Special-shaped catalyst assembly for cultivating diamonds
By designing the special-shaped catalyst components and using the structure of the boss and groove, the problem of uneven pressure and heat transfer during diamond cultivation is solved, and the uniform growth and yield of diamond crystals are improved, saving costs.
Patent Information
- Application Number
- CN202323333207.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-07
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2033-12-07
AI Technical Summary
In the existing diamond cultivation, the pressure transfer and heat transfer of the circular sheet-shaped catalyst assembly in the insulated tube is uneven, resulting in uneven mixing of the catalyst alloy and graphite sheet in the melted state, and the central crystal nucleation rate is low, which affects the cultivation and growth of diamonds.
Design a special-shaped catalyst assembly, where the middle of the catalyst alloy is protruding to form a boss, and a matching groove is provided in the middle of the graphite sheet, and the connection is made through the boss and grooves to ensure uniform heat transfer and pressure transfer, enhance the assembly's consistency and provide uniformity. growth space.
It achieves full growth of diamond crystal particle size, improves overall yield, reduces the use of catalyst alloys, and saves costs.
Smart Images

Figure CN221956233U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of large single crystal cultured diamonds, in particular to a special-shaped catalyst component for cultured diamonds. Background Art
[0002] According to the currently disclosed information in this field, the catalyst alloys used for synthesizing diamonds are all in the form of circular flakes, and their graphite flakes are also in the form of circular flakes. This assembled catalyst component has uneven pressure and heat transfer inside the insulating tube, which causes uneven mixing of the catalyst alloy and the graphite flakes in the molten state, resulting in the center providing less growth space than the outer edge, causing the center crystals to be less full than the outer edge crystals, and the center nucleation rate is low, which is not conducive to the cultivation and growth of diamonds. Utility Model Content
[0003] The utility model aims to provide a special-shaped catalyst component for cultivating diamonds, which can improve the uniformity of pressure and heat transfer in an insulating tube, make the catalyst alloy and graphite sheets mix evenly in a molten state, ensure the full grain size of the overall diamond crystal after synthesis, and provide a favorable space for the cultivation and growth of diamonds.
[0004] The utility model adopts the following technical solutions:
[0005] A special-shaped catalyst component for cultivating diamonds comprises a catalyst alloy and a graphite sheet, wherein a boss is protruded from the middle of the catalyst alloy, and a groove matching the boss is arranged at a position corresponding to the boss in the middle of the graphite sheet; the catalyst alloy and the graphite sheet are connected via the boss and the groove; wherein the graphite sheet is located above the catalyst alloy.
[0006] Preferably, the catalyst alloy and the graphite sheet both have circular cross-sections.
[0007] Preferably, the cross sections of the boss and the groove are both circular structures.
[0008] Preferably, the connection between the boss and the catalyst alloy and the connection between the groove and the graphite sheet are both chamfered.
[0009] Preferably, the chamfer of the connection between the boss and the catalyst alloy is 0°-145°, and the chamfer of the connection between the groove and the graphite sheet is 1°-144°.
[0010] Preferably, the matching angle between the catalyst alloy and the graphite sheet after connection is no greater than 1°.
[0011] Preferably, the total height of the catalyst alloy and the graphite sheet after being connected is 8-12 mm.
[0012] Preferably, the thickness of the catalyst alloy is smaller than the thickness of the graphite sheet.
[0013] Preferably, the thickness of the catalyst alloy is 1-3 mm less than the thickness of the graphite sheet.
[0014] Compared with the prior art, the utility model has the following beneficial effects: the utility model provides a uniform growth space for subsequent diamond synthesis by matching the boss of the catalyst alloy with the groove of the graphite sheet, so that the temperature and pressure of the center and the edge are uniform, the crystal size after synthesis is full, the overall output is improved, the amount of catalyst alloy used is effectively reduced, and the cost is saved. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 This is a cross-sectional view of a special-shaped catalyst component according to an embodiment of the present application;
[0016] Figure 2 A top view of a special-shaped catalyst component according to an embodiment of the present application;
[0017] Figure 3 This is a cross-sectional view of the catalyst alloy of the embodiment of the present application;
[0018] Figure 4 This is a cross-sectional view of a graphite sheet according to an embodiment of the present application. DETAILED DESCRIPTION
[0019] The following is a clear and complete description of the present invention in conjunction with the accompanying drawings and embodiments:
[0020] like Figures 1 to 4 As shown, the utility model discloses a special-shaped catalyst component for cultivating diamonds, comprising a catalyst alloy 1 and a graphite sheet 2, wherein the catalyst alloy 1 and the graphite sheet 2 have the same size, a boss 3 is protruded from the middle of the catalyst alloy 1, and a groove 4 matching the boss 3 is provided at a position corresponding to the boss 3 in the middle of the graphite sheet 2; the catalyst alloy 1 and the graphite sheet 2 are connected through the boss 3 and the groove 4 to increase the fit of the entire catalyst component after connection, so that the pressure and temperature of the center and the edge parts during the diamond cultivation process are uniform, which provides favorable conditions for the growth of crystals, effectively improves the output of diamond cultivation, and saves the cultivation cost; wherein the graphite sheet 2 is located above the catalyst alloy 1 to meet the needs of the cultivation process.
