Method for manufacturing metal shield and metal shield thereof
By using the first photoresist layer and the second photoresist layer in the manufacturing of metal shields to form evaporation holes, the problems of opening consistency and deviation are solved, the design goals of the opening yield and evaporation angle of the metal shield are improved, and the pixel accuracy.
Patent Information
- Application Number
- CN202310100607.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-02-09
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2043-02-09
AI Technical Summary
Existing precision metal shields have problems such as lack of consistency in openings and deviation from the designed shape during the manufacturing process, which affects pixel accuracy and leads to problems such as pattern misalignment and color mixing.
The first photoresist layer and the second photoresist layer are used to form evaporation holes through etching, ensuring that each preset opening area is partially exposed to each first opening, compensating for the deviation caused by the flow of the etching liquid, so that the first opening The error relative to the preset opening area is smaller or zero, improving the opening yield and consistency.
It achieves high yield and consistency of metal shielding openings, improves abnormal conditions during the evaporation process, ensures that the design goals of the evaporation angle meet expectations, and improves pixel accuracy.
Smart Images

Figure CN116145078B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to Taiwan Province of China Patent Application No. 111147016 filed on December 7, 2022, which is incorporated herein by reference for all purposes as if fully set forth herein. Technical Field
[0003] The present invention relates to a method for manufacturing a metal shield, in particular to a method for manufacturing a metal shield that can be used for vapor deposition and the manufactured metal shield. Background Art
[0004] Fine Metal Mask is commonly used in the display industry, for example, in the manufacture of display panels, to evaporate pixel materials onto a substrate to form a pixel array. The fine metal mask has multiple openings, which correspond to the positions on the substrate where the pixel array will be formed during the evaporation process. Currently, in the process of manufacturing fine metal masks by chemical etching, there are problems such as lack of consistency in the openings and deviation from the designed shape. If this poor fine metal mask is used for pixel evaporation, it will affect the pixel accuracy and cause problems such as pattern misalignment and color mixing. Summary of the invention
[0005] In view of the shortcomings of the prior art, the present invention provides a method for manufacturing a metal shield, which can improve the opening yield and opening consistency of the metal shield.
[0006] In order to achieve the above-mentioned object, the present invention also provides a metal shield having better opening yield and opening consistency.
[0007] The manufacturing method of the metal shield provided by the present invention includes providing a metal plate having a first surface and a second surface relative to each other, wherein the first surface has a plurality of preset opening areas, and each preset opening area has a first area; forming a first photoresist layer on the first surface of the metal plate, wherein the first photoresist layer has a plurality of first openings, and each first opening has a second area; the plurality of first openings respectively correspond to the plurality of preset opening areas, and each preset opening area is partially exposed to each first opening, wherein the second area is 75% to 100% of the first area; forming a second photoresist layer on the second surface of the metal plate, wherein the second photoresist layer has a plurality of second openings, and the second surface is exposed to the plurality of second openings; forming a plurality of first etching portions on the first surface, and the plurality of first etching portions respectively correspond to the plurality of first openings; wherein each first etching portion has a first opening, and each first opening is located in each preset opening area; forming a plurality of second etching portions on the second surface, and the plurality of second etching portions respectively correspond to the second openings.
[0008] In one embodiment of the present invention, the manufacturing method of the metal shield further includes performing a first etching and a second etching. The first etching includes forming a plurality of first etching portions on the first surface and forming a plurality of second etching portions on the second surface. The second etching includes: forming a protective layer on the metal plate, wherein the protective layer covers the second photoresist layer and fills the plurality of second etching portions; further etching is performed on the plurality of first etching portions, and each first etching portion is connected to each second etching portion to form a plurality of vapor deposition holes.
[0009] In one embodiment of the present invention, the method for manufacturing the metal shield further includes removing the first photoresist layer, the second photoresist layer and the protective layer.
