Forced polyaluminum chloride hydrolysis system and method based on fine bubbles

By adopting micro bubble forced polymer aluminum chloride hydrolysis technology in drinking water treatment, the problem of excessive use of chemical agents in the prior art has been solved, the coagulation efficiency and environmental protection are improved, and the goal of clean production has been achieved.

CN119016009APending Publication Date: 2024-11-26XI'AN UNIVERSITY OF ARCHITECTURE AND TECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411231420.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The forced hydrolysis method of adding alkaline reagents such as NaOH in the existing drinking water treatment technology cannot meet the needs of clean production, and it is difficult to effectively reduce the use of chemical agents, affecting environmental protection and resource utilization efficiency.

Method used

Using a forced polymer aluminum chloride hydrolysis system based on fine bubbles, by generating fine bubbles in the polymer aluminum chloride solution, the surface of the bubbles is used to adsorb hydroxide to form an alkaline microinterface, and forced hydrolysis of polymer aluminum chloride is achieved and condensation is improved. Effectiveness while reducing the addition of chemical agents.

Benefits of technology

The proportion of dominant aluminum species in polymer aluminum chloride has been improved, the removal efficiency of soluble organic matter during coagulation has been enhanced, the needs of green and clean production have been met, pollution and carbon emissions have been reduced, and the transformation cost is simple, and the transformation cost is low.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119016009A_ABST
    Figure CN119016009A_ABST
Patent Text Reader

Abstract

The invention discloses a system and a method for forcibly hydrolyzing polyaluminum chloride based on microbubbles. The method comprises the following steps: 1, diluting a polyaluminum chloride concentrated solution; 2, adding a polyaluminum chloride solution needing forced hydrolysis into a polyaluminum chloride forced hydrolysis tank by using a first metering pump; 3, starting a self-priming pump to adjust the gas flow and the pressure of a pipeline system so as to generate fine bubbles; and 4, uniformly and forcibly hydrolyzing the polyaluminum chloride through a self-circulation system of the self-priming pump and an alkaline micro-interface formed by hydroxyl adsorbed on the surfaces of the fine bubbles. According to the invention, micro-bubbles are generated by a pressurization and pressure relief method, polyaluminum chloride is forced to hydrolyze under the condition of not additionally adding an alkaline agent through the characteristic that the surfaces of the micro-bubbles adsorb hydroxyl to form an alkaline micro-interface, and the coagulation efficiency is enhanced by regulating and controlling the distribution of dominant aluminum morphological species in the polyaluminum chloride; the method has the advantages of simplicity and convenience in operation, greenness, environmental protection and synergistic interaction of pollution reduction and carbon reduction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of water treatment, relates to drinking water treatment technology, and particularly relates to a new forced polyaluminium chloride hydrolysis process for enhancing coagulation efficiency without the participation of chemical reagents other than coagulants. Background Art

[0002] Coagulation removes suspended particulate matter and dissolved organic matter based on the mechanisms of electrical neutralization, adsorption bridging, and mesh sweeping. It is essentially the effect of the hydrolyzed form of an effective coagulant in multiple mechanisms. b ) and higher polymer aluminum (Al c ) can effectively remove soluble organic matter, so forced polyaluminium chloride hydrolysis increases Al in polyaluminium chloride b and Al c The proportion of dissolved organic matter is of great significance to enhancing the removal of dissolved organic matter and ensuring the safety of drinking water.

[0003] However, in the field of drinking water treatment, the existing forced hydrolysis method by adding alkaline reagents such as NaOH does not meet the needs of clean production. Therefore, we try to develop a new forced polyaluminium chloride hydrolysis process that reduces the addition of chemical agents and meets the needs of green clean production. It increases the proportion of dominant aluminum species in polyaluminium chloride and enhances the coagulation efficiency, which has a very high application prospect. Summary of the invention

[0004] The purpose of the present invention is to reduce the addition of chemical agents other than coagulants while improving the coagulation efficiency by forcing the hydrolysis of polyaluminium chloride, so that the enhanced coagulation process can meet the needs of the national pollution reduction and carbon reduction synergistic efficiency enhancement strategy as much as possible.

