Processing method of water washable wool fabric
A processing method and fabric technology, which is applied in the field of fabric processing, can solve problems such as non-washable, achieve good smoothness, strong clustering, and improve the effects of flying hair and broken ends
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2011-11-02
Abstract
Description
technical field
[0001] The invention relates to a processing method of a fabric, in particular to a processing method of a wool fabric. Background technique
[0002] Due to the structural characteristics of wool covered by natural scales, it is easy to shift the wool fiber and cause felting phenomenon after rubbing and kneading under wet conditions. As a result, the finished product made of wool fabric shrinks and deforms too much after washing, which affects the service life. Dry cleaning costs are much higher than water washing. At present, most of the existing wool worsted fabrics indicate on their labels that they can only be dry-cleaned and not washed.
[0003] Therefore this field needs to provide a kind of processing method of washable wool fabric. Contents of the invention
[0004] The purpose of the present invention is to provide a kind of processing method of washable wool fabric for people.
[0005] Another object of the present invention is to provide a wa...
Examples
Embodiment 1
[0043] Embodiment 1 The processing method of washable wool fabric
[0044] Washable wool fabric, using 18-20μm wool, fine wool with an average length of more than 88 mm and an average strength of more than 40 cattle per ktex, improved on the basis of traditional techniques. It is made by ply yarn interweaving and post-finishing technology.
[0045] A method for processing a washable wool fabric, comprising the steps of:
[0046] Basic process: dyeing-rewashing-strip mixing-combing-carding-roving-spinning-winding-doubling-twisting-steaming-warping-weaving-milling-drying-shearing-machine washable - tweed - finished product. The raw material is fine wool with a fiber fineness of 18-20 μm, an average length of more than 88 mm, and an average strength of more than 40 cattle per ktex. During the dyeing process, leveling agent 1227, wool oil SPINTEX-DSC, and antistatic agent 1827 are added. The dyeing is boiled and dyed for 24 hours at a temperature of 90 degrees in a dyeing vat. ...