Inorganic composite modifying and flooding agent as well as preparation method and application thereof
By using inorganic composite distortion agents in offshore high-water oil fields, the generation of calcium carbonate scale is suppressed by electrostatic repulsion and steric hindrance, the problems of water injection pipeline blockage and large channel blockage are solved, and stronger precipitation and sealing are achieved Effect and environmental performance.
Patent Information
- Application Number
- CN202411185097.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-12-03
AI Technical Summary
In the high-water oil field at sea, under conditions where the divalent ion content in the injected water is low and bicarbonate ions are contained, the added calcium chloride will react quickly with the sodium bicarbonate in the injected water to form calcium carbonate precipitation, resulting in the formation of a water injection pipeline. Calcium carbonate scale coating blocks the water injection pipeline, and traditional regulators are difficult to effectively seal large holes in high temperature and high salt environments.
Inorganic composite mixing agents, including emulsion polymers, calcium chloride, polycarboxylic acid stabilizers and sodium silicate, inhibit the formation of calcium carbonate and calcium silicate scale through electrostatic repulsion and steric hindrance, and prevent the injection pipeline and Calcium carbonate scale is formed near the well area, and it precipitates and accumulates in the deep strata to seal the large pores.
Effectively prevent the water injection pipeline from being blocked, improve the sealing strength of the precipitation system, ensure effective sealing of the large wells, increase the impact volume of injected water, and reduce the amount of polyacrylamide compared with traditional mixing agents, and does not contain phenolic acid Resin ingredients are more green and environmentally friendly.
Smart Images

Figure BDA0005013284420000091 
Figure BDA0005013284420000101 
Figure BDA0005013284420000102
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of oilfield chemistry, and relates to an inorganic composite control and displacement agent, a preparation method and application thereof, and in particular to an inorganic composite control and displacement agent for offshore high-water-content oilfields, a preparation method and application thereof. Background Art
[0002] Injecting sodium silicate solution and precipitation inhibitors (PBTC, ATMP and HEDP, etc.) into the injection wells of offshore high-mineralization blocks (injection water rich in calcium and magnesium ions) can effectively control the generation time and initial particle size of calcium silicate precipitation. The injected liquid system migrates to the deep formation with the injected water and then precipitates and aggregates, achieving the effect of effectively blocking the high-permeability channel. It is applied in offshore high-temperature and high-salinity oil fields and achieves a high oil-increasing and water-reducing effect.
[0003] However, under the condition that the content of divalent ions in the injected water is low and the water contains a certain amount of bicarbonate ions, the added calcium chloride will quickly react with the sodium bicarbonate in the injected water to form calcium carbonate precipitation. 3 / d), during the injection of the profiler, calcium carbonate scale coating is easily formed in the water injection pipeline, blocking the water injection pipeline. At the same time, as the main offshore water drive development oil fields enter the high water content development stage, the reservoir heterogeneity and large pores are significantly developed. While ensuring the good injectability and deep migration of the inorganic precipitation system, it is necessary to further improve the plugging strength of the precipitation system, ensure the effective plugging of the large pores between wells, and increase the swept volume of the injected water. Summary of the invention
[0004] In view of the defects of the prior art, the present invention provides an inorganic composite flooding agent and a preparation method and application thereof.
[0005] Specifically, the inorganic composite displacement agent provided by the present invention comprises an emulsion polymer, calcium chloride, a polycarboxylic acid stabilizer, sodium silicate and water.
[0006] The inorganic composite displacement agent comprises, by weight percentage, 0.03% to 0.05% of emulsion polymer, 0.05% to 0.2% of calcium chloride, 0.15% to 0.6% of polycarboxylic acid stabilizer, 0.05% to 0.2% of sodium silicate and the balance of water.
[0007] The inorganic composite displacement agent comprises, by weight percentage: 0.03% to 0.05% of emulsion polymer, 0.10% to 0.15% of calcium chloride, 0.25% to 0.35% of polycarboxylic acid stabilizer, 0.10% to 0.15% of sodium silicate and the balance of water.
[0008] The inorganic composite displacement agent mentioned above, the emulsion polymer is an emulsion type polyacrylamide, the degree of hydrolysis is 3% to 18%, and the molecular weight is 3 million to 8 million.
[0009] The above-mentioned inorganic composite displacement agent and the polycarboxylic acid stabilizer are prepared by the following method:
[0010] (1) dissolving the substituted polyether compound and the thiol compound in water according to a ratio to prepare a solution A;
[0011] (2) dissolving acrylic acid and methacryloyloxyethyl trimethyl ammonium chloride in water according to a ratio to prepare solution B;
[0012] (3) dissolving ammonium persulfate in water according to the ratio to prepare solution C;
[0013] (4) under nitrogen protection, adding the solution B and the solution C to the solution A in a dropwise manner to obtain a mixed system, and heat-insulating and aging;
[0014] (5) After the reaction is completed, the mixture is cooled to room temperature, and then a base is added to adjust the pH to 6-8 to obtain a polycarboxylic acid stabilizer.
[0015] In the above-mentioned inorganic composite displacement agent, the substituted polyether compound is at least one of methyl allyl polyethylene glycol ether, isopentenyl polyoxyethylene ether, ethylene glycol monovinyl polyoxyethylene ether, and 4-hydroxybutyl vinyl polyoxyethylene ether; and the thiol compound is at least one of thioglycolic acid, mercaptopropionic acid, mercaptoethanol, and mercaptopropanol.
[0016] The inorganic composite displacement agent has a reaction temperature of 60° C. to 70° C. and a reaction time of 4 h to 8 h.
[0017] In the above-mentioned inorganic composite control agent, the weight ratio of the substituted polyether compound, the thiol compound and the water is (35.5-44.6): (0.28-0.32): (48-50); the weight ratio of the acrylic acid, the methacryloyloxyethyltrimethylammonium chloride and the water is (3.20-5.15): (8.2-14.5): (23.5-26); the weight ratio of the ammonium persulfate to the water is (1.00-1.15): (19-20.5).
[0018] In the inorganic composite control agent, the molar ratio of the acrylic acid to the substituted polyether compound is 3.0 to 4.2; the molecular weight of the polycarboxylic acid stabilizer is 20,000 to 29,000. 。
[0019] On the other hand, the present invention also provides a method for preparing the above-mentioned inorganic composite flooding agent, comprising:
[0020] (1) dissolving a polycarboxylic acid stabilizer and sodium silicate in water according to a ratio to obtain a main agent mother solution;
[0021] (2) dissolving calcium chloride in water according to a ratio to obtain an additive mother solution;
[0022] (3) mixing the main agent mother solution and the auxiliary agent mother solution;
[0023] (4) adding an emulsion polymer to the mixed solution in step (3) to obtain the inorganic composite displacement agent.
