Heating cigarette reconstituted tobacco and preparation method and application thereof
By embedding electromagnetic induction materials into the reconstituted tobacco substrate layer, the problems of uneven heating of heated cigarettes and low tobacco utilization rate are solved, achieving more efficient heating uniformity and tobacco utilization rate, and making it highly applicable.
Patent Information
- Application Number
- CN202411380291.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2024-11-22
AI Technical Summary
Existing heated cigarettes suffer from uneven heating and low tobacco utilization, especially when the center is carbonized but the periphery is not sufficiently heated.
Electromagnetic induction material is embedded in the reconstituted tobacco substrate layer, preferably in the form of filaments and/or flakes, and is evenly distributed on the reconstituted tobacco leaf. The electromagnetic induction material is embedded on the surface or inside through a specific drying and coating process.
It achieves higher heating efficiency and more uniform heating of heated cigarettes, improving the utilization rate of tobacco, while not affecting the cigarette-making process and reducing the difficulty of production line upgrades.
Smart Images

Figure CN118985967A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of tobacco, and in particular relates to a heated cigarette reconstituted tobacco leaf and a preparation method and application thereof. Background Art
[0002] Heated cigarettes are usually divided into resistance heating, infrared heating, electromagnetic heating, etc. according to the heating method. At present, electromagnetic heating is mainly achieved by placing a sheet of electromagnetic induction material in the center of the smoking section of the cigarette, and heating the smoking material through the heat of the electromagnetic induction material. This method can better solve the problems of needle sticking and silk falling in hotter cigarettes, and can improve the consumer experience. However, this method is still a central heating method, and has common problems with central resistance heating, that is, the heated part is still located in the middle of the smoking section, the heating is uneven, and the center may be carbonized but the periphery is still not fully heated, resulting in a low tobacco utilization rate. Summary of the invention
[0003] In view of this, the purpose of the present invention is to provide a heated cigarette reconstituted tobacco leaf and its preparation method and application. The reconstituted tobacco leaf provided by the present invention is distributed with electromagnetic induction material, which can make the heating efficiency of the heated cigarette higher and the heating more uniform.
[0004] The invention provides a reconstituted tobacco for heating cigarettes, comprising: a reconstituted tobacco base material layer and an electromagnetic induction material embedded in the reconstituted tobacco base material layer.
[0005] Preferably, the electromagnetic induction material is embedded in the surface or inside of the reconstituted tobacco base material layer.
[0006] Preferably, the electromagnetic induction material is in the shape of a wire and / or a sheet.
[0007] Preferably, the length of the filament is 1 to 200 mm, and the diameter is 0.1 to 0.2 mm; the length of the sheet is 1 to 200 mm, the width is 0.2 to 20 mm, and the thickness is 0.05 to 0.2 mm.
[0008] Preferably, the electromagnetic induction material is arranged on the reconstituted tobacco base material layer in an orderly arrangement or a disordered arrangement;
[0009] The orderly arrangement means that the electromagnetic induction materials are arranged on the reconstituted tobacco base material layer along the same arrangement direction.
[0010] Preferably, the reconstituted tobacco base material layer is formed by drying and molding a reconstituted tobacco base slurry, and the components of the reconstituted tobacco base slurry include: tobacco powder, outer fibers, an atomizer, an adhesive and water.
[0011] Preferably, the content of the electromagnetic induction material is 5-15wt% of the mass of the reconstituted tobacco base material layer.
[0012] The present invention provides a method for preparing heated cigarette reconstituted tobacco, comprising the following steps:
[0013] After spreading the reconstituted tobacco base slurry, the slurry is dried, and then the electromagnetic induction material is added to the reconstituted tobacco base layer that is not completely dried and shaped, and then the slurry is completely dried and shaped to obtain a heated cigarette reconstituted tobacco with the electromagnetic induction material embedded in the surface of the reconstituted tobacco base layer;
[0014] or,
[0015] The reconstituted tobacco base slurry is spread and then dried, and then the electromagnetic induction material is added to the reconstituted tobacco base layer that is not completely dried and shaped, and then the drying and shaping are continued, and then another layer of reconstituted tobacco base slurry is spread, and finally it is completely dried and shaped to obtain the heated cigarette reconstituted tobacco with the electromagnetic induction material embedded in the reconstituted tobacco base layer.
[0016] The present invention provides a heated cigarette, wherein the smoking section of the heated cigarette is filled with the heated cigarette reconstituted tobacco leaves described in the above technical solution or the heated cigarette reconstituted tobacco leaves prepared by the preparation method described in the above technical solution.
