Nitrogen-containing heterocyclic resin, preparation method and application thereof, and adsorbent

By introducing a nitrogen-containing heterocyclic structure into the resin, a highly selective adsorbent was prepared, which solved the problem of insufficient selectivity when adsorbing metals such as nickel and copper in the existing resin solid-phase extraction method, and achieved high efficiency in an acidic environment Separation effect.

CN118930695APending Publication Date: 2024-11-12SHANGHAI XIGU TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310533284.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing resin solid-phase extraction methods are insufficient in adsorbing metals such as nickel and copper, and it is difficult to meet the needs of efficient separation.

Method used

Using nitrogen-containing heterocyclic resin as adsorbent, the connecting bridge structure between the resin matrix and nitrogen-containing heterocyclic substituent is improved to improve the selectivity of metals. The nitrogen-containing heterocyclic resin is prepared by substitution reaction, and its adsorption is applied in acidic solutions. ability.

Benefits of technology

The selectivity and separation effect of metal elements are significantly improved, especially in an acidic environment, which shows excellent performance for separation of copper, nickel, etc., and simplifies the process flow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118930695A_ABST
    Figure CN118930695A_ABST
Patent Text Reader

Abstract

The invention provides nitrogen-containing heterocyclic resin, a preparation method and application thereof and an adsorbent, the nitrogen-containing heterocyclic resin comprises the following structural formula (1): # imgabs0 # P is a resin matrix,-CH2-N-is a connecting bridge of P and R1 or R2; r1 and R2 are the same or different nitrogen-containing heterocyclic ring substituents respectively. According to the nitrogen-containing heterocyclic ring resin provided by the invention, the selectivity on metal elements is high, and a new separation material is provided for an extraction process technology; in addition, the nitrogen-containing heterocyclic resin of the present invention can be used in an acidic solution (pHlt; 3) selectively adsorbing copper, nickel and the like; in addition, the preparation method provided by the invention is simple in process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of organic synthesis, and in particular to a nitrogen-containing heterocyclic resin, a preparation method thereof, a use thereof, and an adsorbent thereof. Background Art

[0002] Resin solid phase extraction is an important method in metal purification and separation processes. It has a wide range of applications in metal separation and purification, including chemical industry, electroplating, metallurgy, non-ferrous metal mining, and new energy industries. Resin solid phase extraction can make the atoms on the functional groups on the resin react with the metal through material design to form a chelate with a stable structure, thereby selectively separating and enriching the metal elements in the dilute solution. Compared with the traditional solvent extraction method, the resin method has the characteristics of fast phase separation, simple operation, low pollution, and low process cost.

[0003] However, the existing resin solid phase extraction method still cannot meet the requirements of high selective adsorption, especially in the application of adsorbing metals such as nickel and copper.

[0004] Therefore, it is necessary to provide a new resin material and a method for solid phase extraction of metals to further improve the selectivity in metal adsorption, thereby improving the separation effect of metal elements, especially metals such as nickel and copper. Summary of the invention

[0005] In view of this, the present invention provides a resin material having a better selective adsorption effect on metal elements, a preparation method, a use thereof, and an adsorbent.

[0006] As described above, the present invention provides the following technical solutions:

[0007] In a first aspect, the present invention discloses a nitrogen-containing heterocyclic resin, comprising a nitrogen-containing heterocyclic resin represented by the following structural formula (1):

[0008]

[0009] in:

[0010] P is the resin matrix;

[0011] -CH2-N- is a connecting bridge between P and R1 or R2;

[0012] R1 and R2, which are the same or different, are nitrogen-containing heterocyclic substituents.

[0013] For the purpose of the present invention, the resin matrix P is not particularly limited.

[0014] Preferably, the resin matrix P is selected from any one or more of polystyrene resin, copolymer of styrene and divinylbenzene, phenolic resin polymer, polyacrylic resin, and silicon-based resin.

[0015] Furthermore, the nitrogen-containing heterocyclic substituents R1 and R2 are independently 2-methylenepyridine and its derivatives, imidazole and its derivatives, benzimidazole and its derivatives, pyrazine and its derivatives, quinoline and its derivatives, triazine and its derivatives or triazole and its derivatives, wherein at least one of R1 and R2 is not a 2-methylenepyridine functional group.

