Composite powdery calcium sulphate sewage treating agent and preparation method thereof
A sewage treatment agent, calcium sulfate technology, applied in the direction of flocculation/sedimentation water/sewage treatment, sterilization/microdynamic water/sewage treatment, complex/solubilizer treatment, etc., can solve the problem of insufficient polymerization degree and complicated operation process , water turbidity and other problems, to achieve the effect of excellent coagulation performance, low operating cost, and tight alum flowers
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] Mix 5 parts by weight of 80 mesh malic acid with 3 parts by weight of 80 mesh tartaric acid for 40 minutes, then add 60 parts by weight of 80 mesh calcium sulfate, mix for 50 minutes, then add 10 parts by weight of 80 mesh magnesium carbonate, mix for 40 minutes, and then add 10 The weight part of 80 mesh calcium carbonate was mixed for 40 minutes, then 10 weight parts of 80 mesh iron trichloride was added, mixed for 40 minutes, then 10 weight parts of 80 mesh calcium oxide was added and mixed for 40 minutes, and then 2 weight parts of 80 mesh polyacrylamide were added, Mix for 120 minutes and that's it.
Embodiment 2
[0029] Mix 7 parts by weight of 200 mesh malic acid with 4 parts by weight of 200 mesh tartaric acid for 50 minutes, then add 65 parts by weight of 200 mesh calcium sulfate, mix for 90 minutes, then add 12 parts by weight of 200 mesh magnesium carbonate, mix for 50 minutes, then add 15 The weight part of 200 mesh calcium carbonate was mixed for 50 minutes, then 15 weight parts of 200 mesh iron trichloride was added, mixed for 50 minutes, then 15 weight parts of 200 mesh calcium oxide was added and mixed for 50 minutes, then 2.5 weight parts of 200 mesh polyacrylamide was added, Mix for 130 minutes and that's it.
Embodiment 3
[0031] Mix 10 parts by weight of 400 mesh malic acid with 5 parts by weight of 400 mesh tartaric acid for 60 minutes, then add 70 parts by weight of 400 mesh calcium sulfate, mix for 120 minutes, then add 15 parts by weight of 400 mesh magnesium carbonate, mix for 60 minutes, and then add 20 The weight part of 400 mesh calcium carbonate was mixed for 60 minutes, then 20 weight parts of 400 mesh iron trichloride was added, mixed for 60 minutes, then 20 weight parts of 400 mesh calcium oxide was added and mixed for 60 minutes, and then 3 weight parts of 400 mesh polyacrylamide was added, Mix for 150 minutes and that's it.
[0032] The technical index of embodiment 1-3 is as shown in table 1:
[0033] Table 1:
[0034]
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com