A technology of concrete block and forming process, which is applied in the field of concrete processing, can solve the problems of strength and impermeability reduction, easy cracking, and difficulty in targeting methods, etc., and achieve the effects of improving safety, improving impermeability, and increasing strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0045] see figure 1 , a pre-embedded concrete block forming process, comprising the following steps:
[0046] S1, weigh the following raw materials according to parts by weight: 20-50 parts of cement, 5-10 parts of slag powder, 4-8 parts of fly ash, 10-15 parts of crushed stone, 15-20 parts of quicklime, 10-15 parts of water parts and 1-5 parts of waterproofing agent;
[0047] S2. After mixing and stirring the above-mentioned raw materials evenly, a slurry is obtained, and a pre-embedded mold is prepared, and a plurality of evenly distributed pre-embedded sinkers are pre-adsorbed in its inner side;
[0048] S3. The slurry is poured into the embedded mold, and then pressed to obtain a semi-finished product, and the semi-finished product is subjected to steam curing;
[0049] S4. After the maintenance, take out the semi-finished product, and separate the part of the pre-embedded sinker extending out of the semi-finished product for recycling;
[0050] S5. Polish the surface o...
Embodiment 2
[0062] The rest of the parts are the same as those in Example 1. The difference is that the adsorption hemisphere 5 is made of a ferromagnetic material, and a corresponding magnetic layer is provided on the inner top of the upper mold 1 to adsorb the adsorption hemisphere 5. After cooling down, remove the formwork and take out the block. At this time, the sensing hemisphere 3 and the adsorption hemisphere 5 are not separated. The anti-seepage powder can be protected to prevent leakage during transportation, and the sensing hemisphere can be separated by temporary heating at the construction site. Although the hemisphere 3 and the adsorption hemisphere 5 are troublesome in operation, they can ensure the integrity of the anti-seepage powder.
[0063] The invention can realize that when the block is formed, a plurality of pre-embedded sinkers can be adhered to the pre-embedded mold in advance, and then the mixed concrete slurry is poured into the mold for forming. At this time, th...
PUM