Method for reinforcing fiber, fastening down and preventing moult in duck goose down making fur process
A technology of duck and goose down and fiber, which is applied in special leather manufacturing, small raw hide/large raw hide/leather/fur treatment, small raw hide/large raw hide/leather skin/fur chemical treatment, etc. It can solve the problem of poor softness and easy hair loss , the product cannot be widely used, etc., to achieve the effect of high tensile strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Embodiment 1: carry out according to the following steps:
[0020] The first step, anti-corrosion treatment: select the peeled 600-900 square centimeters of duck and goose down skin, put the quilt down, stretch it on the table, and apply 150 grams of industrial salt to each skin evenly on the skin board Then use leather antifungal agent and No. 3 antifungal agent, mix each amount of 0.2 grams and spray or smear on the leather board. The model of leather antifungal agent is CJ-11 type leather antifungal agent, leather antifungal agent CJ -11 Production unit: Guangdong Dongguan Changjiang Chemical Industry Company. No. 3 antifungal agent production unit: Beijing Aibole Leather Chemical Co., Ltd.
[0021] The second step, softening and soaking in water: adopt a container with a volume of 2000 liters, which is a kind of chute; inject 1500 liters of clear water into the container, and prepare the liquid medicine according to the amount of water in the container. The formula...
Embodiment 2
[0031] Embodiment 2: carry out according to the following steps:
[0032] The first step, anti-corrosion treatment: peel off 600-900 square centimeters of duck and goose down skin, put the quilt down, stretch it on the table, and spread 150 grams of industrial salt on each skin evenly on the skin board , and then use leather antifungal agent and No. 3 antifungal agent, mix the amount of 0.2 grams each and spray on the leather board,
[0033] The second step, softening and soaking in water: adopt a container with a volume of 2000 liters, which is a kind of chute; inject 1500 liters of clear water into the container, and prepare the liquid medicine according to the amount of water in the container. The formula is: add 12g of industrial salt and formaldehyde per liter of water 0.3g, No. 3 antifungal agent 3 g, after the preparation of the above ratio of agents: industrial salt 18000g, formaldehyde 450g, No. 3 antifungal agent 4500g, mix and pour into the water in the container, p...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com