Rubber-coated glass assembly

By using a rubber-coated glass assembly on the car window glass, combined with photochromic glass, organic tempered glass, protective film and modified rubber materials, the problem of poor compatibility between nail posts and edge strip materials is solved, and the glass quality is improved. The assembly's service life and installation stability achieve efficient glass installation and sealing effects.

CN118769838APending Publication Date: 2024-10-15ANHUI ANJIAN AUTO SKYLIGHT TECH CO LTD LUAN CITY
View PDF 0 Cites 4 Cited by

Patent Information

Application Number
CN202410758034.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-13
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

During the installation process of the existing automobile window glass nail posts, the bonding strength is low or the production cost is high, and the compatibility between the nail posts and the edge strip material is poor, making it difficult to meet the requirements of bonding performance and assembly performance at the same time.

Method used

Adopting a rubber-coated glass assembly, including photochromic glass matrix, organic tempered glass, protective film, elastic rubber glass edging and two-component soundproofing cotton pad, the glass is enhanced by a high-strength lightweight alloy mounting base and modified rubber materials Resistance to corrosion, scratches, vibration and shattering of the assembly.

Benefits of technology

It significantly improves the service life and installation stability of the glass assembly, improves the sealing and assembly performance of the glass assembly on the automobile body, and reduces production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118769838A_ABST
    Figure CN118769838A_ABST
Patent Text Reader

Abstract

The invention relates to a rubber-coated glass assembly which comprises a glass assembly base body, a high-strength light alloy installation base is arranged outside the glass assembly base body in a wrapping mode, and an elastic rubber glass wrapping edge wrapping the glass assembly base body is installed between the glass assembly base body and the high-strength light alloy installation base. The elastic rubber glass covered edge and the high-strength light alloy installation base are provided with a bi-component sound insulation cotton cushion in an attached mode. The glass assembly base body comprises a photochromic glass base body installed in the middle of the glass assembly base body. According to the glass assembly, the glass base body is divided into the photochromic glass and the organic tempered glass attached to the two ends, the whole glass structure is protected through the protective film, the corrosion resistance and scratch resistance of the glass base body are effectively improved, the modified rubber and the two-component cotton serve as buffering materials when the glass assembly is installed, and the service life of the glass assembly is prolonged. The vibration-proof and breakage-proof effects of the glass assembly during working are facilitated, so that the glass assembly can effectively and smoothly work on the mounting mechanism, and the service life of the glass assembly is remarkably prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of automobile parts, and in particular to a rubber-coated glass assembly. Background Art

[0002] At present, the window glass of the car is mainly positioned accurately to the corresponding connection of the car body by nail columns and ensures long-term reliability. The existing nail columns are mainly composed of a base and a column, and the column is also provided with an elastic claw. When installing the car window glass, the base of the nail column is first fixed to the car window glass, and then the column of the nail column is inserted into the mounting hole on the car body sheet metal. In this process, the elastic claw is squeezed by the edge of the sheet metal mounting hole, resulting in radial elastic contraction deformation. When the column is completely entered into the mounting hole, the column and the mounting hole are gap-matched, and the elastic claw is separated from the edge of the mounting hole, so that the elastic force of the elastic claw is released and restored to its original shape, thereby connecting the car window glass to the body side sheet metal, and realizing the installation and fixation of the car window glass on the car body sheet metal.

[0003] In the prior art, there are mainly the following ways to fix the nail column on the window glass:

[0004] 1. Use bonding to fix the nail column to the car window glass. Mainly use double-sided adhesive such as 3M or heat-reactive adhesive such as polyurethane to bond the nail column to the car window glass. This method has low bonding strength, and the nail column has large creep displacement during the use of the car, which affects the sealing between the car glass and the car body;

[0005] 2. Use a clip-on method to fix the nail column to the window glass. When the glass edge strip is injection molded, the nail column fixing seat is wrapped in the edge strip of the window glass in the form of an insert, and then the nail column is clipped into the nail column fixing seat through post-assembly. This method requires the addition of additional inserts and post-assembly processes, and the production cost is high;

[0006] 3. Use insert injection molding to fix the nail column to the window glass. When the glass edge strip is injection molded, the nail column is wrapped in the edge strip of the window glass in the form of an insert. This method has high bonding strength and fast production, and is a commonly used nail column fixing method.