[0010] In one embodiment of the present invention, each of the above-mentioned evaporation holes has a third area, the third area is smaller than the second area, and each of the evaporation holes forms an evaporation angle relative to each of the first openings.
[0011] In one embodiment of the present invention, the above-mentioned evaporation angle is an angle between the hole edge of each evaporation hole and the edge of the first opening relative to the first surface.
[0012] In one embodiment of the present invention, each of the above-mentioned evaporation holes further has a first hole edge, and each first opening further has a first edge corresponding to the first hole edge; each evaporation angle further includes a first evaporation angle, and the connection between the midpoint of each first hole edge and the midpoint of each first edge forms a first evaporation angle relative to the first surface.
[0013] In one embodiment of the present invention, each of the above-mentioned evaporation holes further has a second hole edge, each second hole edge is adjacent to each first hole edge and forms a first intersection; each evaporation angle further includes a second evaporation angle, and the connection between the first intersection and the first edge forms a second evaporation angle relative to the first surface.
[0014] In one embodiment of the present invention, the difference between the first evaporation angle and the second evaporation angle is less than 5 degrees.
[0015] In one embodiment of the present invention, each of the first openings further has a first side; the step of forming the first photoresist layer further includes forming a plurality of first openings, and the first side of each first opening has a curved design.
[0016] In one embodiment of the present invention, the first side edge has an inwardly concave arc curve facing each first opening.
[0017] In one embodiment of the present invention, each of the first openings further has a first edge corresponding to the first side, and the step of forming a plurality of first etching portions further includes making the photoresist of the first photoresist layer extend beyond the first edge and cover a portion of the first etching portion.
[0018] In one embodiment of the present invention, each of the above-mentioned first openings is a geometric figure and has multiple edges, each first opening has multiple sides, and the multiple sides correspond to the multiple edges respectively; the above-mentioned step of forming the first photoresist layer further includes forming multiple first openings, and the multiple sides of each first opening respectively have a curved design.
[0019] The present invention also provides a metal shield, comprising: a metal body, a first etching portion, a second etching portion, and a vapor deposition hole. The metal body has a first surface and a second surface; the first etching portion has a first opening located on the first surface; the second etching portion has a second opening located on the second surface, and the second opening is smaller than the first opening; the vapor deposition hole is located between the first etching portion and the second etching portion, and the first etching portion and the second etching portion are connected to the vapor deposition hole; wherein the vapor deposition hole forms a first vapor deposition angle and a second vapor deposition angle relative to the first opening, and the difference between the first vapor deposition angle and the second vapor deposition angle is less than 5 degrees.
[0020] The present invention also provides a metal shield, which is prepared by the above-mentioned manufacturing method of the metal shield.
[0021] It can be seen from the above scheme that the advantages of the present invention are:
[0022] The present invention adopts a first photoresist layer, and each preset opening area of the first surface of the metal plate is partially exposed to each first opening, and the area of the first opening can be smaller than the area of the preset opening area, so that the deviation caused by the flow of the etching liquid can be compensated, so that the error of the first opening relative to the preset opening area is smaller or zero, and the design goal of the first opening and its evaporation angle is achieved. The metal shield provided by the present invention can improve the abnormal evaporation situation because the yield rate of the first opening is improved and the consistency is high. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 A schematic diagram of a process for manufacturing a metal shield according to an embodiment of the present invention;
[0024] Figure 2 A schematic diagram of a preset opening area of a metal shield according to an embodiment of the present invention;