[0024] In another aspect, the present invention further provides the use of the inorganic composite flooding agent or the inorganic composite flooding agent obtained by the above preparation method in offshore high water content oil fields.
[0025] The technical solution of the present invention has the following beneficial effects:
[0026] (1) The inorganic composite flooding agent of the present invention is suitable for flooding of reservoirs with low divalent ion content and a certain amount of bicarbonate ions in the water injected into the water, ensuring that during the injection of the flooding agent, it is not easy to form a calcium carbonate scale coating in the water injection pipeline to block the water injection pipeline, and at the same time, it settles and gathers in the deep formation to block the high-permeability water channel, thereby achieving the effect of diverting the deep liquid flow;
[0027] (2) The inorganic composite flooding agent of the present invention can effectively improve the plugging strength of the precipitation system, ensure the effective plugging of the large pores between wells, and increase the swept volume of the injected water;
[0028] (3) The inorganic composite flooding agent of the present invention has better aging performance than the traditional polymer gel or pre-crosslinked particle flooding plugging system, and compared with the previous organic flooding agent, the amount of polyacrylamide used is significantly reduced, and it does not contain phenolic resin components, which is more environmentally friendly;
[0029] (4) The inorganic composite flooding agent of the present invention has a simple preparation method and is easy to operate. It can be mixed by stirring at room temperature to 90° C., and is suitable for industrial production and on-site application. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the following detailed description of the preferred embodiment.The drawings are only for the purpose of illustrating the preferred embodiments and are not to be construed as limiting the invention.
[0031] Figure 1 The median particle size result of the first test (5min) of the displacement agent system in Example 1;
[0032] Figure 2 The median particle size result of the second test (10 min) of the initial stage of the displacement agent system of Example 1;
[0033] Figure 3 The initial photo of the control agent system of Example 1;
[0034] Figure 4 Photo of the drive agent system of Example 1 heated for 48 hours;
[0035] Figure 5 Photo of the drive agent system of Example 1 heated for 60 hours;
[0036] Figure 6 The median particle size result of the first test (5min) of the displacement agent system in Example 2;
[0037] Figure 7 The median particle size result of the second test (10 min) of the initial stage of the displacement agent system of Example 2;
[0038] Figure 8 The photo of the control agent system of Example 2 was heated for 96 hours. The system was relatively stable without precipitation.
[0039] Fig. 9 The pressure variation curves of each pressure measuring point in the deep flooding experiment;
[0040] Fig.10 The median particle size result of the first test (5min) of the displacement agent system in Example 3;
[0041] Fig.11 The median particle size result of the second test (10 min) of the initial stage of the displacement agent system of Example 3;
[0042] Fig.12 The photo of the control agent system of Example 3 at the initial stage of heating at 65°C;
[0043] Fig.13 Photo of the control agent system of Example 3 heated at 65°C for 48h;
[0044] Fig.14 Photo of the control agent system of Example 3 heated at 65°C for 56h;
[0045] Fig.15 Photo of the control agent system of Example 3 heated at 65°C for 72h;
[0046] Fig.16 The particle size classification results of the control and displacement agent system of Example 4 from the initial stage to 2 hours after heating;
[0047] Fig.17 The initial photo of the control and displacement agent system of Example 4 shows that the initial particle size is as large as 34.2 μm;
[0048] Fig.18The control agent system of Example 4 was heated at 65°C for 48 hours and remained stable without precipitation;
[0049] Fig.19 The control agent system of Example 4 was heated at 65°C for 72 hours, and insoluble substances appeared;
[0050] Fig. 20 An initial photograph of the displacement agent system of Example 5;
[0051] Fig.21 The initial particle size distribution of the displacement agent system of Example 5;
[0052] Fig. 22 The median particle size result of the first test (5min) of the control agent system of Comparative Example 1;
[0053] Fig.23 The median particle size result of the second test (10min) of the initial stage of the control and displacement agent system of Comparative Example 1;
[0054] Fig.24 Photo of the control agent system of Comparative Example 1 after heating for 16 hours;
[0055] Fig.25 The initial preparation photo of the displacement system of Comparative Example 2 shows the presence of insoluble matter;
[0056] Fig.26 The initial preparation photo of the displacement system of Comparative Example 3 shows the presence of insoluble matter;
[0057] Fig. 27 The initial preparation photo of the displacement system of Comparative Example 4 shows the presence of insoluble matter. DETAILED DESCRIPTION
[0058] In order to fully understand the purpose, features and effects of the present invention, the present invention is described in detail through the following specific embodiments. Except for the following contents, the process method of the present invention adopts conventional methods or devices in the art. Unless otherwise specified, the following terms have the meanings commonly understood by those skilled in the art.
[0059] When a numerical range is disclosed herein, the above range is considered to be continuous and includes the minimum and maximum values of the range, as well as every value between such minimum and maximum values. Further, when a range refers to an integer, every integer between the minimum and maximum values of the range is included. In addition, when multiple ranges are provided to describe a feature or characteristic, the ranges can be combined. In other words, unless otherwise indicated, all ranges disclosed herein should be understood to include any and all subranges included therein.
[0060] It should be noted that, in this article, "inorganic composite displacement agent", "displacement agent", "composite system" and "displacement agent system" have the same meaning and can be used interchangeably.
[0061] Specifically, according to the first aspect of the present invention, the present invention provides an inorganic composite displacement agent, comprising: an emulsion polymer, calcium chloride, a polycarboxylic acid stabilizer, sodium silicate and water.
[0062] The inorganic composite displacement agent of the present invention utilizes divalent ions in the formation and uses calcium chloride and a polycarboxylic acid stabilizer with special properties to effectively inhibit the reaction between the added calcium ions and the bicarbonate in the injected water, thereby preventing the formation of calcium carbonate scale in the injection pipeline and near-well area, thereby blocking the pipeline. At the same time, the electrostatic repulsion and steric hindrance of the polycarboxylic acid stabilizer and the inorganic particle surface are taken into consideration, so that the system can achieve a better dispersion and stabilization effect, and re-precipitate in the deep formation to achieve the effect of blocking large pores.
[0063] The present invention optimizes the polycarboxylic acid dispersant, inhibits the initial formation of calcium carbonate and calcium silicate scale by electrostatic repulsion and steric hindrance, affects the particle dispersion performance, and prevents the added calcium ions from being affected by bicarbonate in the water, thereby enhancing the dispersion stability of the precipitated particles. On the other hand, an emulsion polymer with a low degree of hydrolysis and a low molecular weight is preferred to enhance the strength of the inorganic precipitation control agent, thereby obtaining an inorganic composite control system.