[0005] To achieve the above-mentioned object, the first aspect of the present invention provides a forced polyaluminium chloride hydrolysis system based on fine bubbles;

[0006] The invention is characterized by comprising:

[0007] A polyaluminium chloride spontaneous hydrolysis tank 1, wherein a first stirrer 2-1 is installed in the polyaluminium chloride spontaneous hydrolysis tank 1; the first stirrer 2-1 is used to stir the solution in the polyaluminium chloride spontaneous hydrolysis tank 1;

[0008] A polyaluminium chloride forced hydrolysis tank 4; a second agitator 2-2 and a dissolved oxygen detector 10 are installed in the polyaluminium chloride forced hydrolysis tank 4; the second agitator 2-2 is used to stir the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank 4, and the dissolved oxygen detector 10 is used to detect the oxygen content of the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank;

[0009] The first metering pump 3; one end of the first metering pump 3 is connected to the polyaluminium chloride spontaneous hydrolysis tank 1, and the other end is connected to the polyaluminium chloride forced hydrolysis tank 4; the first metering pump 3 is used to measure the flow rate of the polyaluminium chloride solution flowing through the polyaluminium chloride spontaneous hydrolysis tank 1 and the polyaluminium chloride forced hydrolysis tank 4;

[0010] It also includes a gas regulating mechanism, which includes a check valve 5, a gas flow meter 6, a self-priming pump 7, a pressure gauge 8, a pressure regulating valve 9, and a granular activated carbon adsorption box 11;

[0011] Wherein, the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank 4 is circulated through the self-priming pump 7;

[0012] By installing a check valve 5 at the initial end of the water inlet pipe of the self-priming pump 7 to prevent the polyaluminium chloride solution from flowing back

[0013] The air flow rate is adjusted by adjusting the gas flow meter 6.

[0014] The pressure of the pipeline system is adjusted by rotating the pressure regulating valve 9;

[0015] Monitor the pressure of the pipeline system through the pressure gauge 8;

[0016] The incoming air is filtered through the granular activated carbon adsorption box 11;

[0017] By adjusting the gas flow rate and the pressure in the pipeline system, the self-priming pump 7 can generate fine bubbles in the process of circulating the polyaluminium chloride solution.

[0018] In a second aspect of the present invention, based on the above-mentioned forced polyaluminium chloride hydrolysis system based on fine bubbles, a forced polyaluminium chloride hydrolysis method based on fine bubbles is provided; it is characterized in that it comprises the following steps:

[0019] Step 1: Add a certain amount of polyaluminium chloride concentrate into the polyaluminium chloride spontaneous hydrolysis tank, and dilute the polyaluminium chloride concentrate with clean water. During the dilution process, use the first stirrer to fully stir, so that the polyaluminium chloride can undergo a spontaneous hydrolysis process while being diluted with clean water.

[0020] Step 2: Use the first metering pump to add the diluted polyaluminium chloride solution to the polyaluminium chloride forced hydrolysis tank. When the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank reaches a certain volume, open the second metering at the outlet to maintain a certain volume of the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank.

[0021] Step 3: Turn on the self-priming pump and the second agitator, so that the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank can be stirred evenly by the second agitator when circulating through the self-priming pump. At the same time, the air flow rate is adjusted by adjusting the gas flow meter, and the pressure of the pipeline system is adjusted by rotating the pressure regulating valve. By adjusting the gas flow rate and the pressure in the pipeline system, the self-priming pump can generate fine bubbles in the process of circulating the polyaluminium chloride solution, and the fine bubbles are fully mixed with the polyaluminium chloride solution through the sufficient stirring of the second agitator, and then the alkaline micro-interface formed by the hydroxide adsorbed on the surface of the fine bubbles is used to achieve the purpose of forced polyaluminium chloride.

[0022] In step three, the present invention makes the following arrangement:

[0023] Control of bubble size: The size of the bubble has an important influence on the mixing effect and surface activity. Bubbles that are too large may rise quickly and escape the solution, while bubbles that are too small may not be conducive to sufficient mixing. In the invention, a high-precision gas flow meter and a pressure regulating valve are used to achieve precise control of the bubble generation process. By adjusting the gas flow rate and pressure, we can control the generation rate and size of the bubbles to ensure uniform distribution of the bubbles in the polyaluminium chloride solution. In addition, a real-time monitoring system is integrated to monitor the bubble size and distribution. This system will provide feedback so that the operator can adjust the gas flow rate and pressure in time to ensure that the bubble size is controlled within the optimal range.

