Oscillation sintering method for improving performance of LAGP solid electrolyte

By finely controlling the oscillation frequency and amplitude during the oscillation sintering of LAGP solid electrolyte, combined with real-time monitoring and automatic adjustment technology, the problems of low density and uneven microstructure of traditional sintering methods are solved, which significantly improves the LAGP solid electrolyte performance and stability of sintering process.

CN119059506APending Publication Date: 2024-12-03ZHENGZHOU UNIVERSITY OF AERONAUTICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411276882.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-12
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The LAGP solid electrolyte prepared by traditional sintering methods has low density, high porosity and uneven microstructure, which affects its ionic conductivity, mechanical strength and thermal stability. The application research on oscillating sintering in the preparation of LAGP solid electrolyte has not yet been systematic.

Method used

Using high-precision oscillation sintering equipment, the oscillation frequency and amplitude are finely regulated during the heating, insulation and cooling stages, combined with real-time monitoring and automatic adjustment technology, ensure accurate control of the sintering process, including the use of a laser particle size analyzer to measure the particle size of raw material powder , monitor and adjust the argon input volume in real time, and adjust the equipment operating parameters in a timely manner.

Benefits of technology

Improve the density and microstructure of LAGP solid electrolyte, improve ionic conductivity, mechanical strength and thermal stability, enhance the stability and repeatability of the sintering process, reduce manual operation burden and error, and provide higher performance Electrolyte material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119059506A_ABST
    Figure CN119059506A_ABST
Patent Text Reader

Abstract

The invention discloses an oscillation sintering method for improving performance of LAGP solid electrolyte, which relates to the technical field of solid electrolyte and comprises eight steps of equipment selection, raw material filling, equipment parameter adjustment, oscillation adjustment in a heating stage, oscillation adjustment in a heat preservation stage, atmosphere control, oscillation adjustment in a cooling stage and equipment operation state monitoring. Compared with the prior art, the method has the advantages that through fine regulation and control of the oscillation frequency and amplitude in the heating, heat preservation and cooling stages, uniform contact and close arrangement of raw material powder particles are effectively promoted, the density of a sintered body is improved, the porosity is reduced, the microstructure of the material is optimized, and the preparation process is simple. Therefore, key performance indexes such as ionic conductivity, mechanical strength and thermal stability of the LAGP solid electrolyte are improved, and an electrolyte material with higher performance is provided for application fields such as solid-state batteries.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of solid electrolytes, in particular to an oscillation sintering method for improving the performance of LAGP solid electrolytes. Background Art

[0002] With the rapid development of solid-state battery technology, the requirements for the performance of solid-state electrolyte materials are increasing. LAGP (Li1.5Al0.5Ge1.5(PO4)3), as a solid-state electrolyte material with excellent ionic conductivity and chemical stability, shows great application potential in the field of solid-state batteries. However, LAGP solid electrolytes prepared by traditional sintering methods often have problems such as low density, high porosity, and uneven microstructure. These problems directly affect the key performance indicators of the electrolyte, such as ionic conductivity, mechanical strength and thermal stability, and limit its wide application in solid-state batteries. In order to overcome the shortcomings of traditional sintering methods, researchers continue to explore New sintering technology is used to optimize the performance of LAGP solid electrolyte. Among them, oscillation sintering, as an advanced sintering technology, can effectively promote the rearrangement and densification between particles and improve the quality of the sintered body by introducing mechanical vibration during the sintering process. However, the application research of oscillation sintering in the preparation of LAGP solid electrolyte is still in its infancy. There is still a lack of systematic research and effective solutions on how to finely control the oscillation frequency and amplitude during the heating, insulation and cooling stages, and how to combine real-time monitoring and automatic adjustment technology to achieve precise control of the sintering process. Therefore, we propose an oscillation sintering method to improve the performance of LAGP solid electrolyte. Summary of the invention

[0003] The object of the present invention is to provide an oscillation sintering method for improving the performance of LAGP solid electrolyte.

