Method for preventing cold forging steel continuous casting billet from bending in slow cooling process

By using special continuous casting billets and rotary cross-packing trolleys in the slow cooling process of cold heading steel continuous casting billets, the continuous casting billets are closely arranged to reduce bending caused by temperature gradient, the problem of bending billets of cold heading steel continuous casting billets is solved, and the problem of bending billets of cold heading steel continuous casting billets is realized. Efficient bending prevention and productivity improvement.

CN118989267APending Publication Date: 2024-11-22WUHAN IRON & STEEL GRP ECHENG IRON & STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411209361.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The cold-heading steel continuous casting billet is bending due to temperature unevenness in the red hot state, and the existing anti-bending devices or methods have problems such as high investment, complex operation or safety hazards.

Method used

The special continuous casting billet and the lifting van with 90-degree rotary cross-plating function can reduce the gap between the continuous casting billet by pre-correcting force, and the special continuous casting billet is closely attached to the red hot continuous casting billet to reduce the Bending development space to achieve bending prevention during the slow cooling process.

Benefits of technology

It effectively prevents the occurrence of bending, meets the YB/T2011 standard, reduces the scrap rate, simplifies operations, improves site utilization, and reduces labor intensity and safety hazards for workers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118989267A_ABST
    Figure CN118989267A_ABST
Patent Text Reader

Abstract

The invention discloses a method for preventing a cold heading steel continuous casting billet from bending in a slow cooling process, which is made after the reason that the red hot continuous casting billet is easy to bend when being stacked and cooled is deeply researched, and is characterized in that a specially manufactured special continuous casting billet and the red hot continuous casting billet are cooperatively stacked together; two special continuous casting billets are tightly attached to the two side edges of each layer of red hot continuous casting billets, the continuous casting billets on each layer are also tightly stacked, 4-7 special continuous casting billets which are stacked in a 90-degree crossed mode are pressed at the two ends of the upper layer of the topmost layer of red hot continuous casting billets respectively, gaps between the casting billets are reduced when the red hot continuous casting billets are stacked, the effect of pre-straightening force is utilized, and the red hot continuous casting billets on the topmost layer of the red hot continuous casting billets on the topmost layer of the red hot continuous casting billets are stacked. The red hot continuous casting billet has no bending development space in the cooling process, so that the purpose of preventing bending is achieved; according to the continuous casting blank slowly cooled through the method, the bending degree is not larger than 20 mm per meter, the total bending degree is not larger than 2% of the total length, and the standard requirement of YB / T2011 is met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of slow cooling of steel continuous casting billets, in particular to a method for preventing bending of cold heading steel continuous casting billets during slow cooling. Background Art

[0002] Cold heading steel is usually formed by one or more impact loading at room temperature and is widely used in automobiles, shipbuilding, machinery, white appliances, electronics, furniture, construction fasteners, connectors (such as screws, bolts, nuts, pins, rivets, etc.). With the development of the national economy, the demand for high-strength cold heading steel is increasing. Cold heading steel is in line with national policies in reducing energy consumption and improving product materials. Strengthening the quality control of cold heading steel is conducive to improving the economic benefits of steel companies and upstream and downstream companies, thus becoming a key production variety for the adjustment of product structure of various steel companies.

[0003] Cold heading steel has high quality requirements, especially high requirements on the surface. It needs to have low yield strength and deformation resistance to ensure good cold deformation performance and no surface cracking under a large deformation degree. By slowly cooling the cold heading steel continuous casting billet, the thermal stress in the steel can be effectively reduced, the generation of surface cracks can be prevented, and the quality of the steel can be improved.

[0004] In the actual production process, some manufacturers use the method of slow cooling in a pit for continuous casting of red billets. When there is no slow cooling pit, the red-hot continuous casting billets need to be stacked and slowly cooled before being transported. The red-hot continuous casting billets are prone to bending due to temperature unevenness during the stacking and cooling process.

[0005] When the cold-headed steel continuous casting billet is in a red-hot state, its surface temperature reaches over 600°C, and the internal temperature even exceeds 900°C. During the stacking and cooling process of the red-hot continuous casting billet, due to the high temperature in the middle of the stacking position and the low ambient temperature around, the continuous casting billet around and on the top of the stacking position is very likely to bend sideways and upwards; at the same time, due to the influence of the clamps holding the continuous casting billet, there is inevitably a certain gap between each hanging continuous casting billet, and bracket-shaped bending is also likely to occur between each hanging continuous casting billet on the same layer.