[0016] Furthermore, the nitrogen-containing heterocyclic substituents R1 and R2 are independently selected from any of the following groups:

[0017]

[0018]

[0019] Furthermore, the nitrogen-containing heterocyclic substituents R1 and R2 are independently selected from any of the following groups:

[0020]

[0021]

[0022] In another aspect, the present invention provides a method for preparing a nitrogen-containing heterocyclic resin, which is used to prepare the nitrogen-containing heterocyclic resin of the first aspect comprising the above structural formula (1), the method comprising the following steps:

[0023] S1, providing a resin base material, wherein the resin base material is a resin containing primary amino groups;

[0024] S2, allowing the primary amino group of the resin base material to undergo a substitution reaction with a nitrogen-containing heterocyclic chloride to obtain the nitrogen-containing heterocyclic resin.

[0025] In the present invention, step S2 includes:

[0026] S21a, allowing the primary amino group of the resin base material to undergo one-step substitution with the first nitrogen-containing heterocyclic chloride R1Cl in an alkaline solution under heating conditions to obtain a first intermediate compound, the structural formula of the first intermediate compound being as shown in the following formula (2);

[0027]

[0028] S22a, allowing the first intermediate compound and the second nitrogen-containing heterocyclic chloride R2Cl to undergo two-step substitution under the same conditions as in step S21a to obtain the nitrogen-containing heterocyclic resin, wherein R1 and R2 are as described in the first aspect above.

[0029] Furthermore, the resin base material is selected from any one or more of the following resins: polystyrene microspheres containing primary amino groups, modified phenolic resins containing primary amino groups, polyacrylic acid resins containing primary amino groups, and silicon-based resins containing primary amino groups.

[0030] Furthermore, the molar ratio of the primary amino group of the resin base material to the first nitrogen-containing heterocyclic chloride R1Cl and the second nitrogen-containing heterocyclic chloride R2Cl is 1:(0.5-1.5):(0.5-1.5).

[0031] Furthermore, the alkali contained in the alkaline solution is 1-3 times the equivalent of the nitrogen-containing heterocyclic chloride.

[0032] Furthermore, the solvent of the alkaline solution is 2-50 times the mass of the nitrogen-containing heterocyclic chloride, the heating temperature is 40-120° C., and the reaction time is 3-36 hours.

[0033] Furthermore, the base is selected from any one or more of sodium carbonate, sodium bicarbonate, sodium hydroxide, potassium carbonate, potassium bicarbonate, potassium hydroxide, triethylamine, and N,N-diisopropylethylamine.

[0034] Furthermore, the solvent is selected from any one or more of water, N,N-dimethylformamide, dimethyl sulfoxide, toluene, tetrahydrofuran, ethanol, acetonitrile and acetone.

[0035] In the present invention, step S2 includes:

[0036] The primary amino group of the resin base material and the first nitrogen-containing heterocyclic chloride R1Cl undergo a substitution reaction in an alkaline solution under heating conditions to obtain the nitrogen-containing heterocyclic resin, the structural formula of which is shown in the following formula (3);

[0037]

[0038] Wherein, R1 and R2 are as described above.

[0039] Furthermore, the molar ratio of the resin base material to the nitrogen-containing heterocyclic chloride is 1:(1.5-4).

[0040] According to a third aspect of the present invention, there is provided a use of the nitrogen-containing heterocyclic resin of the first aspect for adsorbing metals, wherein the metal is any one or more of mercury, gallium, iron, cobalt, nickel, copper, zinc, lead, indium, cadmium, manganese, aluminum, uranium, vanadium, platinum group elements, gold, and silver.

[0041] Furthermore, the metal comprises one or more of cobalt, nickel, copper, zinc, cadmium, manganese and aluminum; preferably comprises one or more of nickel and copper.

[0042] Further, the nitrogen-containing hybrid resin is used to adsorb metals in hydrometallurgy, waste disposal, recycling industry or electroplating.

[0043] According to a fourth aspect of the present invention, there is provided an adsorbent comprising the nitrogen-containing heterocyclic resin described in the first aspect.

[0044] According to a fifth aspect of the present invention, there is provided a method for solid phase extraction of metal elements, using the adsorbent provided in the fourth aspect.

[0045] More specifically, the method comprises: using the nitrogen-containing heterocyclic resin as an adsorbent to extract the metal in the metal-containing solution to obtain the metal-loaded nitrogen-containing heterocyclic resin and the residual water phase; then washing and stripping the metal-loaded nitrogen-containing heterocyclic resin in sequence to obtain a metal-rich stripping solution and a stripped resin.