[0025] Figure 3 It is a schematic diagram of the operation of a method for manufacturing a metal shield according to an embodiment of the present invention;
[0026] Figure 4 for Figure 3 Schematic diagram from top view;
[0027] Figure 5 Another schematic diagram of the manufacturing method of the metal shield according to an embodiment of the present invention;
[0028] Figure 6 for Figure 5 A partial bottom-up schematic diagram;
[0029] Figure 7 for Figure 5 Another partial bottom view;
[0030] Figure 8 is a schematic cross-sectional view of a metal shield according to an embodiment of the present invention;
[0031] Fig. 9 It is a partial bottom view schematic diagram of a metal shield according to an embodiment of the present invention;
[0032] Fig.10 is a partial bottom view schematic diagram of a metal shield according to another embodiment of the present invention;
[0033] Fig.11 A partial image schematic diagram of a metal shield according to an embodiment of the present invention;
[0034] Fig.12 It is a schematic diagram of the operation of the method for manufacturing the metal shield according to another embodiment of the present invention;
[0035] Fig.13 A schematic diagram showing the relationship between the design compensation and the opening area in an embodiment of the present invention;
[0036] in:
[0037] 1-Metal shielding;
[0038] 10-Metal sheet (metal body);
[0039] 200-first surface;
[0040] 2000-preset opening area;
[0041] 210-first etching portion;
[0042] 230, 230'-first opening;
[0043] 251, 251' - first edge;
[0044] 252, 252'-second edge;
[0045] 253' - 3rd edge;
[0046] 300- second surface;
[0047] 310-second etching portion;
[0048] 330 - second opening;
[0049] 400-a first photoresist layer;
[0050] 410-first opening;
[0051] 431- first side;
[0052] 432- second side;
[0053] 433-third side;
[0054] 434-fourth side;
[0055] 500- second photoresist layer;
[0056] 510-second opening;
[0057] 600, 600'-evaporation hole;
[0058] 611, 611'-first hole edge;
[0059] 612, 612'-second hole edge;
[0060] 613'-third hole edge;
[0061] 630-first intersection;
[0062] A, A1~A4-area;
[0063] θ, θ3, θ4 - evaporation angle;
[0064] θ1-first evaporation angle;
[0065] θ2-second evaporation angle. DETAILED DESCRIPTION
[0066] In order to make the above and other purposes, features and advantages of the present invention more obvious and understandable, embodiments are given below and described in detail with reference to the accompanying drawings.
[0067] The above-mentioned other technical contents, features and effects of the present invention will be clearly presented in the detailed description of a preferred embodiment in conjunction with the accompanying drawings. The directional terms mentioned in the following embodiments, such as up, down, left, right, front, back, top or bottom, etc., are only based on the directions shown in the drawings. Therefore, the directional terms used are used to illustrate and not to limit the present invention.
[0068] The embodiment of the present invention provides a method for manufacturing a metal shield by chemical etching through a photoresist pattern. Figure 1 FIG. 1 is a schematic diagram of a process for manufacturing a metal shield according to an embodiment of the present invention. Figure 1In the illustrated embodiment, the manufacturing method of the metal shield includes steps S910 to S950, wherein step S910 includes: providing a metal plate, wherein the provided metal plate has a first surface and a second surface opposite to each other, wherein the first surface has a plurality of preset opening areas, and each preset opening area has a first area; step S920 includes: forming a first photoresist layer on the first surface of the metal plate, wherein the first photoresist layer has a plurality of first openings, and each first opening has a second area; the plurality of first openings respectively correspond to the plurality of preset opening areas, and each preset opening area is partially exposed to each first opening, Wherein, the second area is 75% to 100% of the first area; step S930 includes: forming a second photoresist layer on the second surface of the metal plate, wherein the second photoresist layer has a plurality of second openings, and the second surface is exposed to the plurality of second openings; step S940 includes: forming a plurality of first etching portions on the first surface, and the plurality of first etching portions correspond to the plurality of first openings respectively; wherein each first etching portion has a first opening, and each first opening is located in each preset opening area; step S950 includes: forming a plurality of second etching portions on the second surface, and the plurality of second etching portions correspond to the plurality of second openings respectively. Steps S910 to S950 are further described below.