[0004] In order to solve the problems raised in the above background technology, the present invention provides the following technical solution: an oscillating sintering method for improving the performance of LAGP solid electrolyte, comprising the following steps: Step 1. Equipment selection: Choose high-precision and excellent stability oscillation sintering equipment; Step 2: Raw material loading: loading the evenly mixed raw material powder into the furnace of the oscillating sintering equipment; Step 3: Adjust equipment parameters: set the oscillation frequency and amplitude according to the particle size of the raw material powder; Step 4: Oscillation adjustment during the heating stage: during the heating stage, adjust the oscillation frequency and amplitude according to the temperature change; Step 5: Oscillation adjustment during the heat preservation stage: fine-tune the oscillation frequency and amplitude according to the real-time reaction process of the material and the evolution of the microstructure; Step 6: Atmosphere control: Use a flow controller and a pressure sensor to monitor and adjust the input amount of argon in real time; Step 7: Oscillation adjustment during cooling stage: adjust the oscillation frequency and amplitude according to the temperature change during the cooling stage; Step 8. Monitor the operating status of the equipment: Monitor the operating status of the equipment in real time through the temperature, pressure and vibration sensors installed in the equipment.

[0005] As a further solution of the present invention: the high-precision and excellent stability oscillation sintering equipment in step 1 is an oscillation sintering equipment with an oscillation frequency range of 10Hz-60Hz, an amplitude of 1mm-6mm and a temperature control error of 1°C. Here, an OPS-2020 model oscillation sintering furnace is used.

[0006] As a further solution of the present invention: in the step 2, the raw material is loaded using a vibrating feeder, which can slowly and evenly feed the powder into the furnace to ensure that the powder will not be excessively accumulated in a local area of ​​the furnace.

[0007] As a further solution of the present invention: the method of adjusting the equipment parameters in step three is to use a laser particle size analyzer to measure the particle size of the evenly mixed raw material powder, and select corresponding equipment parameters from an equipment parameter setting reference table based on the measurement results. The equipment parameter setting reference table is obtained by pre-experimentally measuring the sintering results of the equipment for raw material powder of the same particle size under different setting parameters.

[0008] As a further solution of the present invention: the method of oscillation adjustment in the heating stage in step 4 is that in the initial stage, low-frequency oscillation is used to avoid excessive impact on the powder particles and unstable heat transfer. As the temperature gradually increases and the thermal motion between the particles intensifies, the oscillation amplitude is gradually increased.

[0009] As a further solution of the present invention: the method of oscillation adjustment in the insulation stage in step five is, after reaching the set sintering temperature, observing the arrangement of particles and the progress of densification through a scanning electron microscope. When the arrangement of particles and the progress of densification are not in line with expectations, adjusting the oscillation frequency and amplitude until they meet expectations.

[0010] As a further solution of the present invention: the atmosphere control method in step six is ​​to use a flow controller and a pressure sensor to monitor and adjust the input amount of argon in real time. When the actual flow deviation of argon exceeds 0.1L / min, the backup high-purity argon source is started, and it is automatically switched when the main gas source flow is abnormal to maintain the stable atmosphere required for the experiment.

[0011] As a further solution of the present invention: the method of oscillation adjustment in the cooling stage in step seven is to reduce the oscillation frequency to below 10 Hz and the amplitude to within 1 mm during the stage when the temperature drops to room temperature, so as to promote uniform cooling and stress release of the material in a gentle manner.

[0012] As a further solution of the present invention: the method of monitoring the operating status of the equipment in step eight is to obtain temperature, pressure and oscillation parameter data in real time through temperature, pressure and oscillation sensors installed in the equipment, and adjust the operating parameters of the equipment in time according to the real-time monitored data. When the temperature deviation value exceeds the preset safety value, take corresponding measures to adjust the temperature immediately. When the oscillation parameters fluctuate abnormally, perform troubleshooting and parameter correction in time to ensure that the sintering process always proceeds smoothly according to the predetermined plan.

