Preparation method of curb stone with high degree of closenness
A technology of curb stone and density, which is applied in the field of preparation of high-density curb stone, which can solve the problems of curb stone not having water permeability, curb stone not having water permeability, blocking drainage channels, etc., and achieving improved compactness and strong weather resistance , the effect of improving the service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] Embodiment 1: a kind of preparation method of high density calculus, comprises the following steps:
[0021] Collect granite scraps, calcinate them at a high temperature of 1000-1100°C, then quench them and roll them into powder under a press, and then undergo wet ball milling to obtain granite powder with a particle size of 60-80 mesh;
[0022] Take 5 parts of calcium dihydrogen phosphate, 5 parts of metakaolin, 10 parts of cement, 10 parts of stone powder, 20 parts of quartz sand, 5 parts of acrylic acid, 1 part of inorganic pigment, 0.2 part of waterproofing agent and 1 part of polypropylene short fiber;
[0023] Add 10-20% water and 20% granite powder of the total weight of raw materials, and then use a mixer to stir and mix until the raw materials are dissolved and gelled;
[0024] Pour the gelled material into the curbstone mold, spread it out, and then spray the coagulant, and finally pour the concrete and send it to the drying room, and steam it at 180-200°C for...
Embodiment 2
[0028] Embodiment 2: a kind of preparation method of high density calculus, comprises the following steps:
[0029] Collect granite scraps, calcinate them at a high temperature of 1000-1100°C, then quench them and roll them into powder under a press, and then undergo wet ball milling to obtain granite powder with a particle size of 60-80 mesh;
[0030] Take 15 parts of calcium dihydrogen phosphate, 15 parts of metakaolin, 30 parts of cement, 25 parts of stone powder, 40 parts of quartz sand, 15 parts of acrylic acid, 2 parts of inorganic pigment, 0.8 part of waterproofing agent and 3 parts of polypropylene short fiber;
[0031] Add 10-20% water and 20% granite powder of the total weight of raw materials, and then use a mixer to stir and mix until the raw materials are dissolved and gelled;
[0032] Pour the gelled material into the curbstone mold, spread it out, and then spray the coagulant, and finally pour the concrete and send it to the drying room, and steam it at 180-200°...