Reworking method of chemical vapor deposition film layer
The semiconductor structure is reworked through chemical mechanical grinding and dry etching, and the film layer is redeposited, which solves the product scrapping problem caused by abnormal film layer in the prior art, improves the yield and reduces the scrapping rate.
Patent Information
- Application Number
- CN202411018104.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-15
AI Technical Summary
In the later metal copper interconnection process, the complexity of the chemical vapor deposition film layer affects the yield of online products. The existing technology can only scrap the defective film layer and cannot effectively solve the abnormal problems.
The semiconductor structure is reworked by chemical mechanical grinding-dry etching-chemical mechanical grinding-chemical vapor deposition method, and the NDC layer, TEOS layer, low k dielectric layer and dielectric layer are redeposited to improve the quality of the film layer.
This method can improve the yield of the production line, reduce the online scrap rate, effectively solve the problem of membrane abnormalities, and improve the production efficiency and quality of the product.
Smart Images

Figure CN118957531A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor manufacturing, in particular to a reworking method for a chemical vapor deposition film layer. Background Art
[0002] In the back-end copper interconnect process, chemical vapor deposition (CVD) layers have become increasingly complex with process development, placing greater demands on production processes. Furthermore, when anomalies (such as film thickness, defects, and stress) occur online, the wafers must be scrapped, impacting product yield. Summary of the Invention
[0003] In view of the above-mentioned shortcomings of the prior art, the object of the present invention is to provide a rework method for chemical vapor deposition films, which is used to solve the problem that the yield of online products is affected by scrapping defective films.
[0004] To achieve the above-mentioned and other related purposes, the present invention provides a method for reworking a chemical vapor deposition film, the method comprising:
[0005] Step 1) providing a semiconductor structure to be reworked, comprising a metal layer and a first NDC layer, a TEOS layer, a low-k dielectric layer, and a dielectric layer formed from bottom to top on the metal layer;
[0006] Step 2) polishing the dielectric layer using a first chemical mechanical polishing process to expose the low-k dielectric layer;
[0007] Step 3) removing the low-k dielectric layer and the TEOS layer by a dry etching process to expose the first NDC layer;
[0008] Step 4) polishing the first NDC layer using a second chemical mechanical polishing process to expose the metal layer;
[0009] Step 5) Re-depositing the first NDC layer, the TEOS layer, the low-k dielectric layer and the dielectric layer from bottom to top on the surface of the metal layer through a CVD process.
[0010] Optionally, the dielectric layer includes, from bottom to top, a second NDC layer, a NF DARC layer, a hard mask layer, and an oxide layer.
[0011] Optionally, the material of the hard mask layer includes TiN.
[0012] Optionally, the low-k dielectric layer includes a BDII layer.
[0013] Optionally, when performing step 3), the etching selectivity ratio of the dry etching process is 1:4.
[0014] Optionally, before executing step 3), the method further comprises the step of performing an ashing process on the semiconductor structure that has leaked out of the BDII layer.
[0015] Optionally, when the semiconductor structure leaking out of the BDII layer is subjected to an ashing process, the gas used includes oxygen.
[0016] Optionally, the metal used for the metal layer is copper.
[0017] Optionally, applicable technology nodes include 40 nm or less than or equal to 28 nm.
[0018] As described above, the rework method of the chemical vapor deposition film layer of the present invention reworks the semiconductor structure with abnormal film layer by adopting chemical mechanical polishing-etching-chemical mechanical polishing-chemical vapor deposition. The above method can improve the production line yield and reduce the online scrap rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 Shown is a flow chart of a method for reworking a chemical vapor deposition film according to the present invention.
[0020] Figures 2 to 5 A schematic cross-sectional view of a semiconductor structure during the rework process of the present invention is shown. DETAILED DESCRIPTION
[0021] The following describes the embodiments of the present invention through specific examples. Those skilled in the art will readily understand the other advantages and benefits of the present invention from the disclosure herein. The present invention may also be implemented or applied through various other specific embodiments, and the details in this specification may be modified or altered based on different viewpoints and applications without departing from the spirit of the present invention.
[0022] See also Figures 1 to 5 It should be noted that the illustrations provided in this embodiment are merely schematic illustrations of the basic concept of the present invention. Although the illustrations only show components related to the present invention and are not drawn according to the number, shape, and size of components in actual implementation, the form, quantity, and proportion of each component in actual implementation may be arbitrarily changed, and the component layout may also be more complex.
[0023] like Figure 1 As shown, this embodiment provides a reworking method for a chemical vapor deposition film layer, the method comprising:
[0024] Step 1) providing a semiconductor structure to be reworked, comprising a metal layer and a first NDC layer, a TEOS layer, a low-k dielectric layer, and a dielectric layer formed from bottom to top on the metal layer;
[0025] Step 2) polishing the dielectric layer using a first chemical mechanical polishing process to expose the low-k dielectric layer;
[0026] Step 3) removing the low-k dielectric layer and the TEOS layer by a dry etching process to expose the first NDC layer;
[0027] Step 4) polishing the first NDC layer using a second chemical mechanical polishing process to expose the metal layer;
[0028] Step 5) Re-depositing the first NDC layer, the TEOS layer, the low-k dielectric layer and the dielectric layer from bottom to top on the surface of the metal layer through a CVD process.
[0029] The following is combined with Figures 1 to 5 The reworking method of the chemical vapor deposition film provided in this embodiment is described in detail.
[0030] like Figure 2 As shown, in step 1), a semiconductor structure requiring rework is provided, which includes a metal layer and a first NDC layer, a TEOS layer, a low-k dielectric layer, and a dielectric layer formed from bottom to top on the metal layer.
