Writing paper capable of preventing myopia
A technology for preventing myopia and writing paper, which is applied in the directions of paper, paper making, paper making machine, etc., can solve the problems of undisclosed paper preparation methods, etc., and achieve the effects of outstanding dyeing effect, soft color and good stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Take 500kg of hardwood pulp and 600kg of softwood pulp to make mixed pulp, bleach using alkaline bleaching process, and loosen pulp in a horizontal pulper to prepare pulp with a concentration of 31wt%, and send it to a refiner at a speed of 1400r / min Refining 40min, adding basic tender yellow 10g, basic orange 50g, and benzidine yellow G 8g, direct frozen yellow G 12g, titanium dioxide 12g to mix slurry and obtain slurry, adopt conventional method to prepare paper, the moisture in the paper molding process When it is less than 7.6wt%, it is sent to a calender, pressed, and dried to obtain a finished paper.
Embodiment 2
[0017] Take 600kg of hardwood pulp and 300kg of softwood pulp to make mixed pulp, use alkaline bleaching process to bleach, loosen the pulp in a horizontal pulper to prepare pulp with a concentration of 28wt%, and send it to the refiner at a speed of 1650r / min Refining for 38 minutes, adding 18g of basic bright yellow, 39g of basic orange, and 12g of benzidine yellow G, 20g of direct frozen yellow G, and 21g of titanium dioxide to obtain slurry, and preparing paper by conventional methods. In the paper forming process, when paper When the moisture in the paper is lower than 7.0wt%, it is sent to a calender, pressed, and dried to obtain a finished paper.
Embodiment 3
[0019] Take 600kg of hardwood pulp and 600kg of softwood pulp to make mixed pulp, use alkaline bleaching process to bleach, loosen the pulp in a horizontal pulper to prepare pulp with a concentration of 32wt%, and send it to the refiner at a speed of 1200r / min Refining for 65min, adding 21g of basic bright yellow, 70g of basic orange, and 15g of benzidine yellow G, 20g of direct frozen yellow G, and 24g of titanium dioxide to obtain slurry, and preparing paper by conventional methods. When the moisture in the paper is lower than 8.6wt%, it is sent to the calender, pressed, and dried to obtain the finished paper.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com