Top gate self-aligned metal oxide semiconductor transistor and preparation method thereof

By using a layered structure of contact metal, oxygen absorbing metal and surface metal in the top gate self-aligning metal oxide semiconductor transistor, the semiconductor and source and drain electrodes are solved by using oxygen absorbing metal to absorb oxygen during annealing process, and The high-resistance problem of contact has achieved improved electrical performance and reduced size of the device, which is suitable for a variety of application scenarios.

CN119029047APending Publication Date: 2024-11-26SHANGHAI JIAOTONG UNIV
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411122734.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

In the prior art, the top gate self-aligned metal oxide semiconductor transistor is difficult and costly to achieve low resistance in the contact portion between the semiconductor and the source and drain, and is not suitable for the field of thin film transistors.

Method used

Using a layered structure of contact metal, oxygen-absorbing metal and surface metal, during the annealing process, the oxygen-absorbing metal absorbs oxygen in the semiconductor layer to form a low-resistance region, simplifying the process and reducing the resistance of the source and drain electrode contact.

Benefits of technology

It effectively reduces parasitic capacitance and channel length, improves the electrical performance of the device, and is suitable for three-dimensional monolithic integration that is compatible with display, logic, RF and post-channel processes, and the process is simple and easy to perform.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119029047A_ABST
    Figure CN119029047A_ABST
Patent Text Reader

Abstract

The invention provides a top gate self-aligned metal oxide semiconductor transistor and a preparation method thereof. The transistor comprises a substrate; the semiconductor layer is located on the substrate, the upper surface of the semiconductor layer sequentially comprises a first low-resistance region, a middle region and a second low-resistance region from left to right, and the middle region is a normal thin film region; the gate dielectric layer is positioned right above the middle region; the gate electrode is positioned right above the gate dielectric layer; the source electrode is positioned right above the first low-resistance region; the drain electrode is positioned right above the second low-resistance region; and the source electrode and the drain electrode sequentially comprise three layers of metal, namely contact metal, oxygen absorption metal and surface metal from bottom to top. The semiconductor layer area in contact with the source electrode and the drain electrode is processed by using the method for realizing oxygen removal by using the oxygen absorbing metal, so that the low-resistance area is formed, and the method is simple and easy to realize; the parasitic capacitance and the device size of the transistor can be reduced, and the overall electrical performance of the device is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of microelectronic devices, and in particular to a top-gate self-aligned metal oxide semiconductor transistor and a preparation method thereof. Background Art

[0002] Metal oxide semiconductors are widely used in fields ranging from large-scale displays to flexible devices due to their moderate mobility, low leakage, low cost, high on-off ratio, high uniformity over large areas, high transparency, and excellent flexibility. In addition, due to low process temperature and extremely low off current, they have great prospects in emerging applications, including the Internet of Things, monolithic three-dimensional integrated nanoelectronics and photonic systems, which require low power consumption and high performance. Compared with the bottom-gate device structure, the top-gate metal oxide semiconductor transistor can have a self-aligned and three-dimensional structure, which can effectively reduce parasitic capacitance and channel length. It is crucial to improve the electrical performance of the device in three-dimensional monolithic integration applications compatible with display, logic, radio frequency and back-end processes. One of the key issues in the preparation of top-gate self-aligned metal oxide semiconductor transistors is the low resistance of the semiconductor contact part with the source and drain.

[0003] Therefore, how to achieve low resistance of the contact part between the semiconductor and the source and drain and prepare high-quality top-gate self-aligned metal oxide semiconductor transistors is a technical problem that needs to be solved urgently.

[0004] After searching, the Chinese invention patent with application publication number CN116895529A discloses a semiconductor structure and its preparation method, the preparation method includes: providing a substrate, a transistor is formed on the substrate, the transistor includes a gate structure formed on the substrate and a source and a drain formed on both sides of the gate structure; forming a dielectric layer on the substrate, and forming a contact hole in the dielectric layer, the contact hole exposing the source / drain of the transistor; forming a doped metal oxide layer in the contact hole; forming a metal silicide layer on the surface of the doped metal oxide layer. This patent involves complex processes such as ion implantation, oxide layer growth, and multi-step annealing to reduce the contact resistance between the metal silicide layer and the source / drain, which has the problems of great difficulty and high cost, and is not suitable for the field of thin film transistors. Summary of the invention

[0005] In view of the defects in the prior art, an object of the present invention is to provide a top-gate self-aligned metal oxide semiconductor transistor and a method for manufacturing the same.

