Novel bone surgery fixing system and method of use thereof and polyurethane applied therein
A fixation system and orthopedic surgery technology, applied in fractures, medical science, surgery, etc., can solve the problems of difficulty in transmitting X-rays, inability to detach, and high cost, achieving superior cost performance, no infection, and ideal effects.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] Mixture B is composed of 90 parts by weight of polyether polyol, 0.3 parts by weight of dimethylcycloethylamine, 2 parts by weight of silicone stabilizer, 7.7 parts by weight of water and 141B, first take 250ml of compound A liquefied MDI Mix with 250ml of mixture B, stir and mix well, fill the polyurethane slurry into the interlayer of two cotton cavities, push it evenly with a roller, and spread it out. After about 1 to 2 minutes, the polyurethane will change from liquid Enter the solid-state softening section. At this time, wrap the two cotton cavities on the desired fixed part. After pulling up the zipper, shape it by hand to make it close to the desired fixed part. The injured part of the patient remains motionless for 8~ After 8.5 minutes, the shaping is completed. At this time, the polyurethane enters the solid hardening section, and after another 20 minutes, the shaping of the orthopedic surgical fixation system is completed, and a flexible fixation system is obt...
Embodiment 2
[0048] Mixture B is composed of 93 parts by weight of polyether polyol, 1 part by weight of dimethylethanolamine, 4 parts by weight of silicone stabilizer, 2 parts by weight of water and 141B, first take 250ml of compound A liquefied MDI and 250ml The mixture B was mixed, and the rest of the operation steps were the same as in Example 1, and finally a flexible fixing system was obtained.
Embodiment 3
[0050] Mixture B consists of 90 parts by weight of polyether polyol, 1 part by weight of dimethylethanolamine, 4 parts by weight of silicone stabilizer, 5 parts by weight of water and 141B, first take 250ml of compound A liquefied MDI and 500ml The mixture B was mixed, and the rest of the operating steps were the same as in Example 1, and finally a rigid fixed system was obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com