[0006] Continuous casting billets with excessive curvature have a great impact on the normal production of steel rolling, and are prone to accidents such as roller conveyor hitting the steel, inability to enter the heating furnace, and roller failure to bite. According to the YB / T2011 standard requirements: "The curvature of the continuous casting billet shall not exceed 20mm per meter, and the total curvature shall not exceed 2% of the total length."

[0007] Before the present invention was proposed, there were many devices or methods for preventing the continuous casting billet from bending, but they had problems such as large investment, limited operating space and difficult operation.

[0008] For example, the Chinese patent "A device for preventing continuous casting billet bending" with patent application number CN202020015172.7 has a first mounting groove on one side of the top surface of the device, and a number of evenly distributed first cylinders are fixedly installed from the front end to the rear end of the inner bottom of the first mounting groove, and the piston rod ends of the first cylinders are fixedly connected to the bottom surface of the first support plate, respectively. A first clamping plate is fixedly installed on the other side of the first support plate, and a second mounting groove is opened on the other side of the top surface of the anti-bending device; the first clamping plate and the second clamping plate are used to clamp the two sides of the continuous casting billet, and the piston rod ends of the third cylinder and the fourth cylinder are used to push the upper pressure plate to correct the continuous casting billet to prevent the continuous casting billet from bending. The device has a complex structure and requires equipment investment. There are problems such as a small amount of billet buffered at one time and high cost.

[0009] For example, the Chinese patent application number CN201020595795.2, "A device for preventing continuous casting billet from bending", manufactures a frame-shaped clamp, and at least one clamp is installed at each end of a continuous casting billet. Although the device is simple to manufacture, it requires manual operation to insert the clamp in each billet, which is labor-intensive for the operator, poses a safety hazard, and cannot solve the problem of continuous casting billet bending upward. Summary of the invention

[0010] The purpose of the present invention is to provide a method to prevent bending of cold heading steel continuous casting billets during the slow cooling process, in order to solve the problem that cold heading steel, which is currently not equipped with a slow cooling pit, is prone to bending due to temperature unevenness during the cooling process of the red hot continuous casting billets.

[0011] A method for preventing a cold heading steel continuous casting billet from bending during a slow cooling process of the present invention comprises the following steps: (1) Preparation of special continuous casting billets: prepare a number of scrapped continuous casting billets with the same cross-sectional dimensions and length specifications as the red-hot continuous casting billets to be stacked. The scrapped continuous casting billets are straight, and their external dimensions and curvature meet the requirements of YB / T2011. The number is not less than 80. As special continuous casting billets, both ends of the special continuous casting billets are painted with bright and non-falling paint. Different specifications are marked with different colors to prevent steel mixing; (2) Equipment preparation: prepare two overhead cranes with 90-degree rotating cross-stacking function for lifting continuous casting billets. One of the overhead cranes is equipped with a suction plate, and the other is equipped with a special fixture for continuous casting billets. The two overhead cranes work together; (3) Stacking rules: Check the stacking position and make sure the stacking feet are flat before starting stacking. The specific stacking rules are as follows: ① According to the normal stacking requirements, place two adjacent special continuous casting billets on one side of the bottom layer using a suction plate crane; ② Use the overhead crane to clamp the red-hot continuous casting billet above the stacking position, and direct it to the inner side of the special continuous casting billet placed in the early stage by a dedicated person. The height is controlled at about 100mm. After getting close, release the clamp to minimize the gap between the red-hot continuous casting billet and the special continuous casting billet; ③ Command the iron-absorbing plate crane to drop the lower edge of the iron-absorbing plate to about 80-90mm below the upper edge of the other side of the red-hot continuous casting billet, and gently knock the continuous casting billet to make the red-hot continuous casting billet and the special continuous casting billet closely attached; ④ Repeat ② and ③ operations for each subsequent continuous casting billet to minimize the gap between each billet; ⑤ After the last hanging billet on the bottom layer is stacked, reserve a certain space and place two special continuous casting billets on the other side of the bottom layer to ensure that they are closely attached to the red-hot continuous casting billets; ⑥ Repeat the stacking method of the upper layer of continuous casting billets according to the bottom layer stacking method, with 90-degree cross stacking between adjacent layers, and the stacking height shall not exceed 4m; ⑦ After the top layer of red-hot continuous casting billets is stacked, 4-7 special continuous casting billets are pressed at both ends of the upper layer of the red-hot continuous casting billets and stacked crosswise at 90 degrees; (4) Billet removal: The continuous casting billet can be transferred after the stacking time is ≥48 hours and the surface temperature of the red hot continuous casting billet is ≤400℃. Pay attention to distinguishing the special continuous casting billet from the normal continuous casting billet to prevent mixing of steel.

