A machine-woven gun-stab carpet
A carpet and gun piercing technology, applied in carpets, fabrics, textiles, etc., can solve the problems of unstable size, deformation, foaming, deformation, etc., and achieve the effects of rich colors, good elasticity and high-end appearance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0035] Prepare novel machine-woven gun-stab carpet, the steps are as follows:
[0036] (1) Machine weaving: Design the pattern (design the background and flower shape blank when designing the pattern), weave the single-color or multi-color background pattern on the carpet with a Wilton loom or Akmin loom, and reserve the stab part blank;
[0037] (2) Gun stabs: leave a gap in the flower-shaped part that requires a single color or multiple colors, and then use gun stabs to implant it manually.
[0038] In the step (1), the warp density adjustment range of the woven carpet is 200-500 warp / meter, and the weft density adjustment range is 150-1000 warp / weft.
[0039] The pile height range of the step (1) is 4 mm.
[0040] In the step (2), the handmade carpet pile and ring height are 15 mm.
[0041] The step (2) is preferably stabbing large and colorful patterns.
[0042] Weft yarn: Twisting 278tex polypropylene fiber monofilament with a twist of 100 twists / m, then plying and tw...
Embodiment 2
[0050] Prepare novel machine-woven gun-stab carpet, the steps are as follows:
[0051] (1) Machine weaving: Design the pattern (design the background and flower shape blank when designing the pattern), weave the single-color or multi-color background pattern on the carpet with a Wilton loom or Akmin loom, and reserve the stab part blank;
[0052] (2) Gun stabs: leave a gap in the flower-shaped part that requires a single color or multiple colors, and then use gun stabs to implant it manually.
[0053] In the step (1), the warp density adjustment range of the woven carpet is 200-500 warp / meter, and the weft density adjustment range is 150-1000 warp / weft.
[0054] The pile height range of the step (1) is 15 mm.
[0055]In the step (2), the handmade carpet pile and loop height are 22 mm.
[0056] The step (2) is preferably stabbing large and colorful patterns.
[0057] Weft yarn: Twisting 278tex polypropylene fiber monofilament with a twist of 100 twists / m, then plying and tw...
Embodiment 3
[0065] Prepare novel machine-woven gun-stab carpet, the steps are as follows:
[0066] (1) Machine weaving: Design the pattern (design the background and flower shape blank when designing the pattern), weave the single-color or multi-color background pattern on the carpet with a Wilton loom or Akmin loom, and reserve the stab part blank;
[0067] (2) Gun stabs: leave a gap in the flower-shaped part that requires a single color or multiple colors, and then use gun stabs to implant it manually.
[0068] In the step (1), the warp density adjustment range of the woven carpet is 200-500 warp / meter, and the weft density adjustment range is 150-1000 warp / weft.
[0069] The pile height range of the step (1) is 18 millimeters.
[0070] In the step (2), the handmade carpet pile and loop height are 22 mm.
[0071] The step (2) is preferably stabbing large and colorful patterns.
[0072] Weft yarn: Twisting 278tex polypropylene fiber monofilament with a twist of 100 twists / m, then ply...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com