[0013] Embodiment 1 adopts the following steps:
[0014] A) take the sample of hardened fur cultural relics, put it into deionized water and fully immerse it for 24 hours;
[0015] B) Immerse the treated sample in step A) in a water bath containing 50% ethanol aqueous solution for treatment, the temperature of the water bath is 20 degrees, and the time is 1 hour;
[0016] C) Soak the sample obtained in step B) in a water bath containing a softening agent, the temperature of the water bath is 20-30 degrees, and soften for 0.5h; the content of each component of the softening agent is calculated by mass fraction: urea 1%, sodium chloride 4 %, polyethylene glycol 5%, ethanol 45%, deionized water 45%;
[0017] D) The sample treated in step C) is completely immersed in a water bath containing a mass fraction of 50% ethanol aqueous solution again for treatment, the temperature of the water bath is 20 degrees, and the time is 1h;
[0018] E) After taking out the sample treated in st...
Embodiment 2
[0020] Embodiment 2 adopts the following steps:
[0021] A) take the sample of hardened fur cultural relics, put it into deionized water and fully immerse it for 24 hours;
[0022] B) Immerse the treated sample in step A) in a water bath containing 50% ethanol aqueous solution for treatment, the temperature of the water bath is 30 degrees, and the time is 1 hour;
[0023] C) Soak the sample obtained in step B) in a water bath containing a softening agent, the temperature of the water bath is 30 degrees, and soften for 1h; the content of each component of the softening agent is calculated by mass fraction: urea 3%, sodium chloride 4%, poly Ethylene glycol 3%, ethanol 45%, deionized water 45%;
[0024] D) The sample treated in step C) is completely immersed in a water bath containing a mass fraction of 50% ethanol aqueous solution again for treatment, the temperature of the water bath is 30 degrees, and the time is 1h;
[0025] E) After taking out the sample treated in step D)...
Embodiment 3
[0027] Embodiment 3 adopts the following steps:
[0028] A) take the sample of hardened fur cultural relics, put it into deionized water and fully immerse it for 24 hours;
[0029] B) Immerse the treated sample in step A) in a water bath containing 50% ethanol aqueous solution for treatment, the temperature of the water bath is 40 degrees, and the time is 1 hour;
[0030] C) soak the sample obtained in step B) in a water bath containing a softener, the temperature of the water bath is 40 degrees, and soften for 1h; the content of each component of the softener is calculated by mass fraction: urea 3%, sodium chloride 4%, poly Ethylene glycol 3%, ethanol 45%, deionized water 45%;
[0031] D) The sample treated in step C) is completely immersed in a water bath containing a mass fraction of 50% ethanol aqueous solution again for treatment, the temperature of the water bath is 40 degrees, and the time is 1h;
[0032] E) After taking out the sample treated in step D), take a glyce...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com