A kind of artificial rockery and artificial technology, which is applied in the field of artificial rockery and its preparation, can solve the problems of endangering the health of operators, pollution of the surrounding environment, and waste of raw materials, and achieve scientific and reasonable raw material formulas, improved ecological performance, and rich nutrients. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Example Embodiment
[0039] Example 1: An artificial rockery comprising the following raw material components in parts by weight: 50 parts of cement, 1 part of wood chips, 10 parts of fertilizer and 60 parts of water.
[0040] The water absorption detection experiment of the artificial rockery of this embodiment:
[0041] Experimental method: Take the artificial rockery prepared in Example 1 and the commercially available ordinary natural absorbent stone, weigh the artificial rockery and natural absorbent stone, and soak them in water for one hour, then put the artificial rockery and natural absorbent stone together Immediately after the surface is wiped dry, weigh the artificial rockery and natural absorbent stone, and calculate the water absorption of each experimental product. The calculation formula for water absorption is as follows:
[0042] Water absorption = (weight after water absorption-weight before water absorption) / weight before water absorption
[0043] The experimental results are shown i...
Example Embodiment
[0048] Example 2: An artificial rockery comprising the following raw material components in parts by weight: 6.345 parts of cement, 6.345 parts of wood chips, 1 part of slow-release fertilizer, and 13.13 parts of water.
[0049] A preparation method of artificial rockery includes the following steps:
[0050] Step 1: Prepare the mold: the mold includes an outer mold and an inner mold;
[0051] Step 2: Pouring: Weigh the cement, wood chips, slow-release fertilizer and water according to the above parts by weight to prepare a mixed raw material, introduce the mixed raw material into the mold, insert the vibrating rod into the mixed raw material and vibrate evenly, into the mold Make up the mixed raw materials to be flush with the mold opening;
[0052] Step 3: Demoulding: Place the casted mold in step 2 at room temperature until the mixed raw materials solidify and form a crude artificial rockery product. Separate the outer mold from the inner mold in turn, and then separate the inner m...
Example Embodiment
[0062] Example 3: An artificial rockery comprising the following raw material components in parts by weight: 30 parts of cement, 5 parts of granular aquatic mud, 15 parts of wood chips, and 50 parts of water.
[0063] A preparation method of artificial rockery includes the following steps:
[0064] Step 1: Prepare the mold: the mold includes an outer mold and an inner mold;
[0065] Step 2: Pouring: Weigh cement, sawdust, granular aquatic mud and water according to the above weight parts to prepare mixed raw materials, introduce the mixed raw materials into the mold, insert the vibrating rod into the mixed raw materials and vibrate evenly, to the mold Fill up the mixed raw materials to be flush with the mold opening;
[0066] Step 3: Demoulding: Place the casted mold in step 2 at room temperature until the mixed raw materials solidify and form a crude artificial rockery product. Separate the outer mold from the inner mold in turn, and then separate the inner mold from the crude artifi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap