] From the above data we can see that:

[0080] 1. Organic matter (OM) is the carbon source and nutrient source that microorganisms rely on for their activities in the aerobic fermentation process. Under the action of microorganisms, organic matter is converted into minerals, humus, CO2 and H2O through mineralization and humification processes, which can achieve the stabilization and resource utilization of municipal sludge. Table 1 shows the change law of organic matter in different treatment groups during the aerobic fermentation of sludge. The organic matter showed a downward trend throughout the aerobic fermentation cycle. At the end of aerobic fermentation, the organic matter content of the AD group was 36.62%, 39.07%, 37.86% and 42.26%, respectively. Compared with the beginning of aerobic fermentation, each group decreased by 21.72%, 19.16%, 20.43% and 14.71%, respectively. It shows that adding coffee grounds sludge aerobic fermentation auxiliary materials can improve the aerobic environment in the pile, increase the activity of microorganisms, and promote the degradation of organic matter in the aerobic fermentation of municipal sludge. Modification of coffee grounds to make modified coffee grounds gel microspheres is more conducive to promoting the degradation of organic matter in the aerobic fermentation of sludge, and the fermentation effect is better.

[0081] 2.AP refers to the phosphorus components that can be absorbed by plants. These phosphorus components include all water-soluble phosphorus, partly adsorbed phosphorus and organic phosphorus, which are of great significance to the growth and development of plants. The change law of AP during aerobic fermentation is shown in Table 2. The AP of each group showed a wave-like upward trend throughout the aerobic fermentation stage, and the AP of the AC group was always higher than that of the D group. At the beginning of aerobic fermentation, the AP content of the AD group was 2674.68 mg / kg, 2645.78 mg / kg, 2684.64 mg / kg, and 2474.09 mg / kg, respectively. When the aerobic fermentation ended, the humification degree continued to increase and the AP content continued to rise. The A content of each treatment group was higher than the initial value, that is, the AD group increased by 26.2%, 24.6%, 25.0%, and 13.2%, respectively. It can be seen that the addition of coffee grounds sludge aerobic fermentation auxiliary materials enhances the dissolution of insoluble phosphate phosphorus in the municipal sludge aerobic fermentation system and significantly increases the AP content in the pile.

[0082] 3. The seed germination index (GI) is one of the indicators for evaluating the maturity of aerobic fermentation and the phytotoxicity of aerobic fermentation. It is generally believed that when the GI is ≥80%, the pile has reached maturity or has no phytotoxicity. Table 3 shows the GI of the aerobic fermentation products of the AD group. It can be seen that the seed germination index of the AD group is greater than 80%, which can be considered to be non-toxic to plants and has reached the maturity standard. The GI of the coffee ground sludge aerobic fermentation auxiliary material made of modified coffee ground gel microspheres is significantly higher than that of the coffee ground sludge aerobic fermentation auxiliary material group made directly from coffee ground biochar. This also shows that the coffee ground sludge aerobic fermentation auxiliary material can promote the maturity of municipal sludge aerobic fermentation and has low toxicity to plants.

[0083] The present invention is described in detail above in conjunction with the embodiments. It should be noted that the various specific technical features described in the above specific embodiments can be combined and changed in any suitable manner without contradiction, and the present invention will not further describe various possible combinations. In addition, other variations and combinations of the various technical features of the present invention should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A coffee grounds sludge aerobic fermentation auxiliary material, characterized in that: The coffee ground sludge aerobic fermentation auxiliary material includes the following raw material components in parts by mass: 100 parts of modified coffee ground gel microspheres, 5-10 parts of porous ceramic particles, 30-40 parts of fly ash, 10-20 parts of bacterial agent, 20-30 parts of adhesive and 5-15 parts of water; the modified coffee ground gel microspheres are made of modified coffee ground biochar, and the modified coffee ground biochar is modified by coffee grounds, magnesium chloride hexahydrate and lanthanum nitrate hexahydrate in a mass ratio of 1:3:1; the adhesive includes bisphenol A epoxy resin, polyvinyl alcohol and sodium alginate, and the mass ratio of bisphenol A epoxy resin, polyvinyl alcohol, sodium alginate and water is 1:4:1:0.5, and the porous ceramic particles are divided into first-level ceramic particles and second-level ceramic particles, and the particle size of the second-level ceramic particles is larger than that of the first-level ceramic particles.

2. The coffee grounds sludge aerobic fermentation auxiliary material according to claim 1, characterized in that: The particle size of the first-grade ceramic particles is 2-4 mm, the particle size of the second-grade ceramic particles is 5-8 mm, and the volume ratio of the first-grade ceramic particles to the second-grade ceramic particles is 2:

1.

3. The coffee grounds sludge aerobic fermentation auxiliary material according to claim 1, characterized in that: The bacterial agent is an EM bacterial agent.

