Embodiment 1
[0020] An aerosol for new energy vehicles, comprising the following components in parts by weight: 35 parts of polyether, 15 parts of ethyl acetate, 2 parts of sodium tetraborate, 8 parts of ethylene glycol, and 2 parts of sodium fatty acid methyl ester sulfonate , xylitol ester 2 parts, glycerin 2 parts.
[0021] The preparation method of the above-mentioned aerosol for new energy vehicles is carried out according to the following steps:
[0022] (1) Under normal temperature conditions, according to parts by weight, get 35 parts of polyether, 15 parts of ethyl acetate, 2 parts of sodium tetraborate, 8 parts of ethylene glycol, add in the magnetic grinder, grind 20min;
[0023] (2) Transfer the ground mixture of step (1) into a new container, add 2 parts of sodium fatty acid methyl ester sulfonate, 2 parts of xylitol ester, and 2 parts of glycerin, and stir evenly to prepare.
Embodiment 2
[0025] An aerosol for new energy vehicles, comprising the following components in parts by weight: 20 parts of polyether, 10 parts of ethyl acetate, 1 part of sodium tetraborate, 3 parts of ethylene glycol, and 1 part of sodium fatty acid methyl ester sulfonate , 1 part of sorbitol monopalmitate, 1 part of polyalkylene glycol.
[0026] The preparation method of the above-mentioned aerosol for new energy vehicles is carried out according to the following steps:
[0027] (1) Under normal temperature conditions, according to parts by weight, get 20 parts of polyether, 10 parts of ethyl acetate, 1 part of sodium tetraborate, 3 parts of ethylene glycol, add in the magnetic grinder, grind 10min;
[0028] (2) Transfer the ground mixture of step (1) into a new container, add 1 part of sodium fatty acid methyl ester sulfonate, 1 part of sorbitol monopalmitate, and 1 part of polyalkylene glycol, stir evenly, and prepare become.
Embodiment 3
[0030] An aerosol for new energy vehicles, comprising the following components in parts by weight: 50 parts of polyether, 20 parts of ethyl acetate, 3 parts of sodium tetraborate, 10 parts of ethylene glycol, and 3 parts of sodium fatty acid methyl ester sulfonate , 3 parts of lauric acid, 3 parts of ethanol.
[0031] The preparation method of the above-mentioned aerosol for new energy vehicles is carried out according to the following steps:
[0032] (1) Under normal temperature conditions, according to parts by weight, get 50 parts of polyether, 20 parts of ethyl acetate, 3 parts of sodium tetraborate, 10 parts of ethylene glycol, add in the magnetic grinder, grind 30min;
[0033] (2) Transfer the ground mixture of step (1) into a new container, add 3 parts of sodium fatty acid methyl ester sulfonate, 3 parts of lauric acid, and 3 parts of ethanol, and stir evenly to prepare.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com