[0064] The components of the inorganic composite flooding agent of the present invention are introduced in detail below:
[0065] Emulsion polymer
[0066] In order to further increase the strength of the inorganic precipitation flooding system, a low mass concentration of emulsion polymer is added to the inorganic flooding system to increase the viscosity of the system and thereby enhance the flow resistance of the water phase.
[0067] The emulsion polymer used in the present invention is a long polymer chain with a charge. In order to utilize the viscosity of the emulsion polymer, the emulsion polymer and the inorganic particles formed after precipitation are mutually wrapped, further increasing the strength and plugging performance of the system, and reducing the influence of the anionic charge of the emulsion polymer on the dispersion performance of the composite system. At the same time, considering that the initial viscosity of the composite system does not need to be high, because a higher initial viscosity will affect the ability of the system to enter the deep formation, we expect that in the injected water with a low content of divalent ions and a certain amount of bicarbonate ions in the water, the composite adjustment and displacement agent has a lower initial viscosity, and at the same time utilizes the interaction between the emulsion polymer and the particles, and does not precipitate initially. As the migration process in the formation, under the action of the formation temperature and salinity, precipitation and mutual wrapping occur again, thereby achieving the purpose of improving the plugging performance of the deep formation.
[0068] The present invention selects an emulsion polymer product with low hydrolysis degree (3% to 18% hydrolysis degree) and low molecular weight (3 million to 8 million).
[0069] Preferably, the emulsion polymer is partially hydrolyzed anionic polyacrylamide obtained by emulsion polymerization, which is an industrial product and has an effective content of 28% to 35%.
[0070] Preferably, the concentration of the emulsion polymer is 300-500 mg / L.
[0071] Preferably, the content of the emulsion polymer in the inorganic composite displacement agent is 0.03% to 0.05% by weight.
[0072] The present invention characterizes the viscosity, adsorption, surface and interface properties and plugging performance of the composite system. Taking a concentration within the preferred use range as an example, when an emulsion polymer solution with a mass concentration of 500 mg / L is added, the aqueous phase viscosity of the composite system, the adsorption amount of the dispersant on the particle surface and the stability performance can be further enhanced. At a simulated permeability of 4500 mD, the plugging rate reaches 82.3%, and the residual resistance coefficient reaches 7.1, achieving the effect of effectively plugging the preferential permeability channel.
[0073] Polycarboxylic acid stabilizer
[0074] Polycarboxylic acid stabilizers inhibit the formation of calcium carbonate and calcium silicate scale through electrostatic repulsion and steric hindrance, affecting the dispersion performance of particles, so that the added calcium ions are not affected by bicarbonate in the water, thereby enhancing the dispersion stability of the precipitated particles.
[0075] Preferably, the polycarboxylic acid stabilizer is prepared by the following method:
[0076] (1) dissolving the substituted polyether compound and the thiol compound in water according to a ratio to prepare a solution A;
[0077] (2) dissolving acrylic acid and methacryloyloxyethyl trimethyl ammonium chloride in water according to a ratio to prepare solution B;
[0078] (3) dissolving ammonium persulfate in water according to the ratio to prepare solution C;
[0079] (4) under nitrogen protection, adding the solution B and the solution C to the solution A in a dropwise manner to obtain a mixed system, and heat-insulating and aging;
[0080] (5) After the reaction is completed, the mixture is cooled to room temperature, and then a base is added to adjust the pH to 6-8 to obtain a polycarboxylic acid stabilizer.
[0081] Preferably, the substituted polyether compound is at least one of methyl allyl polyethylene glycol ether, isopentenyl polyoxyethylene ether, ethylene glycol monovinyl polyoxyethylene ether, and 4-hydroxybutyl vinyl polyoxyethylene ether.
[0082] Wherein, the thiol compound is a molecular weight modifier, preferably at least one of thioglycolic acid, mercaptopropionic acid, mercaptoethanol and mercaptopropanol.
[0083] Preferably, in step (1), the weight ratio of the substituted polyether compound, the thiol compound and the water is (35.5-44.6): (0.28-0.32): (48-50).
[0084] In step (2), the weight ratio of the acrylic acid, the methacryloyloxyethyltrimethylammonium chloride and the water is (3.20-5.15):(8.2-14.5):(23.5-26).
[0085] In step (3), the weight ratio of the ammonium persulfate to the water is (1.00-1.15): (19-20.5). The weight ratio of the ammonium persulfate to the substituted polyether compound, the thiol compound, the acrylic acid, and the methacryloyloxyethyl trimethyl ammonium chloride is (1.00-1.15): (35.5-44.6): (0.28-0.32) (3.20-5.15): (8.2-14.5).
[0086] The acid-ether ratio or acid-ether molar ratio (A / E) of acrylic acid to substituted polyether compound is in the range of 3.0 to 4.2. Meanwhile, the molecular weight of the synthesized polycarboxylic acid stabilizer is in the range of 20,000 to 29,000.
[0087] Preferably, the reaction temperature is 60-70° C., and the reaction time is 4-8 hours.
[0088] Properly increasing the acid-ether ratio or molecular weight in the polycarboxylic acid stabilizer can accelerate the adsorption performance of the dispersant on the surface of the precipitated particles, but too high an acid-ether ratio or molecular weight has an adverse effect on the dispersibility of the dispersant in the inorganic particle system. When the acid-ether ratio (A / E) of the polycarboxylic acid stabilizer is 3.0-4.2 and the molecular weight is 20,000-29,000, the electrostatic repulsion and steric hindrance between the polycarboxylic acid stabilizer and the surface of the inorganic particles are taken into account, and the system can achieve a better dispersion stabilization effect.
[0089] Further preferably, the molecular weight of the polycarboxylic acid stabilizer is 23800, and the A / E ratio of the acrylic acid to the substituted polyether compound is 3.6.
[0090] The molecular structure of the polycarboxylic acid stabilizer affects the dispersibility of the polycarboxylic acid stabilizer. The present invention selects a polycarboxylic acid stabilizer with a suitable acid-ether ratio and molecular weight, so that when an inorganic composite displacement agent is injected into a reservoir containing bicarbonate, the stabilizer does not precipitate during injection, but can achieve effective dispersion, migrate to the deep part of the formation, and then gradually precipitate and aggregate, thereby blocking the high-permeability pores.