[0013] By adopting the above technical solution, compared with the prior art, the beneficial effects of the present invention are: 1. The present invention effectively promotes uniform contact and close arrangement between raw material powder particles by finely controlling the oscillation frequency and amplitude during the heating, heat preservation and cooling stages, improves the density of the sintered body, reduces the porosity, and optimizes the microstructure of the material, thereby improving the key performance indicators of the LAGP solid electrolyte, such as ionic conductivity, mechanical strength and thermal stability, and provides a higher performance electrolyte material for application fields such as solid-state batteries; 2. The present invention introduces a laser particle size analysis method to measure the particle size of the raw material powder, and sets the equipment parameter reference table based on the preliminary experiment, thereby achieving accurate setting of the sintering equipment parameters. At the same time, combined with real-time monitoring and automatic adjustment technology, it ensures accurate control of the temperature, atmosphere and oscillation parameters during the sintering process, improves the stability of the sintering process, thereby enhancing the repeatability and predictability of the experimental results, reducing unnecessary repeated experiments, and saving research and development time and costs; 3. The present invention monitors the temperature, pressure, oscillation parameters and equipment operating status during the sintering process in real time, and automatically adjusts the operating parameters based on the real-time monitoring data, so as to respond to abnormal situations in a timely manner, reduce the burden of manual operation, improve production efficiency, and reduce errors and risks caused by human factors. At the same time, the large amount of accurate data obtained by monitoring provides a reliable basis for subsequent process improvement and quality traceability. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 Schematic diagram of the method flow in an embodiment of the present invention. DETAILED DESCRIPTION

[0015] The specific embodiments of the present invention will be further described below in conjunction with the accompanying drawings. It should be noted that the description of these embodiments is used to help understand the present invention, but does not constitute a limitation of the present invention.

[0016] In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0017] Please refer to the attached Figure 1 The present invention provides an oscillating sintering method for improving the performance of LAGP solid electrolyte, comprising the following steps: Step 1. Equipment selection: Choose high-precision and excellent stability oscillation sintering equipment; Step 2: Raw material loading: loading the evenly mixed raw material powder into the furnace of the oscillating sintering equipment; Step 3: Adjust equipment parameters: set the oscillation frequency and amplitude according to the particle size of the raw material powder; Step 4: Oscillation adjustment during the heating stage: during the heating stage, adjust the oscillation frequency and amplitude according to the temperature change; Step 5: Oscillation adjustment during the heat preservation stage: fine-tune the oscillation frequency and amplitude according to the real-time reaction process of the material and the evolution of the microstructure; Step 6: Atmosphere control: Use a flow controller and a pressure sensor to monitor and adjust the input amount of argon in real time; Step 7: Oscillation adjustment during cooling stage: adjust the oscillation frequency and amplitude according to the temperature change during the cooling stage; Step 8. Monitor the operating status of the equipment: Monitor the operating status of the equipment in real time through the temperature, pressure and vibration sensors installed in the equipment.

[0018] In one embodiment of the present invention: the high-precision and excellent stability oscillation sintering equipment in the step one is an oscillation sintering equipment with an oscillation frequency range of 10Hz-60Hz, an amplitude of 1mm-6mm and a temperature control error of 1°C. Here, an OPS-2020 model oscillation sintering furnace is used, which is an oscillation sintering furnace with a multi-field coupled sintering system, produced by Chengdu Yifeide New Material Technology Co., Ltd.

[0019] In one embodiment of the present invention: in step 2, the raw material is loaded using a vibrating feeder, which can slowly and evenly feed the powder into the furnace to ensure that the powder will not be excessively accumulated in a local area of ​​the furnace.

[0020] In one embodiment of the present invention: the method for adjusting the equipment parameters in step three is to use a laser particle size analyzer to measure the particle size of the evenly mixed raw material powder, and select corresponding equipment parameters from an equipment parameter setting reference table based on the measurement results. The equipment parameter setting reference table is obtained by pre-experimentally measuring the sintering results of the equipment for raw material powder of the same particle size under different setting parameters.

[0021] In one embodiment of the present invention, the oscillation adjustment method in the heating stage in step 4 is that in the initial stage, low-frequency oscillation is used to avoid excessive impact on the powder particles and unstable heat transfer. As the temperature gradually increases and the thermal motion between the particles intensifies, the oscillation amplitude is gradually increased.