[0069] The metal plate provided in step S910 may be pre-processed in any conventional manner to be suitable for steps S920 to S950. Figure 2 As shown in the operation diagram, the metal plate 10 has a plurality of preset opening areas 2000 on the first surface 200. A plurality of first openings 230 (described later) will be formed in the plurality of preset opening areas 2000. Based on the design of the evaporation holes of the metal shield, the plurality of preset openings 2000 can be as follows Figure 2 As shown, the metal plate 10 is distributed in the horizontal direction at a certain interval, but the present invention is not limited thereto. For example, in other embodiments, the metal plate 10 has a plurality of preset openings 2000 arranged in both the longitudinal direction and the transverse direction.
[0070] Step S920 further includes the steps of: coating the first surface 200 with photoresist, exposing and developing. Step S930 further includes the steps of: coating the second surface 300 with photoresist, exposing and developing. The photoresists used for the first surface 200 and the second surface 300 can be the same, for example, both are positive photoresists, and the exposure of the first surface 200 and the second surface 300 can be different, for example, different masks are used to form different photoresist patterns. Steps S920 and S930 can be performed simultaneously or at different times, and step S930 can be performed before S920. Figure 3 The operation diagram of FIG. 1 shows the state after steps S920 and S930 are completed. Figure 3As shown, the photoresist on the first surface 200 is exposed and developed to form a first photoresist layer 400, and a plurality of first openings 410 are formed therein, which correspond to a plurality of preset opening areas 2000, and each preset opening area 2000 is partially exposed to each first opening 410. In other words, the size or shape of the first opening 410 and the preset opening area 2000 should be different. In a preferred embodiment of the present invention, the shape of the first opening 410 and the preset opening area 2000 is different. On the other hand, the photoresist on the second surface 300 is exposed and developed to form a second photoresist layer 500, and a plurality of second openings 510 are formed therein. The second surface 300 is exposed to the plurality of second openings 510, and a plurality of second openings 330 (described later) will be formed from the exposed portions.
[0071] Further references Figure 4 , which is Figure 3 The first opening 410 and the preset opening area 2000 are different in size, so the preset opening area 2000 is partially exposed. Furthermore, the first opening 410 and the preset opening area 2000 are also different in shape. In one embodiment of the present invention, the preset opening area 2000 is rectangular. Figure 4 As shown, the first opening 410 has four sides, which correspond to the four sides of the preset opening area 2000, and has a first side 431 on one side, wherein the first side 431 has a curved design. The first opening 410 may further have a second side 432, a third side 433 and a fourth side 434, and all four sides may have a curved design. For example, the position of the side with the curved design may be most of the middle section of the side.
[0072] The curve design of the first side 431, for example, can be an arc curve concave toward the first opening 410. According to the design of the metal shield 1, the arc curve can have various angles. For example, an arc curve with a larger angle can make the side more concave and the first opening 410 smaller, and an arc curve with a smaller angle can make the side less concave and the first opening 410 larger. Based on the concave curve design of the side, the curve and the preset opening area 2000 form an area A. In an embodiment of the present invention, area A can include, for example, areas A1 to A4, and areas A1 to A4 are respectively formed by the curve and the four sides of the preset opening area 2000. In an embodiment of the present invention, the total area of area A accounts for 0% to 25% of the area of the preset opening area 2000, and is preferably greater than 0% and not greater than 20%. If each preset opening area 2000 has a first area S1, and each first opening 410 has a second area S2, then the second area S2 is 75% to 100% of the first area S1. Based on the concave curve design of the first opening 410 on the side, the embodiment of the present invention helps to compensate for the metal material reduced in the etching step (described later), such as the metal material reduced by the first surface 200, so that the error of the first opening 230 relative to the preset opening area 2000 is smaller or zero, for example, greater than 70% and less than 120% of the preset opening area 2000, and preferably close to 100%, which is more in line with the design objectives.
