Construction method for preventing light partition wall from cracking
By using hot-dip galvanized flat steel and anti-rust treatment combined with expansion bolts and angle steel welding fixation in lightweight partition panel installation, the problem of safety and efficiency of lightweight partition panel installation is solved, and more efficient construction and Higher quality partition panel installation.
Patent Information
- Application Number
- CN202411050894.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing lightweight partition panel installation methods have low safety factor, low construction efficiency, high labor intensity and are prone to cracks.
The partition wall is fixed with hot-dip galvanized flat steel, and is rust-proof and covered with fiberglass mesh cloth at the connection. It is fixed with expansion bolts and angle steel welding, and is filled with crack-resistant mortar to enhance structural stability.
It significantly improves construction efficiency, reduces crack problems, and improves project quality and construction safety.
Smart Images

Figure CN118933229A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of building construction, and in particular to a construction method for preventing a lightweight partition wall from cracking. Background Art
[0002] At present, the installation of lightweight partition boards is all done by manual erection, which not only has a low safety factor and low construction efficiency, but also has high labor intensity and large geometric size differences. In order to facilitate operation during the construction process, workers often add more cement or glue powder when preparing jointing agents or caulking agents. Some simply use pure cement and glue powder without adding sand. The result is not only an increase in cost, but also cracks in the wall panels installed with such materials and the joints processed. Summary of the invention
[0003] In view of this, an object of the present invention is to provide a construction method for preventing lightweight partition walls from cracking.
[0004] The construction method for preventing cracking of lightweight partition walls provided by the present invention adopts the following technical solutions:
[0005] A construction method for preventing cracking of a lightweight partition wall comprises the following steps:
[0006] S1. Preparation: determine the installation location and size, and prepare tools and materials;
[0007] S2. Measurement marking: mark the location and height of the partition wall on the wall;
[0008] S3. Install the partition wall: fix the partition wall to the wall through hot-dip galvanized flat steel;
[0009] S4. Connection treatment: Anti-rust treatment is applied to the connection of the two partition walls, and then Dacron cloth is used at the welding position of the angle steel, and then covered with glass fiber mesh cloth;
[0010] S5. Clean up the scene.
[0011] Further, in step S3, according to the construction drawing, expansion bolts are driven into the wall and fixed by welding with hot-dip galvanized flat steel, connecting pieces are welded and fixed on the hot-dip galvanized flat steel, and the partition wall is fixed on the galvanized flat steel through the connecting pieces.
[0012] Furthermore, the partition wall includes a wall panel and a support member arranged in the wall panel, the support member is connected and fixed to a connecting member, and the other end of the support member is fixedly connected to a connecting member connected to an adjacent partition wall.
[0013] Furthermore, the support member includes two support rods which are respectively diagonally arranged in the wall panel, and the two support rods are fixedly connected at the intersection position.
[0014] Furthermore, the connecting piece is a hot-dip galvanized angle steel, one side of the connecting piece is fixedly connected to the hot-dip galvanized flat steel, and the other side of the connecting piece is attached to the wall panel.
[0015] Furthermore, the opening and closing angles of the two sides of the connecting piece are 105°.
[0016] Furthermore, cement panels are laid on both sides of the wall panel, and both ends of the cement panels are in contact with the ends of the connecting piece.
[0017] Furthermore, in step S4, the connection between the partition wall and the partition wall is covered with a Dacron cloth which is treated for rust prevention, and a glass fiber mesh cloth is laid on the Dacron cloth.
[0018] In summary, the present invention includes at least one of the following beneficial effects: simplifying the construction process, significantly improving work efficiency, and effectively reducing the occurrence of common quality problems such as cracks, making construction faster and more efficient, while ensuring that the project quality reaches higher standards. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a structural schematic diagram of an embodiment of the present invention;
[0020] Figure 2 for Figure 1 A magnified view of part A;
[0021] Figure 3 for Figure 1 Enlarged view of part B.
[0022] Description of reference numerals:
[0023] 1. Connectors; 2. Wall panels; 3. Supports; 4. Cement panels. DETAILED DESCRIPTION
[0024] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0025] The following is combined with Figure 1-3 The present invention is described in further detail.
[0026] The embodiment of the present invention discloses a construction method for preventing cracking of a lightweight partition wall. Figure 1-Figure 3 , the construction method to prevent cracking of lightweight partition walls includes the following steps:
[0027] Step 1. Preparation: First lay out the center line of the wall on the ground according to the axis of the partition wall in the drawing, and then lay out the control line of the lightweight partition board according to the center line of the wall as a basis for checking the position of the wall.
