Graphical processing method for resistive sensor and resistive sensor
Through magnetron sputtering and ultraviolet lithography, conductive metal layer is formed on the alumina substrate, and temporary substrates and UV adhesives are used to solve the peeling difficulties caused by the sputtering process, achieving high-quality patterning , improves product reliability and preparation efficiency.
Patent Information
- Application Number
- CN202311786698.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-22
- Publication Date
- 2024-12-03
AI Technical Summary
In the prior art, the film formation process mainly adopts a sputtering process, which leads to photoresist cross-sectional coating, which leads to difficulty in peeling, severely leads to failure to achieve peeling, and the electrode edges are not smooth, affecting the patterning treatment effect.
Magneto-controlled sputtering technology is used to form a conductive metal layer on the surface of the alumina substrate. Combined with ultraviolet lithography and IBE etching technology, the patterning of the conductive metal layer is achieved through the use of temporary substrates and UV adhesives to avoid peeling Difficult and improves graphical effects.
A patterned structure with low roughness, high depth and aspect ratio and high reliability is realized, reducing the difficulty of peeling the photoresist, and improving product yield and preparation efficiency.
Smart Images

Figure CN119061366A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of resistive sensors, and in particular to a graphical processing method for resistive sensors and the resistive sensors. Background Art
[0002] Traditional resistive sensors use a stripping process, firstly exposing the photoresist coated on the substrate in a pattern, then developing and removing the exposed photoresist, then performing a film forming process, and finally stripping off the remaining photoresist and the film formed on the photoresist together, leaving the required film pattern on the substrate.
[0003] In the prior art, during the preparation process, the film formation process mainly adopts the sputtering process. The sputtering coating will cover the entire photoresist cross section. Mild cases will make it difficult to peel off, or the edge of the formed electrode will be rough and have burrs. Severe cases will make it impossible to peel off. Summary of the invention
[0004] In view of the deficiencies in the prior art, the purpose of the present invention is to provide a graphical processing method for a resistive sensor and a resistive sensor, aiming to solve the technical problem in the prior art that, during the preparation process, the film forming process mainly adopts a sputtering process, and the sputtering coating will cover the entire photoresist cross section, which will cause mild difficulties in peeling, or the formed electrode edge will be rough and have burrs, and severe problems will make it impossible to peel off.
[0005] In order to achieve the above object, the present invention is implemented by the following technical solution: a graphical processing method for a resistive sensor, comprising the following steps:
[0006] Providing an aluminum oxide substrate, and performing film forming treatment on the surface of the aluminum oxide substrate based on magnetron sputtering technology to form a conductive metal layer on the surface of the aluminum oxide substrate;
[0007] Coating a photoresist on the aluminum oxide substrate after the film forming process to form a first photoresist layer;
[0008] Selectively irradiating the first photoresist layer based on ultraviolet photolithography technology, and dissolving part of the first photoresist layer by a developer to expose part of the conductive metal layer, thereby obtaining a first target pattern corresponding to the first photoresist layer;
[0009] Etching the aluminum oxide substrate after the development process to remove a portion of the conductive metal layer;
[0010] The etched aluminum oxide substrate is cleaned to complete the patterning process of the aluminum oxide substrate.
[0011] According to one aspect of the above technical solution, the step of coating photoresist on the aluminum oxide substrate after film formation to form a first photoresist layer specifically includes:
[0012] Transferring a temporary substrate onto the conductive metal layer, wherein the temporary substrate and the conductive metal layer are fixed by UV adhesive;
[0013] coating a photoresist on the temporary substrate to form a second photoresist layer;
[0014] Selectively irradiating the second photoresist layer based on ultraviolet lithography technology, and dissolving a portion of the second photoresist layer by a developer to obtain a target pattern;
[0015] Removing a portion of the temporary substrate by IBE etching technology to form a pattern groove corresponding to the target image on the temporary substrate;
[0016] A photoresist is coated on the temporary substrate to form a first photoresist layer.
[0017] According to one aspect of the above technical solution, the step of etching the aluminum oxide substrate that has completed the development process to remove part of the conductive metal layer specifically includes:
[0018] The aluminum oxide substrate that has been developed is subjected to IBE etching to remove a portion of the first photoresist layer and a portion of the conductive metal layer corresponding to the first target pattern.
[0019] According to one aspect of the above technical solution, the temporary substrate is made of glass.
[0020] According to one aspect of the above technical solution, before the step of cleaning the etched aluminum oxide substrate, the method further includes:
[0021] The etched aluminum oxide substrate is irradiated with UV light field to transfer the temporary substrate.