[0017] Preferably, the heated cigarette reconstituted tobacco is filled in the smoking section by filling after cutting or re-rolling.
[0018] Compared with the prior art, the present invention provides a reconstituted tobacco leaf for heating cigarettes and a preparation method and application thereof. The reconstituted tobacco leaf for heating cigarettes provided by the present invention comprises: a reconstituted tobacco leaf base material layer and an electromagnetic induction material embedded in the reconstituted tobacco leaf base material layer. The present invention improves the smoking material of heated cigarettes, distributes the electromagnetic induction material on the reconstituted tobacco leaf, and after the reconstituted tobacco leaf is made into a heated cigarette, the electromagnetic induction material can be more evenly distributed in the smoking section, thereby making the heating efficiency of the heated cigarette higher and the heating more uniform. Moreover, the technical solution of the present invention does not affect the rolling and splicing process of the heated cigarette, and the technical implementation and production line upgrading and transformation are easy and have strong applicability. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.
[0020] Figure 1 It is a schematic diagram of orderly arranging the filamentary electromagnetic induction materials provided by an embodiment of the present invention on a reconstituted tobacco leaf base material layer;
[0021] Figure 2It is a schematic diagram of orderly arranging the sheet-like electromagnetic induction material provided by an embodiment of the present invention on a reconstituted tobacco leaf base material layer;
[0022] Figure 3 is a schematic diagram of the disorderly arrangement of the filamentary electromagnetic induction material provided by an embodiment of the present invention on a reconstituted tobacco leaf base material layer;
[0023] Figure 4 It is a schematic diagram of the disorderly arrangement of the sheet-like electromagnetic induction material provided by the embodiment of the present invention on the reconstituted tobacco leaf base material layer;
[0024] Figure 5 It is a schematic diagram of the heated cigarette reconstituted tobacco leaves with orderly arranged filamentary electromagnetic induction provided by an embodiment of the present invention after being cut into shreds;
[0025] Figure 6 It is a schematic diagram of the shredded reconstituted tobacco leaves heated by electromagnetic induction disorderly arrangement of filaments provided by an embodiment of the present invention;
[0026] Figure 7 It is a schematic diagram of the sheet-shaped electromagnetic induction disorderly arranged heated cigarette reconstituted tobacco leaves after being cut into shreds provided by an embodiment of the present invention;
[0027] Figure 8 This is a schematic diagram of the structure of a cigarette filled with shredded reconstituted tobacco leaves of a heated cigarette provided by an embodiment of the present invention;
[0028] Fig. 9 It is a schematic structural diagram of the re-rolling and filling of heated cigarette reconstituted tobacco leaves provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0029] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] The invention provides a reconstituted tobacco for heating cigarettes, comprising: a reconstituted tobacco base material layer and an electromagnetic induction material embedded in the reconstituted tobacco base material layer.
[0031] In the reconstituted tobacco provided by the present invention, the reconstituted tobacco base material layer is formed by drying a reconstituted tobacco base slurry, and the components of the reconstituted tobacco base slurry preferably include: tobacco powder, outer fibers, an atomizer, an adhesive and water; wherein the tobacco powder is preferably one or more of flue-cured tobacco powder, burley tobacco powder and cigar tobacco powder; the particle size of the tobacco powder is preferably 200-500 meshes, more preferably 200-300 meshes; the outer fibers are preferably wood pulp fibers, more preferably coniferous wood pulp fibers, and the coniferous wood pulp fibers are preferably from coniferous wood high The invention relates to one or more of yield pulp, softwood kraft pulp and softwood bleached kraft pulp; the addition amount of the external fiber is preferably 1-5wt% of the mass of tobacco powder, specifically 1wt%, 1.5wt%, 2wt%, 2.5wt%, 3wt%, 3.5wt%, 4wt%, 4.5wt% or 5wt%; the atomizer is preferably propylene glycol and / or glycerol, and the mass ratio of propylene glycol to glycerol is preferably 1:(2-15); the addition amount of the atomizer is preferably 10-40wt% of the mass of tobacco powder, Specifically, it can be 10wt%, 15wt%, 20wt%, 25wt%, 30wt%, 35wt% or 40wt%; the adhesive is preferably one or more of carboxymethyl cellulose (CMC), sodium alginate and chitosan; the amount of the adhesive added is preferably 1-5wt% of the mass of the tobacco powder, specifically 1wt%, 1.5wt%, 2wt%, 2.5wt%, 3wt%, 3.5wt%, 4wt%, 4.5wt% or 5wt%; the amount of water added is preferably 1-5wt% of the mass of the tobacco powder. 3 to 5 times, specifically 3 times, 3.2 times, 3.5 times, 3.7 times, 4 times, 4.2 times, 4.5 times, 4.7 times or 5 times; the reconstituted tobacco base slurry preferably also contains spices; the spices are preferably water-soluble spices, including but not limited to fruits, mints, tobacco characteristic fragrances and other spices; the added amount of the spices is preferably 1 to 5wt% of the mass of the tobacco powder, specifically 1wt%, 1.5wt%, 2wt%, 2.5wt%, 3wt%, 3.5wt%, 4wt%, 4.5wt% or 5wt%.