[0007] Thermoplastic Elastomer (TPE) is a material that has the characteristics of high elasticity, high strength, high resilience of rubber and can be processed by injection molding. It is environmentally friendly, non-toxic, safe, weather-resistant, fatigue-resistant and temperature-resistant, with excellent processing performance, no need for vulcanization, and can be recycled to reduce costs. Due to the above excellent properties of TPE materials, it is increasingly widely used as a edging material in glass injection molding.

[0008] However, when the nail column is used as an insert for injection molding of TPE edge strip, the material selection of the nail column is subject to certain restrictions. In order to meet the bonding performance between the nail column and the edge strip, the nail column and the edge strip must be selected from the same material or different materials with good compatibility; in order to meet the assembly performance, the nail column must be selected from an elastic material with a certain strength. The existing nail column is usually composed of one material, or has poor compatibility with the TPE edge strip. For example, the nail column made of POM material has excellent elasticity and strength performance. POM also has self-lubricating properties, which can reduce the assembly force when nailing and inserting the sheet metal. However, POM is a crystalline material with good chemical resistance and self-lubricating properties, so it is difficult to bond with TPE, and the bonding performance does not meet the requirements; or the strength and elasticity do not meet the requirements. For example, the nail column made of glass fiber reinforced PP material, because TPE contains PP material, the two materials can be well soluble together, but the claws of the nail column are insufficiently elastic and the assembly performance is very poor. Therefore, the existing nail column cannot meet the two requirements of bonding performance and assembly performance at the same time. Summary of the invention

[0009] In order to overcome the problems existing in the background technology, the present invention provides a rubber-coated glass assembly, which divides the glass substrate into photochromic glass and organic tempered glass bonded at both ends, and protects the overall glass structure with a protective film, effectively improving the corrosion and scratch resistance of the glass substrate. Modified rubber and two-component cotton are used as buffer materials during the installation of the glass assembly, which is beneficial to the anti-vibration and anti-shattering effects of the glass assembly during operation, so that the glass assembly can work effectively and smoothly on the installation mechanism, and significantly improve the service life of the glass assembly, which has good practicality and application value.

[0010] To achieve the purpose of the present invention, the technical solution adopted is:

[0011] A rubber-coated glass assembly includes a glass assembly substrate, the exterior of the glass assembly substrate is wrapped with a high-strength light-weight alloy mounting base, an elastic rubber glass edging wrapped around the glass assembly substrate is installed between the glass assembly substrate and the high-strength light-weight alloy mounting base, and a double set of sound-isolating cotton pads are bonded to the elastic rubber glass edging and the high-strength light-weight alloy mounting base; the glass assembly substrate includes a photochromic glass substrate installed in the middle thereof, glass inner-layer buffer protective films are installed on both sides of the photochromic glass substrate, an organic tempered glass substrate is wrapped on the outer side of the glass inner-layer buffer protective film, the outer peripheral side of the organic tempered glass substrate is wrapped with a glass outer-layer buffer protective film, and the outer peripheral side of the glass outer-layer buffer protective film is wrapped with a glass anti-scratch and anti-fingerprint transparent film.

[0012] Preferably, the high-strength lightweight alloy mounting base comprises the following components in weight percentage: nano-Si 0.2-1.0%, Mn 1.5-5.0%, Mo 0.04-0.08%, Nd 0.04-0.06%, V0.05-0.09%, Sc 0.02-0.03%, La 0.03-0.07%, Cu 0.1-0.4%, Zn 0.1-0.3%, Cr 0.3-0.6%, Ti 2.5-3.6%, Fe0.3-1.1%, Ru 0.01-0.03%, W 0.3-0.8%, Sr 0.02-0.06%, Ce 0.01-0.03%, carbon nanotubes 0.3-1.2%, aluminum alloy inoculant 0.4-0.8%, and the balance is Al.

