A kind of slagging agent and preparation method thereof

A technology of slagging agent and weight percentage, which is applied in the field of slagging agent and its preparation, can solve the problems of non-permanent slagging, environmental pollution, polluted water quality, etc., and achieve the effects of reducing consumption, reducing the cost per ton of steel, and prolonging the service life

Inactive Publication Date: 2015-10-14
河南鹏钰集团有限公司
View PDF3 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Although the content of fluorite in this technical solution is small, the content is still controlled at 0-6%. Fluorite slag is used in the converter in the traditional steelmaking process, and the slag adjustment speed is fast, but the disadvantages are too great, and the slag is not durable. Fluorite is composed of CaF and CaF 2 Composition, not only serious environmental pollution, but also damage the furnace lining, CaF 2 >2% It is difficult to improve the life of the furnace, and the ladle lining is severely eroded. The gas and water generated when using fluorite as a slagging agent do not meet environmental protection regulations, shorten the service life of the ladle lining, and increase the cost per ton of steel
The use of fluorspar pollutes water quality and damages equipment

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0013] A slagging agent, the raw material of which is composed of the following ingredients in weight percentage: 20% of aluminate, 80% of aluminum ferrite ore;

[0014] The slagging agent may contain the following active ingredients in weight percent: SiO 2 15%, CaO 10%, Al 2 o 3 52%, Fe 2 o 3 14%, S 0.05%, P 0.05%, and the rest are impurities.

[0015] Further, the particle size of the aluminate soil and the aluminum ferrite ore is 5-30mm.

[0016] Provide a kind of preparation method of producing described slagging agent, its steps are:

[0017] a. The raw material is broken into particles with a particle size of 30mm by a jaw crusher;

[0018] b. artificially stirring and mixing the particles in step a;

[0019] c. Put the mixed granules in step b into the kang for drying, the drying temperature is 230°C, and the drying time depends on the quantity, generally 4 hours;

[0020] d. Packing the dried granules in step c into bags is the finished product.

[0021]...

Embodiment 2

[0023] A slagging agent, the raw materials of which are composed of the following ingredients in weight percentage: 40% of aluminate, 60% of aluminum ferrite ore;

[0024] The slagging agent contains the following active ingredients in weight percentage: SiO 2 8%, CaO 5%, Al 2 o 3 40%, Fe 2 o 3 7%, S 0.04%, P 0.04%, and the rest are impurities.

[0025] Further, the particle size of the aluminate soil and the aluminum ferrite ore is 5-30mm.

[0026] Provide a kind of preparation method of producing described slagging agent, its steps are:

[0027] a. The raw material is broken into particles with a particle size of 20mm by a jaw crusher;

[0028] b. artificially stirring and mixing the particles in step a;

[0029] c. Put the mixed granules in step b into the kang for drying, the drying temperature is 130°C, and the drying time depends on the quantity, generally 4 hours;

[0030] d. Packing the dried granules in step c into bags is the finished product.

[0031] ...

Embodiment 3

[0033] A slagging agent, the raw materials of which are composed of the following components in weight percentage: 30% of aluminate, 70% of aluminum ferrite ore;

[0034] The slagging agent contains the following active ingredients in weight percentage: SiO 2 11%, CaO 4%, Al 2 o 3 45%, Fe 2 o 3 10%, S 0.03%, P 0.03%, and the rest are impurities.

[0035] Further, the particle size of the aluminate soil and the aluminum ferrite ore is 5-30mm.

[0036] Provide a kind of preparation method of producing described slagging agent, its steps are:

[0037] a. The raw material is broken into particles with a particle size of 5mm by a jaw crusher;

[0038] b. artificially stirring and mixing the particles in step a;

[0039] c. Put the mixed granules in step b into the kang for drying, the drying temperature is 180°C, the drying time depends on the quantity, generally 4 hours;

[0040] d. Packing the dried granules in step c into bags is the finished product.

[0041] The b...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
particle sizeaaaaaaaaaa
particle sizeaaaaaaaaaa
particle sizeaaaaaaaaaa
Login to view more

Abstract

The invention discloses a slagging constituent. Raw materials of the slagging constituent comprise the following components: by weight, 20%-40% of aluminic acid soil and 60%-80% of ferrous acid aluminum ore. The slagging constituent comprises the following effective components: by weight, 8%-15% of SiO<2>, smaller than or equal to 10% of CaO, 40%-52% of Al<2>O<3>, 7%-14% of Fe<2>O<3>, smaller than or equal to 0.05% of S, smaller than or equal to 0.05% of P, and the balance impurities. Further, particle sizes of the aluminic acid soil and the ferrous acid aluminum ore are both 5mm-30mm. The invention provides a preparation method of the slagging constituent. The preparation method of the slagging constituent comprises the steps that (a) the raw materials are broken to particles with the particle sizes of 5mm-30mm through a jaw crusher; (b) the particles in the step (a) are stirred to mix manually; (c) the particles after being mixed in the step (b) are put into a kang to dry, the drying temperature is 180 DEG C + / - 50 DEG C, the drying time is determined by the quantity, and the dry time generally is 4 hours; (d) the particles after being dried in the step (c) are packed into a bag to be an end product. The slagging constituent and the preparation method of the slagging constituent can prolong the service life of a steel ladle brusque, reduce the cost of per ton steel, and are environment-friendly.

Description

technical field [0001] The invention belongs to the technical field of smelting auxiliary materials, and in particular relates to a slagging agent and a preparation method thereof. Background technique [0002] The invention of application number: 200910103667.3 discloses a converter dephosphorization composite slagging agent, which contains the following components by weight percentage: active lime: 30-40%; rolled steel sheet: 30-40%; quartz sand: 13-18%; Soda: 11-13%; Fluorite: 0-6%; the composite slagging agent is made by crushing the above-mentioned raw materials into powder, mixing and sieving, and then pelletizing. The composite slagging agent of the present invention has a low melting point and can quickly form slagging; the composition is uniform and the performance is stable; the dephosphorization agent has a large phosphorus capacity and high dephosphorization efficiency, and can be applied to the dephosphorization of medium-high phosphorus molten iron converter; ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): C21C7/076C21C5/36
CPCC21C5/36C21C7/076Y02P10/20
Inventor 李耀峰程卓武毅胡玉冰冯亿霖
Owner 河南鹏钰集团有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products