[0022] In one embodiment of the present invention: the oscillation adjustment method during the insulation stage in step five is to observe the arrangement and densification progress of the particles through a scanning electron microscope after reaching the set sintering temperature. When the arrangement and densification progress of the particles are not in line with expectations, adjust the oscillation frequency and amplitude until they meet expectations.

[0023] In one embodiment of the present invention: the atmosphere control method in step six is ​​to use a flow controller and a pressure sensor to monitor and adjust the input amount of argon gas in real time. When the actual flow deviation of argon gas exceeds 0.1L / min, the backup high-purity argon gas source is started, and it is automatically switched when the flow of the main gas source is abnormal to maintain the stable atmosphere required for the experiment.

[0024] In one embodiment of the present invention: the method of oscillation regulation in the cooling stage in step seven is to reduce the oscillation frequency to below 10 Hz and the amplitude to within 1 mm during the stage when the temperature drops to room temperature, so as to promote uniform cooling and stress release of the material in a gentle manner.

[0025] In one embodiment of the present invention: the method of monitoring the operating status of the equipment in step eight is to obtain temperature, pressure and oscillation parameter data in real time through temperature, pressure and oscillation sensors installed in the equipment, and adjust the operating parameters of the equipment in time according to the real-time monitored data. When the temperature deviation value exceeds the preset safety value, take corresponding measures to adjust the temperature immediately. When the oscillation parameters fluctuate abnormally, perform troubleshooting and parameter correction in time to ensure that the sintering process always proceeds smoothly according to the predetermined plan.

[0026] Example 1, please refer to the attached Figure 1First, according to the particle size distribution of the raw material powder, the appropriate initial oscillation parameters are determined by a laser particle size analyzer. Then, in the heating stage, we adopt a gradually increasing oscillation frequency and amplitude strategy to adapt to the enhanced thermal motion of the powder particles as the temperature rises. In the insulation stage, we use a real-time monitoring system to observe the microstructural changes of the material and fine-tune the oscillation parameters as needed to promote the close arrangement and densification of the particles. Finally, in the cooling stage, we use low-frequency and small-amplitude oscillations to ensure uniform cooling of the material and reduce internal stress. Through this series of fine-tuning, we have successfully prepared LAGP solid electrolytes with high density, low porosity and excellent performance. According to the thermal stability of LAGP materials and the sintering process requirements, a maximum temperature limit of 850°C is set. When the temperature exceeds this limit, the system should immediately take measures to reduce the temperature, such as reducing the heating power or increasing the cooling rate. At the same time, the allowable temperature fluctuation range may be ±5°C. When the temperature deviates from the set value beyond this range, the system will automatically adjust the heating or cooling rate to restore temperature stability.

[0027] Example 2, please refer to the attached Figure 1 First, we measured the particle size of the raw powder to obtain its particle size distribution data. Then, based on these data and the equipment parameter setting reference table established in the preliminary experiment, we accurately set the key parameters such as the oscillation frequency and amplitude in the sintering process. This parameter setting method based on scientific data not only improves the controllability of the sintering process, but also ensures the repeatability and predictability of the experimental results. The reference table records the experimental serial number, raw powder particle size range, sintering temperature, holding time, heating rate, sintering pressure and frequency data.

[0028] Example 3, please refer to the attached Figure 1 By setting up a sintering device that integrates temperature, pressure, oscillation sensors and real-time monitoring and automatic adjustment systems, during the sintering process, these sensors collect and transmit various parameter data to the control system in real time. The control system automatically adjusts the operating parameters of the equipment, such as heating power, oscillation frequency and amplitude, according to the preset algorithm and real-time monitored data to ensure that the sintering process proceeds smoothly according to the predetermined plan. At the same time, when an abnormal situation is detected, the control system can respond quickly and take appropriate measures to intervene to prevent accidents.