[0073] Step S940 and step S950 further include performing a first etching process to allow the etching liquid to etch the exposed portions of the first surface 200 and the second surface 300 of the metal plate 10. Steps S940 and S950 may be performed simultaneously or asynchronously. In an embodiment of the present invention, the first etching process may initially complete the first etching portion 210 and the second etching portion 310. Steps S940 and step S950 may further include performing a second etching process to allow the etching liquid to further etch the first etching portion 210. The second etching process may include forming a protective layer (not shown) on the second photoresist layer 500. Preferably, the protective layer is filled in the plurality of second etching portions 310. In an embodiment of the present invention, the protective layer may maintain the shape of the second etching portion 310 during the second etching process. The second etching process may connect the first etching portion 210 with the second etching portion 310 and form a vapor deposition hole 600.
[0074] Figure 5 The operation diagram of FIG. 1 shows the state after steps S940 and S950 are completed. Figure 5As shown, steps S940 and S950 form a plurality of first etching portions 210 from the first surface 200, and a plurality of second etching portions 310 from the second surface 300. The plurality of first etching portions 210 correspond to the plurality of first openings 410, respectively, and each first etching portion 210 has a first opening 230 located on the first surface 200. The plurality of second etching portions 310 correspond to the plurality of second openings 510, respectively, and each second etching portion 310 has a second opening 330 located on the second surface 300. In an embodiment of the present invention, each first opening 230 may be approximately located in each predetermined opening area 2000. For example, when the predetermined opening area 2000 is rectangular, the first opening 230 is approximately rectangular. Each first opening 230 may have a third area S3.
[0075] In step S940, the etching liquid flows in the first etching portion 210. Generally speaking, the flow of the etching liquid may be non-directional, thus causing the first opening 230 to deviate from the target design. However, in the embodiment of the present invention, due to the pattern design of the first photoresist layer 400, the side of the first opening 410 has a concave curve design and forms areas A such as A1 to A4, thereby compensating for the deviation caused by the flow of the etching liquid.
[0076] Further references Figures 6-7 , which are Figure 5 A partial bottom view of a part of the Figure 6 The relationship between the first photoresist layer 400 and the first opening 230 is shown. Figure 7 The relationship between the first photoresist layer 400 and the second opening 330 is shown. The first opening 230 may be a geometric shape. In one embodiment of the present invention, the first opening 230 is substantially rectangular. Figure 6 As shown, the first opening 230 has approximately four sides, including a first edge 251 corresponding to the first side 431 of the first opening 410. In an embodiment of the present invention, step S940 may further include making the photoresist of the first photoresist layer 400 extend beyond the first edge 251 and cover a portion of the first etching portion 210. That is, even if the side of the first opening 410 has a concave curve design based on the pattern design of the first photoresist layer 400, it does not mean that the edge of the first opening 230 also has the same concave curve. In some embodiments of the present invention, the first opening 230 may have other geometric shapes other than a rectangle. The present invention may design the total area of the first opening 410 and / or the region A according to the shape of the first opening 230, the number of edges, and other conditions. For example, the first opening 410 may have multiple sides corresponding to or approximately corresponding to multiple edges, and some or all of the sides may further have a curve design. The curve design of each side may be the same or different.
[0077] The manufacturing method of the present invention may further include the step of removing the first photoresist layer 400, the second photoresist layer 500 and the protective layer. The removal may be performed in any conventional manner and will not be described in detail herein. After the removal, a metal shield is obtained. Figures 8-9 FIG. 1 is a schematic cross-sectional view and a partial bottom view of a metal shield according to an embodiment of the present invention. Figures 8-9 As shown, the metal shield 1 includes a metal body 10, a first opening 210, a second opening 310 and a vapor deposition hole 600. Figures 8-9 In the embodiment of the present invention, the shape of the evaporation hole 600 is the same as the first opening 310 and is a rectangle, but the present invention is not limited thereto. In some embodiments of the present invention, the shape of the evaporation hole 600 may be different from the first opening 310. Fig.10 As shown in the example, the evaporation hole 600 ′ has an elongated octagonal shape, and the shape of the first opening 230 ′ is similar to but not the same as the elongated octagonal shape.
