Dexamethasone slow-release microsphere for injection in glass body
A technology of dexamethasone and sustained-release microspheres, which is applied in microcapsules, medical preparations with inactive ingredients, and medical preparations containing active ingredients, etc. Inappropriate path and other problems, achieve good stability and reconstitution ability, facilitate clinical application, and reduce the effect of drug burden
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2019-10-29
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure 1 
Figure 2 
Figure 3
Abstract
Description
technical field
[0001] The invention belongs to the field of pharmaceutical preparations, in particular to a dexamethasone slow-release microsphere, which can be used for intravitreal injection.
[0002] technical background
[0003] Dexamethasone is a glucocorticoid drug with various pharmacological effects such as anti-inflammatory, anti-allergic and immune suppression. It is widely used in various diseases, such as autoimmune diseases, asthma, allergies, inflammation, and dermatology and ophthalmology diseases. At present, ophthalmic drugs are mainly used in the treatment of iridocyclitis, iritis, keratitis, allergic conjunctivitis, blepharitis, dacryocystitis and other anterior segment diseases in clinical practice. Its commercially available dosage forms are mainly eye drops, eye ointments, and suspensions. These traditional dosage forms are restricted by factors such as corneal barrier, tear dilution, and nasolacrimal duct elimination. They have weak retention capacity,...
Examples
Embodiment 1
[0038] Dexamethasone 300mg
[0039] Ester-terminated glycolide-lactide copolymer ( RG 502) 400mg
[0040] Carboxyl-terminated glycolide-lactide copolymer ( RG 502 H) 0mg
[0041] (1) take by weighing the dexamethasone of formula quantity, ester group terminal glycolide lactide copolymer and carboxyl terminal glycolide lactide copolymer, be dissolved in 1.75ml dichloromethane and dimethyl sulfoxide volume ratio is In the mixed solvent of 5:2, make the inner oil phase for standby;
[0042] Weigh polyvinyl alcohol and add water, and prepare an aqueous solution with a mass concentration of 1% at 60-80° C., which is used as the external aqueous phase I for subsequent use;
[0043] Weigh polyvinyl alcohol and add water to prepare an aqueous solution with a mass concentration of 0.2% at 60-80°C, which will be used as the external aqueous phase II for later use;
[0044] (2) Add the above-mentioned inner oil phase into 300ml of outer water phase I, and emulsify at 1700rpm for...
Embodiment 2
[0049] Dexamethasone 300mg
[0050] Ester-terminated glycolide-lactide copolymer ( RG 502) 0mg
[0051] Carboxyl-terminated glycolide-lactide copolymer ( RG 502 H) 400mg
[0052] (1) take by weighing the dexamethasone of formula quantity, ester group terminal glycolide lactide copolymer and carboxyl terminal glycolide lactide copolymer, be dissolved in 1.75ml dichloromethane and dimethyl sulfoxide volume ratio is In the mixed solvent of 5:2, make the inner oil phase for standby;
[0053] Weigh polyvinyl alcohol and add water, and prepare an aqueous solution with a mass concentration of 1% at 60-80° C., which is used as the external aqueous phase I for subsequent use;
[0054] Weigh polyvinyl alcohol and add water to prepare an aqueous solution with a mass concentration of 0.2% at 60-80°C, which will be used as the external aqueous phase II for later use;
[0055] (2) Add the above-mentioned inner oil phase into 300ml of outer water phase I, and emulsify at 1700rpm for...
Embodiment 3
[0060] Dexamethasone 150mg
[0061] Ester-terminated glycolide-lactide copolymer ( RG 502) 250mg
[0062] Carboxyl-terminated glycolide-lactide copolymer ( RG 502 H) 250mg
[0063] (1) take by weighing the dexamethasone of formula quantity, ester group terminal glycolide lactide copolymer and carboxyl terminal glycolide lactide copolymer, be dissolved in 1.75ml dichloromethane and dimethyl sulfoxide volume ratio is In the mixed solvent of 5:2, make the inner oil phase for standby;
[0064] Weigh polyvinyl alcohol and add water, and prepare an aqueous solution with a mass concentration of 1% at 60-80° C., which is used as the external aqueous phase I for subsequent use;
[0065] Weigh polyvinyl alcohol and add water to prepare an aqueous solution with a mass concentration of 0.2% at 60-80°C, which will be used as the external aqueous phase II for later use;
[0066] (2) Add the above-mentioned inner oil phase into 300ml of outer water phase I, and emulsify at 2500rpm f...