[0029] Specifically, by finely controlling the oscillation frequency and amplitude during the heating, insulation and cooling stages, the uniform contact and close arrangement between the raw powder particles are effectively promoted, the density of the sintered body is improved, and not only the porosity is reduced, but also the microstructure of the material is optimized, thereby improving the key performance indicators of the LAGP solid electrolyte, such as ionic conductivity, mechanical strength and thermal stability, providing higher performance electrolyte materials for application fields such as solid-state batteries.

[0030] Specifically, by introducing a laser particle size analyzer to measure the particle size of the raw material powder and setting the reference table of equipment parameters based on the preliminary experiment, the precise setting of the sintering equipment parameters was achieved. At the same time, combined with real-time monitoring and automatic adjustment technology, the precise control of temperature, atmosphere and oscillation parameters during the sintering process was ensured, and the stability of the sintering process was improved, thereby enhancing the repeatability and predictability of the experimental results, reducing unnecessary repeated experiments, and saving R&D time and costs.

[0031] Specifically, by real-time monitoring of the temperature, pressure, oscillation parameters and equipment operating status during the sintering process, and automatically adjusting the operating parameters based on the real-time monitoring data, abnormal situations can be responded to in a timely manner, thereby reducing the burden of manual operations, improving production efficiency, and reducing errors and risks caused by human factors. At the same time, the large amount of accurate data obtained from monitoring provides a reliable basis for subsequent process improvements and quality traceability.

[0032] Working principle: First, the laser particle size analysis method is used to accurately measure the particle size of the raw material powder. Based on the measurement results and preliminary experimental data, the initial parameters of the sintering equipment, especially the oscillation frequency and amplitude, are accurately set to ensure the controllability of the sintering process. Subsequently, during the sintering process, the key indicators such as temperature, pressure and oscillation parameters are monitored in real time, combined with intelligent and automated control technology, to dynamically adjust the sintering parameters to adapt to the physical and chemical changes of the material at different stages. In the heating stage, the oscillation frequency and amplitude are gradually increased to promote the initial contact between the particles; in the insulation stage, the optimal oscillation parameters are maintained to optimize the microstructure; in the cooling stage, the oscillation is reduced to avoid internal stress concentration. At this point, the entire workflow is completed.

[0033] The above-mentioned front, back, left, right, top and bottom are all based on the figures in the specification. Figure 1 As a benchmark, according to the person's observation perspective, the side of the device facing the observer is defined as the front, the left side of the observer is defined as the left, and so on.

[0034] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the scope of protection of the present invention.

[0035] It should be noted that the device structure and the drawings of the present invention mainly describe the principle of the present invention. In terms of the technology of the design principle, the settings of the power mechanism, power supply system and control system of the device are not fully described. On the premise that the technical personnel in this field understand the principle of the above invention, the details of the power mechanism, power supply system and control system can be clearly known. The control method of the application document is automatic control through a controller, and the control circuit of the controller can be realized by simple programming by the technical personnel in this field. The standard parts used therein can all be purchased from the market and can be customized according to the instructions and drawings. The specific connection methods of each part adopt conventional means such as mature bolts, rivets, welding, etc. in the prior art. The machinery, parts and equipment all adopt conventional models in the prior art, and the structures and principles of the components known to technical personnel in this field can be known by these technical personnel through technical manuals or through conventional experimental methods.

[0036] The above describes in detail the embodiments of the present invention in conjunction with the accompanying drawings, but the present invention is not limited to the described embodiments. For those skilled in the art, various changes, modifications, substitutions and variations are made to these embodiments without departing from the principle and spirit of the present invention, and they still fall within the protection scope of the present invention.