[0024] Efficiency of the second agitator: The design and operating conditions of the second agitator need to ensure sufficient mixing of the solution and the bubbles while avoiding excessive shear force, which may destroy the bubbles. In the invention, the second agitator adopts a low-shear stirring blade to promote liquid flow in a gentle manner to ensure uniform mixing between the bubbles and the solution. The second agitator is equipped with an adjustable speed control system, allowing the operator to adjust the stirring speed according to the viscosity of the solution and the stability of the bubbles to achieve the best mixing effect. In addition, the present invention adopts streamlined airfoil section blades, and accurately optimizes the size and angle through computational fluid dynamics (CFD) simulation to ensure that the shear force generated by the blades during the stirring process is minimized. At the same time, a staggered blade layout is adopted to reduce the direct collision of bubbles. The method of combining experimental verification with simulation results is used to iteratively optimize the design until the optimal performance of efficient mixing and bubble protection is achieved.

[0025] For further optimization, the gas source connected to the gas flow meter can be connected to oxygen in addition to air to increase the ability of micro-bubbles to generate hydroxyl radicals. At the same time, in order to prevent dust in the air from entering the micro-bubble generation system and the polyaluminium chloride dilution solution and thus affecting the subsequent coagulation efficiency, a granular activated carbon adsorption box can be connected to the gas flow meter inlet to minimize the impact of air pollution on the process device.

[0026] After further optimization, the gas flow meter can adjust the gas flow rate in the range of 20-60 mL / min. When the gas flow rate is 20 mL / min, the concentration of fine bubbles is high, and the effect of forced hydrolysis of polyaluminium chloride by fine bubbles is the best.

[0027] Further optimization, the pressure of the pipeline system can be adjusted by rotating the pressure regulating valve. When the pressure in the pressure gauge is 0.7-0.8MPa, the fine bubble effect produced by the system is the best.

[0028] Further optimization, because a pressure regulating valve is added to the pipeline system to change the water inlet pressure and outlet pressure in the pipeline system, this operation will inevitably affect the water outlet flow rate in the outlet pipe of the self-priming pump. The solution in the pipeline system cannot be discharged in time, which will further affect the water inlet flow of the inlet pipe of the self-priming pump. The reduction of the inlet flow and outlet flow will significantly affect the efficiency of the system for preparing microbubbles. In order to minimize the impact of the pressure regulating valve on the inlet and outlet flow of the self-priming pump, the diameter of the inlet pipe of the self-priming pump can be appropriately reduced, and the diameter of the outlet pipe can be appropriately increased and the length of the outlet pipe can be extended. The diameter of the outlet pipe needs to be greater than 1.5 times the diameter of the inlet pipe, and the length of the outlet pipe needs to be greater than 2.0 times the length of the inlet pipe.

[0029] For further optimization, in order to avoid the annihilation of micro bubbles caused by the extension of the outlet pipe, thereby affecting the mixing efficiency of micro bubbles and polyaluminium chloride and the efficiency of forced polyaluminium chloride, a tubular static mixer can be added to the outlet pipe at the rear end of the pressure regulating valve to fully mix the micro bubbles with polyaluminium chloride.

[0030] Further optimization is carried out by adjusting the flow rates of the first metering pump and the second metering pump to adjust the hydraulic retention time of the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank, thereby adjusting the time for the fine bubbles to force the polyaluminium chloride to hydrolyze.

[0031] Further optimization, in the polyaluminium chloride forced hydrolysis tank, the excessively fast stirring speed of the second agitator will accelerate the escape of fine bubbles and affect the efficiency of forced hydrolysis of polyaluminium chloride by fine bubbles. Therefore, a dissolved oxygen detector can be added to the polyaluminium chloride forced hydrolysis tank to adjust the stirring speed in the polyaluminium chloride forced hydrolysis tank by detecting the dissolved oxygen concentration in the solution.