[0078] Each evaporation hole 600 may have a fourth area S4, and the fourth area S4 is smaller than the third area S3. In the embodiment of the present invention, the metal shield 1 may use the first surface 200 as an evaporation surface to face the evaporation source, and each evaporation hole 600 forms an evaporation angle θ relative to the first opening 230. The evaporation angle θ may be the angle between the hole edge of the evaporation hole 600 and the edge of the first opening 230 relative to the first surface 200. Generally speaking, the value of the evaporation angle θ is one of the design targets of the metal shield 1, and the evaporation angle θ of the metal shield 1 obtained by the embodiment of the present invention can better meet the design target. In other words, the manufacturing method of the present invention helps to improve the deviation between the finished product and the design.
[0079] The aforementioned evaporation angle θ meets the design target, and also includes the consistency of the evaporation angle θ on each evaporation hole 600. For example, even if the evaporation hole 600 can measure a first evaporation angle θ1 and a second evaporation angle θ2 due to different reference points, θ1 and θ2 meet the design target and have high consistency. Fig. 9 As shown in the example, the evaporation hole 600 has a first hole edge 611 corresponding to the first edge 251 of the first opening 230, wherein the angle between the midpoint of the first hole edge 611 and the midpoint of the first edge 251 relative to the first surface 200 is the first evaporation angle θ1. The evaporation hole 600 also has a second hole edge 612 corresponding to the second edge 252 of the first opening 230, wherein the second hole edge 252 is adjacent to the first hole edge 251 and forms a first intersection 630. The angle between the first intersection 630 and one of the two adjacent edges relative to the first surface 200 is the second evaporation angle θ2. Fig. 9In the example of , the connection between the first intersection 630 and the first hole edge 251 forms a second evaporation angle θ2 relative to the first surface 200, wherein the projection of the connection on the first opening 230 is perpendicular to the first hole edge 251. In addition, the evaporation angle θ can also be measured from other hole edges of the evaporation hole 600. In the embodiment of the present invention, the difference between the first evaporation angle θ1 and the second evaporation angle θ2 is less than 5 degrees. In summary, the metal shield 1 manufactured in the embodiment of the present invention has a compensation for the deviation between its first opening 230 and the design target, so the evaporation angle θ can better meet the design target. Fig.10 Another embodiment is described as a reference for measuring the deposition angle θ of the deposition hole 600 ′.
[0080] Fig.11 FIG. 2 is a partial image diagram of a metal shielding product on a vapor deposition surface according to an embodiment of the present invention. In an embodiment of the present invention, the vapor deposition hole 600 and the first opening 230 are preset to be rectangular. Preferably, Fig.11 As shown, based on steps S910-S950 and the concave curve design of the first opening 410, the error of the first opening 230 relative to the preset opening area 2000 is small, so it can meet the rectangular design goal. Fig.11 As shown, the evaporation angle θ of the evaporation hole 600 has high consistency. For example, the first evaporation angle θ1 of the evaporation hole 600 is, for example, 50.5 degrees, and other evaporation angles on the hole edge, such as θ3 and θ4, can be measured as, for example, 49.0 degrees and 48.5 degrees, and the difference from θ1 is less than 5 degrees, thereby achieving the design goal of consistency of the evaporation angle θ.
[0081] As mentioned above, the area between the curve and the preset opening area 2000 constitutes an area A. The area A may also be called a design compensation. Fig.12 The design compensation of different embodiments of the present invention is shown, wherein the design compensation increases from left to right. As mentioned above, the total area of region A accounts for 0% to 25% of the area of the preset opening area 2000 (first area S1). The percentage is also called the design compensation percentage. Fig.13 The relationship between the design compensation percentage and the first opening 230 of the metal shield 1 in different embodiments of the present invention is shown. Fig.13As shown, as the design compensation percentage increases, the percentage of the actual area of the first opening 230 (the third area S3) relative to the preset opening area 2000 can be lower. For example, when the design compensation percentage is zero, the percentage of the third area S3 relative to the first area S1 is much greater than 100%, indicating that the first opening 230 is larger than the preset opening area 2000, deviating from the design target. When the design compensation percentage increases, the percentage of the third area S3 relative to the first area S1 can be lowered to approach 100%, that is, the error between the first opening 230 and the preset opening area 2000 is within the allowable range, meeting the design target. In the embodiment of the present invention, the first opening 230 obtained with a design compensation percentage of 0% to 25% has an area (the third area S3) within the allowable range and achieves the design target of a consistent evaporation angle θ.
