Method for manufacturing bamboo charcoal antibacterial fiber
The technology of an antibacterial fiber and a production method, which is applied in the field of fiber processing and production, can solve the problem of no women's physiological period, etc., and achieve the effect of smooth fabric
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] The production method of the bamboo charcoal antibacterial fiber of the present invention is: firstly select the old bamboo that has grown for more than two years, remove the branches and leaves, leave the trunk and cut it into short rods, conduct low-temperature carbonization at 450°C with the air isolated, and then heat up to 800°C for high-temperature carbonization , made of bamboo charcoal. Then the bamboo charcoal obtained is sprayed while it is hot, and the bamboo charcoal is cooled rapidly to extinguish the fire to obtain activated bamboo charcoal; at this time, due to the physical and chemical interaction between high-temperature bamboo charcoal and water, the bamboo charcoal has a complex porous structure, and the surface area is increased several times, which can be greatly improved. Improve adsorption capacity. The activated bamboo charcoal has increased tissue bonding density, becomes extremely hard, and the carbon content can reach more than 85%. Then the ...
Embodiment 2
[0018] In the production method of the present invention, first select old bamboos that have grown for more than two years to remove the branches and leaves, leave the trunk and cut them into short rods, and then conduct low-temperature carbonization at 500°C in isolation from the air, and then heat up to 850°C for high-temperature carbonization to make bamboo charcoal . Then the bamboo charcoal obtained is sprayed while it is hot, and the bamboo charcoal is cooled rapidly to extinguish the fire to obtain activated bamboo charcoal; at this time, due to the physical and chemical interaction between high-temperature bamboo charcoal and water, the bamboo charcoal has a complex porous structure, and the surface area is increased several times, which can be greatly improved. Improve adsorption capacity. The activated bamboo charcoal has increased tissue bonding density, becomes extremely hard, and the carbon content can reach more than 85%. Then the activated bamboo charcoal is dr...
Embodiment 3
[0020] In the production method of the present invention, first select old bamboos that have grown for more than two years to remove the branches and leaves, leave the trunk and cut them into short rods, then conduct low-temperature carbonization at 550°C with air isolation, and then heat up to 900°C for high-temperature carbonization to make bamboo charcoal . Then the bamboo charcoal obtained is sprayed while it is hot, and the bamboo charcoal is cooled rapidly to extinguish the fire to obtain activated bamboo charcoal; at this time, due to the physical and chemical interaction between high-temperature bamboo charcoal and water, the bamboo charcoal has a complex porous structure, and the surface area is increased several times, which can be greatly improved. Improve adsorption capacity. The activated bamboo charcoal has increased tissue bonding density, becomes extremely hard, and the carbon content can reach more than 85%. Then the activated bamboo charcoal is dropped into ...