[0032] For further optimization, a check valve is installed at the initial end of the self-priming pump water inlet pipe to prevent the backflow of the polyaluminium chloride solution.

[0033] Compared with the prior art, the present invention has the following beneficial effects:

[0034] 1. The invention utilizes the property of fine bubble surface adsorbing hydroxide to form alkaline microinterface to force polyaluminium chloride to hydrolyze, which can enhance the coagulation efficiency by increasing the proportion of dominant aluminium species in polyaluminium chloride and improve the removal of soluble organic matter during the coagulation process.

[0035] 2. In addition to adding a certain amount of polyaluminium chloride, the invention does not add any chemical agents. Compared with the existing enhanced coagulation process, the enhanced coagulation process that enhances the coagulation efficiency by forcing the hydrolysis of polyaluminium chloride through fine bubbles meets the needs of clean production and the country's needs for synergistic efficiency improvement in pollution reduction and carbon reduction.

[0036] 3. The invention is easy to operate, and in the actual engineering application process, only the existing coagulant hydrolysis tank needs to be modified. The modification cost is low, the cycle is short and the floor space is small. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 It is an overall schematic diagram of the forced polyaluminium chloride hydrolysis system and method based on microbubbles of the present invention.

[0038] In the figure: 1. Polyaluminium chloride spontaneous hydrolysis tank; 2-1. First agitator; 2-2. Second agitator; 3-1. First metering pump; 3-2. Second metering pump; 4. Polyaluminium chloride forced hydrolysis tank; 5. Check valve; 6. Gas flow meter; 7. Self-priming pump; 8. Pressure gauge; 9. Pressure regulating valve; 10. Dissolved oxygen detector; 11. Granular activated carbon adsorption box. DETAILED DESCRIPTION

[0039] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are only a part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0040] like Figure 1 As shown in the figure, the forced polyaluminium chloride hydrolysis system based on fine bubbles includes several main parts:

[0041] 1. Spontaneous hydrolysis tank 1, in which a first stirrer 2-1 is provided, the main function of which is to stir the solution in the spontaneous hydrolysis tank 1;

[0042] 2. A forced hydrolysis tank 4, in which a second agitator 2-2 is provided and a dissolved oxygen detector 10 is provided, which is used to stir the polyaluminium chloride solution in the forced hydrolysis tank 4, while the dissolved oxygen detector 10 is responsible for monitoring the oxygen content of the solution in the polyaluminium chloride forced hydrolysis tank;

[0043] 3. A first metering pump 3, one end of which is connected to the spontaneous hydrolysis tank 1, and the other end is connected to the forced hydrolysis tank 4, and is mainly used to measure the flow rate of the polyaluminium chloride solution flowing between the two tanks;

[0044] In addition, the system is also equipped with other parts, such as a gas regulating mechanism, including a check valve 5, a gas flow meter 6, a self-priming pump 7, a pressure gauge 8, a pressure regulating valve 9, a granular activated carbon adsorption box 11, etc. Among them, the function of the self-priming pump 7 is to circulate the polyaluminium chloride solution in the forced hydrolysis tank 4; the check valve 5 is set at the initial position of the water inlet pipe of the self-priming pump 7 to prevent the solution from flowing back; the gas flow meter 6 can be used to adjust the air flow; the pressure regulating valve 9 can adjust the pressure of the pipeline system by rotating; the pressure gauge 8 can be used to check the pressure of the pipeline system; the granular activated carbon adsorption box 11 is responsible for filtering the incoming air. Through these regulating devices and operations, it can be ensured that the self-priming pump 7 generates fine bubbles in the process of circulating the polyaluminium chloride solution.

[0045] like Figure 1 As shown, the forced polyaluminium chloride hydrolysis method based on microbubbles has the following specific steps:

[0046] Step 1: Add a certain amount of polyaluminium chloride concentrate into the polyaluminium chloride spontaneous hydrolysis tank 1, and dilute the polyaluminium chloride concentrate with clean water. During the dilution process, use the first stirrer 2-1 to fully stir at a speed of 200 rpm / min, so that the polyaluminium chloride undergoes a spontaneous hydrolysis process while being diluted with clean water.