[0046] Furthermore, the metal adsorbed by the solid phase extraction method of metal elements is selected from any one or more of mercury, gallium, iron, cobalt, nickel, copper, zinc, lead, indium, cadmium, manganese, aluminum, uranium, vanadium, platinum group elements, gold and silver.

[0047] Furthermore, the adsorbed metal is selected from one or more of cobalt, nickel, copper, zinc, cadmium, manganese, and aluminum, and further selected from one or more of nickel, copper, and cobalt.

[0048] Preferably, the detergent used for washing in the method is a dilute acid solution, and the stripping agent used for stripping is a sulfuric acid or hydrochloric acid solution, further a sulfuric acid solution.

[0049] The method is simple to operate and has good metal separation effect.

[0050] The above technical solution of the present invention has at least one of the following beneficial effects:

[0051] The nitrogen-containing heterocyclic resin according to the embodiment of the present invention has high selectivity for metal elements through the nitrogen-containing functional group, and provides a new separation material for new extraction process technology;

[0052] Moreover, the selectivity for metal elements can be improved by increasing the number of nitrogen-containing functional groups;

[0053] In addition, the nitrogen-containing heterocyclic resin of the present invention can adsorb copper, nickel, etc. in an acidic solution (pH <3), and can separate copper and nickel from impurity metals such as iron, zinc, and cadmium, with good separation effect;

[0054] In addition, the preparation method provided by the present invention has simple process. DETAILED DESCRIPTION

[0055] In the following, various aspects of the invention will be described in more detail as well as further objects, features and advantages.

[0056] Unless otherwise defined, the technical terms or scientific terms used in the present invention shall have the common meanings understood by persons with ordinary skills in the field to which the present invention belongs. The words "first", "second" and similar words used in the present invention do not indicate any order, quantity or importance, but are only used to distinguish different components.

[0057] Hereinafter, the nitrogen-containing heterocyclic resin according to the present invention is first described.

[0058] The nitrogen-containing heterocyclic resin according to the present invention comprises a nitrogen-containing heterocyclic resin represented by the following structural formula (1):

[0059]

[0060] in:

[0061] P is the resin matrix;

[0062] -CH2-N- is a connecting bridge between P and R1 or R2;

[0063] R1 and R2, which are the same or different, are nitrogen-containing heterocyclic substituents.

[0064] The inventors unexpectedly found that the nitrogen-containing heterocyclic resin according to the present invention has high selectivity for metal elements; and the selectivity for metal ions can be improved by increasing the number of nitrogen-containing functional groups; in addition, the nitrogen-containing heterocyclic resin of the present invention can adsorb copper, nickel, etc. in an acidic solution (pH<3), providing a new separation material for new extraction process technology.

[0065] Furthermore, the resin matrix P is not particularly limited, and is preferably selected from any one or more of polystyrene resin, copolymer of styrene and divinylbenzene, phenolic resin polymer, polyacrylic resin, and silicon-based resin.

[0066] Preferably, the resin matrix P described in the present invention is one or more of polystyrene resin and copolymers of styrene and divinylbenzene.

[0067] Further, the nitrogen-containing heterocyclic substituents R1 and R2 are independently 2-methylenepyridine and its derivatives, imidazole and its derivatives, benzimidazole and its derivatives, pyrazine and its derivatives, quinoline and its derivatives, triazine and its derivatives or triazole and its derivatives, wherein at least one of R1 and R2 is not a 2-methylenepyridine functional group. These nitrogen-containing functional groups have high selectivity for metal elements and are therefore preferred.

[0068] The R1 and R2 can be the same or different groups. Furthermore, they are preferably the same group. When R1 and R2 are the same group, the preparation method is simpler and the three wastes in the production process are less.

[0069] Furthermore, the nitrogen-containing heterocyclic substituents R1 and R2 are independently selected from any of the following groups:

[0070]

[0071]

[0072] These nitrogen-containing functional groups are preferred because of their strong selectivity for metals.

[0073] Furthermore, the nitrogen-containing heterocyclic substituents R1 and R2 are independently selected from any of the following groups:

[0074]

[0075]

[0076] In the present invention, a nitrogen-containing heterocyclic resin having the following structure is provided:

[0077]

[0078]

[0079] Next, the preparation of the nitrogen-containing heterocyclic resin represented by the above structural formula (1) using a resin containing a primary amino group as a starting material is further described by the following exemplary preparation method.

