Adhesive with indicating function
A binder and functional technology, applied in the field of binders with indicating functions, can solve problems such as waste and increased production costs, and achieve the effects of simple formula, low cost and reduced waste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] 1) Weigh 1g of gelatin, soak it in 1mL of water, and swell for later use.
[0028] 2) Weigh 0.06g thymolphthalein, dissolve it with 0.5mL ethanol, and set aside.
[0029] 3) Add 39mL of water into the beaker, heat to 50°C, add 3.5g of polyvinyl alcohol (the degree of polymerization is 1700, the degree of alcoholysis is 99%), heat up to boiling, make it fully dissolved, cool to room temperature, add 2.5g Sodium carboxymethyl cellulose (viscosity between 300-600 centipoise), stirring and dissolving, warming up to 50°C, adding the swelling gelatin prepared in step 1), stirring and dissolving, adding 1mL of 50% glutaraldehyde, stirring continuously to make React for 15 minutes, cool to room temperature, add thymolphthalein ethanol solution prepared in step 2), then add 0.5mL 5% sodium hydroxide solution, stir evenly, and obtain blue binder.
[0030] Take the prepared blue adhesive and apply it on the envelope, the coated part will show blue color, seal the envelope, the co...
Embodiment 2
[0032] 1) Weigh 1.5g of gelatin, soak it in 1.5mL of water, and swell it for later use.
[0033] 2) Weigh 0.1g thymolphthalein, dissolve it with 0.5mL ethanol, and set aside.
[0034] 3) Add 40mL of water into the beaker, heat it to 50°C, add 3g of polyvinyl alcohol (the degree of polymerization is 1700, the degree of alcoholysis is 99%), heat up to boiling, make it fully dissolved, cool to room temperature, add 3.5g of carboxy Sodium methylcellulose (viscosity between 300-600 centipoise), stirring and dissolving, warming up to 40°C, adding the swelling gelatin prepared in step 1), stirring and dissolving, adding 3mL of 25% glutaraldehyde, stirring constantly to make it React for 20 minutes, cool to room temperature, add the thymolphthalein ethanol solution prepared in step 2), then add 1.3mL 3% sodium hydroxide solution, stir evenly, and obtain the blue binder.
[0035] Take the prepared blue adhesive and apply it on the envelope, the coated part will show blue color, seal t...
Embodiment 3
[0037] 1) Weigh 1.5g of gelatin, soak it in 1.5mL of water, and swell it for later use.
[0038] 2) Weigh 0.1g of phenolphthalein, dissolve it with 0.5mL of ethanol, and set aside.
[0039] 3) Add 41mL of water into the beaker, heat it to 50°C, add 3g of polyvinyl alcohol (the degree of polymerization is 1700, the degree of alcoholysis is 99%), heat up to boiling, make it fully dissolved, cool to room temperature, add 3.5g of carboxyl Sodium methylcellulose (viscosity between 300-600 centipoise), stirring and dissolving, warming up to 40°C, adding the swelling gelatin prepared in step 1), stirring and dissolving, adding 2mL of 50% glutaraldehyde, stirring constantly to make it React for 20 minutes, cool to room temperature, add the phenolphthalein ethanol solution prepared in step 2), then add 1.3mL 3% sodium hydroxide solution, add an appropriate amount of cinnamic acid until there is a fragrance, and stir evenly to obtain a red binder.
[0040] Take the prepared red adhesiv...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com