[0047] Step 2: Use the first metering pump 3-1 to add the diluted polyaluminium chloride solution to the polyaluminium chloride forced hydrolysis tank 4. When the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank 4 reaches a certain volume, open the outlet of the second metering pump 3-2 to maintain a certain volume of the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank 4.

[0048] Step 3: Turn on the self-priming pump 7 and the second agitator 2-2, so that the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank 4 can be stirred evenly by the second agitator 2-2 when circulating through the self-priming pump 7. At the same time, the air flow rate is adjusted by adjusting the gas flow meter 6, and the pressure of the pipeline system is adjusted by rotating the pressure regulating valve 9. By adjusting the gas flow rate and the pressure in the pipeline system, the self-priming pump 7 can generate fine bubbles in the process of circulating the polyaluminium chloride solution, and the second agitator 2-2 is fully stirred at a speed of 200rpm / min to fully mix the fine bubbles with the polyaluminium chloride, and then the alkaline micro-interface formed by the hydroxide adsorbed on the surface of the fine bubbles is used to achieve the purpose of forced polyaluminium chloride.

[0049] Among them, the gas source connected to the gas flow meter 6 can be connected to oxygen in addition to air to increase the ability of microbubbles to generate hydroxyl radicals. At the same time, in order to prevent dust in the air from entering the microbubble generation system and entering the polyaluminium chloride dilution liquid to affect the subsequent coagulation efficiency, a granular activated carbon adsorption box 11 can be connected to the gas inlet of the gas flow meter to minimize the impact of air pollution on the process device.

[0050] The gas flow meter 6 can adjust the gas flow rate in the range of 20-60 mL / min. When the gas flow rate is 20 mL / min, the concentration of fine bubbles is high, and the effect of forced hydrolysis of polyaluminium chloride by fine bubbles is the best.

[0051] Wherein, the pressure of the pipeline system can be adjusted by rotating the pressure regulating valve 9. When the pressure in the pressure gauge 8 is 0.7-0.8MPa, the fine bubbles generated by the system have the best effect.

[0052] Among them; because a pressure regulating valve 9 is added to the pipeline system to change the water inlet pressure and water outlet pressure in the pipeline system, this operation is bound to affect the water outlet flow rate in the outlet pipe of the self-priming pump 7. The solution in the pipeline system cannot be discharged in time, which will further affect the water inlet flow of the inlet pipe of the self-priming pump 7. The reduction of the inlet flow and the outlet flow will significantly affect the efficiency of the system for preparing microbubbles. In order to minimize the impact of the pressure regulating valve 9 on the inlet and outlet flow of the self-priming pump 7, the diameter of the inlet pipe of the self-priming pump 7 can be appropriately reduced, and the diameter of the outlet pipe can be appropriately increased and the length of the outlet pipe can be extended. The diameter of the outlet pipe needs to be greater than 1.5 times the diameter of the inlet pipe, and the length of the outlet pipe needs to be greater than 2.0 times the length of the inlet pipe.

[0053] Among them; in order to avoid the annihilation of fine bubbles caused by the extension of the outlet pipe length and thus affect the mixing efficiency of fine bubbles and polyaluminium chloride and the efficiency of forced polyaluminium chloride, a tubular static mixer can be added to the outlet pipe at the rear end of the pressure regulating valve 9 to fully mix the fine bubbles with polyaluminium chloride.

[0054] By adjusting the flow rate of the first metering pump 3-1 and the second metering pump 3-2, the hydraulic retention time of the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank 4 is adjusted, so as to adjust the time for the fine bubble forced hydrolysis of polyaluminium chloride.

[0055] Among them, the excessive stirring speed of the second stirrer 2-2 in the polyaluminium chloride forced hydrolysis tank 4 will accelerate the escape of fine bubbles and affect the efficiency of forced hydrolysis of polyaluminium chloride by fine bubbles. Therefore, a dissolved oxygen detector 10 can be added to the polyaluminium chloride forced hydrolysis tank 4 to adjust the stirring speed in the polyaluminium chloride forced hydrolysis tank 4 by detecting the dissolved oxygen concentration in the solution.