[0012] In the above method, the gap between adjacent continuous casting billets (between dedicated adjacent continuous casting billets, between dedicated continuous casting billets and adjacent red-hot continuous casting billets) is ≤10mm.

[0013] The method of the present invention is made after an in-depth study of the reasons why red-hot continuous casting billets are prone to bending when they are stacked and cooled. The reason why the continuous casting billets are bent during the cooling process when they are stacked in the red-hot state is that the temperature gradients on both sides of the continuous casting billets are different and there is bending space. This stacking method mainly utilizes special continuous casting billets to reduce the gaps between the billets when the red-hot continuous casting billets are stacked. Through the effect of pre-straightening force, there is no space for bending to develop during the cooling process of the red-hot continuous casting billets, thereby achieving the purpose of preventing bending.

[0014] The beneficial effects of the present invention are as follows: (1) The stacking method can effectively prevent the cold-headed steel continuous casting billet in the red-hot state from being bent significantly due to uneven temperature during the cooling process, thereby reducing the waste caused by excessive bending. The continuous casting billet that is slowly cooled by the method of the present invention has a bending degree of no more than 20 mm per meter and a total bending degree of no more than 2% of the total length, meeting the standard requirements of YB / T2011; (2) The special continuous casting billet of this stacking method is simple to manufacture, and the existing stacking and overhead crane equipment is used, without the need for additional investment; (3) Compared with the stacking method using a bench device, this stacking method has a high site utilization rate and can stack more continuous casting billets without affecting the stacking of continuous casting billets under normal production conditions; (4) Compared with placing continuous casting billet clips, this stacking method reduces the labor intensity of workers and reduces safety hazards. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the stacking state of the red-hot continuous casting billets in Example 1 of the present invention.

[0016] In the figure, 1 is a special continuous casting billet, 2 is a red hot continuous casting billet. DETAILED DESCRIPTION

[0017] In order to better explain the technical solution of the present invention, the technical solution of the present invention is further described below in conjunction with specific embodiments. The following embodiments are merely exemplary of the technical solution of the present invention and do not limit the present invention in any form. The serial numbers of the following embodiments are only for description and do not represent the advantages and disadvantages of the embodiments.

[0018] Example 1 The steelmaking plant of a certain steel enterprise adopts the process flow of 130-ton top and bottom combined blowing converter - LF furnace - square billet continuous casting machine to produce cold heading steel ML40Cr. The square billet continuous casting machine has 7 machines and 7 streams, an arc radius of 10m, a cross-sectional size of 160mm×160mm, and a fixed length of 9m. The continuous casting billet span is equipped with 2 16-ton overhead cranes with 90-degree rotation function and 4 12m×12m stacking positions.

[0019] Due to the slow cooling process requirements of the steel grade, the continuous casting billets are stacked and slowly cooled in a red hot state at the billet discharging site. In order to prevent the continuous casting billets from bending, the method of the present invention is adopted.