[0022] According to one aspect of the above technical solution, the parameters for film forming on the surface of the aluminum oxide substrate based on magnetron sputtering technology include:
[0023] The preheating temperature is 50°C-60°C, the power is 400W-600W, and the flow rate of Ar gas is 10scm-20scm.
[0024] According to one aspect of the above technical solution, the developer is a tetramethylammonium hydroxide developer with a concentration of 2.3%-2.45%.
[0025] According to one aspect of the above technical solution, the conductive metal layer is made of Pt.
[0026] According to one aspect of the above technical solution, the thickness a of the first photoresist layer and the thickness b of the conductive metal layer satisfy:
[0027] a:b=1:2-2.5.
[0028] On the other hand, the present solution also provides a resistive sensor, which is prepared by using a graphical processing method for the resistive sensor in the above technical solution.
[0029] Compared with the prior art, the beneficial effect of the present invention is that: a conductive metal layer is formed by first performing a film forming process on the surface of a substrate based on a magnetron sputtering technology, a first target pattern is further formed by photolithography and development, and then the target pattern is transferred to the conductive metal layer by etching to complete the imaging process of the conductive metal layer. Compared with the process of first preparing the pattern and then forming the film, the problem of difficult stripping and poor imaging effect is avoided, and a graphical structure with low roughness, high aspect ratio and high reliability is obtained. At the same time, in the prior art, in order to improve the stability of the photoresist, a hard film treatment is required before etching, resulting in a high degree of difficulty in subsequent photoresist stripping, which affects the product yield. A temporary substrate is set, a graphic groove corresponding to the target pattern is etched on the temporary substrate, and a photolithography and development process is performed on the temporary substrate, and then the etching process is performed to pass through the graphic groove to perform a graphic process on the conductive metal layer. The temporary substrate and the substrate are connected by UV debonding glue, and the UV debonding glue is reduced by the UV light field to remove the temporary substrate, and the residual photoresist on the temporary substrate is removed at the same time, thereby reducing the difficulty of stripping the photoresist, ensuring the product yield and improving the preparation efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 A flowchart of a graphical processing method for a resistive sensor in a first embodiment of the present invention;
[0031] The following specific implementation manner will further illustrate the present invention in conjunction with the above-mentioned drawings. DETAILED DESCRIPTION
[0032] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. Several embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive.
[0033] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only.
[0034] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0035] See also Figure 1 , which shows a graphical processing method for a resistive sensor in a first embodiment of the present invention, comprising the following steps:
[0036] Step S100, providing an aluminum oxide substrate, and performing film forming treatment on the surface of the aluminum oxide substrate based on magnetron sputtering technology to form a conductive metal layer on the surface of the aluminum oxide substrate. Specifically, in this embodiment, using the magnetron sputtering process, in a vacuum reaction chamber, the target material Pt composed of the metal required for film formation, first fills argon gas into the chamber, and ionizes into positive charge, the positively charged argon ions are attracted by the grounded target, and accelerate toward the target. During the acceleration process, these ions are subject to gravity and gain momentum to bombard the target material, so that momentum transfer will occur on the target. The main feature of the sputtering process is that the target material deposited on the wafer will not undergo chemical or composition changes. Further, the parameters in the above-mentioned magnetron sputtering technology meet the following requirements: preheating temperature 50-60°C, power 400-600W, Ar gas flow rate 10-20sccm, target material 99.99%, and Pt material (conductive metal layer) thickness 7mm.
[0037] Step S200, coating photoresist on the aluminum oxide substrate after the film forming process to form a first photoresist layer.
[0038] Specifically, in this embodiment, the above step S200 specifically includes:
[0039] Step S210, transferring a temporary substrate onto the conductive metal layer, wherein the temporary substrate and the conductive metal layer are fixed by UV de-viscosity adhesive. Specifically, in this embodiment, the temporary substrate is made of glass, and the UV de-viscosity adhesive is of high viscosity to ensure a stable connection with the conductive metal layer. After irradiation, the viscosity of the UV de-viscosity adhesive will decrease, so as to facilitate the subsequent removal of the temporary substrate. In some application scenarios of other embodiments,
[0040] Step S220: coating photoresist on the temporary substrate to form a second photoresist layer.
[0041] Step S230, selectively irradiating the second photoresist layer based on ultraviolet photolithography technology, and dissolving a portion of the second photoresist layer by a developer to obtain a target pattern.
[0042] Step S240, removing part of the temporary substrate by IBE etching technology to form a pattern groove corresponding to the target image on the temporary substrate. Specifically, in this step, the etching technology adopts IBE etching.
[0043] Step S250: coating photoresist on the temporary substrate to form a first photoresist layer.