[0013] Preferably, the high-strength light-alloy mounting base is provided with a mounting base fixing groove for fixing the high-strength light-alloy mounting base, and the mounting base fixing groove is provided with a mounting base annular through hole and a mounting base circular through hole for fixing the high-strength light-alloy mounting base.

[0014] Preferably, both the fixed glass assembly base and the elastic rubber glass edging are provided with glass edging annular mounting holes for fixedly mounting the glass assembly base, and the sizes and positions of the glass edging annular mounting holes on the fixed glass assembly base and the elastic rubber glass edging are completely aligned.

[0015] Preferably, the elastic rubber glass edging includes the following components in weight percentage: 10-50% of woven carbon fiber modified isoprene rubber, 10-40% of nano-ceramic matrix modified butadiene rubber, 10-50% of metal magnetic powder, 5-15% of graphene modified Teflon short fiber, 5-10% of graphene modified polyimide short fiber, 5-20% of filler, 3-8% of nano zinc oxide, 3-8% of plasticizer, 2-5% of vulcanizer, 2-5% of antioxidant, 2-5% of lubricant, 2-5% of chitosan quaternary ammonium salt and 2-4% of organic rare earth.

[0016] Preferably, the metal magnetic powder in the elastic rubber glass edging is one or more of iron oxide magnetic powder, chromium dioxide magnetic powder, cobalt-iron oxide magnetic powder, nickel-iron oxide magnetic powder, barium-iron oxide magnetic powder, cobalt-nickel-iron oxide magnetic powder, cobalt-nickel-aluminum-iron oxide magnetic powder, cobalt-nickel-chromium-iron oxide magnetic powder, neodymium-boron-iron oxide magnetic powder, and cobalt-samarium-iron oxide magnetic powder.

[0017] Preferably, the filler in the elastic rubber glass edging includes the following components in weight percentage: 10-30% of nano rare earth modified porous silica aerogel, 10-20% of precipitated barium sulfate, 10-15% of zirconium composite silicon powder, 10-15% of red vermiculite powder, 10-15% of calcined ultrafine kaolin, 5-10% of cryolite powder, 3-8% of FeTiO3-MgTiO3 and 2-5% of graphene.

[0018] As a preferred embodiment, the double-group sound insulation pad includes the following components in weight percentage: component A 50-60%, component B 40-50%, wherein component A includes the following components in weight percentage: polydopamine modified silicone elastomer 30-55%, polysiloxane and polystyrene double modified polyoxyxylene 10-35%, chitosan hydrochloride modified cellulose acetate resin 10-30%, organic rare earth 2-8%, nano-metal silver fiber 1-5%, promoter 1-2%, dispersant 0.5-0.8%, curing agent 0.2-0.5%, antioxidant 0.2-0.4%; component B includes the following components in weight percentage: The composition ratio is: metal oxide modified polyethylene terephthalate 10-55%, melamine modified polymethyl methacrylate 15-45%, carbon fiber modified high toughness radiation proof silicone rubber 10-30%, antibacterial polypeptide modified chitosan hydrochloride 3-8%, inorganic rare earth 1-5%, accelerator 0.5-1.5%, dispersant 1.0-3.5%, curing agent 1.5-3.0%, antistatic agent 0.2-0.6%, defoaming agent 0.1-0.3%, antioxidant 0.1-0.3%.

