A kind of dyeing method of willow made of wicker
A dyeing method and wicker technology, which is applied in the field of willow dyeing, can solve the problems of easy fading and low dyeing rate, and achieve the effects of small damage, increased dyeing rate, and mild treatment environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0016] The invention relates to a dyeing method of willow made of wicker. The dyeing method is to fumigate the wicker made of wicker treated with a coupling agent under low pressure and high temperature, and then dye with basic dyes.
[0017] The coupling agent is a silane coupling agent.
[0018] The wicker made of wicker treated with the coupling agent is as follows: soak the wicker made of wicker in a potassium chloride solution with a mass concentration of 0.2% for 2 hours, then take it out, dry it until the water content reaches 18%, and then put it in the mass concentration Soak in an aqueous solution of silane coupling agent with a concentration of 0.22% for 3 hours, then dry with hot air at 60°C until the water content reaches 15%.
[0019] The low pressure is 0.03MPa.
[0020] The high temperature is 115°C.
[0021] The fumigation treatment is as follows: use water vapor and chlorine gas to mix at a mass ratio of 100:1 to fumigate wicker made of wicker for 10 minute...
Embodiment 2
[0026] The invention relates to a dyeing method of willow made of wicker. The dyeing method is to fumigate the wicker made of wicker treated with a coupling agent under low pressure and high temperature, and then dye with basic dyes.
[0027] The coupling agent is a silane coupling agent.
[0028] The wicker made of wicker treated with the coupling agent is as follows: soak the wicker made of wicker in a potassium chloride solution with a mass concentration of 0.5% for 2 hours, then take it out, dry it until the water content reaches 20%, and then put it in the mass concentration Soak in an aqueous solution of silane coupling agent with a concentration of 0.24% for 3 hours, then dry with hot air at 60°C until the water content reaches 18%.
[0029] The low pressure is 0.05MPa.
[0030] The high temperature is 118°C.
[0031] The fumigation treatment is as follows: use water vapor and chlorine gas to mix at a mass ratio of 100:1 to fumigate wicker made of wicker for 12 minute...
Embodiment 3
[0036] The invention relates to a dyeing method of willow made of wicker. The dyeing method is to fumigate the wicker made of wicker treated with a coupling agent under low pressure and high temperature, and then dye with basic dyes.
[0037] The coupling agent is a silane coupling agent.
[0038] The wicker made of wicker treated with the coupling agent is as follows: soak the wicker made of wicker in a potassium chloride solution with a mass concentration of 0.3% for 2 hours, then take it out, dry it until the water content reaches 18-20%, and then dry it until the water content reaches 18-20%. Soak in an aqueous solution of silane coupling agent with a mass concentration of 0.23% for 3 hours, and dry with hot air at 60°C until the water content reaches 16%.
[0039] The low pressure is 0.04MPa.
[0040] The high temperature is 116°C.
[0041] The fumigation treatment is as follows: use water vapor and chlorine gas to mix at a mass ratio of 100:1 to fumigate wicker made of...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com