[0006] According to one aspect of the present invention, there is provided a top-gate self-aligned metal oxide semiconductor transistor, the transistor comprising:

[0007] substrate;

[0008] A semiconductor layer is located on the substrate, wherein the upper surface of the semiconductor layer includes a first low resistance region, a middle region and a second low resistance region from left to right, wherein the middle region is a normal thin film region;

[0009] A gate dielectric layer, located directly above the middle region;

[0010] A gate, located directly above the gate dielectric layer;

[0011] A source electrode, located directly above the first low resistance region;

[0012] The drain is located directly above the second low resistance region; the source and drain include three layers of metal from bottom to top, namely, contact metal, oxygen absorbing metal and surface metal.

[0013] Furthermore, the oxygen-absorbing metal is a metal that easily reacts with oxygen to form an oxide.

[0014] Furthermore, the surface metal is a metal that does not react easily with oxygen.

[0015] Furthermore, the contact metal is a metal that matches the work function of the semiconductor layer.

[0016] Optionally, the material of the gate is at least one of tungsten, Mo, nickel and ITO.

[0017] Optionally, the material of the semiconductor layer is indium gallium zinc oxide, or an oxide containing at least one of indium oxide, zinc oxide, gallium oxide and tin oxide.

[0018] Optionally, the transistor further includes: a buffer layer, wherein the buffer layer is located between the substrate and the semiconductor layer.

[0019] According to another aspect of the present invention, a method for preparing the top-gate self-aligned metal oxide semiconductor transistor is provided, the method comprising:

[0020] providing a substrate;

[0021] depositing a metal oxide semiconductor thin film on the substrate;

[0022] performing photolithography and etching on the metal oxide semiconductor film to obtain a patterned metal oxide semiconductor;

[0023] depositing a gate dielectric layer on the patterned metal oxide semiconductor;

[0024] Depositing metal on the gate dielectric layer and then patterning it or depositing metal after photolithography-defining a pattern, and peeling off to obtain a metal pattern;

[0025] Etching the gate dielectric on the semiconductor layer without gate metal protection;

[0026] The source and drain regions are defined by photolithography, and contact metal, oxygen-absorbing metal, and surface metal are deposited from bottom to top;

[0027] The device is annealed so that the film contacting the source and drain electrodes forms a low resistance region, thereby obtaining a top-gate self-aligned metal oxide semiconductor transistor.

[0028] Furthermore, the device is annealed so that the thin film contacting the source and drain electrodes forms a low resistance region, wherein: during the annealing process, the oxygen-absorbing metal of the source and drain absorbs oxygen in the semiconductor layer to form a first low resistance region and a second low resistance region respectively.

[0029] Furthermore, the device is annealed so that the thin film contacting the source and drain electrodes forms a low resistance region, wherein: the annealing temperature is 200° C. to 1000° C., and the annealing atmosphere is at least one of nitrogen, oxygen, ammonia and argon.

[0030] Compared with the prior art, the present invention has at least one of the following beneficial effects:

[0031] The top-gate self-aligned metal oxide semiconductor transistor provided by the present invention adopts a top-gate structure, which can effectively reduce the parasitic capacitance formed by the overlap of the gate and the source and drain electrodes, and is helpful to reduce the size of the device; the source and drain are respectively located directly above the low-resistance region of the semiconductor layer, which can effectively reduce the parasitic capacitance and the channel length, and improve the overall electrical performance of the device, thereby making the device more suitable for application in three-dimensional monolithic integration compatible with display, logic, radio frequency and back-end processes.

[0032] The source and drain of the present invention adopt a layered structure of contact metal, oxygen-absorbing metal and surface metal. During the annealing process, the oxygen-absorbing metal absorbs oxygen in the semiconductor to form a source-drain contact low-resistance region. The semiconductor layer region in contact with the source and drain is treated by a method of oxygen removal using the oxygen-absorbing metal to form a low-resistance region, thereby solving the problem of metal and semiconductor contact in top-gate transistors. The present invention can realize low resistance of metal oxide semiconductors in the source and drain metal contact regions through simple annealing, and the process is simple and easy to implement. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Other features, objects and advantages of the present invention will become more apparent from the detailed description of non-limiting embodiments made with reference to the following drawings:

[0034] Figure 1 is a schematic structural diagram of a top-gate self-aligned metal oxide semiconductor transistor in one embodiment of the present invention;

