Tungsten-strengthened wear-resistant submerged-arc overlaying welding flux-cored wire
A technology of submerged arc surfacing and flux-cored welding wire, which is applied in welding medium, welding equipment, welding/cutting medium/material, etc., and can solve problems such as inability to meet
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach
[0028] The second specific implementation mode, as attached figure 1 shown.
[0029] A tungsten-enhanced submerged-arc surfacing flux-cored welding wire, comprising an H10 low-carbon steel hollow welding wire and a powder flux core arranged in the hollow welding wire, the proportion of the powder flux core being: the high-carbon ferrochrome 50%, 12% of the tungsten powder, 8% of the ferromanganese deoxidizer, and 30% of the iron powder. The filling rate is 45%. The average hardness of the surfacing layer of flux-cored wire is HRC63.
PUM
Property | Measurement | Unit |
---|---|---|
hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com