[0044] Step S300, selectively irradiating the first photoresist layer based on ultraviolet photolithography technology, and dissolving part of the first photoresist layer by a developer to expose part of the conductive metal layer, thereby obtaining a first target pattern corresponding to the first photoresist layer.
[0045] Specifically, in the present embodiment, the photoresist (positive / negative) is selectively irradiated using ultraviolet lithography technology, and the photosensitizer in the photoresist undergoes a chemical reaction, thereby causing the chemical composition of the irradiated area (photosensitive area) of the positive photoresist and the unirradiated area (non-photosensitive area) of the negative photoresist to change. These areas where the chemical composition has changed can be dissolved in a specific developer in the next step. The developer is a tetramethylammonium hydroxide developer with a concentration of 2.3%-2.45%, which has a strong alkalinity and is stable at a temperature not exceeding the decomposition point. When the decomposition point is exceeded, it is quickly decomposed into trimethylamine and methanol. It is easy to remove after the catalysis is completed without leaving any residue. In the present embodiment, a tetramethylammonium hydroxide developer with a concentration of 2.38% is preferably used. Photoresist, also known as photoresist, refers to an etching-resistant film material whose solubility changes through ultraviolet light. A light-sensitive mixed liquid composed of three main components: a photosensitive resin, a sensitizer, and a solvent. The above-mentioned photosensitive material is naphthoquinone diazide, combined with phenolic resin. When irradiated with light, nitrogen will be separated and become a ketone structure. When developed with alkaline aqueous solution, it will become a water-soluble carboxylic acid and then be removed. In other words, the pattern will be left in the area that is not irradiated. For negative photoresist, the resin is polyisoprene, a natural rubber; the solvent is xylene; the photosensitive agent is a photosensitizer that releases nitrogen after exposure, and the generated free radicals form crosslinks between rubber molecules. Thus, it becomes insoluble in the developer. Negative photoresist swells in the exposed area due to the solvent; when exposed, the photoresist easily reacts with nitrogen and inhibits crosslinking. For positive photoresist, after being exposed to ultraviolet light, the photosensitive agent DQ in the positive photoresist will undergo a chemical reaction and turn into vinyl ketone, and further hydrolyze into indene carboxylic acid (CA). The solubility of carboxylic acid in alkaline solvents is higher than that of the non-photosensitive part. The produced carboxylic acid will also promote the dissolution of phenolic resin. By utilizing the different solubilities of sensitive and non-photosensitive photoresists in alkaline solvents, the mask pattern can be transferred.
[0046] Step S400, etching the aluminum oxide substrate after the development process to remove a portion of the conductive metal layer.
[0047] Specifically, in this embodiment, the above step S400 specifically includes:
[0048] Step S410, IBE etching is performed on the aluminum oxide substrate that has completed the development process to remove part of the first photoresist layer and part of the conductive metal layer corresponding to the first target pattern. The part of the conductive metal layer corresponding to the first target pattern is the part of the conductive metal layer corresponding to the pattern groove. It should be noted that in this embodiment, the thickness of the photoresist is determined according to the thickness of the etching material and the etching selectivity. Taking the etching selectivity of 1:2 as an example, the thickness a of the first photoresist layer and the thickness b of the conductive metal layer satisfy: a:b=1:2-2.5. Specifically, in order to prevent the fluorine-based etching gas from reacting with aluminum oxide to produce aluminum fluoride deposition during the etching process, thereby causing problems such as rough etching surface and low steepness of the side wall of the pattern, the thickness of the photoresist needs to be thick enough, and the problem of difficulty in stripping caused by excess photoresist can also be avoided by setting a temporary substrate. It can be understood that in this embodiment, IBE etching is used to remove the above-mentioned part of the first photoresist layer and the part of the conductive metal layer corresponding to the first target pattern. Specifically, using the ion beam etching process (IBE), the wafer is placed on a fixture in a vacuum reaction chamber, and an argon gas flow is introduced into the reaction chamber. When entering the reaction chamber, the argon gas is affected by a high-energy electron beam from a pair of negative (-) and positive (+) electrodes. The electrons ionize the argon atoms into a high-energy state with a positive charge. Since the wafer is located on a fixture connected to the negative electrode, the sub-ions are attracted to the fixture. When the argon atoms move toward the wafer fixture, momentum transfer is achieved. They will accelerate and increase their energy, bombard the exposed wafer layer on the wafer surface, and blow off a small part from the wafer surface.
[0049] Step S500, cleaning the etched aluminum oxide substrate to complete the patterning process of the aluminum oxide substrate.
[0050] Specifically, in this embodiment, before the above step S500, the method further includes:
[0051] Step S501, UV light field irradiation is performed on the etched aluminum oxide substrate to transfer the temporary substrate. Specifically, the UV light field irradiation can reduce the viscosity of the UV viscosity-reducing adhesive, so as to facilitate the removal of the temporary substrate.