[0019] The beneficial effects of the present invention are:

[0020] The glass assembly of the present invention divides the glass substrate into photochromic glass and organic tempered glass bonded to both ends, and protects the overall glass structure through a protective film, effectively improving the corrosion and scratch resistance of the glass substrate. Modified rubber and two-component cotton are used as buffer materials when the glass assembly is installed, which is beneficial to the anti-vibration and anti-shattering effects of the glass assembly during operation, so that the glass assembly can work effectively and smoothly on the installation mechanism, and the service life of the glass assembly is significantly improved. It has good practicality and application value. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is a schematic diagram of the overall structure of the encapsulated glass assembly of the present invention. Figure 1 ;

[0022] Figure 2 This is a schematic diagram of the overall structure of the encapsulated glass assembly of the present invention. Figure 2 ;

[0023] Figure 3It is a schematic diagram of the side structure of the encapsulated glass assembly of the present invention;

[0024] Figure 4 It is a schematic diagram of the side cross-section structure of the encapsulated glass assembly of the present invention;

[0025] In the figure: 1. Glass assembly substrate; 2. High-strength lightweight alloy mounting base; 3. Elastic rubber glass edging; 4. Double-group sound insulation pads; 5. Annular through hole of mounting base; 6. Circular through hole of mounting base; 7. Fixing groove of mounting base; 8. Annular mounting hole of glass edging; 9. Anti-scratch and anti-fingerprint transparent film for glass; 10. Buffer protective film for outer layer of glass; 11. Organic tempered glass substrate; 12. Buffer protective film for inner layer of glass; 13. Photochromic glass substrate. DETAILED DESCRIPTION

[0026] The following will combine the technical content of the embodiments described in the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0027] Example 1

[0028] like Figure 1 , 2 As shown in Figure 3, a rubber-coated glass assembly includes a glass assembly substrate 1, the outer part of the glass assembly substrate 1 is wrapped with a high-strength light-weight alloy mounting base 2, an elastic rubber glass edging 3 wrapped around the glass assembly substrate 1 is installed between the glass assembly substrate 1 and the high-strength light-weight alloy mounting base 2, and the elastic rubber glass edging 3 and the high-strength light-weight alloy mounting base 2 are fitted with double sets of sound-isolating cotton pads 4; a mounting base fixing groove 7 for mounting and fixing the high-strength light-weight alloy mounting base 2 is provided on the high-strength light-weight alloy mounting base 2, a mounting base annular through hole 5 and a mounting base circular through hole 6 for fixing and installing the high-strength light-weight alloy mounting base 2 are provided on the mounting base fixing groove 7, a glass edging annular mounting hole 8 for fixing and installing the glass assembly substrate 1 is provided on the fixedly installed glass assembly substrate 1 and the elastic rubber glass edging 3, and the size and position of the glass edging annular mounting hole 8 on the fixedly installed glass assembly substrate 1 and the elastic rubber glass edging 3 are completely aligned.

[0029] like Figure 4As shown, a rubber-encapsulated glass assembly, the glass assembly substrate 1 includes a photochromic glass substrate 13 installed in the middle thereof, a glass inner layer buffer protective film 12 is installed on both sides of the photochromic glass substrate 13, an organic tempered glass substrate 11 is wrapped around the outer side of the glass inner layer buffer protective film 12, a glass outer layer buffer protective film 10 is wrapped around the outer peripheral side of the organic tempered glass substrate 11, and a glass anti-scratch and anti-fingerprint transparent film 9 is wrapped around the outer peripheral side of the glass outer layer buffer protective film 10.

[0030] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, a high-strength lightweight alloy mounting base 2 includes the following components in weight percentage: nano-Si 0.2%, Mn 5.0%, Mo 0.04%, Nd 0.04%, V 0.05%, Sc0.02%, La 0.03%, Cu 0.4%, Zn 0.1%, Cr0.6%, Ti 3.6%, Fe 1.1%, Ru 0.01%, W0.8%, Sr 0.02%, Ce 0.01%, carbon nanotube 0.3%, aluminum alloy inoculant 0.8%, and the balance is Al.

[0031] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, the elastic rubber glass edging 3 includes the following components in weight percentage: 30% of woven carbon fiber modified isoprene rubber, 29% of nano-ceramic matrix modified butadiene rubber, 10% of metal magnetic powder, 5% of graphene modified Teflon short fiber, 5% of graphene modified polyimide short fiber, 5% of filler, 3% of nano zinc oxide, 3% of plasticizer, 2% of vulcanizer, 2% of antioxidant, 2% of lubricant, 2% of chitosan quaternary ammonium salt and 2% of organic rare earth.

