Preparation method of lithium iron phosphate

A technology of lithium iron phosphate and iron phosphate, applied in chemical instruments and methods, phosphorus compounds, inorganic chemistry, etc., can solve the problem of low purity of lithium iron phosphate materials, achieve significant pH buffering effect, good fluidity, and reduce reaction costs Effect

CN112938927AActive Publication Date: 2021-06-11SVOLT ENERGY TECHNOLOGY CO LTD
4 Cites 3 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Publication Date
2021-06-11

Smart Images

  • Figure 1
    Figure 1
  • Figure 2
    Figure 2
Patent Text Reader

Abstract

The invention provides a preparation method of lithium iron phosphate. The preparation method comprises the following steps: S1, mixing an iron source, a phosphorus source and a pH buffer agent to obtain a mixed solution; S2, carrying out hydrothermal reaction on the mixed solution to obtain an iron phosphate precursor; and S3, mixing and sintering the iron phosphate precursor, a lithium source and a carbon source to obtain lithium iron phosphate. The pH buffer agent comprises a compound containing carboxylate radicals. The pH buffer agent containing carboxylate radicals can play a complexing role and also has an extremely remarkable pH buffering role, and is crucial for controlling the stability of the whole reaction system, so that the phase of the final lithium iron phosphate is simplified, the product is stable in performance, good in fluidity and high in conductivity, and further, the lithium iron phosphate is used as a positive electrode material to make the battery have excellent electrical properties such as conductivity and rate capability. The preparation method is simple, energy is saved, and the reaction cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to the technical field of synthesis of lithium iron phosphate, in particular to a preparation method of lithium iron phosphate. Background technique

[0002] As a chemical raw material, iron phosphate has a wide range of applications, and because of its unique electrochemical properties, it plays a huge role in the field of lithium-ion battery materials. In the field of battery materials, iron phosphate has become an ideal electrode material for electric vehicle batteries because it can be directly used as an intercalation electrode for lithium-ion batteries, has high thermal stability and good electrochemical cycle performance.

[0003] At present, the traditional process uses ammonium dihydrogen phosphate, ferrous oxalate and lithium carbonate for physical mixing and high-temperature calcination to synthesize lithium iron phosphate. Irregular, gradually replaced by other methods.

[0004] In fact, there are many synthetic tech...

Examples

preparation example Construction

[0034] In a typical embodiment of the present application, a preparation method of lithium iron phosphate is provided, the preparation method comprising: step S1, mixing iron source, phosphorus source, and pH buffer to obtain a mixed solution; step S2, The mixed solution is subjected to a hydrothermal reaction to obtain an iron phosphate precursor; step S3, the iron phosphate precursor, lithium source, and carbon source are mixed and sintered to obtain lithium iron phosphate, wherein the pH buffer agent includes a carboxylate-containing compound.

[0035] The pH buffer containing carboxylate can not only act as a complexing effect, but also have an extremely significant pH buffering effect, which is very important for controlling the stability of the entire reaction system. On the one hand, the pH buffering agent can complex with the iron ions in the mixed liquid, thereby greatly inhibiting the premature precipitation of iron ions in the form of iron hydroxide, thereby reducing...

Embodiment 1

[0050] According to 1.05:1, take by weighing 1.05 parts of ferric chloride and 1 part of phosphoric acid to be mixed with the first solution, the molar concentration of ferric chloride in this first solution is 5mol / L, then take by weighing monochloroacetic acid (one The volume ratio of the mass of chloroacetic acid to the first solution is 2g:1L), ammonium acetate (the volume ratio of the mass of ammonium acetate to the first solution is 2g:1L), and sodium dodecylbenzenesulfonate (dodecylbenzenesulfonate The volume ratio of sodium phthalate to the first solution is 0.5g: 1L) into the first solution, weigh potassium hydrogen phthalate and add it into the first solution to make 0.04mol / L, and then add sodium hydroxide (0.5mol / L) and hydrochloric acid (0.5mol / L) to adjust the pH of the system to 3.5 to obtain a mixed solution.

[0051] Then raise the temperature of the mixed solution to 70°C, control the rotational speed at 1500r / min, continuously control the temperature at 70°C...

Embodiment 2

[0053] According to 1.03:1, take by weighing 1.03 parts of ferric nitrate and 1 part of phosphoric acid to be mixed with the first solution, the molar concentration of ferric chloride in this first solution is 5mol / L, then take by weighing monochloroacetic acid (monochloroacetic acid The volume ratio of the mass to the first solution is 3g:1L), ammonium acetate (the volume ratio of the mass of ammonium acetate to the first solution is 4g:1L), and sodium dodecylbenzenesulfonate (sodium dodecylbenzenesulfonate The volume ratio to the first solution is 1g:1L) into the first solution, weigh potassium hydrogen phthalate and add it to the first solution to make 0.04mol / L, and then use sodium hydroxide (0.5mol / L) and hydrochloric acid ( 0.5mol / L) to adjust the pH of the system to 2.8 to obtain a mixed solution.

[0054] Then raise the temperature of the mixed solution to 90°C, control the rotating speed to 2000r / min, continuously control the temperature to 70°C, control the pH value ...