Claims

1. An oscillating sintering method for improving the performance of LAGP solid electrolyte, characterized in that: The oscillating sintering method for improving the performance of LAGP solid electrolyte comprises the following steps: Step 1. Equipment selection: Choose high-precision and excellent stability oscillation sintering equipment; Step 2: Raw material loading: loading the evenly mixed raw material powder into the furnace of the oscillating sintering equipment; Step 3: Adjust equipment parameters: set the oscillation frequency and amplitude according to the particle size of the raw material powder; Step 4: Oscillation adjustment during the heating stage: during the heating stage, adjust the oscillation frequency and amplitude according to the temperature change; Step 5: Oscillation adjustment during the heat preservation stage: fine-tune the oscillation frequency and amplitude according to the real-time reaction process of the material and the evolution of the microstructure; Step 6: Atmosphere control: Use a flow controller and a pressure sensor to monitor and adjust the input amount of argon in real time; Step 7: Oscillation adjustment during cooling stage: adjust the oscillation frequency and amplitude according to the temperature change during the cooling stage; Step 8. Monitor the operating status of the equipment: Monitor the operating status of the equipment in real time through the temperature, pressure and vibration sensors installed in the equipment.

2. The oscillating sintering method for improving the performance of LAGP solid electrolyte according to claim 1, characterized in that: The high-precision and excellently stable oscillating sintering equipment in the step 1 is an oscillating sintering equipment with an oscillation frequency range of 10 Hz-60 Hz, an amplitude of 1 mm-6 mm, and a temperature control error of 1° C. Here, an OPS-2020 model oscillating sintering furnace is used.

3. The oscillating sintering method for improving the performance of LAGP solid electrolyte according to claim 1, characterized in that: In the step 2, the raw material is loaded by a vibrating feeder, which can slowly and evenly feed the powder into the furnace, ensuring that the powder will not be excessively accumulated in a local area of ​​the furnace.

4. The oscillating sintering method for improving the performance of LAGP solid electrolyte according to claim 1, characterized in that: The method for adjusting the equipment parameters in step three is to use a laser particle size analyzer to measure the particle size of the evenly mixed raw material powder, and select corresponding equipment parameters from an equipment parameter setting reference table based on the measurement results. The equipment parameter setting reference table is obtained by pre-experimentally measuring the sintering results of the equipment for raw material powder of the same particle size under different setting parameters.

5. The oscillating sintering method for improving the performance of LAGP solid electrolyte according to claim 1, characterized in that: The oscillation adjustment method during the heating stage in step 4 is as follows: in the initial stage, low-frequency oscillation is used to avoid excessive impact on the powder particles and unstable heat transfer. As the temperature gradually rises and the thermal motion between the particles intensifies, the oscillation amplitude is gradually increased.

6. The oscillating sintering method for improving the performance of LAGP solid electrolyte according to claim 1, characterized in that: The oscillation adjustment method during the insulation stage in step 5 is to observe the arrangement and densification progress of the particles through a scanning electron microscope after reaching the set sintering temperature. When the arrangement and densification progress of the particles are not in line with expectations, adjust the oscillation frequency and amplitude until they meet expectations.

7. The oscillating sintering method for improving the performance of LAGP solid electrolyte according to claim 1, characterized in that: The atmosphere control method in step six is ​​to use a flow controller and a pressure sensor to monitor and adjust the input amount of argon in real time. When the actual flow deviation of argon exceeds 0.1L / min, the backup high-purity argon source is started, and it is automatically switched when the main gas source flow is abnormal to maintain the stable atmosphere required for the experiment.

8. The oscillating sintering method for improving the performance of LAGP solid electrolyte according to claim 1, characterized in that: The method of oscillation regulation in the cooling stage in step seven is to reduce the oscillation frequency to below 10 Hz and the amplitude to within 1 mm during the stage when the temperature drops to room temperature, so as to promote uniform cooling and stress release of the material in a gentle manner.

9. The oscillating sintering method for improving the performance of LAGP solid electrolyte according to claim 1, characterized in that: The method of monitoring the operating status of the equipment in step eight is to obtain temperature, pressure and oscillation parameter data in real time through temperature, pressure and oscillation sensors installed in the equipment, and adjust the operating parameters of the equipment in time according to the real-time monitored data. When the temperature deviation value exceeds the preset safety value, take corresponding measures to adjust the temperature immediately. When the oscillation parameter fluctuates abnormally, perform troubleshooting and parameter correction in time to ensure that the sintering process always proceeds smoothly according to the predetermined plan.