Single-concave embossed oil printing process
A technology and printing speed technology, applied in the field of single embossed ink printing technology, can solve the problems of low production efficiency and ink waste in embossed ink printing, and achieve the effect of high production efficiency and small ink waste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A single embossed word oil printing process, comprising the following steps:
[0022] 1) The manufacture of ink, the ink includes the following raw materials: 8-10 parts of UV hyperbranched polyester acrylic resin, 15-20 parts of polyamide resin, 2-5 parts of silane, 1-3 parts of titanate, 2 parts of potassium sorbate -4 parts, 0.6-1.5 parts of antioxidant, 3-7 parts of dispersant, 1.5-4.5 parts of defoamer, 20-50 parts of pigment, 10-30 parts of water;
[0023] 2) Corona treatment of the substrate: use a corona device to corona treat the surface of the substrate to increase the surface tension of the substrate and form a polar surface layer;
[0024] 3) Printing plate pretreatment: Add the prepared ink into the ink tank, and let the gravure cylinder printing plate idle in the ink tank. The idling time is 22.5 minutes, and the plate is moistened and stirred. 15U;
[0025] 4) Adjustment rules: lower the pressure roller to the plate, put down the scraper, so that the lo...
Embodiment 2
[0028] A single embossed word oil printing process, comprising the following steps:
[0029] 1) The manufacture of ink, the ink includes the following raw materials: 8-10 parts of UV hyperbranched polyester acrylic resin, 15-20 parts of polyamide resin, 2-5 parts of silane, 1-3 parts of titanate, 2 parts of potassium sorbate -4 parts, 0.6-1.5 parts of antioxidant, 3-7 parts of dispersant, 1.5-4.5 parts of defoamer, 20-50 parts of pigment, 10-30 parts of water;
[0030] 2) Corona treatment of the substrate: use a corona device to corona treat the surface of the substrate to increase the surface tension of the substrate and form a polar surface layer;
[0031] 3) Printing plate pretreatment: add the prepared ink into the ink tank, and let the gravure cylinder printing plate idle in the ink tank. The idling time is 35 minutes, and the plate is moistened and stirred. 20U;
[0032] 4) Adjustment rules: lower the pressure roller to the plate, put down the scraper, so that the load...
Embodiment 3
[0035] A single embossed word oil printing process, comprising the following steps:
[0036] 1) The manufacture of ink, the ink includes the following raw materials: 8-10 parts of UV hyperbranched polyester acrylic resin, 15-20 parts of polyamide resin, 2-5 parts of silane, 1-3 parts of titanate, 2 parts of potassium sorbate -4 parts, 0.6-1.5 parts of antioxidant, 3-7 parts of dispersant, 1.5-4.5 parts of defoamer, 20-50 parts of pigment, 10-30 parts of water;
[0037] 2) Corona treatment of the substrate: use a corona device to corona treat the surface of the substrate to increase the surface tension of the substrate and form a polar surface layer;
[0038] 3) Printing plate pretreatment: Add the prepared ink into the ink tank, and let the gravure cylinder printing plate idle in the ink tank. The idling time is 47.5 minutes, and the plate is moistened and stirred. 25U;
[0039] 4) Adjustment rules: lower the pressure roller to the plate, put down the scraper, so that the lo...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More