[0056] Wherein, a check valve 5 is installed at the initial end of the water inlet pipe of the self-priming pump 7 to prevent the polyaluminium chloride solution from flowing back.

[0057] Example 1

[0058] For polyaluminium chloride (PACl 0.5 ) The forced hydrolysis experimental steps are as follows:

[0059] Step 1: In the polyaluminium chloride spontaneous hydrolysis tank, use deionized water with a pH of 6-8 to mix the pre-prepared PACl 0.5 The concentrate was diluted to 4 mg / L and continuously stirred at 200 rpm / min using the first stirrer.

[0060] Step 2: Use the first metering pump at the front end of the polyaluminium chloride forced hydrolysis tank to pump 1L of diluted PACl 0.5 Add it into the polyaluminium chloride forced hydrolysis tank, and close the first metering pump at the front end of the polyaluminium chloride forced hydrolysis tank.

[0061] Step 3, turn on the self-priming pump and adjust the air flow rate to 20 mL / min, and rotate the pressure regulating valve to adjust the pressure of the pipeline system to 0.7-0.8 MPa. While turning on the self-priming pump, turn on the second agitator and continue stirring at a speed of 200 rpm / min.

[0062] Step 4, after the self-priming pump circulates for 5 minutes, the first metering pump at the front end and the second metering pump at the rear end of the polyaluminium chloride forced hydrolysis tank are turned on, and the flow rates of the first metering pump and the second metering pump are adjusted to meet the required coagulant concentration in the coagulation stirring tank while ensuring continuous operation of the device.

[0063] PACl before and after 5 minutes of forced hydrolysis by fine bubbles 0.5 The changes in the hydrolysis form distribution are shown in Table 1.

[0064] Table 1 PACl before and after forced hydrolysis of fine bubbles for 5 min 0.5 Hydrolysis form distribution

[0065]

[0066] Example 2

[0067] For polyaluminium chloride (PACl 1.0 ) The forced hydrolysis experimental steps are as follows:

[0068] Step 1: In the polyaluminium chloride spontaneous hydrolysis tank, use deionized water with a pH of 6-8 to mix the pre-prepared PACl 1.0 The concentrate was diluted to 4 mg / L and continuously stirred at 200 rpm / min using the first stirrer.

[0069] Step 2: Use the first metering pump at the front end of the polyaluminium chloride forced hydrolysis tank to pump 1L of diluted PACl 1.0 Add it into the polyaluminium chloride forced hydrolysis tank, and close the first metering pump at the front end of the polyaluminium chloride forced hydrolysis tank.

[0070] Step 3, turn on the self-priming pump and adjust the air flow rate to 20 mL / min, and rotate the pressure regulating valve to adjust the pressure of the pipeline system to 0.7-0.8 MPa. While turning on the self-priming pump, turn on the second agitator and continue stirring at a speed of 200 rpm / min.

[0071] Step 4, after the self-priming pump circulates for 5 minutes, the first metering pump at the front end and the second metering pump at the rear end of the polyaluminium chloride forced hydrolysis tank are turned on, and the flow rates of the first metering pump and the second metering pump are adjusted to meet the required coagulant concentration in the coagulation stirring tank while ensuring continuous operation of the device.

[0072] PACl before and after 5 minutes of forced hydrolysis by fine bubbles 1.0 The changes in the hydrolysis form distribution are shown in Table 2.

[0073] Table 2 PACl before and after forced hydrolysis of fine bubbles for 5 minutes 1.0 Hydrolysis form distribution

[0074]

[0075] Example 3

[0076] For polyaluminium chloride (PACl 2.0 ) The forced hydrolysis experimental steps are as follows:

[0077] Step 1: In the polyaluminium chloride spontaneous hydrolysis tank, use deionized water with a pH of 6-8 to mix the pre-prepared PACl 2.0 The concentrate was diluted to 4 mg / L and continuously stirred at 200 rpm / min using the first stirrer.

[0078] Step 2: Use the first metering pump at the front end of the polyaluminium chloride forced hydrolysis tank to pump 1L of diluted PACl 2.0 Add it into the polyaluminium chloride forced hydrolysis tank, and close the first metering pump at the front end of the polyaluminium chloride forced hydrolysis tank.

