Embodiment 1
[0018] A rubber sealing material for chemical pumps, which is made of the following components in parts by weight: styrene-butadiene rubber 62, fluorine rubber 25, polyethylene glycol 2, stearic acid 6, anti-aging agent 0.2, sulfur 1, polypropylene 8, modified Sexual filler12.
[0019] The modified filler is made of the following components in parts by weight: alumina micropowder 12, ceramic micropowder 8, white carbon black 4, manganese powder 1, attapulgite 0.2; the preparation method of the modified filler is: (1 ), 12 parts of alumina micropowder, 8 parts of ceramic micropowder and 0.1 part of attapulgite were uniformly mixed together by weight to obtain mixture 1, and the mixture 1 was heated to 255°C and pressurized to 0.5MPa, and kept After holding the pressure for 30 minutes, add 50% absolute ethanol by mass of the mixture 1, grind evenly after stirring, remove the absolute ethanol after grinding for 30 minutes, and let it stand for use; (2), mix 4 parts of white carbo...
Embodiment 2
[0024] A rubber sealing material for chemical pumps, which is made of the following components in parts by weight: styrene-butadiene rubber 68, fluorine rubber 30, polyethylene glycol 4, stearic acid 10, anti-aging agent 0.6, sulfur 4, polypropylene 12, modified Sexual filler18.
Embodiment 3
[0026] A rubber sealing material for chemical pumps, which is made of the following components in parts by weight: styrene-butadiene rubber 64, fluorine rubber 28, polyethylene glycol 3, stearic acid 8, anti-aging agent 0.4, sulfur 2, polypropylene 10, modified Sexual filler15.
[0027] Test and compare the compression set rate % of the sealing material under high temperature compression set (compression condition: 25% compression, 24h):
[0028] Table 1
[0029]
[0030] Among them, Comparative Example 1 is: a rubber sealing material for chemical pumps, made of the following components in parts by weight: styrene-butadiene rubber 68, fluororubber 30, polyethylene glycol 4, stearic acid 10, anti-aging agent 0.6, sulfur 4. Polypropylene 12, filler 18, the filler is made of the following ingredients in parts by weight: alumina micropowder 12, ceramic micropowder 8, white carbon black 4, manganese powder 1, attapulgite 0.2, directly added to the rubber sealing material...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com