[0035] Figure 2 is a schematic cross-sectional view of a buffer layer formed on a substrate in one embodiment of the present invention;

[0036] Figure 3 is a schematic cross-sectional view of an embodiment of the present invention after an oxide film is deposited;

[0037] Figure 4 is a schematic cross-sectional view after a gate dielectric layer is deposited in one embodiment of the present invention;

[0038] Figure 5 is a cross-sectional schematic diagram of depositing a gate electrode on a gate dielectric layer in one embodiment of the present invention;

[0039] Figure 6 It is a schematic diagram of patterning a semiconductor layer using a deposited gate electrode as a mask in one embodiment of the present invention.

[0040] In the figure, the reference numerals correspond to: 101-substrate, 102-buffer layer, 11-semiconductor layer, 111-second low resistance region, 112-first low resistance region, 113-middle region, 103-gate dielectric layer, 104-gate, 12-source, 121-source contact metal, 122-source oxygen absorbing metal, 123-source surface metal, 13-drain, 131-drain contact metal, 132-drain oxygen absorbing metal, 133-drain surface metal. DETAILED DESCRIPTION

[0041] The present invention is described in detail below in conjunction with specific embodiments. The following embodiments will help those skilled in the art to further understand the present invention, but are not intended to limit the present invention in any form. It should be noted that, for those of ordinary skill in the art, several variations and improvements may be made without departing from the concept of the present invention. These all belong to the protection scope of the present invention.

[0042] It should be noted that the terms "first", "second", etc. are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. Moreover, the terms "first", "second", etc. are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable where appropriate so that the embodiments of the present application described herein can be implemented in an order other than that illustrated or described herein.

[0043] Reference Figure 1A top-gate self-aligned metal oxide semiconductor transistor provided by an embodiment of the present invention comprises: a substrate 101, a semiconductor layer 11, a gate dielectric layer 103, a gate 104, a source 12 and a drain 13, wherein the semiconductor layer 11 is located on the substrate 101, and the upper surface of the semiconductor layer 11 comprises a first low resistance region 112, a middle region 113 and a second low resistance region 111 from left to right, wherein the middle region 113 is a normal thin film region, i.e., an untreated region of the semiconductor layer thin film, and the first low resistance region 112 and the second low resistance region 111 have lower resistance than the middle region 113, which is equivalent to the existing mainstream level (about ~kΩ / μm); the gate dielectric layer 103 is located directly above the middle region 113; the gate 104 is located directly above the gate dielectric layer 103; the source 12 is located directly above the first low resistance region 112; the drain 13 is located directly above the second low resistance region 111; the source 12 and the drain 13 comprise three layers of metal, i.e., contact metal, oxygen absorbing metal and surface metal, from bottom to top, such as Figure 1 The middle source 12 includes three metal layers from bottom to top, namely, a source contact metal 121, a source oxygen absorbing metal 122, and a source surface metal 123. The drain 13 includes three metal layers from bottom to top, namely, a drain contact metal 131, a drain oxygen absorbing metal 132, and a drain surface metal 133. The oxygen absorbing metal is used to absorb oxygen in the semiconductor layer 11 to form oxygen vacancies Vo. The oxygen vacancies Vo generate two free electrons in the conductor band and act as shallow donors to form a low resistance region in the corresponding area on the semiconductor layer 11.

[0044] The embodiment of the present invention adopts a self-aligned top gate structure, which ensures the precise alignment between the gate 104 and the source 12 and the drain 13, avoids possible alignment errors, simplifies the process steps, and improves the performance and reliability of the transistor; moreover, there is no overlapping area between the gate electrode and the source 12 and the drain 13, which can effectively reduce the parasitic capacitance formed by the overlap of the gate 104 and the source 12 and the drain 13, and helps to reduce the size of the device; the source 12 and the drain 13 include three layers of metal from bottom to top, namely, contact metal, oxygen absorbing metal and surface metal, and the semiconductor region in contact with the source 12 and the drain 13 is treated by a method of oxygen removal using oxygen absorbing metal, so that it forms a low resistance region, which solves the problem of metal-semiconductor contact in the top gate transistor. The embodiment of the present invention efficiently achieves low resistance between the semiconductor and the source / drain by simply adding a layer of oxygen absorbing metal and annealing process. In the embodiment of the present invention, the source 12 and the drain 13 are respectively located directly above the low resistance region of the semiconductor layer, which can effectively reduce the parasitic capacitance and the channel length and improve the overall electrical performance of the device, thereby making the device more suitable for application in three-dimensional monolithic integration compatible with display, logic, radio frequency and back-end processes.