[0080] The method according to the present invention comprises the following steps:

[0081] S1, providing a resin base material, wherein the resin base material is a resin containing primary amino groups;

[0082] S2, allowing the primary amino group of the resin base material to undergo a substitution reaction with a nitrogen-containing heterocyclic chloride to obtain the nitrogen-containing heterocyclic resin.

[0083] Specifically, the synthetic route of the method of the present invention is as follows:

[0084]

[0085] That is to say, in the method of the present invention, step S2 specifically includes:

[0086] S21a, allowing the primary amino group of the resin base material to undergo one-step substitution with the first nitrogen-containing heterocyclic chloride R1Cl in an alkaline solution under heating conditions to obtain a first intermediate compound, the structural formula of the first intermediate compound being as shown in the following formula (2);

[0087]

[0088] S22a, subjecting the first intermediate compound and the second nitrogen-containing heterocyclic chloride R2Cl to two-step substitution under the same conditions as in step S21a, to obtain the nitrogen-containing heterocyclic resin, wherein R1 and R2 are as described above for the nitrogen-containing heterocyclic resin. Preferably, the resin base material is selected from any one or more of the following resins: polystyrene microspheres containing primary amino groups, modified phenolic resins containing primary amino groups, polyacrylic resins containing primary amino groups, and silicon-based resins containing primary amino groups.

[0089] Preferably, the molar ratio of the resin base material to the first nitrogen-containing heterocyclic chloride R1Cl and the second nitrogen-containing heterocyclic chloride R2Cl is 1:(0.5-1.5):(0.5-1.5).

[0090] Preferably, the base contained in the alkaline solution is 1-3 times the equivalent of the nitrogen-containing heterocyclic chloride.

[0091] Preferably, the solvent of the alkaline solution is 2-50 times the mass of the nitrogen-containing heterocyclic chloride, the heating temperature is 40-120° C., and the reaction time is 3-36 hours.

[0092] Preferably, the base is selected from any one or more of sodium carbonate, sodium bicarbonate, sodium hydroxide, potassium carbonate, potassium bicarbonate, potassium hydroxide, triethylamine, and N,N-diisopropylethylamine.

[0093] Preferably, the solvent is selected from any one or more of water, N,N-dimethylformamide, dimethyl sulfoxide, toluene, tetrahydrofuran, ethanol, acetonitrile and acetone.

[0094] In the above step S22a, the two-step substitution reaction is carried out under the same conditions as step S21a except that the second nitrogen-containing heterocyclic chloride R2Cl is used instead of the first nitrogen-containing heterocyclic chloride R1Cl. Of course, in step S22a, the specific base and solvent used can be selected from the above reagents and can be different from step S21a.

[0095] It should be noted that, similarly, in the above method, there is also a situation where R1 and R2 are the same nitrogen-containing heterocyclic substituents and different nitrogen-containing heterocyclic substituents, respectively. For R1 and R2 being the same nitrogen-containing heterocyclic substituents, that is to say, the above step S2 can be completed by a one-step reaction. That is, compared to the above preparation method, in the step S2, the resin base material and the first nitrogen-containing heterocyclic chloride R1Cl are substituted in an alkaline solution under heating conditions to obtain the nitrogen-containing heterocyclic resin, and the molar ratio of the resin base material to the nitrogen-containing heterocyclic chloride is 1: (1.5-4). In addition, the target compound can be prepared by the same steps as the above preparation method.

[0096] The "selectivity" described in the present invention is represented by the separation coefficient β of the metal element. Further, the separation coefficient is obtained by the following formula:

[0097] β A / B =D A / D B =E A .(1-E B ) / ((1-E A ).E B )

[0098] Where D A It indicates the ratio of the content of metal element A in the resin to the content of metal element A in the raffinate water phase after one extraction is completed;

[0099] D B It indicates the ratio of the content of metal element B in the resin to the content of metal element B in the raffinate water phase after one extraction is completed;

[0100] E A 、E B It represents the extraction rate of metal element A and metal element B (extraction rate E=the content of metal element in the resin after one extraction / the content of metal element in the initial water phase×100%).

