A kind of production method of unsaturated polyester resin
The technology of a polyester resin and a production method, which is applied in the production field of unsaturated polyester resin, can solve the problems of blocking condensation pipes, increasing the pressure of sewage treatment, increasing the loss of benzoic acid, etc.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Publication Date
- 2021-08-03
Smart Images

Figure 1 
Figure 2
Abstract
Description
Background technique
[0001] UPR, Unsaturated Polyester Resin, unsaturated polyester resin, is the most common type of thermosetting resin. It is a linear polymer formed by polycondensation of saturated dibasic acid, unsaturated dibasic acid and diol. A resin solution with a certain viscosity formed by diluting a cross-linking monomer (generally styrene) or an active solvent. Unsaturated polyester resin is the most used variety of thermosetting resins in my country, and it is also the most used matrix resin in domestic glass fiber reinforced plastics, artificial stone, handicrafts, etc. From 2001 to the present, UPR has continued to grow, from 500,000 in that year tons increased to 1.85 million tons in 2014, an increase of 3.7 times.
[0002] UPR produced by traditional methods generally has performance defects, mainly because: 1. General unsaturated polyester resins have more active groups, such as hydroxyl groups, carboxyl groups and other hydrophilic groups, and are extremel...
Examples
Embodiment 1
[0011] Embodiment 1: the production of unsaturated polyester resin (UPR)
[0012] Unsaturated polyester resin is made of propylene glycol, phthalic anhydride, maleic anhydride, etc. according to a certain proportion, through polycondensation reaction at 160-210°C, then add paraffin, styrene and accelerator, etc., and mix at 70-80°C Dissolved to obtain a liquid resin product with a certain viscosity. Specific process such as figure 1 Shown:
[0013] Add materials according to different types of unsaturated polyester resin formulas, first add glycol (propylene glycol, diethylene glycol, ethylene glycol, etc.) In the case of feeding nitrogen, and then gradually adding solid materials (phthalic anhydride, maleic anhydride, PET, etc.), after the feeding of each component is completed, continue to gradually heat for esterification reaction, raise the temperature to 190-200 ° C, and keep warm to a certain extent. Add crude monoesters (accounting for 5%-25% of the amount of diols) ...
Embodiment 2
[0014] Embodiment 2: benzoic esterification process
[0015] Benzoic acid monoester is to adopt benzoic acid and dibasic alcohol to make through esterification reaction, and reaction process flow chart is as follows figure 2 Shown:
[0016] Benzoic acid and diols (diethylene glycol, glycerol, ethylene glycol, propylene glycol) are fed into the reaction kettle according to the ratio of 1:1.1, nitrogen deoxidation, and the temperature is slowly raised to about 200 ° C for 4 to 6 hours. Reaction to the end of the reaction (acid value below 50mg.koh / g), to obtain benzoic acid monoester.