[0091] In a second aspect, the present invention further provides a method for preparing an inorganic composite control and displacement agent, comprising:
[0092] (1) dissolving a polycarboxylic acid stabilizer and sodium silicate in water according to a ratio to obtain a main agent mother solution;
[0093] (2) dissolving calcium chloride in water according to a ratio to obtain an additive mother solution;
[0094] (3) mixing the main agent mother solution and the auxiliary agent mother solution;
[0095] (4) adding an emulsion polymer to the mixed solution in step (3) to obtain the inorganic composite displacement agent.
[0096] The ratios of the polycarboxylic acid stabilizer, sodium silicate, calcium chloride and other raw materials can be made according to the ratios specified in the inorganic composite displacement agent provided in the first aspect of the present invention. The present invention will not be described repeatedly here.
[0097] In a preferred embodiment, the preparation method of the inorganic composite displacement agent of the present invention comprises:
[0098] (1) Preparation of main agent mother liquor: Take a certain amount of simulated formation water, add 15% mass concentration of dispersant, and add 5% mass concentration of sodium silicate powder at a stirring speed of 300 r / min until it is completely dissolved; (2) Preparation of auxiliary agent mother liquor: Take deionized water at room temperature and prepare 15% mass concentration of calcium chloride solution; (3) Preparation of inorganic composite displacement agent: Weigh the main agent mother liquor and auxiliary agent mother liquor in a specified proportion at room temperature, mix them, add emulsion polyacrylamide after mixing evenly, and place them in a colorimetric tube.
[0099] The preparation of common gel-type control agents in the prior art requires a temperature of more than 40°C, while the control agent of the present invention can be obtained at room temperature. Compared with the prior art, the preparation conditions of the control agent of the present invention are milder. In addition, the commonly used pre-crosslinked particle control agents require bulk polymerization to form, and polymer microspheres need to be prepared by emulsion polymerization, while the control agent of the present invention only needs stirring and mixing to achieve rapid dispersion. Not only is the production simple, but it can also be injected online with water injection without the need for dissolving or maturation equipment.
[0100] The previous water glass-calcium chloride inorganic adjustment and displacement system has the problem of rapid reaction precipitation after contact, and the addition of precipitation inhibitors (PBTC, ATMP and HEDP, etc.) can effectively control the generation time of calcium silicate precipitation and the initial particle size of particles, and is applied in offshore high-temperature and high-salt oil fields, and achieves a higher oil-increasing and water-reducing effect. However, for the low content of divalent ions in the injected water, calcium chloride needs to be added, and under the condition that the water contains a certain amount of bicarbonate ions, the added calcium chloride will quickly form calcium carbonate precipitation with the sodium bicarbonate in the injected water. The adjustment and displacement agent of the present invention can ensure that the adjustment and displacement agent is quickly dispersed and not precipitated when injected for the adjustment and displacement of the reservoir with a low content of divalent ions in the injected water and a certain amount of bicarbonate ions in the water, and it is not easy to form a calcium carbonate scale coating in the water injection line, block the water injection line, and migrate to the deep part of the formation to precipitate and aggregate to block the large pores. Therefore, the present invention has a good application prospect in the reservoir with a low content of divalent ions in the injected water and a certain amount of bicarbonate ions in the water and the offshore oil field with limited platform space.
[0101] Example
[0102] The present invention is further described below by way of examples, but the present invention is not limited to the scope of the examples. The experimental methods in the following examples where specific conditions are not specified are carried out according to conventional methods and conditions. The raw materials used in the following examples are all obtained from conventional commercial sources. The sources of the raw materials used in the following examples are shown in Table 1, and the simulated water components used are shown in Table 2.
[0103] Table 1 Summary of raw material sources
[0104]
[0105]
[0106] Table 2 Composition of simulated water used in the experiment (mg / L)
[0107]
[0108] Example 1
[0109] Synthesis of polycarboxylic acid stabilizer: First, weigh 44.52g of methyl allyl polyethylene glycol ether (HPEG) and 0.30g of thioglycolic acid (TGA) and dissolve them in 50g of deionized water to make solution A. Weigh 3.20g of acrylic acid (AA) and 11.82g of methacryloyloxyethyl trimethyl ammonium chloride (DMC) and dissolve them in 25g of deionized water to make solution B. Weigh 1.07g of ammonium persulfate (APS) and dissolve it in 19.6g of deionized water to make solution C for use. Then add solution A to a four-necked flask, stir and pass nitrogen for 20min, and then heat to 65°C. Add solutions B and C dropwise for 3.5h and 3.5h respectively, and then keep warm and age for 0.5h before the reaction is terminated. After cooling to room temperature, add 5g of sodium hydroxide aqueous solution (sodium hydroxide mass fraction 40%), adjust the pH to 6-8, and obtain a light yellow slightly viscous solution.
[0110] The relative molecular mass of HPEG is 3000, the relative molecular mass of AA is 72, and the acid-ether ratio (n(AA):n(HPEG)) of Example 1 is 3.0. The molecular weight of the prepared polycarboxylic acid stabilizer is 22560.
[0111] The polycarboxylic acid stabilizer formed in Example 1 was tested for initial particle size and stability performance.
[0112] First, prepare the main agent mother liquor: use deionized water to prepare a 15% mass concentration of polycarboxylic acid stabilizer solution, and then add sodium silicate powder at a stirring speed of 300r / min until it is completely dissolved. The mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother liquor: take deionized water at room temperature and prepare a 15% mass concentration of calcium chloride solution. Then, prepare the inorganic composite adjustment and displacement agent: the total solution mass at room temperature is 25g, among which, first weigh 24.304g of simulated water sample, first add 0.5g of main agent mother liquor (the effective concentration of sodium silicate in the total solution is 0.1%), and then slowly add 0.17g of auxiliary agent mother liquor (the effective concentration of calcium chloride in the total solution is 0.1%), mix well, and slowly add 0.026g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.03%) at a speed of 200r / min. The total mass of the entire solution is 25g. Within 30 minutes of placing the colorimetric tube, the initial particle size of the system was measured using a Malvern laser particle size analyzer at a stirring rate of 3000 r / min. After stirring for 10 minutes, the median particle size results of the initial two tests were 8.126 μm and 8.328 μm, respectively (see Figure 1 and Figure 2 ).
[0113] Place the colorimetric tube in a 65°C oven and take it out every hour to observe the precipitate morphology. Figure 3 To prepare the initial photos, Figure 4 Photographs were taken after heating for 48 hours. Figure 5This is a photo taken after heating for 60 hours. White insoluble matter can be seen, indicating that the system is unstable.
[0114] It was observed that the stabilization time was 55 hours, which could meet the requirement of no precipitation for at least 48 hours under simulated reservoir temperature conditions.