[0032] In the reconstituted tobacco provided by the present invention, the components of the electromagnetic induction material preferably include one or more of iron, nickel, chromium, tungsten, and aluminum oxide. In one embodiment provided by the present invention, the components of the electromagnetic induction material are composed of iron, nickel and chromium, the content of the iron is preferably 40-60wt%, more preferably 50wt%, the content of the nickel is preferably 20-40wt%, more preferably 30wt%, and the chromium is the balance.
[0033] In the reconstituted tobacco provided by the present invention, the shape of the electromagnetic induction material is preferably filamentous and / or sheet-like; wherein the length of the filament is preferably 1-200 mm, more preferably 1-50 mm, specifically 1 mm, 2 mm, 3 mm, 4 mm, 5 mm, 7 mm, 10 mm, 15 mm, 20 mm, 25 mm, 30 mm, 35 mm, 40 mm, 45 mm or 50 mm; the diameter of the filament is preferably 0.1-0.2 mm, specifically 0.1 mm, 0.11 mm, 0.12 mm, 0.13 mm, 0.14 mm, 0.15 mm, 0.16 mm, 0.17 mm, 0.18 mm, 0.19 mm or 0.2 mm; the length of the sheet is preferably 1-200 mm, more preferably 1-50 mm, specifically 1 mm, 2 mm, 3 mm, 4 mm, 5 mm, 6 mm, 7 mm, 8 mm, 9 mm, 10 mm, 15 mm, 20 mm, 25 mm, 30 mm, 35 mm, 40 mm, 45 mm or 50 mm. The width of the sheet is preferably 0.2-20mm, more preferably 0.2-5mm, specifically 0.2mm, 0.5mm, 0.7mm, 1mm, 1.2mm, 1.5mm, 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm or 5mm; the thickness of the sheet is preferably 0.05-0.2mm, specifically 0.05mm, 0.06mm, 0.07mm, 0.08mm, 0.09mm, 0.1mm, 0.11mm, 0.12mm, 0.13mm, 0.14mm, 0.15mm, 0.16mm, 0.17mm, 0.18mm, 0.19mm or 0.2mm.
[0034] In the reconstituted tobacco provided by the present invention, the arrangement of the electromagnetic induction material on the reconstituted tobacco base material layer can be an ordered arrangement or a disordered arrangement; wherein the ordered arrangement means that the electromagnetic induction material is arranged on the reconstituted tobacco base material layer along the same arrangement direction.
[0035] In the reconstituted tobacco provided by the present invention, the structure in which the filamentary electromagnetic induction materials are orderly arranged on the reconstituted tobacco base material layer is schematically shown as follows: Figure 1 As shown; the structure diagram of the orderly arrangement of the sheet-like electromagnetic induction material on the reconstituted tobacco base material layer is shown as Figure 2 In the present invention, as shown. Figure 1-2 As shown, the electromagnetic induction materials are arranged in parallel on the reconstituted tobacco base material layer, and the upper and lower spacing is adjusted according to the width of the electromagnetic induction materials, preferably 5 to 30 mm, and the spacing between the left and right electromagnetic induction materials is preferably 5 to 15 mm.
[0036] In the reconstituted tobacco provided by the present invention, the structure of the filamentary electromagnetic induction material being randomly arranged on the reconstituted tobacco base material layer is schematically shown as follows: Figure 3As shown; the structure of the sheet-like electromagnetic induction material being randomly arranged on the reconstituted tobacco base material layer is shown as follows Figure 4 shown.
[0037] In the reconstituted tobacco provided by the present invention, the electromagnetic induction material can be embedded in the surface of the reconstituted tobacco base material layer, or embedded in the interior of the reconstituted tobacco base material layer.