[0082] The present invention also provides a metal shield. Figures 8-9 In one embodiment of the present invention, the metal shield 1 includes a metal body 10, a first etching portion 210, a second etching portion 310 and a vapor deposition hole 600. The metal body 10 has a first surface 200 and a second surface 300, the first etching portion 210 has a first opening 230 located on the first surface 200, the second etching portion 310 has a second opening 330 located on the second surface 300, and the second opening 330 is smaller than the first opening 230. The vapor deposition hole 600 is located between the first etching portion 210 and the second etching portion 230, and the first etching portion 210 and the second etching portion 310 are connected to the vapor deposition hole 600, wherein the vapor deposition angle θ formed by the vapor deposition hole 600 relative to the first opening 230 includes a first vapor deposition angle θ1 and a second vapor deposition angle θ2, and the difference between the first vapor deposition angle θ1 and the second vapor deposition angle θ2 is less than 5 degrees. The metal shield 1 is preferably prepared by the above-mentioned manufacturing method. The metal shield 1 of the embodiment of the present invention can be prepared by steps S910 to S950, wherein the area of the first opening 230 can be smaller than the area of the preset opening area 2000 to compensate for the deviation caused by the flow of the etching solution, so that the error of the first opening 230 relative to the preset opening area 2000 is smaller or zero, achieving the design goal of the first opening 230 and its evaporation angle θ. Therefore, the plurality of first openings 230 have a higher shape consistency, and the value of the evaporation angle θ can meet the expected range.
[0083] The embodiments of the present application are described above in conjunction with the accompanying drawings, but the present application is not limited to the above-mentioned specific implementation methods. The above-mentioned specific implementation methods are merely illustrative and not restrictive. Under the guidance of the present application, ordinary technicians in this field can also make many forms without departing from the purpose of the present application and the scope of protection of the claims, all of which are within the protection of the present application.
Claims
1. A method for manufacturing a metal shield, characterized in that: include: A metal plate, the metal plate having a first surface and a second surface opposite to each other, wherein the first surface has a plurality of preset opening areas, and each of the preset opening areas has a first area; A first photoresist layer is formed on the first surface of the metal plate, wherein the first photoresist layer has a plurality of first openings, and each of the first openings has a second area; the plurality of first openings correspond to the plurality of preset opening areas, respectively, and each of the preset opening areas is partially exposed to each of the first openings, wherein the second area is 75% to 100% of the first area; forming a second photoresist layer on the second surface of the metal plate, wherein the second photoresist layer has a plurality of second openings, and the second surface is exposed to the plurality of second openings; forming a plurality of first etching portions on the first surface, the plurality of first etching portions respectively corresponding to the plurality of first openings; wherein each of the first etching portions has a first opening, and each of the first openings is located in each of the preset opening regions; and forming a plurality of second etching portions on the second surface, wherein the plurality of second etching portions respectively correspond to the plurality of second openings; Each of the first openings has a first side; the step of forming the first photoresist layer further includes forming the plurality of first openings, and the first side of each of the first openings has a curved design; The first side has an arc curve which is concave toward each of the first openings.
2. The method for manufacturing a metal shield according to claim 1, characterized in that: Also includes: performing a first etching and a second etching; The first etching comprises forming the plurality of first etching portions on the first surface and forming the plurality of second etching portions on the second surface; the second etching comprises: forming a protective layer on the metal plate, wherein the protective layer covers the second photoresist layer and fills the plurality of second etching portions; and Further etching is performed on the plurality of first etching portions, and each of the first etching portions is connected to each of the second etching portions to form a plurality of vapor deposition holes.