[0045] In the embodiment of the present invention, the oxygen absorbing layer is used for reactive oxygen absorption. The oxygen absorbing metal is a metal that easily reacts with oxygen to form an oxide during annealing. For example, the oxygen absorbing metal uses metal scandium, titanium, etc. The surface metal is a metal that does not easily react with oxygen to block the oxygen absorbing layer from reacting with the outside world. For example, the surface metal uses gold, tungsten, etc. The contact metal is a metal that matches the work function of the semiconductor layer 11. For example, the contact metal uses nickel, molybdenum, tungsten, ITO, etc., so as to form a good ohmic contact and reduce the contact resistance.

[0046] The material work function of the gate 104 is related to the work function of the device. Generally, a metal with a relatively large work function is selected to make the threshold voltage more positive. In addition, since the process requires annealing, the material is required to have good thermal stability. In some embodiments, the material of the gate 104 is at least one of tungsten, Mo, nickel and ITO, which can well meet the above requirements.

[0047] In some embodiments, the semiconductor layer 11 can be formed by magnetron sputtering, solution method, atomic layer deposition, chemical vapor deposition, pulsed laser deposition, etc. The material of the semiconductor layer 11 is indium gallium zinc oxide, or an oxide containing at least one of indium oxide, zinc oxide, gallium oxide, and tin oxide, thereby forming a metal oxide semiconductor layer.

[0048] In some embodiments, the transistor further includes a buffer layer 102 , where the buffer layer 102 is located between the substrate 101 and the semiconductor layer 11 , and the metal oxide semiconductor layer 11 is grown on the buffer layer 102 .

[0049] Exemplarily, the material of the buffer layer 102 is aluminum oxide, or other thin films that are convenient for photolithography.

[0050] In the above embodiment of the present invention, a transistor is formed on a substrate, and the transistor includes a dielectric layer and a semiconductor layer formed on the substrate, and a gate is formed on the semiconductor layer, and a contact hole is formed in the dielectric layer, and the contact hole exposes the semiconductor layer; a contact metal, an oxygen-absorbing metal, and a surface metal are formed in the contact hole, and the oxygen-absorbing metal reacts with the semiconductor during the annealing process, so that a large number of oxygen vacancies are generated in the semiconductor in the metal-semiconductor contact part, thereby reducing the contact resistance. The low-resistance semiconductor in metal oxides is mostly made by etching bombardment and other methods, which often have problems such as poor thermal stability. The embodiment of the present invention increases the thermal stability of the device while achieving low resistance by adding a layer of oxygen-absorbing metal and using a relatively simple process.

[0051] Another embodiment of the present invention provides a method for preparing the top-gate self-aligned metal oxide semiconductor transistor. Figure 2-Figure 6 , the method comprising:

[0052] S1, providing a substrate 101;

[0053] S2, depositing a metal oxide semiconductor thin film on the substrate 101;

[0054] S3, performing photolithography and etching on the metal oxide semiconductor film to obtain a patterned metal oxide semiconductor;

[0055] S4, depositing a gate dielectric layer 103 on the patterned metal oxide semiconductor;

[0056] S5, depositing metal on the gate dielectric layer 103 and then patterning it or depositing metal after photolithography-defining a pattern, and peeling off to obtain a metal pattern, namely, the gate 104;

[0057] S6, etching the gate dielectric on the semiconductor layer 11 without gate metal protection;

[0058] S7, photolithography defines the source 12 and drain 13 regions on both sides of the gate 104, and deposits contact metal, oxygen absorbing metal and surface metal in sequence from bottom to top;

[0059] S8. Annealing the device so that the thin film in contact with the source and drain electrodes forms a low resistance region, thereby obtaining a top-gate self-aligned metal oxide semiconductor transistor.

[0060] In the above embodiment, during the annealing process, the oxygen-absorbing metals of the source 12 and the drain 13 absorb oxygen in the semiconductor layer 11 to form oxygen vacancies, thereby forming the first low-resistance region 112 and the second low-resistance region 111 , respectively.