[0032] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, the metal magnetic powder in the elastic rubber glass edging 3 is a mixture of cobalt-nickel-aluminum-iron oxide magnetic powder, cobalt-nickel-chromium-iron oxide magnetic powder, neodymium-boron-iron oxide magnetic powder, and cobalt-samarium-iron oxide magnetic powder.

[0033] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, the elastic rubber glass edging 3 includes the following components in weight percentage: 25% of nano rare earth modified porous silica aerogel, 10% of precipitated barium sulfate, 12% of zirconium composite silicon powder, 15% of red vermiculite powder, 15% of calcined ultrafine kaolin, 10% of cryolite powder, 8% of FeTiO3-MgTiO3 and 5% of graphene.

[0034] like Figure 1 ,2 As shown in 3, a plastic-coated glass assembly, a double-group sound insulation pad 4 includes the following components in weight percentage: component A 50%, component B 50%, wherein component A comprises the following components in weight percentage: 40% of polydopamine modified silicone elastomer, 30% of polysiloxane and polystyrene double modified polyoxyxylene, 20% of chitosan hydrochloride modified cellulose acetate resin, 5% of organic rare earth, 2% of nano metal silver fiber, 1.7% of accelerator, 0.7% of dispersant, 0.3% of curing agent, and 0.3% of antioxidant; component B comprises the following components in weight percentage: 40% of metal oxide modified polyethylene terephthalate, 30% of melamine modified polymethyl methacrylate, 15% of carbon fiber modified high toughness radiation-proof silicone rubber, 5% of antibacterial polypeptide modified chitosan hydrochloride, 3% of inorganic rare earth, 1% of accelerator, 3% of dispersant, 2.3% of curing agent, 0.3% of antistatic agent, 0.2% of defoaming agent, and 0.2% of antioxidant.

[0035] During installation, the size and position of the glass assembly base 1 and the glass edging annular mounting hole 8 on the elastic rubber glass edging 3 are completely aligned, and the annular mounting piece on the mounting frame that matches the glass edging annular mounting hole 8 is inserted into the glass edging annular mounting hole 8 to achieve fixed installation of the glass assembly base 1 and the elastic rubber glass edging 3;

[0036] Through the mounting base annular through hole 5 and the mounting base circular through hole 6 of the mounting base fixing groove 7 on the high-strength light-alloy mounting base 2, the high-strength light-alloy mounting base 2 is mounted on the fixing frame to achieve the installation and fixation of the glass assembly substrate 1;

[0037] The elastic rubber glass edging 3 and the double-group sound insulation cotton pads 4 play a role in vibration reduction and buffering. The glass anti-scratch and anti-fingerprint transparent film 9, the glass outer buffer protection film 10 and the glass inner buffer protection film 12 effectively prevent the surfaces of the organic tempered glass substrate 11 and the photochromic glass substrate 13 from being scratched.

[0038] Example 2

[0039] The difference between this embodiment and embodiment 1 is that:

[0040] like Figure 1 , 2As shown in 3, a rubber-coated glass assembly, a high-strength lightweight alloy mounting base 2 includes the following components in weight percentage: nano-Si 0.2%, Mn 5.0%, Mo 0.04%, Nd 0.05%, V 0.07%, Sc0.03%, La 0.05%, Cu 0.3%, Zn 0.2%, Cr0.4%, Ti 2.5-3.6%, Fe 0.7%, Ru 0.02%, W0.5%, Sr 0.04%, Ce 0.02%, carbon nanotube 0.3%, aluminum alloy inoculant 0.5%, and the balance is Al.