[0021] Furthermore, in the present embodiment, the cross-sections of the catalyst alloy 1 and the graphite sheet 2 are both circular structures, and the cross-sections of the boss 3 and the groove 4 are also circular structures; this can ensure the uniformity of heat and pressure transfer of the catalyst assembly during use; preferably, the connection between the boss 3 and the catalyst alloy 1 and the connection between the groove 4 and the graphite sheet 2 are chamfered to enhance the tightness of the connection between the catalyst alloy 1 and the graphite sheet 2; specifically, the chamfer of the connection between the boss 3 and the catalyst alloy 1 is 0°-145°, and the chamfer of the connection between the groove 4 and the graphite sheet 2 is 1°-144°, wherein the matching angle between the catalyst alloy 1 and the graphite sheet 2 after connection is not greater than 1°, which can further ensure the tightness of the catalyst alloy 1 and the graphite sheet 2 after connection.
[0022] In addition, in this embodiment, the total height of the catalyst alloy 1 and the graphite sheet 2 after being connected is 8-12 mm, and the thickness of the catalyst alloy 1 is less than the thickness of the graphite sheet 2; preferably, the thickness of the catalyst alloy 1 is 1-3 mm less than the thickness of the graphite sheet 2. This meets the needs of diamond cultivation and provides favorable conditions for the uniform growth of diamond crystal particles.
[0023] When the utility model is used, the graphite sheet 2 is first placed on the top of the catalyst alloy 1 for assembly and connection, and then the crystal bed with the seed crystal is placed under the special-shaped catalyst component, the catalyst component is placed inside the insulating tube, and the insulating tube and the catalyst component have the same height. Finally, the assembled synthesis block is placed in a six-sided top press with a pressure of 5.40 GPa and a temperature of 1400°C for 5 days. The utility model provides a uniform growth space for subsequent synthesis of diamonds through the optimized arrangement of the catalyst alloy 1 and the graphite sheet 2, so that the temperature and pressure of the center and the edge are uniform, resulting in full crystal size after synthesis, and an increase in overall output, which effectively reduces the amount of the catalyst alloy 1 and saves costs.
Claims
1. A special-shaped catalyst component for growing diamonds, characterized in that: It comprises a catalyst alloy and a graphite sheet, wherein a boss is protruded from the middle of the catalyst alloy, and a groove matching the boss is arranged at a position corresponding to the boss in the middle of the graphite sheet; the catalyst alloy and the graphite sheet are connected via the boss and the groove; wherein the graphite sheet is located above the catalyst alloy.
2. The special-shaped catalyst component for cultivating diamonds according to claim 1, characterized in that: The catalyst alloy and the graphite sheet both have circular cross-sections.
3. The special-shaped catalyst component for cultivating diamonds according to claim 2, characterized in that: The cross sections of the boss and the groove are both circular structures.
4. The special-shaped catalyst component for cultivating diamonds according to claim 3, characterized in that: The connection between the boss and the catalyst alloy and the connection between the groove and the graphite sheet are both chamfered.
5. The special-shaped catalyst component for cultivating diamonds according to claim 4, characterized in that: The chamfer of the connection between the boss and the catalyst alloy is 0°-145°, and the chamfer of the connection between the groove and the graphite sheet is 1°-144°.
6. The special-shaped catalyst component for cultivating diamonds according to claim 4, characterized in that: The matching angle between the catalyst alloy and the graphite sheet after connection is no greater than 1°.
7. The special-shaped catalyst component for cultivating diamonds according to claim 1, characterized in that: The total height of the catalyst alloy and the graphite sheet after being connected is 8-12 mm.
8. The special-shaped catalyst component for cultivating diamonds according to claim 7, characterized in that: The thickness of the catalyst alloy is smaller than the thickness of the graphite sheet.
9. The special-shaped catalyst component for cultivating diamonds according to claim 8, characterized in that: The thickness of the catalyst alloy is 1-3 mm less than the thickness of the graphite sheet.