[0115] Example 2
[0116] Synthesis of polycarboxylic acid stabilizer: First, weigh 42.04g of methyl allyl polyethylene glycol ether (HPEG) (molecular weight 3000) and 0.32g of thioglycolic acid (TGA) and dissolve them in 49g of deionized water to make solution A. Weigh 3.63g of acrylic acid and 11.94g of methacryloyloxyethyl trimethyl ammonium chloride (DMC) and dissolve them in 24g of deionized water to make solution B. Weigh 1.12g of ammonium persulfate (APS) and dissolve it in 19.5g of deionized water to make solution C for use. Then add solution A to a four-necked flask, stir and pass nitrogen for 20min, and heat to 65°C. Add solutions B and C dropwise for 3h and 3.5h, respectively, and then keep warm and age for 0.5h before the reaction is terminated. After cooling to room temperature, add 5g of sodium hydroxide aqueous solution (sodium hydroxide mass fraction 40%), adjust the pH to 6-8, and obtain a light yellow slightly viscous solution.
[0117] The relative molecular weight of HPEG is 3000, the relative molecular weight of AA is 72, and the acid-ether ratio (n(AA):n(HPEG)) of Example 2 is 3.6. The molecular weight of the prepared polycarboxylic acid stabilizer is 24120.
[0118] The polycarboxylic acid stabilizer formed in Example 2 was tested for initial particle size and stability performance.
[0119] First, prepare the main agent mother solution: use deionized water to prepare a 15% mass concentration of polycarboxylic acid stabilizer solution, and then add sodium silicate powder at a stirring speed of 300r / min until it is completely dissolved, and the mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother solution: take deionized water at room temperature and prepare a 15% mass concentration of calcium chloride solution; then prepare the inorganic composite adjustment agent: the total solution mass at room temperature is 25g, wherein, first weigh 24.627g of simulated water sample, first add 0.25g of main agent mother solution (the effective concentration of sodium silicate in the total solution is 0.05%), and then slowly add 0.08g of auxiliary agent mother solution (the total solution contains 0.05% effective concentration of calcium chloride), after mixing evenly, slowly add 0.043g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.05%) at a speed of 200r / min. The total mass of the whole solution is 25g. Within 30 minutes of placing the colorimetric tube, the initial particle size of the system was measured using a Malvern laser particle size analyzer at a stirring rate of 3000 r / min. After stirring for 10 minutes, the median particle size results of the initial two tests were 6.431 μm and 6.672 μm, respectively (see Figure 6 and Figure 7 ).
[0120] The colorimetric tube was placed in a 65°C oven and taken out every hour to observe the morphology of the precipitation. Figure 8 This is a photo of the system after heating for 96 hours. The system is relatively stable without precipitation. According to experiments, the stability time of the system is 106 hours, which can meet the requirement of no precipitation for at least 48 hours under the simulated reservoir temperature conditions, and can maintain no precipitation for 4 days, ensuring that the system can be transported to the deep formation and achieve the effect of deep displacement.
[0121] The plugging performance of Example 2 was evaluated, and the evaluation method and results were as follows:
[0122] The deep profile control performance of the profile control agent of Example 2 was further tested using a long sand-filled pipe model with multiple pressure measurement points. The specific steps are as follows:
[0123] (1) The sand-filled tube is filled with sand and saturated with simulated water, and the pore volume and porosity are calculated;
[0124] (2) Inject simulated water at a constant flow rate (0.25 mL / min), record the pressure difference ΔP between the inlet and outlet, and calculate the permeability of the sand-filled tube, which is 4200 mD;
[0125] (3) Inject 0.25 PV of the solution in Example 2 and record the pressure at the inlet, outlet and three pressure measuring points;
[0126] (4) After injection of the profile control system, the sand filling tube was left to stand at 65°C for 12 h;
[0127] (5) 65℃ water drive at a constant flow rate (0.25mL / min), record the pressure at the inlet, outlet and three pressure measuring points, and calculate the permeability and plugging rate. Fig. 9 shown.
[0128] Depend on Fig. 9 It can be seen that the sediment has the ability to conduct and migrate in porous media. During the water flooding and injection of adjustment and displacement agents, the pressure change trends at the inlet and the three pressure measuring points are basically the same, and the pressure difference in each section is equal. After standing for 12 hours, in the subsequent water flooding stage, the pressures at the inlet and each pressure measuring point were 0.35MPa, 0.31MPa, 0.22MPa, and 0.12MPa, respectively, and the pressure differences in each section were 0.04MPa, 0.09MPa, 0.1MPa, and 0.12MPa, respectively, indicating that the sediment is gradually enriched from the first section to the fourth section. Therefore, the sediment can gradually migrate to the deep part of the reservoir, with good deep adjustment and displacement performance and plugging performance, and the plugging rate reaches 87%.
[0129] Example 3
[0130] Synthesis of polycarboxylic acid stabilizer: First, weigh 40.55g of methyl allyl polyethylene glycol ether (HPEG) and 0.30g of thioglycolic acid (TGA) and dissolve them in 50g of deionized water to make solution A. Weigh 5.11g of acrylic acid and 14.14g of methacryloyloxyethyl trimethyl ammonium chloride (DMC) and dissolve them in 26g of deionized water to make solution B. Weigh 1.03g of ammonium persulfate (APS) and dissolve it in 20g of deionized water to make solution C for use. Then add solution A to a four-necked flask, stir and pass nitrogen for 20min, and heat to 65°C. Add solutions B and C dropwise for 3h and 3.5h, respectively, and then keep warm and age for 0.5h before the reaction is terminated. After cooling to room temperature, add 5g of sodium hydroxide aqueous solution (sodium hydroxide mass fraction 40%), adjust the pH to 6-8, and obtain a light yellow slightly viscous solution.
[0131] The relative molecular weight of HPEG is 2400, the relative molecular weight of AA is 72, and the acid-ether ratio (n(AA):n(HPEG)) of Example 3 is 4.2. The molecular weight of the prepared polycarboxylic acid stabilizer is 23430.
[0132] The polycarboxylic acid stabilizer formed in Example 3 was tested for initial particle size and stability performance.
[0133] First, prepare the main agent mother liquor: use deionized water to prepare a 15% mass concentration of polycarboxylic acid stabilizer solution, and then add sodium silicate powder at a stirring speed of 300r / min until it is completely dissolved. The mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother liquor: take deionized water at room temperature and prepare a 15% mass concentration of calcium chloride solution. Then prepare the inorganic composite adjustment and displacement agent: the total solution mass at room temperature is 25g, among which, first weigh 24.287g of simulated water sample, first add 0.5g of main agent mother liquor (the total solution contains 0.1% effective concentration of sodium silicate), and then slowly add 0.17g of auxiliary agent mother liquor (the total solution contains 0.1% effective concentration of calcium chloride), after mixing evenly, slowly add 0.043g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.05%) at a speed of 200r / min, and the total mass of the whole solution is 25g. Within 30 minutes of placing the colorimetric tube, the initial particle size of the system was measured using a Malvern laser particle size analyzer at a stirring rate of 3000 r / min. After stirring for 10 minutes, the median particle size results of the initial two tests were 10.37 μm and 10.93 μm, respectively (see Fig.10 and Fig.11 ).
