Crawling marker for high-speed wire rod variety steel air cooling roller way
By automatically marking and cutting the supercooled sections with crawler markers on the air-cooled rollers, the abnormal performance problems caused by excessive cooling of finished products in rolling steel production are solved, improving the yield rate and reducing costs.
Patent Information
- Application Number
- CN202411292351.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-12-06
AI Technical Summary
During the steel rolling production process, the finished steel products after crawling are over-cooled, resulting in abnormal tissues, affecting the performance of the finished product, and cannot meet customer needs. Unqualified finished products need to be discarded after the roll is collected, resulting in a decrease in the yield rate and an increase in cost. high.
Design a high-speed wire type steel air-cooled roller crawler marker, and use glass water and pneumatic control systems to automatically mark the supercooled section on the air-cooled roller, identify and cut unqualified sections through marking points to ensure that qualified products are in the warehouse , improve the yield rate.
It realizes automatic identification and cutting of unqualified sections caused by overcooling on the air-cooled rollers, ensuring that the finished product performance is qualified, improving the yield rate and reducing production costs.
Smart Images

Figure CN119076690A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of steel rolling production equipment, and in particular to a crawling marker for an air-cooled roller table of a high-speed wire rod steel variety. Background Art
[0002] When producing wire rod steel, different air-cooling line process parameters need to be set according to different grades. Through multi-stage fan cooling, the required metallographic structure can be obtained to ensure that the finished product structure and performance meet the standard requirements and meet various deep processing needs of downstream customers.
[0003] When the steel is rolled out, due to various reasons such as poor head and tail circle shape, steel hanging on the roller side plate, improper operation of the head and tail hook by personnel, etc., it will be impossible to complete the normal collection of finished products, resulting in failures and requiring crawling post-processing;
[0004] After the crawling is stopped, that is, the speed of the air-cooled roller slows down, when the air volume and intensity of the fan remain unchanged, the finished products still in the fan area will be overcooled and below the process temperature requirement due to the slower roller speed, causing abnormal finished product structure, which in turn affects the performance of the finished product and makes it unusable for customers. However, for the finished products not in the fan area, after the crawling is stopped, the temperature drops normally without the influence of the fan, and the structure and performance are not affected and can continue to be used. However, after the finished products after the crawling are collected and rolled, considering the quality of the finished products, all the crawling packages will be scrapped, resulting in a decrease in the yield rate and an increase in costs. Summary of the invention
[0005] In view of this, the purpose of the present invention is to provide a crawling marker for high-speed wire steel air-cooled rollers, which can automatically mark the finished product sections that are under strong cooling by fans after crawling. After the finished products are rolled up, the sections with abnormal organizational properties can be cut by checking the marking points, and the remaining finished products can be put into storage normally as qualified products, thereby improving the yield rate.
[0006] In order to achieve the above-mentioned invention object, the technical solution adopted is as follows:
[0007] A crawling marker for an air-cooled roller table of a high-speed wire rod steel variety, comprising a box body filled with glass water, a water inlet pipe installed on the top of the box body, a water inlet control valve for controlling the amount of glass water added installed on the water inlet pipe, an air inlet pipe connected to the upper part of the side wall of the box body, a spray pipe connected to the lower part of the side wall of the box body, a pneumatic control valve installed on the spray pipe, a first connecting air pipe and a second connecting air pipe connected in sequence to the air inlet direction of the air inlet pipe, a triplet one and a triplet two installed on the first connecting air pipe and the second connecting air pipe respectively, an air outlet end of the first connecting air pipe is connected to a solenoid valve, the solenoid valve is connected to the pneumatic control valve, and an air outlet end of the second connecting air pipe is connected to the spray pipe.
[0008] As a further improvement of the present invention, when it is detected that the air-cooled roller is creeping, triplet one is opened, the solenoid valve is actuated, and the pneumatic control valve is controlled to open. At this time, the glass water in the box can be sprayed on the finished product section through the spray pipe. Due to the high temperature, the glass water mark on the finished product will turn white, thereby completing the continuous marking of the finished product that has been cooled over a certain period of time; when production is normal, triplet one is closed, and the pneumatic control valve is in a closed state, triplet two is normally open, and the gas is sprayed out through the second connecting air pipe and the spray pipe, without affecting the quality of the finished product.
[0009] As a further improvement of the present invention, the water inlet control valve is a DN40 ball valve.
[0010] As a further improvement of the present invention, the air source pressure at the air inlet end of the air inlet pipe is 0.5 mPa.
[0011] As a further improvement of the present invention, the gas source pressure at the gas outlet end of the second connecting air pipe is 0.15 mPa.
[0012] As a further improvement of the present invention, a spray head is installed at the outlet end of the spray pipe.
[0013] The beneficial effects of the present invention are as follows: the present invention provides a crawling marker for a high-speed wire steel air-cooled roller, which can be adjusted to different positions on the air-cooled roller according to the number of fans required for the steel, and can automatically identify unqualified sections of the steel due to overcooling after the air-cooled roller crawls. After the rolls are collected, the unqualified sections are manually cut by identifying the marked sections, ensuring that the remaining finished products are of qualified performance and quality, and can be put into storage normally, thereby improving the yield rate and reducing costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] The drawings constituting a part of this application are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:
[0015] Figure 1 It is a structural schematic diagram of the present invention;
[0016] Figure 2 It is a schematic diagram of the position of the marker of the present invention on the air-cooled roller table;
[0017] Figure 3 This is the situation of the finished steel product on the air-cooled roller after spinning.