[0101] The metal extraction rate in the formula is measured by the following method:

[0102] Resin pretreatment: Mix the resin with 2 mol / L sulfuric acid and stir until the supernatant is colorless, then wash with 0.25 mol / L sodium hydroxide solution until the supernatant is alkaline, then wash the resin with pure water until it is neutral, filter and set aside;

[0103] 30 mL of sulfate solution containing 0.05 g / L of each metal element was prepared as the initial aqueous phase, and the pH value of the initial aqueous phase was adjusted. Then, it was mixed and stirred with 5 g of pretreated resin at room temperature for 60 min at a rotation speed of 250 rpm / min to allow the adsorption to reach equilibrium. After stirring, the solid-liquid separation was performed to obtain a raffinate (equilibrium) aqueous phase, and the concentration of each metal element in the raffinate aqueous phase was determined by inductively coupled plasma emission spectroscopy (ICP), and the content of the metal elements in the resin was calculated by subtraction.

[0104] The "load amount" described in the present invention is obtained by the following method:

[0105] Prepare 0.5 mol / L sulfate solution of each metal element respectively, adjust the pH value of the initial aqueous phase, take 2 g of the pretreated resin in a beaker respectively, add 20 mL of the prepared metal element solution to each, stir at room temperature for 60 min, rotate at 250 rpm / min, after stirring, separate the solid and liquid, and obtain the raffinate aqueous phase. Repeat three times, contacting with a fresh initial aqueous phase each time, and use inductively coupled plasma emission spectroscopy (ICP) to determine the concentration of each metal element in the raffinate aqueous phase. The content of the metal element in the resin is calculated by subtraction to obtain the loading capacity of the resin for each metal element.

[0106] Example

[0107] In order to make the purpose, technical scheme and advantages of the present invention clearer, the technical scheme of the present invention will be clearly and completely described in conjunction with the embodiments below. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all the embodiments. Based on the described embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field belong to the scope of protection of the present invention.

[0108] Example 1: Preparation of Resin 1

[0109] The synthetic route of resin 1 is as follows:

[0110]

[0111] Specifically, 10 g (30 mmol, -NH2) of primary amino polystyrene microspheres (Lanxiao Technology, model LX-D30) and 5.94 g (36 mmol) of 2-chloromethylpyrazine hydrochloride were placed in a 100 ml three-necked flask, and 60 g of N,N-dimethylformamide and 7.27 g (72 mmol) of triethylamine were added in sequence. The mixture was heated to 80 °C under mechanical stirring and reacted for 24 hours to generate Microspheres.

[0112] Thereafter, 7.15 g (36 mmol) of 2-chloromethyl-4-chloropyridine hydrochloride and 7.27 g (72 mmol) of triethylamine were added to the reaction system in sequence, and the reaction was continued at 80° C. for 24 hours to obtain resin 1 with a yield of 87%.

[0113] Example 2: Preparation of Resin 2

[0114] The synthetic route of resin 2 is as follows:

[0115]

[0116] Take 10g (30mmol, -NH2) of primary amino polystyrene microspheres (Lanxiao Technology, model LX-D30) and 11.88g (72mmol) of 2-chloromethylpyrazine hydrochloride in a 100ml three-necked flask, add 60g of N,N-dimethylformamide and 14.54g (144mmol) of triethylamine in sequence, heat to 80°C under mechanical stirring, react for 24 hours, and generate resin 2 with a yield of 88%.

[0117] Example 3: Preparation of Resin 3

[0118] The synthetic route of resin 3 is shown below:

[0119]

[0120] Take 10g (30mmol, -NH2) of primary amino polystyrene microspheres (Lanxiao Technology, model LX-D30) and 3.8g (30mmol) of 2-chloromethylpyridine in a 100ml three-necked flask, add 60g of acetonitrile and 2.88g (72mmol) of sodium hydroxide in turn, heat to 60℃ under mechanical stirring, react for 24 hours, and the reaction generates Microspheres (hereinafter referred to as intermediate microspheres).

[0121] Thereafter, the intermediate microspheres were filtered out by suction, rinsed twice with acetonitrile, placed in a 100 ml three-necked flask, and 8.25 g (50 mmol) of 2-chloromethylpyrazine hydrochloride and 10.6 g (100 mmol) of sodium carbonate were added in sequence. The reaction was continued at 60° C. for 24 hours to obtain resin 3 with a yield of 85%.