[0038] In the reconstituted tobacco provided by the present invention, the content of the electromagnetic induction material is preferably 5 to 15wt% of the mass of the reconstituted tobacco base material layer, specifically 5wt%, 5.5wt%, 6wt%, 6.5wt%, 7wt%, 7.5wt%, 8wt%, 8.5wt%, 9wt%, 9.5wt%, 10wt%, 10.5wt%, 11wt%, 11.5wt%, 12wt%, 12.5wt%, 13wt%, 13.5wt%, 14wt%, 14.5wt% or 15wt%.
[0039] In the reconstituted tobacco provided by the present invention, the thickness of the reconstituted tobacco is preferably 0.1-0.5 mm, specifically 0.1 mm, 0.15 mm, 0.2 mm, 0.25 mm, 0.3 mm, 0.35 mm, 0.4 mm, 0.45 mm or 0.5 mm.
[0040] The present invention also provides a method for preparing the heated cigarette reconstituted tobacco described in the above technical solution, comprising the following steps:
[0041] After spreading the reconstituted tobacco base slurry, the slurry is dried, and then the electromagnetic induction material is added to the reconstituted tobacco base layer that is not completely dried and shaped, and then the slurry is completely dried and shaped to obtain a heated cigarette reconstituted tobacco with the electromagnetic induction material embedded in the surface of the reconstituted tobacco base layer;
[0042] or,
[0043] The reconstituted tobacco base slurry is spread and then dried, and then the electromagnetic induction material is added to the reconstituted tobacco base layer that is not completely dried and shaped, and then the drying and shaping are continued, and then another layer of reconstituted tobacco base slurry is spread, and finally it is completely dried and shaped to obtain the heated cigarette reconstituted tobacco with the electromagnetic induction material embedded in the reconstituted tobacco base layer.
[0044] In the preparation method provided by the present invention, the specific composition of the reconstituted tobacco-based slurry, the size specifications of the electromagnetic induction material, the addition ratio of the electromagnetic induction material and the arrangement form of the electromagnetic induction material have been introduced in the previous text and will not be repeated here; the coating is preferably carried out on a steel belt; the heating temperature of the drying is preferably 70-90°C.
[0045] The present invention also provides a heated cigarette, wherein the smoking section of the heated cigarette is filled with the heated cigarette reconstituted tobacco leaves described in the above technical solution or the heated cigarette reconstituted tobacco leaves prepared by the preparation method described in the above technical solution.
[0046] In the heated cigarette provided by the present invention, there are preferably two ways to fill the heated cigarette reconstituted tobacco leaves in the smoking section, one is to fill the heated cigarette reconstituted tobacco leaves after cutting them into shreds, and the other is to reroll the heated cigarette reconstituted tobacco leaves and fill them.
[0047] In the heated cigarette provided by the present invention, for the shredding scheme, if the electromagnetic induction material is arranged in an orderly manner on the reconstituted tobacco base material layer, the shredding is performed perpendicular to the arrangement direction of the electromagnetic induction material; if the electromagnetic induction material is arranged disorderly on the reconstituted tobacco base material layer, there is no special requirement for the shredding direction. In the present invention, the width of the shredded wire is preferably 0.8 to 1.5 mm, specifically 0.8 mm, 0.9 mm, 1 mm, 1.1 mm, 1.2 mm, 1.3 mm, 1.4 mm or 1.5 mm.
[0048] In the heated cigarette provided by the present invention, for the shredding solution, the structure of the heated cigarette reconstituted tobacco leaves with orderly arranged filaments of electromagnetic induction after shredding is schematically shown as follows: Figure 5 As shown; the structure of the heated cigarette reconstituted tobacco leaves with disordered arrangement of filamentary electromagnetic induction after being cut into shreds is shown as follows Figure 6 As shown; the structure of the sheet-like electromagnetic induction randomly arranged heated cigarette reconstituted tobacco leaves after being cut into shreds is shown as follows Figure 7 shown.
[0049] In the heated cigarette provided by the present invention, for the shredded solution, the shredded reconstituted tobacco leaves are compounded, rolled and packaged according to a conventional rolling method to obtain a heated cigarette product, the structure of which is shown in FIG. Figure 8 shown.
[0050] In the heating cigarette provided by the present invention, for the rewinding scheme, it is not necessary to cut the reconstituted tobacco leaves, and the reconstituted tobacco leaves are cut and then rerolled to form a reel-shaped tobacco rod, and then the tobacco rod is wrapped with cigarette paper and then ternary or quaternary composite, and finally rolled to form a heating cigarette. In the present invention, the diameter of the tobacco rod is preferably 6 to 7 mm, and the length is preferably 80 to 120 mm; the center of the tobacco rod preferably has a certain gap, such as Fig. 9 shown.