[0018] In the figure: 1. box body, 2. water inlet pipe, 3. water inlet control valve, 4. air inlet pipe, 5. spray pipe, 6. pneumatic control valve, 7. first connecting air pipe, 8. second connecting air pipe, 9. triplex one, 10. triplex two, 11. solenoid valve. DETAILED DESCRIPTION
[0019] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0020] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present application.
[0021] like Figure 1 As shown, a crawling marker for an air-cooled roller table of a high-speed wire rod variety steel comprises a box body 1 filled with glass water, a water inlet pipe 2 is installed on the top of the box body 1, a water inlet control valve 3 for controlling the amount of glass water added is installed on the water inlet pipe 2, an air inlet pipe 4 is connected to the upper part of the side wall of the box body 1, a spray pipe 5 is connected to the lower part of the side wall of the box body 1, a pneumatic control valve 6 is installed on the spray pipe 5, a first connecting air pipe 7 and a second connecting air pipe 8 are sequentially connected to the air inlet pipe 4 along the air inlet direction, a triplet 9 and a triplet 10 are respectively installed on the first connecting air pipe 7 and the second connecting air pipe 8, an air outlet end of the first connecting air pipe 7 is connected to the solenoid valve 11, the solenoid valve 11 is connected to the pneumatic control valve 6, and an air outlet end of the second connecting air pipe 8 is connected to the spray pipe 5.
[0022] The triplex 1 9 and the triplex 2 10 are triplexes commonly used by those skilled in the art, and include an air filter, a pressure reducing valve and an oil mist collector.
[0023] When the creeping of the air-cooled roller is detected, the triplet 9 is opened, the solenoid valve 11 is actuated, and the pneumatic control valve 6 is controlled to be opened. At this time, the glass water in the box 1 can be sprayed on the finished product section through the spray pipe 5. Due to the high temperature, the glass water mark on the finished product will turn white, thereby completing the continuous marking of the finished product that has been cooled. When the production is normal, the triplet 9 is closed. At this time, the pneumatic control valve 6 is in a closed state, the triplet 10 is normally open, and the gas is sprayed out through the second connecting air pipe 8 and the spray pipe 5, which does not affect the quality of the finished product.
[0024] The water inlet control valve 3 is a DN40 ball valve.
[0025] The air source pressure at the air inlet end of the air inlet pipe 4 is 0.5 mPa.
[0026] The gas source pressure at the gas outlet end of the second connecting gas pipe 8 is 0.15 mPa.
[0027] A spray head is installed at the outlet end of the spray pipe 5.
[0028] The present invention can adjust different positions on the air-cooled roller according to the number of fans required for different types of steel, and requires moving to the position of the last fan. Figure 2 The present invention is arranged at the end position of fan No. 13. Figure 3 This is the situation of the finished steel product on the air-cooled roller after spinning. After being cooled by the fan, the temperature gradually decreases.
[0029] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, component splitting or combination, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A crawling marker for high-speed wire steel air-cooled roller, characterized in that: It includes a box body filled with windshield washer water, a water inlet pipe is installed on the top of the box body, a water inlet control valve for controlling the amount of windshield washer water added is installed on the water inlet pipe, an upper part of the side wall of the box body is connected to an air inlet pipe, a lower part of the side wall of the box body is connected to a spray pipe, a pneumatic control valve is installed on the spray pipe, a first connecting air pipe and a second connecting air pipe are sequentially connected to the air inlet pipe along the air inlet direction, a triplet one and a triplet two are installed on the first connecting air pipe and the second connecting air pipe respectively, an air outlet end of the first connecting air pipe is connected to a solenoid valve, the solenoid valve is connected to the pneumatic control valve, and an air outlet end of the second connecting air pipe is connected to the spray pipe.
2. The crawling marker for high-speed wire steel air-cooled roller according to claim 1 is characterized in that: When the creeping of the air-cooled roller is detected, the first triplet opens, the solenoid valve is actuated, and the pneumatic control valve is controlled to open. At this time, the glass water in the box can be sprayed on the finished product section through the spray pipe. Due to the high temperature, the glass water mark on the finished product will turn white, thereby completing the continuous marking of the finished product that has been cooled. When the production is normal, the first triplet is closed, and the pneumatic control valve is in a closed state. The second triplet is normally open, and the gas is sprayed out through the second connecting air pipe and the spray pipe, which does not affect the quality of the finished product.
3. The crawling marker for high-speed wire steel air-cooled roller according to claim 1 is characterized in that: The water inlet control valve is a DN40 ball valve.
4. The crawling marker for high-speed wire steel air-cooled roller according to claim 1 is characterized in that: The air source pressure at the air inlet end of the air inlet pipe is 0.5 mPa.
5. The crawling marker for high-speed wire steel air-cooled roller according to claim 1 is characterized in that: The gas source pressure at the gas outlet end of the second connecting air pipe is 0.15mPa.
6. The crawling marker for high-speed wire steel air-cooled roller according to claim 1, characterized in that: A spray head is installed at the outlet end of the spray pipe.
Citation Information
Patent Citations
Method for identifying casting blank by glass water
CN103008197A
Windshield washer fluid spraying device for mining explosion-proof locomotive
CN210585491U
improvements to marker devices
FR1267401A