[0134] The colorimetric tube was placed in a 65°C oven and taken out every hour to observe the morphology of the precipitation. Figures 12 to 15 The photos of the system of Example 3 at the initial stage of heating at 65°C and after heating for 48h, 56h and 72h are shown. It can be seen from the observation that the system of Example 3 has a stable time of 48 hours, which can meet the requirement of no precipitation for at least 48 hours under the simulated reservoir temperature conditions. When heated for 56h, white insoluble matter can be seen, indicating that the system begins to be unstable.
[0135] Example 4
[0136] Synthesis of polycarboxylic acid stabilizer: First, weigh 44.43g of methyl allyl polyethylene glycol ether (HPEG) and 0.30g of thioglycolic acid (TGA) and dissolve them in 48g of deionized water to make solution A. Weigh 3.65g of acrylic acid and 10.50g of methacryloyloxyethyl trimethyl ammonium chloride (DMC) and dissolve them in 23.5g of deionized water to make solution B. Weigh 1.07g of ammonium persulfate (APS) and dissolve it in 20g of deionized water to make solution C for use. Then add solution A to a four-necked flask, stir and pass nitrogen for 20min, and heat to 65°C. Add solutions B and C dropwise for 3h and 3.5h, respectively, and then keep warm and age for 0.5h before the reaction is terminated. After cooling to room temperature, add 4.5g of sodium hydroxide aqueous solution (sodium hydroxide mass fraction 40%), adjust the pH to 6-8, and obtain a light yellow slightly viscous solution.
[0137] The relative molecular mass of HPEG is 3000, the relative molecular mass of AA is 72, and the acid-ether ratio (n(AA):n(HPEG)) of Example 4 is 3.4. The molecular weight of the prepared polycarboxylic acid stabilizer is 28200.
[0138] The polycarboxylic acid stabilizer formed in Example 4 was tested for initial particle size and stability performance.
[0139] First, prepare the main agent mother solution: use deionized water to prepare a 15% mass concentration of polycarboxylic acid stabilizer solution, and then add sodium silicate powder at a stirring speed of 300r / min until it is completely dissolved, and the mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother solution: take deionized water at room temperature and prepare a 15% mass concentration of calcium chloride solution; then prepare the inorganic composite adjustment and displacement agent: the total solution mass at room temperature is 25g, wherein, first weigh 24.287g of simulated water sample, first add 0.5g of main agent mother solution (the total solution contains 0.1% effective concentration of sodium silicate), and then slowly add 0.17g of auxiliary agent mother solution (the total solution contains 0.1% effective concentration of calcium chloride), after mixing evenly, slowly add 0.043g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.05%) at a speed of 200r / min, and the total mass of the whole solution is 25g. Within 30 minutes of placing the colorimetric tube, the initial particle size of the system was tested using a Malvern laser particle size analyzer with a stirring rate of 3000r / min for 10 minutes. The median particle size results of the initial two tests were 34.20μm and 33.83μm respectively. The particle size test results of the first test within 2 hours of heating are shown in Fig.16 The initial system can be free of precipitation (see Fig.17 ), no insoluble matter appeared after heating for two hours, and the mixture could maintain stability (see Table 2).
[0140] After heating for 48 hours, the system was stable and no insoluble matter appeared (see Fig.18 After heating for 72 hours, insoluble matter appeared in the system and precipitation began. When the liquid was introduced into a beaker, flocculent precipitates were observed (see Fig.19 ).
[0141] Table 2 Results of Example 4 from the initial stage of heating to 2 hours later
[0142]
[0143] Example 5
[0144] Synthesis of polycarboxylic acid stabilizer: First, weigh 35.58g of isopentenyl polyoxyethylene ether and 0.28g of thioglycolic acid (TGA) and dissolve them in 50g of deionized water to make solution A. Weigh 3.45g of acrylic acid and 8.27g of methacryloyloxyethyl trimethylammonium chloride (DMC) and dissolve them in 26g of deionized water to make solution B. Weigh 1.05g of ammonium persulfate (APS) and dissolve it in 19.4g of deionized water to make solution C for use. Then add solution A to a four-necked flask, introduce nitrogen for 20min under stirring, and heat to 65°C. Add solutions B and C dropwise for 3h and 3.5h, respectively, and then heat and age for 0.5h before the reaction is terminated. After cooling to room temperature, add 5.3g of sodium hydroxide aqueous solution (sodium hydroxide mass fraction 40%), adjust the pH to 6-8, and obtain a light yellow slightly viscous solution.
[0145] The relative molecular weight of isopentenyl polyoxyethylene ether is 2400, the relative molecular weight of AA is 72, and the acid-ether ratio (n(AA):n(TPEG)) of Example 7 is 3.2. The molecular weight of the prepared polycarboxylic acid stabilizer is 21400.
[0146] The polycarboxylic acid stabilizer formed in Example 5 was tested for initial particle size and stability performance.
[0147] First, prepare the main agent mother solution: use deionized water to prepare a 15% mass concentration of polycarboxylic acid stabilizer solution, and then add sodium silicate powder at a stirring speed of 300r / min until it is completely dissolved. The mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother solution: take deionized water at room temperature and prepare a 15% mass concentration of calcium chloride solution. Then prepare the inorganic composite displacement agent: the total solution mass at room temperature is 25g, wherein, first weigh 24.287g of simulated water sample, first add 0.5g of main agent mother solution (the total solution contains 0.1% sodium silicate effective concentration), then slowly drop 0.17g of auxiliary agent mother solution (the total solution contains 0.1% calcium chloride effective concentration), after mixing evenly, slowly drop 0.043g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.05%) at a speed of 200r / min, and place it in a colorimetric tube. The total mass of the whole solution is 25g, and its initial morphology is shown in FIG. Fig. 20 The laser particle analyzer was used to test twice, and the initial particle size of the test system was 22.43μm and 22.26μm.
[0148] Table 3 Particle size changes at different times in Example 5 system
[0149]
[0150] like Fig.21The results shown in Table 3 show that the median particle size at the initial stage of preparation is 22.43 μm. As the heating time increases, the particle size of the system continues to increase. After heating for 2 hours, the particle size reaches 46.3 μm, but the aggregation of the precipitated particles is weakened. After heating for 48 hours, the median particle size is 53.2 μm, and the system remains stable. When heated for 54 hours, some particles form precipitation.