[0041] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, the elastic rubber glass edging 3 includes the following components in weight percentage: 30% of woven carbon fiber modified isoprene rubber, 20% of nano-ceramic matrix modified butadiene rubber, 10% of metal magnetic powder, 5% of graphene modified Teflon short fiber, 5% of graphene modified polyimide short fiber, 10% of filler, 5% of nano zinc oxide, 3% of plasticizer, 2% of vulcanizer, 2% of antioxidant, 2% of lubricant, 2% of chitosan quaternary ammonium salt and 4% of organic rare earth.

[0042] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, the metal magnetic powder in the elastic rubber glass edging 3 is a mixture of iron oxide magnetic powder, cobalt-iron oxide magnetic powder, nickel-iron oxide magnetic powder, and barium-iron oxide magnetic powder.

[0043] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, the elastic rubber glass edging 3 includes the following components in weight percentage: 30% of nano rare earth modified porous silica aerogel, 20% of precipitated barium sulfate, 15% of zirconium composite silicon powder, 10% of red vermiculite powder, 15% of calcined ultrafine kaolin, 5% of cryolite powder, 3% of FeTiO3-MgTiO3 and 2% of graphene.

[0044] like Figure 1 , 2As shown in 3, a plastic-coated glass assembly, a double-group sound insulation pad 4 includes the following components in weight percentage: component A 55%, component B 45%, wherein component A comprises the following components in weight percentage: 35% of polydopamine modified silicone elastomer, 35% of polysiloxane and polystyrene double modified polyoxyxylene, 20% of chitosan hydrochloride modified cellulose acetate resin, 5% of organic rare earth, 2% of nano metal silver fiber, 1.8% of accelerator, 0.6% of dispersant, 0.3% of curing agent, and 0.3% of antioxidant; component B comprises the following components in weight percentage: 30% of metal oxide modified polyethylene terephthalate, 30% of melamine modified polymethyl methacrylate, 25% of carbon fiber modified high toughness radiation-proof silicone rubber, 5% of antibacterial polypeptide modified chitosan hydrochloride, 4% of inorganic rare earth, 1% of accelerator, 2% of dispersant, 2.2% of curing agent, 0.4% of antistatic agent, 0.2% of defoaming agent, and 0.2% of antioxidant.

[0045] Example 3

[0046] The difference between this embodiment and embodiments 1 and 2 is that:

[0047] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, a high-strength lightweight alloy mounting base 2 includes the following components in weight percentage: nano-Si 1.0%, Mn 1.5%, Mo 0.08%, Nd 0.04%, V 0.09%, Sc0.02%, La 0.07%, Cu 0.1%, Zn 0.3%, Cr0.3%, Ti 3.6%, Fe 0.3%, Ru 0.03%, W0.3%, Sr 0.06%, Ce 0.01%, carbon nanotubes 1.2%, aluminum alloy inoculant 0.4%, and the balance is Al.

[0048] like Figure 1 , 2 As shown in 3, a rubber-coated glass assembly, the elastic rubber glass edging 3 includes the following components in weight percentage: 35% of woven carbon fiber modified isoprene rubber, 20% of nano-ceramic matrix modified butadiene rubber, 10% of metal magnetic powder, 5% of graphene modified Teflon short fiber, 9% of graphene modified polyimide short fiber, 5% of filler, 3% of nano zinc oxide, 3% of plasticizer, 2% of vulcanizer, 2% of antioxidant, 2% of lubricant, 2% of chitosan quaternary ammonium salt and 2% of organic rare earth.

[0049] like Figure 1 , 2As shown in 3, a rubber-coated glass assembly, the metal magnetic powder in the elastic rubber glass edging 3 is a mixture of cobalt-nickel-iron oxide magnetic powder, cobalt-nickel-aluminum-iron oxide magnetic powder, cobalt-nickel-chromium-iron oxide magnetic powder, neodymium-boron-iron oxide magnetic powder, and cobalt-samarium-iron oxide magnetic powder.