[0122] Example 4: Preparation of Resin 4

[0123] The synthetic route of resin 4 is shown below:

[0124]

[0125] Take 10 g (30 mmol, -NH2) of primary amino polystyrene microspheres (Lanxiao Technology, model LX-D30), 14.95g (72mmol) of 1-hydroxy-2-nitropropene was placed in a 100ml three-necked flask, and 60g of ethanol and 3.6g (90mmol) of sodium hydroxide were added in sequence. The mixture was heated to 40°C with mechanical stirring and reacted for 36 hours to generate resin 4 with a yield of 87%.

[0126] Evaluation Experiment 1 Evaluation Experiment 1

[0127] Configuration containing Cu 2+ 、Ni 2+ 、Co 2+ 、Al 3+ , Fe3+ , Mn 2+ 、Cd 2+ 、Zn 2+ , Ca 2+ Mg 2+ Cr 2+ , Li + 30 mL of each 0.05 g / L sulfate solution was used as the initial aqueous phase, and the pH value of the initial aqueous phase was adjusted to 1. Then, 5 g of the above resin was mixed and stirred at room temperature for 60 min, with a rotation speed of 250 rpm / min. After the extraction was completed, the concentration of each metal element in the raffinate aqueous phase was determined by inductively coupled plasma emission spectroscopy (ICP), and the content of metal elements in the resin was calculated by subtraction. The extraction rate of each resin for each ion was calculated, and then the separation coefficient between the resin and each ion was calculated based on the extraction rate (Table 1).

[0128] Table 1 Separation coefficients of resin 1 for various ions when the initial aqueous phase pH is about 1

[0129]

[0130]

[0131] The results show that when the pH value of the initial aqueous phase is about 0.5, the extraction rates of Cu and Ni by resin 1 are 98.5% and 61.4%, respectively, the extraction rate of Fe is 9.7%, and the extraction rates of other metals are all less than 13%; when the pH value of the initial aqueous phase is about 1, the extraction rates of Cu and Ni by resin 1 are 99.1% and 93.1%, respectively, and the extraction rates of Co, Zn, Cd and Fe are 46.2%, 15.6%, 30.4% and 25.2%, respectively, and the extraction rates of other metals are all less than 13%; when the pH value of the initial aqueous phase is about 2.5, the extraction rates of Ni, Co, Cu, Fe, Mn, Cd, Zn, Al and Cr by resin 1 are all greater than 85%, and the extraction rates of Ca, Mg and Li are all less than 11%.

[0132] As shown in Table 1, when the initial pH value of the aqueous phase is about 1, the separation coefficients of Cu and Ni, Co, Zn, Cd, and Fe are 128, 597, 252, and 327, respectively, and the separation coefficients of Cu and other metal elements (except Ni) are all above 700. The separation coefficients of Ni and Co, Zn, Cd, and Fe are 15.7, 73.2, 30.9, and 40.1, respectively. This shows that copper and nickel have a high degree of separation from impurity elements such as iron. Based on the above results, the resin has good selectivity for copper and nickel.

[0133] Evaluation experiment 2

[0134] The method in Evaluation Experiment 1 was referred to, except that Resin 1 was replaced with Dowex M4195 (commercially available from Dow). The results are shown in Table 2.

[0135] Table 2 Separation coefficients of resin 1 and Dowex M4195 for various ions

[0136]

[0137] As shown in Table 2, under the same experimental conditions, compared with Dowex M4195, the separation coefficient of resin 1 for each ion is higher, about 1 times higher. When the pH value of the initial aqueous phase is about 1, the separation coefficients of resin 1 for Cu / Fe, Cu / Zn, Cu / Cd, Ni / Fe, Ni / Zn, and Ni / Cd are 327, 597, 252, 40.1, 73.2, and 30.9, respectively, while the separation coefficients of Dowex M4195 for Cu / Fe, Cu / Zn, Cu / Cd, Ni / Fe, Ni / Zn, and Ni / Cd are 101, 90.7, 112, 9.8, 8.8, and 10.8, respectively. The results show that compared with Dowex M4195, resin 1 has significant selectivity for copper and nickel.