[0151] Comparative Example 1
[0152] First, weigh 38.68g of methyl allyl polyethylene glycol ether (HPEG) and 0.30g of thioglycolic acid (TGA) and dissolve them in 50g of deionized water to make solution A. Weigh 5.22g of acrylic acid and 13.56g of methacryloyloxyethyl trimethyl ammonium chloride (DMC) and dissolve them in 25g of deionized water to make solution B. Weigh 1.05g of ammonium persulfate (APS) and dissolve it in 20.2g of deionized water to make solution C for use. Then add solution A to a four-necked flask, introduce nitrogen for 20min under stirring, and heat to 65°C. Add solutions B and C dropwise for 3.5h and 4h, respectively, and then heat and age for 0.5h before the reaction is terminated. After cooling to room temperature, add 5g of sodium hydroxide aqueous solution (sodium hydroxide mass fraction 40%), adjust the pH to 6-8, and obtain a light yellow slightly viscous solution.
[0153] The relative molecular weight of HPEG is 2400, the relative molecular weight of AA is 72, and the acid-ether ratio (n(AA):n(HPEG)) of Comparative Example 1 is 4.5. The molecular weight of the prepared polycarboxylic acid stabilizer is 24580.
[0154] The polycarboxylic acid stabilizer formed in Comparative Example 1 was tested for initial particle size and stability performance.
[0155] First, prepare the main agent mother solution: use deionized water to prepare a 15% mass concentration of polycarboxylic acid stabilizer solution, and then add sodium silicate powder at a stirring speed of 300r / min until it is completely dissolved, and the mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother solution: take deionized water at room temperature and prepare a 15% mass concentration of calcium chloride solution; then prepare the inorganic composite adjustment and displacement agent: the total solution mass at room temperature is 25g, wherein, first weigh 24.287g of simulated water sample, first add 0.5g of main agent mother solution (the total solution contains 0.1% effective concentration of sodium silicate), and then slowly add 0.17g of auxiliary agent mother solution (the total solution contains 0.1% effective concentration of calcium chloride), after mixing evenly, slowly add 0.043g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.05%) at a speed of 200r / min, and the total mass of the whole solution is 25g. Within 30 minutes of placing the colorimetric tube, the initial particle size of the system was measured using a Malvern laser particle size analyzer at a stirring rate of 3000 r / min. After stirring for 10 minutes, the median particle size results of the initial two tests were 19.46 μm and 20.27 μm, respectively (see Fig. 22 and Fig.23 ).
[0156] Place the colorimetric tube in a 65°C oven and take it out every hour to observe the precipitate morphology. After heating for 16 hours, a precipitate ( Fig.24 ), indicating that the system is beginning to become unstable and cannot remain stable after heating for 48 hours, and thus cannot be transported to the deep formation for plugging.
[0157] Comparative Example 2
[0158] First, weigh 34.37g of isopentanol polyoxyethylene ether (TPEG) and 0.30g of thioglycolic acid (TGA) and dissolve them in 50g of deionized water to make solution A. Weigh 3.48g of acrylic acid and 14.12g of methacryloyloxyethyl trimethylammonium chloride (DMC) and dissolve them in 25g of deionized water to make solution B. Weigh 1.07g of ammonium persulfate (APS) and dissolve it in 20.3g of deionized water to make solution C for use. Then add solution A to a four-necked flask, introduce nitrogen for 20min under stirring, and heat to 65°C. Add solutions B and C dropwise for 3.5h and 4h, respectively, and then heat and age for 0.5h before the reaction is terminated. After cooling to room temperature, add 4.5g of sodium hydroxide aqueous solution (sodium hydroxide mass fraction 40%), adjust the pH to 6-8, and obtain a light yellow slightly viscous solution.
[0159] The relative molecular weight of prenol polyoxyethylene ether (TPEG) is 2400, the relative molecular weight of AA is 72, and the acid-ether ratio (n(AA):n(TPEG)) of Comparative Example 1 is 3.4. The molecular weight of the prepared polycarboxylic acid stabilizer is 17120.
[0160] The polycarboxylic acid stabilizer formed in Comparative Example 2 was tested for initial particle size and stability performance.
[0161] First, prepare the main agent mother solution: use deionized water to prepare a 15% mass concentration of polycarboxylic acid stabilizer solution, and then add sodium silicate powder at a stirring speed of 300r / min until it is completely dissolved. The mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother solution: take deionized water at room temperature and prepare a calcium chloride solution with a mass concentration of 15%; then prepare the inorganic composite displacement agent: the total solution mass at room temperature is 25g, wherein, first weigh 24.287g of simulated water sample, first add 0.5g of main agent mother solution (the total solution contains 0.1% effective concentration of sodium silicate), and then slowly drop 0.17g of auxiliary agent mother solution (the total solution contains 0.1% effective concentration of calcium chloride), after mixing evenly, slowly drop 0.043g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.05%) at a speed of 200r / min, the total mass of the whole solution is 25g, after mixing evenly, put it in a colorimetric tube, and you can see that insoluble floccules appear (see Fig.25 ).
[0162] Comparative Example 3
[0163] First, weigh 44.01g of methyl allyl polyethylene glycol ether (HPEG) and 0.33g of thioglycolic acid (TGA) and dissolve them in 50g of deionized water to make solution A. Weigh 4.62g of acrylic acid and 8.78g of methacryloyloxyethyl trimethyl ammonium chloride (DMC) and dissolve them in 25.5g of deionized water to make solution B. Weigh 1.07g of ammonium persulfate (APS) and dissolve it in 20g of deionized water to make solution C for use. Then add solution A to a four-necked flask, introduce nitrogen for 20min under stirring, and heat to 65°C. Add solutions B and C dropwise for 3h and 3.5h, respectively, and then heat and age for 0.5h before the reaction is terminated. After cooling to room temperature, add 4.5g of sodium hydroxide aqueous solution (sodium hydroxide mass fraction 40%), adjust the pH to 6-8, and obtain a light yellow slightly viscous solution.
[0164] The relative molecular mass of HPEG is 3000, the relative molecular mass of AA is 72, and the acid-ether ratio (n(AA):n(HPEG)) of Example 7 is 4.4. The molecular weight of the prepared polycarboxylic acid stabilizer is 34600.
[0165] The polycarboxylic acid stabilizer formed in Comparative Example 3 was tested for initial particle size and stability performance.