[0031] In this embodiment, the semiconductor structure that needs to be reworked is a semiconductor structure with film thickness anomalies, defects or stress problems. The NDC layer is a silicon carbonitride layer. Moreover, in this embodiment, the thickness of the first NDC layer is The thickness of the TEOS layer is The thickness of the low-k dielectric layer is
[0032] Specifically, the metal used in the metal layer is copper.
[0033] In this embodiment, the metal layer is formed in the interlayer dielectric layer by forming a trench in the interlayer dielectric layer and then filling the trench with metal copper.
[0034] Specifically, the dielectric layer includes, from bottom to top, a second NDC layer, a NF DARC layer, a hard mask layer, and an oxide layer.
[0035] In this embodiment, the NF DARC layer is a nitrogen-free anti-reflective coating, and the oxide layer is a silicon oxide layer. Moreover, in this embodiment, the thickness of the second NDC layer is The thickness of the NF DARC layer is The thickness of the hard mask layer is The thickness of the oxide layer is
[0036] More specifically, the material of the hard mask layer includes TiN.
[0037] Specifically, the low-k dielectric layer includes a BDII layer.
[0038] like Figure 3 As shown, in step 2), a first chemical mechanical polishing process is used to polish the dielectric layer to expose the low-k dielectric layer.
[0039] In this embodiment, the dielectric layer located above the low-k dielectric layer is removed at one time using a first chemical mechanical polishing process, and the process stops on the low-k dielectric layer, thereby ensuring a certain in-plane uniformity.
[0040] like Figure 4 As shown, in step 3), the low-k dielectric layer and the TEOS layer are removed by a dry etching process to expose the first NDC layer.
[0041] Specifically, when performing step 3), the etching selectivity ratio of the dry etching process is 1:4.
[0042] In this embodiment, by adopting an etching selectivity ratio of 1:4, it is ensured that when etching the low-k dielectric layer and the TEOS layer, the etching stops on the first NDC layer, thereby protecting the metal of the metal layer from being etched.
[0043] like Figure 5 As shown, in step 4), a second chemical mechanical polishing process is used to polish the first NDC layer to expose the metal layer.
[0044] Specifically, before executing step 3), the method further includes a step of ashing the semiconductor structure that has leaked out of the BDII layer.
[0045] More specifically, when the semiconductor structure leaking out of the BDII layer is subjected to an ashing process, the gas used includes oxygen.
[0046] In this embodiment, since excessive carbon polymers will cause the etching rate (ER) to slow down or even stop during the dry etching process in step 3), before the dry etching is performed, the carbon elements in the BDII are removed through an ashing process using a large flow of oxygen, thereby ensuring the normal progress of the product rework operation and the normal operation of the cavity.
[0047] In step 5), the first NDC layer, the TEOS layer, the low-k dielectric layer, and the dielectric layer are redeposited from bottom to top on the surface of the metal layer by a CVD process.
[0048] Specifically, applicable technology nodes include 40nm or less than or equal to 28nm.
[0049] In summary, the present invention's CVD film rework method utilizes a chemical mechanical polishing (CMP)-etching-CMP-CVD process to rework semiconductor structures with abnormal film layers. This method can improve production line yields and reduce scrap rates. Therefore, the present invention effectively overcomes the shortcomings of existing technologies and possesses high industrial value.
[0050] The above embodiments are merely illustrative of the principles and effects of the present invention and are not intended to limit the present invention. Anyone skilled in the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by one of ordinary skill in the art without departing from the spirit and technical principles disclosed herein are intended to be covered by the claims of the present invention.
Claims
1. A method for reworking a chemical vapor deposition film, characterized in that: The method comprises: Step 1) providing a semiconductor structure to be reworked, comprising a metal layer and a first NDC layer, a TEOS layer, a low-k dielectric layer and a dielectric layer formed from bottom to top on the metal layer; Step 2) polishing the dielectric layer using a first chemical mechanical polishing process to expose the low-k dielectric layer; Step 3) removing the low-k dielectric layer and the TEOS layer by a dry etching process to leak out the first NDC layer; Step 4) grinding the first NDC layer using a second chemical mechanical polishing process to expose the metal layer; Step 5) re-depositing the first NDC layer, the TEOS layer, the low-k dielectric layer and the dielectric layer on the surface of the metal layer from bottom to top through a CVD process.
2. The reworking method of a chemical vapor deposition film according to claim 1, characterized in that: The dielectric layer includes, from bottom to top, a second NDC layer, a NF DARC layer, a hard mask layer and an oxide layer.
3. The reworking method of a chemical vapor deposition film according to claim 2, characterized in that: The material of the hard mask layer includes TiN.
4. The reworking method of a chemical vapor deposition film according to claim 1, characterized in that: The low-k dielectric layer includes a BDII layer.
5. The reworking method of a chemical vapor deposition film according to claim 1, characterized in that: When executing step 3), the etching selectivity ratio of the dry etching process is 1:
4.
6. The reworking method of a chemical vapor deposition film according to claim 4, characterized in that: Before executing step 3), the method further includes a step of ashing the semiconductor structure that has leaked out of the BDII layer.
7. The reworking method of a chemical vapor deposition film according to claim 5, characterized in that: When the semiconductor structure leaking out of the BDII layer is subjected to an ashing process, the gas used includes oxygen.
8. The reworking method of a chemical vapor deposition film according to claim 1, characterized in that: The metal used in the metal layer is copper.