[0138] Evaluation experiment 3

[0139] Referring to the method in evaluation experiment 1, the difference from evaluation experiment 1 is that resin 1 is replaced by resin 2, and the initial pH value of the aqueous phase is adjusted to 1.2. The results show that when the pH value of the initial aqueous phase is about 1.2, the extraction rates of resin 2 for Cu and Ni are 98.2% and 91.5%, respectively, and the extraction rates for Zn, Cd, and Fe are 21.3%, 36.9%, and 21.9%, respectively. The extraction rates for other metals are all less than 17%. At this pH, the separation coefficients of Cu and Co, Zn, Cd, and Fe are 55.0, 206, 95.2, and 198, respectively, and the separation coefficients with other metal elements (except Ni) are all above 280. The separation coefficients of Ni and Co, Zn, Cd, and Fe are 10.6, 39.7, 18.4, and 38.4, respectively. This shows that the separation degree of copper and nickel from impurity elements such as iron is high, and the resin has good selectivity for copper and nickel.

[0140] Evaluation experiment 4

[0141] The method in Evaluation Experiment 3 was referred to, except that Resin 2 was replaced with Dowex M4195 (commercially available from Dow). The results are shown in Table 3.

[0142] Table 3 Separation coefficients of resin 2 and Dowex M4195 for various ions

[0143]

[0144] As shown in Table 3, under the same experimental conditions, compared with Dowex M4195, the separation coefficient of resin 2 for each ion is higher, about 1.5 times higher. When the pH value of the initial aqueous phase is about 1.2, the separation coefficients of resin 2 for Cu / Fe, Cu / Zn, Cu / Cd, Ni / Fe, Ni / Zn, and Ni / Cd are 198, 206, 95.2, 38.4, 39.7, and 18.4, respectively, while the separation coefficients of Dowex M4195 for Cu / Fe, Cu / Zn, Cu / Cd, Ni / Fe, Ni / Zn, and Ni / Cd are 22.7, 17.0, 19.8, 8.2, 6.1, and 7.1, respectively. The results show that compared with Dowex M4195, resin 2 has significant selectivity for copper and nickel.

[0145] Evaluation Experiment 5

[0146] Referring to the method in evaluation experiment 1, the difference from evaluation experiment 1 is that resin 1 is replaced by resin 3. The results show that when the pH value of the initial aqueous phase is about 1.2, the extraction rates of Cu and Ni by resin 3 are 98.4% and 94.9%, respectively, and the extraction rates of Co, Zn, Cd, and Fe are 58.6%, 25.5%, 42.4%, and 27.0%, respectively. The extraction rates of other metals are all less than 19%. At this pH, the separation coefficients of Cu and Co, Zn, Cd, and Fe are 43.0, 178, 82.8, and 165, respectively, and the separation coefficients with other metal elements are all above 270. The separation coefficients of Ni and Co, Zn, Cd, and Fe are 13.1, 54.1, 25.1, and 50.1, respectively. This shows that copper and nickel have high separation from impurity elements such as iron. The above results show that compared with Dowex M4195, resin 3 has significant selectivity for copper and nickel.

[0147] Evaluation experiment 6

[0148] The difference from the evaluation experiment 1 is that resin 1 is replaced by resin 4. The results show that when the pH value of the initial aqueous phase is about 1, the extraction rates of resin 4 for Cu and Ni are 97.3% and 87.7% respectively, and the extraction rates for Co, Zn, Cd, and Fe are 42.8%, 18.2%, 31.7%, and 18.9% respectively. The extraction rates for other metals are all less than 15%. At this pH, the separation coefficients of Cu with Co, Zn, Cd, and Fe are 47.8, 161, 77.0, and 153 respectively, and the separation coefficients with other metal elements (except Ni) are all above 200. The separation coefficients of Ni with Co, Zn, Cd, and Fe are 9.6, 32.2, 15.4, and 30.6 respectively. This shows that copper and nickel have a high separation degree from impurity elements such as iron. The above results show that the resin has good selectivity for copper and nickel.

[0149] Evaluation experiment 7

[0150] The results of the load capacity test on the products in Examples 1 to 4 are shown in Table 4.

[0151] Table 4 Initial aqueous phase pH value is 1.2, extraction is performed 3 times, and the loading amount of copper and nickel on the resin / mg / g

[0152] Resin copper nickel Resin 1 95 62 Resin 2 93 60 Resin 3 97 64 Resin 4 90 58

[0153] It can be seen from Table 4 that the copper and nickel loadings of resin 1, resin 2, resin 3, and resin 4 are high. When the initial aqueous phase pH value is 1.2, the extraction is repeated three times, and each time the initial aqueous phase is contacted with a fresh one, the copper loadings of resin 1, resin 2, resin 3, and resin 4 are 95 mg / g, 93 mg / g, 97 mg / g, and 90 mg / g, respectively, and the nickel loadings are 62 mg / g, 60 mg / g, 64 mg / g, and 58 mg / g, respectively.