[0166] First, prepare the main agent mother solution: use deionized water to prepare a 15% mass concentration of polycarboxylic acid stabilizer solution, and then add sodium silicate powder at a stirring speed of 300r / min until it is completely dissolved. The mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother solution: take deionized water at room temperature and prepare a calcium chloride solution with a mass concentration of 15%; then prepare the inorganic composite displacement agent: the total solution mass at room temperature is 25g, wherein, first weigh 24.287g of simulated water sample, first add 0.5g of main agent mother solution (the total solution contains 0.1% effective concentration of sodium silicate), and then slowly drop 0.17g of auxiliary agent mother solution (the total solution contains 0.1% effective concentration of calcium chloride), after mixing evenly, slowly drop 0.043g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.05%) at a speed of 200r / min, the total mass of the whole solution is 25g, after mixing evenly, put it in a colorimetric tube, and you can see that insoluble floccules appear (see Fig.26 ).
[0167] The present invention has been disclosed above with preferred embodiments, but those skilled in the art should understand that these embodiments are only used to describe the present invention and should not be understood as limiting the scope of the present invention. It should be noted that all changes and substitutions equivalent to these embodiments should be deemed to be included in the scope of the claims of the present invention. Therefore, the scope of protection of the present invention should be based on the scope defined in the claims.
[0168] Comparative Example 4
[0169] Using PBTC as a dispersing stabilizer, first, prepare the main agent mother solution: use deionized water, at a stirring speed of 300r / min, add sodium silicate powder until it is completely dissolved, and the mass concentration of sodium silicate is 5%. Then prepare the auxiliary agent mother solution: take deionized water at room temperature and prepare a 15% mass concentration calcium chloride solution. Then prepare the inorganic composite displacement agent: the total solution mass at room temperature is 25g, of which 24.137g of simulated water sample is weighed, 0.15g of PBTC is added first (equivalent to 0.3% of the effective ingredient of PBTC in the total solution), and after stirring and dissolving fully, 0.5g of the main agent mother solution is added (the total solution contains 0.1% of the effective concentration of sodium silicate), and then 0.17g of the auxiliary agent mother solution is slowly added thereto (the total solution contains 0.1% of the effective concentration of calcium chloride), and after mixing evenly, 0.043g of 29% emulsion polyacrylamide solution (the concentration of emulsion polyacrylamide in the total solution is 0.05%) is slowly added at a speed of 200r / min. The total mass of the entire solution is 25g. After mixing evenly, it is placed in a colorimetric tube, and insoluble matter can be seen after 4 hours (see Fig. 27 ).
[0170] The present invention has been disclosed above with preferred embodiments, but those skilled in the art should understand that these embodiments are only used to describe the present invention and should not be understood as limiting the scope of the present invention. It should be noted that all changes and substitutions equivalent to these embodiments should be deemed to be included in the scope of the claims of the present invention. Therefore, the scope of protection of the present invention should be based on the scope defined in the claims.
Claims
1. An inorganic composite flooding agent, It is characterized in that include: Emulsion polymer, calcium chloride, polycarboxylic acid stabilizer, sodium silicate and water.
2. The inorganic composite displacement agent according to claim 1, It is characterized in that Calculated by weight percentage, the invention comprises: 0.03% to 0.05% of emulsion polymer, 0.05% to 0.2% of calcium chloride, 0.15% to 0.6% of polycarboxylic acid stabilizer, 0.05% to 0.2% of sodium silicate and the balance of water.
3. The inorganic composite displacement agent according to claim 2, It is characterized in that Calculated by weight percentage, the invention comprises: 0.03% to 0.05% of emulsion polymer, 0.10% to 0.15% of calcium chloride, 0.25% to 0.35% of polycarboxylic acid stabilizer, 0.10% to 0.15% of sodium silicate and the balance of water.
4. The inorganic composite displacement agent according to claim 1, It is characterized in that The emulsion polymer is an emulsion type polyacrylamide with a hydrolysis degree of 3% to 18% and a molecular weight of 3 million to 8 million.
5. The inorganic composite displacement agent according to claim 1, It is characterized in that The polycarboxylic acid stabilizer is prepared by the following method: (1) dissolving the substituted polyether compound and the thiol compound in water according to a ratio to prepare a solution A; (2) dissolving acrylic acid and methacryloyloxyethyl trimethyl ammonium chloride in water according to a ratio to prepare solution B; (3) dissolving ammonium persulfate in water according to the ratio to prepare solution C; (4) under nitrogen protection, adding the solution B and the solution C to the solution A in a dropwise manner to obtain a mixed system, and heat-insulating and aging; (5) After the reaction is completed, the mixture is cooled to room temperature, and then a base is added to adjust the pH to 6-8 to obtain a polycarboxylic acid stabilizer.
6. The inorganic composite displacement agent according to claim 5, It is characterized in that The substituted polyether compound is at least one of methyl allyl polyethylene glycol ether, isopentenyl polyoxyethylene ether, ethylene glycol monovinyl polyoxyethylene ether, and 4-hydroxybutyl vinyl polyoxyethylene ether; the thiol compound is at least one of thioglycolic acid, mercaptopropionic acid, mercaptoethanol, and mercaptopropanol.
7. The inorganic composite displacement agent according to claim 5, It is characterized in that The reaction temperature is 60° C. to 70° C., and the reaction time is 4 h to 8 h.
8. The inorganic composite displacement agent according to claim 5, It is characterized in that The weight ratio of the substituted polyether compound, the thiol compound and the water is (35.5-44.6):(0.28-0.32):(48-50); the weight ratio of the acrylic acid, the methacryloyloxyethyltrimethylammonium chloride and the water is (3.20-5.15):(8.2-14.5):(23.5-26); the weight ratio of the ammonium persulfate and the water is (1.00-1.15):(19-20.5).
9. The inorganic composite displacement agent according to claim 5, It is characterized in that The molar ratio of the acrylic acid to the substituted polyether compound is 3.0 to 4.2; the molecular weight of the polycarboxylic acid stabilizer is 20,000 to 29,000. 。 10. The method for preparing the inorganic composite displacement agent according to any one of claims 1 to 9, It is characterized in that include: (1) dissolving a polycarboxylic acid stabilizer and sodium silicate in water according to a ratio to obtain a main agent mother solution; (2) dissolving calcium chloride in water according to a ratio to obtain an additive mother solution; (3) mixing the main agent mother solution and the auxiliary agent mother solution; (4) adding an emulsion polymer to the mixed solution in step (3) to obtain the inorganic composite displacement agent.
11. Use of the inorganic composite control and displacement agent according to any one of claims 1 to 9 or the inorganic composite control and displacement agent obtained by the preparation method according to claim 10 in offshore high water content oil fields.