[0051] For the purpose of greater clarity, the present invention is described in detail with reference to the following examples and comparative examples.
[0052] Example 1
[0053] The flue-cured tobacco leaves are crushed into tobacco powder of 200-300 meshes, and an atomizer (glycerol) accounting for 30% of the weight of the tobacco powder, an adhesive (CMC) accounting for 3.5% of the weight of the tobacco powder, an outer fiber (coniferous wood pulp fiber) accounting for 4% of the weight of the tobacco powder, and water 3 times the weight of the tobacco powder are added to the tobacco powder, and the mixture is fully stirred to obtain a reconstituted tobacco leaf-based slurry;
[0054] The above-mentioned reconstituted tobacco leaf base slurry is evenly spread on a steel belt and heated to dry; a sheet-like electromagnetic induction material (composition is 50wt% iron, 30wt% nickel and 20wt% chromium, size is 0.05mm×2mm×1mm, and the amount is 10% of the sheet mass) is laid in order on the not completely dried reconstituted tobacco leaf base layer, such as Figure 2 As shown, the upper and lower spacings of adjacent sheet-shaped electromagnetic induction materials are 6 mm, and the left and right spacings are 5 mm; heating and drying are continued, and then the reconstituted tobacco base material slurry is secondarily coated on the reconstituted tobacco base material layer that has not been completely dried and formed; heating is continued until it is completely dried and formed, and a heated cigarette reconstituted tobacco with a thickness of 0.3 mm and an electromagnetic induction material embedded inside is obtained;
[0055] The reconstituted tobacco leaves were cut into shreds with a width of 1.0 mm and a length of 30 mm to obtain heated cigarette reconstituted tobacco shreds.
[0056] Example 2
[0057] The flue-cured tobacco leaves are crushed into tobacco powder of 200-300 meshes, and an atomizer (glycerol) accounting for 30% of the weight of the tobacco powder, an adhesive (CMC) accounting for 3.5% of the weight of the tobacco powder, an outer fiber (coniferous wood pulp fiber) accounting for 4% of the weight of the tobacco powder, and water 3 times the weight of the tobacco powder are added to the tobacco powder, and the mixture is fully stirred to obtain a reconstituted tobacco leaf-based slurry;
[0058] The above-mentioned reconstituted tobacco leaf base slurry is evenly spread on a steel belt and heated to dry; a sheet-like electromagnetic induction material (composition is 50wt% iron, 30wt% nickel and 20wt% chromium, size is 0.05mm×2mm×1mm, and the amount is 10% of the sheet mass) is randomly laid on the not completely dried reconstituted tobacco leaf base layer, such as Figure 4 As shown; continue heating and drying, and then apply the reconstituted tobacco base slurry for the second time on the reconstituted tobacco base material layer that has not been completely dried and formed; continue heating until it is completely dried and formed, and obtain a heated cigarette reconstituted tobacco with an electromagnetic induction material having a thickness of 0.3 mm embedded inside;
[0059] The reconstituted tobacco leaves were cut into shreds with a width of 1.0 mm and a length of 30 mm to obtain heated cigarette reconstituted tobacco shreds.
[0060] Comparative Example 1
[0061] The flue-cured tobacco leaves are crushed into tobacco powder of 200-300 meshes, and an atomizer (glycerol) accounting for 30% of the weight of the tobacco powder, an adhesive (CMC) accounting for 3.5% of the weight of the tobacco powder, an outer fiber (coniferous wood pulp fiber) accounting for 4% of the weight of the tobacco powder, and water 3 times the weight of the tobacco powder are added to the tobacco powder, and the mixture is fully stirred to obtain a reconstituted tobacco leaf-based slurry;
[0062] The reconstituted tobacco leaf-based slurry is evenly spread on a steel belt and heated until it is completely dried and shaped to obtain heated cigarette reconstituted tobacco leaves with a thickness of 0.2 mm;
[0063] The reconstituted tobacco leaves were cut into shreds with a width of 1.0 mm and a length of 30 mm to obtain heated cigarette reconstituted tobacco shreds.