[0154] Evaluation experiment 8

[0155] Repeatability test

[0156] The resin products of Examples 1 to 4 were extracted and regenerated 6 times, and the loading amount of metal elements of the resin products of Examples 1 to 4 was not much different from that of the first time.

[0157] The above is a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and changes can be made without departing from the principles of the present invention. These improvements and changes should also be regarded as the scope of protection of the present invention.

Claims

1. A nitrogen-containing heterocyclic resin, characterized in that The invention comprises a nitrogen-containing heterocyclic resin represented by the following structural formula (1): in: P is the resin matrix; -CH2-N- is a connecting bridge between P and R1 or R2; R1 and R2, which are the same or different, are nitrogen-containing heterocyclic substituents.

2. The nitrogen-containing heterocyclic resin according to claim 1, characterized in that The resin matrix P is selected from any one or more of polystyrene resin, copolymer of styrene and divinylbenzene, phenolic resin polymer, polyacrylic resin, and silicon-based resin.

3. The nitrogen-containing heterocyclic resin according to claim 1, characterized in that The nitrogen-containing heterocyclic substituents R1 and R2 are independently 2-methylenepyridine and its derivatives, imidazole and its derivatives, benzimidazole and its derivatives, pyrazine and its derivatives, quinoline and its derivatives, triazine and its derivatives or triazole and its derivatives, wherein at least one of R1 and R2 is not a 2-methylenepyridine functional group.

4. The nitrogen-containing heterocyclic resin according to claim 3, characterized in that The nitrogen-containing heterocyclic substituents R1 and R2 are independently selected from any of the following groups:

5. A method for preparing the nitrogen-containing heterocyclic resin according to any one of claims 1 to 4, characterized in that: The method comprises the following steps: S1, providing a resin base material, wherein the resin base material is a resin containing primary amino groups; S2, allowing the primary amino group of the resin base material to undergo a substitution reaction with a nitrogen-containing heterocyclic chloride to obtain the nitrogen-containing heterocyclic resin.

6. The preparation method according to claim 5, characterized in that: The step S2 comprises: S21a, allowing the primary amino group of the resin base material to undergo one-step substitution with the first nitrogen-containing heterocyclic chloride R1Cl in an alkaline solution under heating conditions to obtain a first intermediate compound, the structural formula of the first intermediate compound being as shown in the following formula (2); S22a, subjecting the first intermediate compound to a second nitrogen-containing heterocyclic chloride R2Cl, to undergo a two-step substitution under the same conditions as in step S21a to obtain the nitrogen-containing heterocyclic resin, wherein R1 and R2 are as described in claims 1-4, and R1 and R2 are different.

7. The method for preparing the nitrogen-containing heterocyclic resin according to claim 6, characterized in that: The molar ratio of the primary amino group of the resin base material to the first nitrogen-containing heterocyclic chloride R1Cl and the second nitrogen-containing heterocyclic chloride R2Cl is 1:(0.5-1.5):(0.5-1.5).

8. The preparation method according to claim 5, characterized in that: The step S2 comprises: The primary amino group of the resin base material and the first nitrogen-containing heterocyclic chloride R1Cl undergo a substitution reaction in an alkaline solution under heating conditions to obtain the nitrogen-containing heterocyclic resin, the structural formula of which is shown in the following formula (3); Wherein, R1 and R2 are as described in claims 1-4.

9. Use of the nitrogen-containing heterocyclic resin according to any one of claims 1 to 4, characterized in that: Used for adsorbing metals, wherein the metal is any one or more of mercury, gallium, iron, cobalt, nickel, copper, zinc, lead, indium, cadmium, manganese, aluminum, uranium, vanadium, platinum group elements, gold, and silver.

10. The use according to claim 9, characterized in that The metal comprises one or more of cobalt, nickel, copper, zinc, cadmium, manganese and aluminum.

11. The use according to claim 10, characterized in that The metal includes one or more of copper and nickel.

12. An adsorbent for solid phase extraction of metal elements, characterized in that: Contains the nitrogen-containing heterocyclic resin according to any one of claims 1 to 4.

13. A method for solid phase extraction of metal elements, characterized in that: Use the adsorbent as claimed in claim 12.