Efficient compound powdered sewage treatment agent and preparation method thereof
A kind of sewage treatment agent and treatment agent technology, applied in the direction of water/sludge/sewage treatment, flocculation/sedimentation water/sewage treatment, sterilization/microdynamic water/sewage treatment, etc., can solve the problem that the recovery rate can only reach 60- 70%, the removal rate can only reach 60-70%, can not meet the requirements of environmental protection and recycling, etc., to achieve the effect of excellent coagulation performance, high recovery rate, and easy production
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] 7 parts by weight of 80-mesh tartaric acid and 1 part by weight of 80-mesh ursodeoxycholic acid were mixed for 50 minutes, then 1 part by weight of 80-mesh 2-phenylthio-5-propionylphenylacetic acid was added, mixed for 50 minutes, and then 60 80 mesh calcium sulfate, mixed for 50 minutes, then added 10 weight parts of 80 mesh magnesium carbonate, mixed for 40 minutes, then added 10 weight parts of 80 mesh calcium carbonate and mixed for 40 minutes, then added 10 weight parts of 80 mesh ferric chloride, Mix for 40 minutes, then add 10 parts by weight of 80-mesh calcium oxide and mix for 40 minutes, then add 10 parts by weight of 80-mesh borax, and mix for 120 minutes.
Embodiment 2
[0021] 7 parts by weight of 200 mesh tartaric acid and 1.5 parts by weight of 200 mesh ursodeoxycholic acid were mixed for 90 minutes, then 1.6 parts by weight of 200 mesh 2-phenylthio-5-propionylphenylacetic acid was added, mixed for 90 minutes, and then 70 200 meshes of calcium sulfate in parts by weight, mixed for 90 minutes, then 20 parts by weight of 200 meshes of magnesium carbonate were added, mixed for 50 minutes, 20 parts by weight of 200 meshes of calcium carbonate were added and mixed for 50 minutes, then 20 parts by weight of 200 meshes of ferric chloride were added, Mix for 50 minutes, then add 20 parts by weight of 200-mesh calcium oxide and mix for 50 minutes, then add 20 parts by weight of 200-mesh borax, and mix for 130 minutes.
Embodiment 3
[0023] 8 parts by weight of 400 mesh tartaric acid and 2 parts by weight of 400 mesh ursodeoxycholic acid were mixed for 120 minutes, then 2 parts by weight of 400 mesh 2-phenylthio-5-propionyl phenylacetic acid were added, mixed for 120 minutes, and then 70 400 mesh calcium sulfate in parts by weight, mixed for 120 minutes, then added 15 parts by weight of 400 mesh magnesium carbonate, mixed for 60 minutes, then added 20 parts by weight of 400 mesh calcium carbonate and mixed for 60 minutes, then added 20 parts by weight of 400 mesh ferric chloride, Mix for 60 minutes, then add 20 parts by weight of 400-mesh calcium oxide and mix for 60 minutes, then add 16 parts by weight of 400-mesh borax, and mix for 150 minutes.
[0024] The technical index of embodiment 1-3 is as shown in table 1:
[0025] Table 1:
[0026] Example 1 Example 2 Example 3 Density g / cm 3 (20℃)
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
concentration | aaaaa | aaaaa |
clearance rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com