[0020] See also Figure 1 A method for preventing bending of a cold heading steel continuous casting billet during a slow cooling process comprises the following steps: (1) Production of special continuous casting billets 1: 96 160 mm × 160 mm × 9000 mm special continuous casting billets were produced on site using scrapped continuous casting billets. The continuous casting billets were straight without obvious bending or square defects. The end faces of the special continuous casting billets were marked with yellow paint (the end faces are marked with “×” to represent the color in the figure); (2) Equipment preparation: prepare two overhead cranes with 90-degree rotating cross-stacking function for lifting continuous casting billets. One of the overhead cranes is equipped with a suction plate, and the other is equipped with a special fixture for continuous casting billets. The two overhead cranes work together; (3) Stacking rules: Check the stacking position and make sure the stacking feet are flat before starting stacking. The specific stacking rules are as follows: ① First, place two special continuous casting billets on one side of the bottom layer using a suction plate crane; ② The clamp-hanging crane clamps the first six red-hot continuous casting billets 2 and places them on the inner side of the scrapped continuous casting billets. A dedicated person directs the clamps to be loosened. The gap between the red-hot continuous casting billet and the special continuous casting billet is about 200mm. ③Special personnel direct the iron-absorbing plate crane to lightly knock the other side of the red-hot continuous casting billet, so that the adjacent red-hot continuous casting billets are closely attached to each other, with a gap of ≤10mm; ④ Repeat ② and ③ operations for each subsequent hanging of red hot continuous casting billets, and check that the gap between each hanging of red hot continuous casting billets is ≤10mm; ⑤There are 7 hangers with 42 red hot continuous casting billets on the bottom floor ( Figure 1 The number of continuous casting billets is only an example and does not represent the actual number of billets stacked). Two special continuous casting billets are placed on both sides of the red hot continuous casting billet; ⑥ According to the bottom layer stacking method, the overhead crane rotates 90 degrees to cross-stack the second layer of continuous casting billets; after the second layer of continuous casting billets are stacked, the upper layer of continuous casting billets are stacked cross-stacked 90 degrees in turn; ⑦ There are 408 red-hot continuous casting billets in 68 hangers stacked in this stacking position, which are stacked in 10 layers with a stacking height of about 1.8m. After the 10th layer of continuous casting billets are stacked, 4 special continuous casting billets are pressed on each end of the continuous casting billets.

[0021] (4) Unloading After the red-hot continuous casting billets were stacked for 56 hours, the highest surface temperature of the continuous casting billets was measured to be 236°C, and the maximum curvature of the continuous casting billets was measured to be 1.28%, meeting the requirement of ≤2%. The billets were then discharged normally and transported by car to the next process.

[0022] Through the above slow cooling process, the cold heading steel was used to roll φ6.5-16mm wire rod. No cracking occurred in the 1 / 2 cold heading test, and the quality was normal for users.

[0023] Example 2 The steelmaking plant of a certain steel enterprise adopts the process flow of 130-ton top and bottom combined blowing converter - LF furnace - VD - square billet continuous casting machine to produce cold heading steel SCM435. The square billet continuous casting machine has 7 machines and 7 streams, an arc radius of 10m, a cross-sectional size of 200mm×200mm, and a fixed length of 12m. The continuous casting billet span is equipped with two 16-ton overhead cranes with 90-degree rotation function and two 15m×15m stacking positions.

[0024] Due to the slow cooling process requirements of the steel grade, the continuous casting billets are stacked and slowly cooled in a red hot state at the billet discharging site. In order to prevent the continuous casting billets from bending, the method of the present invention is adopted.

[0025] A method for preventing bending of a cold heading steel continuous casting billet during a slow cooling process comprises the following steps: (1) Production of special continuous casting billets 3: 80 special continuous casting billets with a size of 200 mm × 200 mm × 12000 mm were produced on site using scrapped continuous casting billets. The continuous casting billets were straight without obvious bending or square defects. The end faces of the special continuous casting billets were painted with red paint. (2) Equipment preparation: prepare two overhead cranes with 90-degree rotating cross-stacking function for lifting continuous casting billets. One of the overhead cranes is equipped with a suction plate, and the other is equipped with a special fixture for continuous casting billets. The two overhead cranes work together; (3) Stacking rules: Check the stacking position and make sure the stacking feet are flat before starting stacking. The specific stacking rules are as follows: ① First, place two special continuous casting billets 3 on one side of the bottom layer using a suction plate crane; ② The clamp-hanging crane clamps the first hanging of 5 red-hot continuous casting billets 4 and places them on the inner side of the scrapped continuous casting billets. A special person directs to loosen the clamps. The gap between the red-hot continuous casting billet and the special continuous casting billet is about 200mm. ③Special personnel direct the iron-absorbing plate crane to lightly knock the other side of the red-hot continuous casting billet, so that the adjacent red-hot continuous casting billets are closely attached to each other, with a gap of ≤10mm; ④ Repeat ② and ③ operations for each subsequent hanging of red hot continuous casting billets, and check that the gap between each hanging of red hot continuous casting billets is ≤10mm; ⑤ A total of 9 hangings with 45 red-hot continuous casting billets are stacked on the bottom layer, and two special continuous casting billets are pressed against each other on both sides of the red-hot continuous casting billet; ⑥ According to the bottom layer stacking method, the overhead crane rotates 90 degrees to cross-stack the second layer of continuous casting billets; after the second layer of continuous casting billets are stacked, the upper layer of continuous casting billets are stacked cross-stacked 90 degrees in turn; ⑦ There are 72 hangers of red-hot continuous casting billets, totaling 360 pieces, stacked in 8 layers with a stacking height of about 1.8m. After the 8th layer of continuous casting billets were stacked, 4 special continuous casting billets were pressed on each end of the continuous casting billets.