[0064] Heating efficiency evaluation
[0065] The reconstituted tobacco shreds obtained in Examples 1 to 2 and Comparative Example 1 were respectively made into 7.16 specification (cigarette length (filter length + cigarette length) = 45 (33 + 12) mm, circumference = 22.5 mm) heated cigarettes for comparison; among them, the cigarette made of reconstituted tobacco shreds not containing electromagnetic induction material (Comparative Example 1) had a sheet of electromagnetic induction material with a length of about 12 mm, a width of about 4 mm, and a thickness of 0.1 mm built into the center of the smoking section; the weight of tobacco shreds in different cigarette samples was consistent, and the output power of the device was the same; and the smoke concentration, smoke temperature and other indicators were tested.
[0066] The test results are shown in Table 1:
[0067] Table 1 Evaluation results of heating efficiency of different cigarette samples
[0068]
[0069] In Table 1, cigarette sample A is a cigarette with a sheet-like electromagnetic induction material built into the center (corresponding to tobacco shreds in Example 1), cigarette sample B is a cigarette with a smoking segment containing disordered electromagnetic induction material (corresponding to tobacco shreds in Example 2), and cigarette sample C is a cigarette with a smoking segment containing ordered electromagnetic induction material (corresponding to tobacco shreds in Example 1).
[0070] It can be seen from Table 1 that compared with cigarette A with built-in electromagnetic induction material in the center, cigarettes B and C have higher smoke temperatures under the same heating conditions, and the initial and later smoke concentrations are also significantly higher than those of cigarette A; this shows that heated cigarettes made from reconstituted tobacco leaves with embedded electromagnetic induction materials have higher heating efficiency.
[0071] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A heated cigarette reconstituted tobacco, characterized in that: include: A reconstituted tobacco base material layer and an electromagnetic induction material embedded in the reconstituted tobacco base material layer.
2. The heated cigarette reconstituted tobacco according to claim 1, characterized in that: The electromagnetic induction material is embedded on the surface or inside of the reconstituted tobacco leaf base material layer.
3. The heated cigarette reconstituted tobacco according to claim 1, characterized in that: The electromagnetic induction material is in the shape of a wire and / or a sheet.
4. The heated cigarette reconstituted tobacco according to claim 3, characterized in that: The length of the filament is 1 to 200 mm, and the diameter is 0.1 to 0.2 mm; the length of the sheet is 1 to 200 mm, the width is 0.2 to 20 mm, and the thickness is 0.05 to 0.2 mm.
5. The heated cigarette reconstituted tobacco according to claim 3, characterized in that: The electromagnetic induction material is arranged in an orderly or disordered manner on the reconstituted tobacco leaf base material layer; The orderly arrangement means that the electromagnetic induction materials are arranged on the reconstituted tobacco base material layer along the same arrangement direction.
6. The heated cigarette reconstituted tobacco according to claim 1, characterized in that: The reconstituted tobacco base material layer is formed by drying and shaping reconstituted tobacco base slurry, and the components of the reconstituted tobacco base slurry include: tobacco powder, outer fiber, atomizer, adhesive and water.
7. The heated cigarette reconstituted tobacco according to claim 1, characterized in that: The content of the electromagnetic induction material is 5-15wt% of the mass of the reconstituted tobacco base material layer.
8. A method for preparing heated cigarette reconstituted tobacco, characterized in that: The following steps are involved: After spreading the reconstituted tobacco base slurry, the slurry is dried, and then the electromagnetic induction material is added to the reconstituted tobacco base layer that is not completely dried and shaped, and then the slurry is completely dried and shaped to obtain a heated cigarette reconstituted tobacco with the electromagnetic induction material embedded in the surface of the reconstituted tobacco base layer; or, The reconstituted tobacco base slurry is spread and then dried, and then the electromagnetic induction material is added to the reconstituted tobacco base layer that is not completely dried and shaped, and then the drying and shaping are continued, and then another layer of reconstituted tobacco base slurry is spread, and finally it is completely dried and shaped to obtain the heated cigarette reconstituted tobacco with the electromagnetic induction material embedded in the reconstituted tobacco base layer.
9. A heated cigarette, characterized in that: The smoking section of the heated cigarette is filled with the heated cigarette reconstituted tobacco leaves according to any one of claims 1 to 7 or the heated cigarette reconstituted tobacco leaves prepared by the preparation method according to claim 8.
10. The heated cigarette according to claim 9, characterized in that: The heating cigarette reconstituted tobacco is filled in the smoking section by cutting and then filling or re-rolling and filling.
Citation Information
Patent Citations
Smoking body matched with electromagnetic heating smoking set
CN215936306U
Method for making a continuous web of reconstituted material of plant origin containing inductively heatable metallic elements
WO2024018375A1