[0050] like Figure 1 , 2 As shown in 3, a rubber-encapsulated glass assembly, the filler in the elastic rubber glass edging 3 includes the following components in weight percentage: 30% of nano rare earth modified porous silica aerogel, 20% of precipitated barium sulfate, 15% of zirconium composite silicon powder, 15% of red vermiculite powder, 10% of calcined ultrafine kaolin, 5% of cryolite powder, 3% of FeTiO3-MgTiO3 and 2% of graphene.

[0051] like Figure 1 , 2 As shown in 3, a plastic-coated glass assembly, a double-group sound insulation pad 4 includes the following components in weight percentage: component A 60%, component B 40%, wherein component A comprises the following components in weight percentage: 30% of polydopamine modified silicone elastomer, 30% of polysiloxane and polystyrene double modified polyoxyxylene, 30% of chitosan hydrochloride modified cellulose acetate resin, 5% of organic rare earth, 2% of nano metal silver fiber, 1.3% of accelerator, 0.8% of dispersant, 0.5% of curing agent, and 0.4% of antioxidant; component B comprises the following components in weight percentage: 30% of metal oxide modified polyethylene terephthalate, 30% of melamine modified polymethyl methacrylate, 22% of carbon fiber modified high toughness radiation-proof silicone rubber, 8% of antibacterial polypeptide modified chitosan hydrochloride, 4% of inorganic rare earth, 1.2% of accelerator, 1.8% of dispersant, 1.8% of curing agent, 0.6% of antistatic agent, 0.3% of defoaming agent, and 0.3% of antioxidant.

[0052] In the present invention, the glass assembly divides the glass substrate into photochromic glass and organic tempered glass bonded to both ends, and protects the overall glass structure through a protective film, effectively improving the corrosion and scratch resistance of the glass substrate. Modified rubber and two-component cotton are used as buffer materials during the installation of the glass assembly, which is beneficial to the anti-vibration and anti-shattering effects of the glass assembly during operation, so that the glass assembly can work effectively and smoothly on the installation mechanism, and significantly improve the service life of the glass assembly, which has good practicality and application value.

[0053] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A plastic-coated glass assembly, characterized in that: The invention comprises a glass assembly substrate (1), the exterior of the glass assembly substrate (1) is wrapped with a high-strength light-weight alloy mounting base (2), an elastic rubber glass edging (3) wrapped around the glass assembly substrate (1) is installed between the glass assembly substrate (1) and the high-strength light-weight alloy mounting base (2), and a double set of sound insulation cotton pads (4) are provided in contact with the elastic rubber glass edging (3) and the high-strength light-weight alloy mounting base (2); The glass assembly substrate (1) comprises a photochromic glass substrate (13) installed in the middle thereof, a glass inner layer buffer protection film (12) is installed on both sides of the photochromic glass substrate (13), an organic tempered glass substrate (11) is wrapped around the outer side of the glass inner layer buffer protection film (12), a glass outer layer buffer protection film (10) is wrapped around the outer peripheral side of the organic tempered glass substrate (11), and a glass anti-scratch and anti-fingerprint transparent film (9) is wrapped around the outer peripheral side of the glass outer layer buffer protection film (10); The high-strength light-weight alloy mounting base (2) comprises the following components in weight percentage: nano-Si 0.2-1.0%, Mn 1.5-5.0%, Mo 0.04-0.08%, Nd 0.04-0.06%, V0.05-0.09%, Sc 0.02-0.03%, La 0.03-0.07%, Cu 0.1-0.4%, Zn 0.1-0.3%, Cr 0.3-0.6%, Ti 2.5-3.6%, Fe 0.3-1.1%, Ru 0.01-0.03%, W 0.3-0.8%, Sr 0.02-0.06%, Ce 0.01-0.03%, carbon nanotubes 0.3-1.2%, aluminum alloy inoculant 0.4-0.8%, and the balance is Al.

2. The encapsulated glass assembly according to claim 1, characterized in that: The high-strength light-weight alloy mounting base (2) is provided with a mounting base fixing groove (7) for fixing and mounting the high-strength light-weight alloy mounting base (2), and the mounting base fixing groove (7) is provided with a mounting base annular through hole (5) and a mounting base circular through hole (6) for fixing and mounting the high-strength light-weight alloy mounting base (2).