3. The method for manufacturing a metal shield according to claim 2, characterized in that: Also includes: The first photoresist layer, the second photoresist layer and the protection layer are removed.
4. The method for manufacturing a metal shield according to claim 2, characterized in that: Each of the evaporation holes has a third area, the third area is smaller than the second area, and each of the evaporation holes forms an evaporation angle relative to each of the first openings.
5. The method for manufacturing a metal shield according to claim 4, characterized in that: The evaporation angle is an angle between the hole edge of each evaporation hole and the edge of the first opening relative to the first surface.
6. The method for manufacturing a metal shield according to claim 5, characterized in that: Each of the evaporation holes further has a first hole edge, and each of the first openings further has a first edge corresponding to the first hole edge; each of the evaporation angles further includes a first evaporation angle, and the connection between the midpoint of each of the first hole edges and the midpoint of each of the first edges forms the first evaporation angle relative to the first surface.
7. The method for manufacturing a metal shield according to claim 6, characterized in that: Each of the evaporation holes further has a second hole edge, each of the second hole edges is adjacent to each of the first hole edges and forms a first intersection; each of the evaporation angles further includes a second evaporation angle, and the connection between the first intersection and the first edge forms the second evaporation angle relative to the first surface.
8. The method for manufacturing a metal shield according to claim 7, characterized in that: The difference between the first evaporation angle and the second evaporation angle is less than 5 degrees.
9. The method for manufacturing a metal shield according to claim 1, characterized in that: Each of the first openings further has a first edge corresponding to the first side, and the step of forming the plurality of first etching portions further includes making the photoresist of the first photoresist layer extend out of the first edge and cover a portion of the first etching portion.
10. The method for manufacturing a metal shield according to claim 1, characterized in that: Each of the first openings is a geometric figure and has multiple edges, each of the first openings has multiple side edges, and the multiple side edges correspond to the multiple edges respectively; the step of forming the first photoresist layer further includes forming the multiple first openings, and the multiple side edges of each of the first openings have a curve design respectively.
11. A metal shield, characterized in that: include: A metal body having a first surface and a second surface; a first etching portion, wherein the first etching portion has a first opening located on the first surface; a second etching portion, wherein the second etching portion has a second opening located on the second surface, and the second opening is smaller than the first opening; and an evaporation hole, located between the first etching portion and the second etching portion, and the first etching portion and the second etching portion are connected to the evaporation hole; The evaporation hole forms a first evaporation angle and a second evaporation angle relative to the first opening, and the difference between the first evaporation angle and the second evaporation angle is less than 5 degrees; The first evaporation angle is an angle between the edge of the evaporation hole and the edge of the first opening relative to the first surface; the second evaporation angle is an angle between the edge of the evaporation hole and the edge of the second opening relative to the first surface.
12. The metal shield according to claim 11, characterized in that: The evaporation hole further has a first hole side, the first opening further has a first edge corresponding to the first hole side, and a line connecting a midpoint of the first hole side and a midpoint of the first edge forms the first evaporation angle relative to the first surface.
13. The metal shield according to claim 12, characterized in that: The evaporation hole further has a second hole edge, the second hole edge is adjacent to the first hole edge and forms a first intersection, and the connection between the first intersection and the first edge forms the second evaporation angle relative to the first surface.
14. A metal shield, characterized in that: The metal shield is prepared according to the manufacturing method of any one of claims 1 to 10.
Citation Information
Patent Citations
Mask and manufacturing method thereof, evaporation mask assembly and manufacturing method thereof
CN106119773A
Metal mask plate preparation method
CN107419216A
Metal mask and preparation method thereof
CN107447190A
Metal mask and preparation method thereof
CN107447191A
A shadow mask for organic light emitting diode manufacture
CN108026628A