[0026] (4) Unloading After the red-hot continuous casting billets were stacked for 72 hours, the highest surface temperature of the continuous casting billets was measured to be 243°C, and the maximum curvature of the continuous casting billets was measured to be 0.96%, meeting the requirement of ≤2%. The billets were then discharged normally and transported by car to the next process.

[0027] Through the above slow cooling process, the cold heading steel is used to roll φ40-70mm round steel. No cracking occurs in the 1 / 2 cold heading test, and the quality is normal for users.

[0028] The above embodiments are only specific examples for explaining the present invention and do not limit the present invention in any form. Any non-substantial changes made by anyone based on the above contents and forms without departing from the protection scope of the claims of the present invention shall be deemed to fall within the protection scope of the claims of the present invention. The present invention is not limited to the above specific implementation examples.

Claims

1. A method for preventing bending of a cold heading steel continuous casting billet during a slow cooling process, comprising the following steps: (1) Preparation of special continuous casting billets: prepare a number of scrapped continuous casting billets with the same cross-sectional dimensions and length specifications as the red-hot continuous casting billets to be stacked. The scrapped continuous casting billets are straight, and their external dimensions and curvature meet the requirements of YB / T2011. The number of scrapped continuous casting billets of each specification shall not be less than 80. As special continuous casting billets, both ends of the special continuous casting billets are painted with bright and non-falling paint. Different specifications are marked with different colors to prevent steel mixing; (2) Equipment preparation: prepare two overhead cranes with 90-degree rotating cross-stacking function for lifting continuous casting billets. One of the overhead cranes is hung with a suction plate, and the other is hung with a special fixture for continuous casting billets. The two overhead cranes work together; (3) Stacking rules: Check the stacking position and make sure the stacking feet are flat before starting stacking. The specific stacking rules are as follows: ① According to the normal stacking requirements, first place two special continuous casting billets on one side of the bottom layer with a suction plate crane and stack them closely; ② Use the overhead crane to clamp the red-hot continuous casting billet above the stacking position, and direct it to the inner side of the special continuous casting billet placed in the early stage by a dedicated person. The height is controlled at about 100mm. After getting close, release the clamp to minimize the gap between the red-hot continuous casting billet and the special continuous casting billet; ③ Command the iron-absorbing plate crane to drop the lower edge of the iron-absorbing plate to about 80-90mm below the upper edge of the other side of the red-hot continuous casting billet, and gently knock the continuous casting billet to make the red-hot continuous casting billet and the special continuous casting billet closely attached; ④ Repeat ② and ③ operations for each subsequent continuous casting billet, and try to reduce the gap between each red-hot continuous casting billet; ⑤ After the last hanging casting billet is stacked on the bottom layer, reserve a certain space and lift two special continuous casting billets to the other side of the bottom layer to ensure that they are closely attached to the red-hot continuous casting billets; ⑥ Repeat the stacking method of the upper layer of continuous casting billets according to the bottom layer stacking method, with 90-degree cross stacking between adjacent layers, and the stacking height shall not exceed 4m; ⑦ After the top layer of red-hot continuous casting billets is stacked, 4-7 special continuous casting billets are pressed at both ends of the upper layer of the red-hot continuous casting billets and stacked crosswise at 90 degrees; (4) Billet removal: The continuous casting billet can be transferred after the stacking time is ≥48 hours and the surface temperature of the red hot continuous casting billet is ≤400℃. Pay attention to distinguishing the special continuous casting billet from the normal continuous casting billet to prevent mixing of steel.

2. A method for preventing bending of cold heading steel continuous casting billet during slow cooling according to claim 1, characterized in that: The gap between adjacent continuous casting billets is ≤10mm.