3. The encapsulated glass assembly according to claim 1, characterized in that: The fixed glass assembly base (1) and the elastic rubber glass edging (3) are both provided with glass edging annular mounting holes (8) for fixedly mounting the glass assembly base (1), and the sizes and positions of the glass edging annular mounting holes (8) on the fixed glass assembly base (1) and the elastic rubber glass edging (3) are completely aligned.

4. The encapsulated glass assembly according to claim 1, characterized in that: The elastic rubber glass edging (3) comprises the following components in percentage by weight: 10-50% of braided carbon fiber modified isoprene rubber, 10-40% of nano-ceramic matrix modified butadiene rubber, 10-50% of metal magnetic powder, 5-15% of graphene modified Teflon short fiber, 5-10% of graphene modified polyimide short fiber, 5-20% of filler, 3-8% of nano zinc oxide, 3-8% of plasticizer, 2-5% of vulcanizer, 2-5% of antioxidant, 2-5% of lubricant, 2-5% of chitosan quaternary ammonium salt and 2-4% of organic rare earth.

5. The encapsulated glass assembly according to claim 1, characterized in that: The metal magnetic powder in the elastic rubber glass edging (3) is one or more of iron oxide magnetic powder, chromium dioxide magnetic powder, cobalt-iron oxide magnetic powder, nickel-iron oxide magnetic powder, barium-iron oxide magnetic powder, cobalt-nickel-iron oxide magnetic powder, cobalt-nickel-aluminum-iron oxide magnetic powder, cobalt-nickel-chromium-iron oxide magnetic powder, neodymium-boron-iron oxide magnetic powder, and cobalt-samarium-iron oxide magnetic powder.

6. The encapsulated glass assembly according to claim 5, characterized in that: The filler in the elastic rubber glass edging (3) comprises the following components in weight percentage: 10-30% of nano rare earth modified porous silica aerogel, 10-20% of precipitated barium sulfate, 10-15% of zirconium composite silicon powder, 10-15% of red vermiculite powder, 10-15% of calcined ultrafine kaolin, 5-10% of cryolite powder, 3-8% of FeTiO3-MgTiO3 and 2-5% of graphene.

7. The encapsulated glass assembly according to claim 1, characterized in that: The double-group sound insulation cotton pad (4) comprises the following components in weight percentage: component A 50-60%, component B 40-50%, wherein component A comprises the following components in weight percentage: polydopamine modified silicone elastomer 30-55%, polysiloxane and polystyrene double modified polyoxyxylene 10-35%, chitosan hydrochloride modified cellulose acetate resin 10-30%, organic rare earth 2-8%, nano-metal silver fiber 1-5%, accelerator 1-2%, dispersant 0.5-0.8%, curing agent 0.2-0.5%, antioxidant 0.2-0.4%; component B comprises The following components are included in weight percentage: 10-55% of metal oxide modified polyethylene terephthalate, 15-45% of melamine modified polymethyl methacrylate, 10-30% of carbon fiber modified high-toughness radiation-proof silicone rubber, 3-8% of antibacterial polypeptide modified chitosan hydrochloride, 1-5% of inorganic rare earth, 0.5-1.5% of accelerator, 1.0-3.5% of dispersant, 1.5-3.0% of curing agent, 0.2-0.6% of antistatic agent, 0.1-0.3% of defoaming agent and 0.1-0.3% of antioxidant.

Citation Information

Cited By

  • Flexible electromagnetic shielding material with heat conduction and sensing properties and preparation method and application thereof

    CN119161640A

  • Foldable magnetic shock-resistant vehicle skylight glass framework

    CN119590183A

  • Foldable magnetic impact-resistant vehicle sunroof glass skeleton

    CN119590183B

  • High-strength good-toughness damping vehicle skylight glass framework

    CN119974928A