Embodiment 1
[0018] 1) Put 0.35g of silver nitrate in a beaker, mix 18ml of acetone and 20ml of ethanol, pour it into the beaker filled with silver nitrate, and place it on an ultrasonic oscillator to vibrate for 15 minutes. This mixture is marked as developer A.
[0019] 2) Put 0.5 g of solid ninhydrin in a beaker, mix it with 10 ml of acetone and 10 ml of ethyl acetate solution, pour it into the beaker containing ninhydrin, and stir it with a glass rod until there is no precipitation at the bottom of the beaker. This mixture is marked For developer solution B.
[0020] 3) Mix developing solution A and developing solution B with the same volume in milliliters, and slowly add developing solution A to developing solution B dropwise to prepare a composite developing solution.
[0021] 4) Dilute the prepared composite display solution at 20 μl / cm 2 Evenly add the concentration of 100% to the viscous side of the scotch tape and let it dry naturally for 10 minutes to produce a sticky flexible ...
Embodiment 2
[0024] 1) Put 0.5g of silver nitrate in a beaker, mix 17ml of acetone and 22ml of ethanol, pour it into the beaker filled with silver nitrate, and place it on an ultrasonic oscillator to vibrate for 18 minutes. This mixture is marked as developer solution A.
[0025] 2) Put 0.45g of solid ninhydrin in a beaker, mix 13ml of acetone and 13ml of ethyl acetate solution, pour it into the beaker containing ninhydrin, and stir it with a glass rod until there is no precipitation at the bottom of the beaker. This mixture is marked For developer solution B.
[0026] 3) Mix developing solution A and developing solution B with the same volume in milliliters, and slowly add developing solution A to developing solution B dropwise to prepare a composite developing solution.
[0027] 4) Dilute the prepared composite display solution at 20 μl / cm 2 Evenly drop the concentration of the transparent tape onto the sticky side of the scotch tape, and let it dry naturally for 15 minutes to prepare a...
Embodiment 3
[0030] 1) Put 0.65g of silver nitrate in a beaker, mix 19ml of acetone and 24ml of ethanol, pour it into the beaker filled with silver nitrate, and place it on an ultrasonic oscillator to vibrate for 18 minutes. This mixture is marked as developer A.
[0031] 2) Put 0.45g of solid ninhydrin in a beaker, mix 14ml of acetone and 14ml of ethyl acetate solution, pour it into the beaker containing ninhydrin, and stir it with a glass rod until there is no precipitation at the bottom of the beaker. This mixture is marked For developer solution B.
[0032] 3) Mix developing solution A and developing solution B with the same volume in milliliters, and slowly add developing solution A to developing solution B dropwise to prepare a composite developing solution.
[0033] 4) Dilute the prepared composite display solution at 22 μl / cm 2 Evenly drop the concentration of the transparent tape onto the sticky side of the scotch tape, and let it dry naturally for 15 minutes to prepare a flexibl...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com