[0079] Step 3, turn on the self-priming pump and adjust the air flow rate to 20 mL / min, and rotate the pressure regulating valve to adjust the pressure of the pipeline system to 0.7-0.8 MPa. While turning on the self-priming pump, turn on the second agitator and continue stirring at a speed of 200 rpm / min.

[0080] Step 4, after the self-priming pump circulates for 5 minutes, the first metering pump at the front end and the second metering pump at the rear end of the polyaluminium chloride forced hydrolysis tank are turned on, and the flow rates of the first metering pump and the second metering pump are adjusted to meet the required coagulant concentration in the coagulation stirring tank while ensuring continuous operation of the device.

[0081] PACl before and after 5 minutes of forced hydrolysis by fine bubbles 2.0 The changes in the hydrolysis form distribution are shown in Table 3.

[0082] Table 3 PACl before and after forced hydrolysis of fine bubbles for 5 min 2.0 Hydrolysis form distribution

[0083]

[0084] Example 4

[0085] On the basis of Example 3, the concentration of polyaluminium chloride in the coagulation stirring tank was adjusted to 8 mg / L by adjusting the concentration of polyaluminium chloride dilution and the flow rates of the first metering pump and the second metering pump, and the simulated surface water containing 5 mg / L protein and 15 mg / L humic acid was treated at this concentration under the condition of pH = 7. Compared with the conventional coagulation process without the participation of fine bubbles, the average removal rate of DOC in the coagulation precipitated water after forced hydrolysis of PACl by fine bubbles was increased by about 20%, among which the average removal efficiency of small molecular hydrophilic organic matter protein that is difficult to effectively remove by conventional coagulation process was increased by about 17.7%.

[0086] Based on the above ideal embodiments of the present invention, the relevant staff can make various changes and modifications without departing from the technical concept of the present invention through the above description. The technical scope of the present invention is not limited to the contents of the specification, and its technical scope must be determined according to the scope of the claims.

Claims

1. A forced polyaluminium chloride hydrolysis system based on microbubbles, characterized in that: include: A polyaluminium chloride spontaneous hydrolysis tank (1), wherein a first stirrer (2-1) is installed in the polyaluminium chloride spontaneous hydrolysis tank (1), and the first stirrer (2-1) is used to stir the solution in the polyaluminium chloride spontaneous hydrolysis tank (1); A polyaluminium chloride forced hydrolysis tank (4), wherein a second agitator (2-2) and a dissolved oxygen detector (10) are installed in the polyaluminium chloride forced hydrolysis tank (4), wherein the second agitator (2-2) is used to stir the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank (4), and the dissolved oxygen detector (10) is used to detect the oxygen content of the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank; a first metering pump (3), one end of the first metering pump (3) being connected to the polyaluminium chloride spontaneous hydrolysis tank (1), and the other end of the first metering pump (3) being connected to the polyaluminium chloride forced hydrolysis tank (4), and the first metering pump (3) being used to measure the flow rate of the polyaluminium chloride solution flowing between the polyaluminium chloride spontaneous hydrolysis tank (1) and the polyaluminium chloride forced hydrolysis tank (4); It also includes a gas regulating mechanism, which includes a check valve (5), a gas flow meter (6), a self-priming pump (7), a pressure gauge (8), a pressure regulating valve (9), and a granular activated carbon adsorption box (11); wherein the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank (4) is circulated by the self-priming pump (7); A check valve (5) is installed at the initial end of the water inlet pipe of the self-priming pump (7) to prevent the polyaluminium chloride solution from flowing back; The air flow rate is adjusted by adjusting the gas flow meter (6); The pressure of the pipeline system is adjusted by rotating the pressure regulating valve (9); The pressure of the pipeline system is monitored by a pressure gauge (8); Filtering the incoming air through a granular activated carbon adsorption box (11); By adjusting the gas flow rate and the pressure in the pipeline system, the self-priming pump (7) can generate fine bubbles in the process of circulating the polyaluminium chloride solution.