[0052] In summary, the resistive sensor patterning method in the above-mentioned embodiment of the present invention forms a conductive metal layer by first performing film forming processing on the substrate surface based on magnetron sputtering technology, further forms a first target pattern by photolithography development, and then transfers the target pattern to the conductive metal layer by etching to complete the patterning of the conductive metal layer. Compared with the process of preparing the pattern first and then forming the film, the problem of difficult stripping and poor patterning effect is avoided, and a patterned structure with low roughness, high aspect ratio and high reliability is obtained. At the same time, in the prior art, in order to improve the stability of the photoresist, the etching Before etching, hardening treatment is required, which makes it difficult to strip the subsequent photoresist, affecting the product yield. A temporary substrate is set up, and a graphic groove corresponding to the target pattern is etched on the temporary substrate, and photolithography development treatment is performed on the temporary substrate. Then, the conductive metal layer is patterned through the graphic groove through etching. The temporary substrate and the substrate are connected by UV debonding adhesive, and the UV debonding adhesive is reduced by UV light field to remove the temporary substrate, and the residual photoresist on the temporary substrate is removed at the same time, reducing the difficulty of stripping the photoresist, ensuring product yield and improving preparation efficiency.
[0053] Embodiment 2
[0054] A second embodiment of the present invention provides a resistive sensor, which is prepared by using a graphical processing method of the resistive sensor in the above embodiment.
[0055] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.
[0056] The above-described embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the present invention. It should be pointed out that, for a person of ordinary skill in the art, several modifications and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the attached claims.
Claims
1. A graphical processing method for a resistive sensor, It is characterized in that The following steps are involved: Providing an aluminum oxide substrate, and performing film forming treatment on the surface of the aluminum oxide substrate based on magnetron sputtering technology to form a conductive metal layer on the surface of the aluminum oxide substrate; Coating a photoresist on the aluminum oxide substrate after the film forming process to form a first photoresist layer; Selectively irradiating the first photoresist layer based on ultraviolet photolithography technology, and dissolving part of the first photoresist layer by a developer to expose part of the conductive metal layer, thereby obtaining a first target pattern corresponding to the first photoresist layer; Etching the aluminum oxide substrate after the development process to remove a portion of the conductive metal layer; The etched aluminum oxide substrate is cleaned to complete the patterning process of the aluminum oxide substrate.
2. The resistive sensor patterning method according to claim 1, It is characterized in that The step of coating photoresist on the aluminum oxide substrate after film formation to form a first photoresist layer specifically includes: Transferring a temporary substrate onto the conductive metal layer, wherein the temporary substrate and the conductive metal layer are fixed by UV adhesive; coating a photoresist on the temporary substrate to form a second photoresist layer; Selectively irradiating the second photoresist layer based on ultraviolet lithography technology, and dissolving a portion of the second photoresist layer by a developer to obtain a target pattern; Removing a portion of the temporary substrate by IBE etching technology to form a pattern groove corresponding to the target image on the temporary substrate; A photoresist is coated on the temporary substrate to form a first photoresist layer.
3. The resistive sensor patterning method according to claim 1, It is characterized in that The step of etching the aluminum oxide substrate after the development process to remove part of the conductive metal layer specifically includes: The aluminum oxide substrate that has been developed is subjected to IBE etching to remove a portion of the first photoresist layer and a portion of the conductive metal layer corresponding to the first target pattern.
4. The resistive sensor patterning method according to claim 2, It is characterized in that The temporary substrate is made of glass.
5. The resistive sensor patterning method according to claim 4, It is characterized in that Before the step of cleaning the etched aluminum oxide substrate, the method further comprises: The etched aluminum oxide substrate is irradiated with UV light field to transfer the temporary substrate.
6. The resistive sensor patterning method according to claim 1, It is characterized in that The parameters for film forming on the surface of the aluminum oxide substrate based on magnetron sputtering technology include: The preheating temperature is 50°C-60°C, the power is 400W-600W, and the flow rate of Ar gas is 10scm-20scm.
7. The resistive sensor patterning method according to claim 1, It is characterized in that The developer is a tetramethylammonium hydroxide developer with a concentration of 2.3%-2.45%.
8. The resistive sensor patterning method according to claim 1, It is characterized in that The conductive metal layer is made of Pt.
9. The resistive sensor patterning method according to claim 1, It is characterized in that The thickness a of the first photoresist layer and the thickness b of the conductive metal layer satisfy: a:b=1:2-2.
5.
10. A resistive sensor, It is characterized in that The resistive sensor is prepared by using a graphical processing method from the resistive sensor according to any one of claims 1 to 9.