4. A method for preparing a coffee grounds sludge aerobic fermentation auxiliary material, used for preparing the coffee grounds sludge aerobic fermentation auxiliary material according to any one of claims 1 to 3, characterized in that: The steps for preparing the coffee grounds sludge aerobic fermentation auxiliary material are as follows: S1: uniformly mixing the modified coffee grounds gel microspheres, second-grade ceramic particles, fly ash, a binder and water to obtain a blank; S2: evenly spread the first-grade ceramic particles on the inner surface of the mold, then fill the blank into the mold, press-form and demold to obtain spherical particles with a diameter of 15-25 mm, dry the spherical particles, and naturally cure for 7-14 days to obtain the prepared auxiliary material; S3: The prepared auxiliary material is evenly sprayed with the bacterial agent to obtain coffee ground sludge aerobic fermentation auxiliary material.

5. The method for preparing coffee grounds sludge aerobic fermentation auxiliary material according to claim 4, characterized in that: The preparation steps of the modified coffee grounds gel microspheres are as follows: 1) crushing coffee grounds to remove impurities, washing, air-drying and sieving to obtain coffee grounds powder, preparing magnesium chloride hexahydrate and lanthanum nitrate hexahydrate into a solution in proportion, pouring the solution into a container containing coffee grounds powder, stirring and soaking for 12 hours, and then vacuum filtering, adding pure water for washing 3-5 times during the filtration process, putting the separated solid into an oven for drying at 100°C, and then pyrolyzing at 600°C for 2 hours with limited oxygen, and cooling to room temperature to obtain modified coffee grounds biochar; 2) preparing a 6.7% mass fraction of NaOH and a urea-based A mixed solution with a mass fraction of 12%, cellulose and sodium alginate are added while stirring to obtain a cellulose-sodium alginate composite gel, and then the modified coffee grounds biochar is added under continuous stirring, and the suspension is evenly stirred at room temperature. The mass ratio of the cellulose, sodium alginate and modified coffee grounds biochar is 2:2:0.

9. The suspension is dropwise added into a mixed solution containing 5% mass fraction of CaCl2 and 5% HCl, and cured for 20 hours. The solid is filtered and separated and rinsed with pure water until the solid surface is neutral, and freeze-dried to obtain the modified coffee grounds gel microspheres.

6. The method for preparing coffee grounds sludge aerobic fermentation auxiliary material according to claim 4, characterized in that: The preparation steps of the adhesive are as follows: polyvinyl alcohol, sodium alginate and water are added into a container and placed in a 70° C. water bath, and stirred at 500 r / min for 1 hour to obtain a polyvinyl alcohol-sodium alginate solution; The adhesive is obtained by adding bisphenol A epoxy resin dropwise to the polyvinyl alcohol-sodium alginate solution under a constant temperature state, stirring while adding until the mixture is evenly mixed.

7. An application of coffee grounds sludge as an auxiliary material for aerobic fermentation, characterized in that: The coffee grounds sludge aerobic fermentation auxiliary material is used for aerobic fermentation of municipal sludge.

8. The use of coffee grounds sludge aerobic fermentation auxiliary material according to claim 7, characterized in that: The following steps are involved: The sludge and the coffee ground sludge aerobic fermentation auxiliary material are fully mixed to obtain a mixed pile, the moisture content of the mixed pile is adjusted to 55% to 65%, and then the mixed pile is placed in an aerobic fermentation reaction tank for aerobic fermentation for 30-40 days to obtain an aerobic fermentation product, and the mixed pile is turned over several times during the aerobic fermentation process; after the aerobic fermentation is completed, the coffee ground sludge aerobic fermentation auxiliary material is screened out from the aerobic fermentation product using a sifter for recovery.

9. The use of coffee grounds sludge aerobic fermentation auxiliary material according to claim 8, characterized in that: The coffee grounds sludge aerobic fermentation auxiliary material to be recycled is soaked and rinsed until there is no obvious solid cover on the surface. After drying, the coffee grounds sludge aerobic fermentation auxiliary material to be recycled is placed in an ethanol solution and soaked for 6 to 12 hours. After natural air drying, it is sprayed with a bacterial agent again and can be used again.

10. The use of coffee grounds sludge as an auxiliary material for aerobic fermentation according to claim 8, characterized in that: The mass ratio of the sludge to the coffee grounds sludge aerobic fermentation auxiliary material is 10:3-6.

Citation Information

Patent Citations

  • Biological mixed bacterial fertilizer and preparation method and application thereof

    CN107285918A

  • Adsorption ball for organic pollutants in water

    CN108190995A

  • Sewage processing process using microbial carrier

    CN110981079A

  • Preparation method and application of perishable garbage fermentation inoculant carrier

    CN112812333A

  • Synthesis method of magnetic phosphate adsorbent for algae inhibition and agricultural fertilizer

    CN115990461A

Cited By

  • Activated sludge index monitoring device and detection method thereof

    CN120009267A