2. A forced polyaluminium chloride hydrolysis method based on microbubbles, characterized in that: The steps include: Step 1: Add a certain amount of polyaluminium chloride concentrate into a polyaluminium chloride spontaneous hydrolysis tank (1), and dilute the polyaluminium chloride concentrate with clean water. During the dilution process, use a first stirrer (2-1) to fully stir at a speed of 200 rpm / min, so that the polyaluminium chloride undergoes a spontaneous hydrolysis process while being diluted with clean water; Step 2: using a first metering pump (3-1) to add the diluted polyaluminium chloride solution to the polyaluminium chloride forced hydrolysis tank (4); when the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank (4) reaches a certain volume, opening the second metering pump (3-2) at the outlet to maintain the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank (4) at a certain volume; Step 3: Turn on the self-priming pump (7) and the second agitator (2-2), so that the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank (4) can be uniformly stirred by the second agitator (2-2) when circulating through the self-priming pump (7), the air flow rate is adjusted by adjusting the gas flow meter (6), and the pressure of the pipeline system is adjusted by rotating the pressure regulating valve (9). By adjusting the gas flow rate and the pressure in the pipeline system, the self-priming pump (7) can generate fine bubbles in the process of circulating the polyaluminium chloride solution, and the second agitator (2-2) is used to fully stir at a speed of 200 rpm / min so that the fine bubbles and the polyaluminium chloride are fully mixed, and then the purpose of forced polyaluminium chloride is achieved through the alkaline micro-interface formed by the hydroxide adsorbed on the surface of the fine bubbles.

3. The microbubble-based forced polyaluminium chloride hydrolysis method according to claim 2, characterized in that: The gas source connected to the gas flow meter (6) can be not only air but also oxygen to increase the ability of fine bubbles to generate hydroxyl free radicals. The granular activated carbon adsorption box (11) is connected to the gas inlet of the gas flow meter.

4. The microbubble-based forced polyaluminium chloride hydrolysis method according to claim 2, characterized in that: The gas flow meter (6) can adjust the gas flow rate in the range of 20-60 mL / min; when the gas flow rate is 20 mL / min, the concentration of fine bubbles is relatively high.

5. The microbubble-based forced polyaluminium chloride hydrolysis method according to claim 2, characterized in that: The pressure of the pipeline system can be adjusted by rotating the pressure regulating valve (9). When the pressure in the pressure gauge (8) is between 0.7 and 0.8 MPa, the fine bubbles generated by the system have the best effect.

6. The microbubble-based forced polyaluminium chloride hydrolysis method according to claim 2, characterized in that: The diameter of the water inlet pipe of the self-priming pump (7) is appropriately reduced, and the diameter of the water outlet pipe is appropriately increased and the length of the water outlet pipe is extended. The diameter of the water outlet pipe needs to be greater than 1.5 times the diameter of the water inlet pipe, and the length of the water outlet pipe needs to be greater than 2.0 times the length of the water inlet pipe.

7. The microbubble-based forced polyaluminium chloride hydrolysis method according to claim 2, characterized in that: A tubular static mixer is added to the water outlet pipeline at the rear end of the pressure regulating valve (9) to fully mix the fine bubbles with the polyaluminium chloride.

8. The method for forced polyaluminium chloride hydrolysis based on microbubbles according to claim 2, characterized in that: The flow rates of the first metering pump (3-1) and the second metering pump (3-2) are adjusted to adjust the hydraulic retention time of the polyaluminium chloride solution in the polyaluminium chloride forced hydrolysis tank (4), thereby adjusting the time for the fine bubbles to force the polyaluminium chloride to hydrolyse.

9. The microbubble-based forced polyaluminium chloride hydrolysis method according to claim 2, characterized in that: A dissolved oxygen detector (10) is added to the polyaluminium chloride forced hydrolysis tank (4) to adjust the stirring speed in the polyaluminium chloride forced hydrolysis tank (4) by detecting the dissolved oxygen concentration in the solution.

10. The method for forced polyaluminium chloride hydrolysis based on microbubbles according to claim 2, characterized in that: A check valve (5) is installed at the initial end of the water inlet pipe of the self-priming pump (7) to prevent the polyaluminium chloride solution from flowing back.