[0061] In some embodiments, the device is annealed so that the thin film contacting the source and drain electrodes forms a low resistance region, wherein: the annealing after the deposition of the source 12 and the drain 13 can be performed by rapid thermal annealing, a muffle furnace or a hot stage and other equipment. Depending on the properties of the oxygen-absorbing metal, the annealing temperature is 200°C to 1000°C, and the annealing atmosphere is at least one of nitrogen, oxygen, ammonia and argon.

[0062] The above embodiment of the present invention uses oxygen-absorbing metals for the source and drain electrodes, and through a simple annealing process, the contact resistance of the source and drain metals in the contact area with the semiconductor layer can be reduced. The process is simple and feasible, and can be widely used in the semiconductor field. The transistor in the above embodiment can effectively reduce parasitic capacitance and channel length, and has the advantages of small parasitic capacitance and strong proportional reduction capability, making the device more suitable for use in three-dimensional monolithic integration compatible with display, logic, radio frequency and back-end processes.

[0063] The above describes the specific embodiments of the present invention. It should be understood that the present invention is not limited to the above specific embodiments, and those skilled in the art can make various modifications or variations within the scope of the claims, which does not affect the essence of the present invention. The above preferred features can be used in any combination without conflicting with each other.

Claims

1. A top-gate self-aligned metal oxide semiconductor transistor, It is characterized in that include: substrate; A semiconductor layer is located on the substrate, wherein the upper surface of the semiconductor layer includes a first low resistance region, a middle region and a second low resistance region from left to right, wherein the middle region is a normal thin film region; A gate dielectric layer, located directly above the middle region; A gate, located directly above the gate dielectric layer; A source electrode, located directly above the first low resistance region; The drain is located directly above the second low resistance region; the source and drain include three layers of metal from bottom to top, namely, contact metal, oxygen absorbing metal and surface metal.

2. The top-gate self-aligned metal oxide semiconductor transistor according to claim 1, It is characterized in that The oxygen-absorbing metal is a metal that easily reacts with oxygen to form an oxide.

3. The top-gate self-aligned metal oxide semiconductor transistor according to claim 1, It is characterized in that The surface metal is a metal that is not easy to react with oxygen.

4. The top-gate self-aligned metal oxide semiconductor transistor according to claim 1, It is characterized in that The contact metal is a metal having a work function matching that of the semiconductor layer.

5. The top-gate self-aligned metal oxide semiconductor transistor according to claim 1, It is characterized in that The gate is made of at least one of tungsten, Mo, nickel and ITO.

6. The top-gate self-aligned metal oxide semiconductor transistor according to claim 1, It is characterized in that The material of the semiconductor layer is indium gallium zinc oxide, or an oxide containing at least one of indium oxide, zinc oxide, gallium oxide, and tin oxide.

7. The top-gate self-aligned metal oxide semiconductor transistor according to claim 1, It is characterized in that Also includes: A buffer layer is located between the substrate and the semiconductor layer.

8. A method for preparing a top-gate self-aligned metal oxide semiconductor transistor according to any one of claims 1 to 7, It is characterized in that include: providing a substrate; depositing a metal oxide semiconductor thin film on the substrate; performing photolithography and etching on the metal oxide semiconductor film to obtain a patterned metal oxide semiconductor; depositing a gate dielectric layer on the patterned metal oxide semiconductor; Depositing metal on the gate dielectric layer and then patterning it or depositing metal after photolithography-defining a pattern, and peeling off to obtain a metal pattern; Etching the gate dielectric on the semiconductor layer without gate metal protection; The source and drain regions are defined by photolithography, and contact metal, oxygen-absorbing metal, and surface metal are deposited from bottom to top; The device is annealed so that the film contacting the source and drain electrodes forms a low resistance region, thereby obtaining a top-gate self-aligned metal oxide semiconductor transistor.

9. The method for preparing a top-gate self-aligned metal oxide semiconductor transistor according to claim 8, It is characterized in that The device is annealed so that the thin film contacting the source and drain electrodes forms a low resistance region, wherein: during the annealing process, the oxygen-absorbing metal of the source and drain electrodes absorbs oxygen in the semiconductor layer to form a first low resistance region and a second low resistance region respectively.

10. The method for preparing a top-gate self-aligned metal oxide semiconductor transistor according to claim 8, It is characterized in that The device is annealed so that the film contacting the source and drain electrodes forms a low resistance region, wherein: the annealing temperature is 200° C. to 1000° C., and the annealing atmosphere is at least one of nitrogen, oxygen, ammonia and argon.

Citation Information

Cited By

  • Metal oxide thin film transistor and preparation method thereof

    CN119894054A