[0028] Step 2, measurement and marking: Use the hanging method to bounce the control line on the ground onto the beam or board on the top surface according to the control line on the ground. Use ink lines to bounce the control line on the wall facade according to the control line on the ground on the column or wall that intersects with the lightweight partition board wall.
[0029] Step 3, install the partition wall: according to the construction drawing, drive M10*80 expansion bolts into the wall and use 30*50*3mm hot-dip galvanized flat steel to weld and fix it, and use 200mm thick polystyrene particle lightweight composite partition wall produced by the manufacturer; a connector 1 is welded and fixed on the hot-dip galvanized flat steel, and the partition wall is fixed to the galvanized flat steel through the connector 1. The partition wall includes a wall panel 2 and a support member 3 arranged in the wall panel 2, and the support member 3 is connected and fixed to the connector 1. The other end of the support member 3 is fixedly connected to the connector 1 connected to the adjacent partition wall, and the support member 3 is a L30*30*3mm hot-dip galvanized angle steel processing part.
[0030] The connector 1 is a hot-dip galvanized angle steel, one side of the connector 1 is fixedly connected to the hot-dip galvanized flat steel, and the other side of the connector 1 is attached to the wall panel 2; the opening and closing angles of the two sides of the connector 1 are 105°.
[0031] Step 4. Connection treatment: The joints of the two partition walls are treated with anti-rust treatment, and then Dacron cloth is used at the welding position of the angle steel, which not only enhances the stability of the structure, but also improves the overall aesthetics. The Dacron cloth with anti-rust treatment is laid at the joints of the partition walls for covering, and the fiberglass mesh cloth is laid on the Dacron cloth.
[0032] At the end of the partition wall, M10*80 expansion bolts are used, supplemented by L50*5mm galvanized angle codes and grade 3 steel for welding and fixing. The remaining part is filled with anti-crack mortar to make it flush with the partition wall to enhance the stability of the structure.
[0033] Cement panels 4 are laid on both sides of the wall panel 2. Both ends of the cement panels 4 are in contact with the ends of the connectors 1. The cement panels 4 are calcium silicate cement board layers.
[0034] Step 5: Clean up the scene.
[0035] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.
Claims
1. A construction method for preventing cracking of lightweight partition walls, characterized in that: The following steps are involved: S1. Preparation: determine the installation location and size, and prepare tools and materials; S2. Measurement marking: mark the location and height of the partition wall on the wall; S3. Install the partition wall: fix the partition wall to the wall through hot-dip galvanized flat steel; S4. Connection treatment: Anti-rust treatment is applied to the connection of the two partition walls, and then Dacron cloth is used at the welding position of the angle steel, and then covered with glass fiber mesh cloth; S5. Clean up the scene.
2. The construction method for preventing cracking of lightweight partition walls according to claim 1 is characterized in that: In step S3, according to the construction drawing, expansion bolts are driven into the wall and hot-dip galvanized flat steel is used for welding and fixing, a connecting piece (1) is welded and fixed on the hot-dip galvanized flat steel, and the partition wall is fixed on the galvanized flat steel through the connecting piece (1).
3. The construction method for preventing cracking of lightweight partition walls according to claim 2 is characterized in that: The partition wall comprises a wall panel (2) and a support member (3) arranged in the wall panel (2); the support member (3) is connected and fixed to a connecting member (1); and the other end of the support member (3) is fixedly connected to a connecting member (1) connected to an adjacent partition wall.
4. The construction method for preventing cracking of lightweight partition walls according to claim 3 is characterized in that: The support member (3) comprises two support rods which are respectively arranged diagonally in the wall panel (2), and the two support rods are fixedly connected at the intersection position.
5. The construction method for preventing cracking of lightweight partition walls according to claim 3 is characterized in that: The connecting piece (1) is a hot-dip galvanized angle steel, one side of the connecting piece (1) is fixedly connected to the hot-dip galvanized flat steel, and the other side of the connecting piece (1) is attached to the wall panel (2).
6. The construction method for preventing cracking of a lightweight partition wall according to claim 5, characterized in that: The opening and closing angles of the two sides of the connecting piece (1) are 105°.
7. The construction method for preventing cracking of lightweight partition walls according to claim 5 is characterized in that: Cement panels (4) are laid on both sides of the wallboard (2), and both ends of the cement panels (4) are in contact with the ends of the connecting piece (1).
8. The construction method for preventing cracking of lightweight partition walls according to claim 1 is characterized in that: In step S4, the connection between the partition wall and the partition wall is covered with a Dacron cloth which is treated for rust prevention, and a glass fiber mesh cloth is laid on the Dacron cloth.