A system reconstruction and soil technology, applied in the field of environmental restoration, can solve problems such as environmental hazards, lack of management methods and treatment and disposal technologies, and achieve the effects of accelerating construction, facilitating plant growth, and ensuring safe utilization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] This embodiment provides a method for reconfiguring the mine soil system, including the following steps:
[0025] (1) Use a rotary tiller to plow the hardened soil on the surface of the mine to a depth of 5cm, and collect the hardened soil, which needs to be collected after passing through a 2mm sieve to remove large-size gravel;
[0026] (2) Mix municipal sludge, straw, and biochar with a water content of 80% according to the material mass ratio of 100:20:9, and the fermentation period is 35 days to obtain stabilized sludge;
[0027] (3) The step of covering the mine with a thickness of 20cm after cleaning the hardened soil (2) Stabilizing sludge;
[0028] (3) On the basis of covering the stabilized sludge, cover the loam soil with a thickness of 25cm;
[0029] (4) On the basis of covering the loam, cover the hardened soil collected in step (1) with a thickness of 10cm;
[0030] (5) On the basis of covering the hardened soil, cover the stabilized sludge with a thickn...
Embodiment 2
[0034] This embodiment provides a method for reconfiguring the mine soil system, including the following steps:
[0035] (1) Use a rotary tiller to plow the hardened soil on the surface of the mine to a depth of 12cm, and collect the hardened soil, which needs to be collected after passing through a 2mm sieve to remove large-size gravel;
[0036] (2) Mix municipal sludge, straw, and biochar with a water content of 80% according to the material mass ratio of 100:20:9, and the fermentation period is 40 days to obtain stabilized sludge;
[0037] (3) The step of covering the mine with a thickness of 23cm after cleaning the hardened soil (2) Stabilizing sludge;
[0038] (3) On the basis of covering the stabilized sludge, cover the loam with a thickness of 22cm;
[0039] (4) On the basis of covering loam, cover the hardened soil collected in step (1) with a thickness of 12cm;
[0040] (5) On the basis of covering the hardened soil, cover the stabilized sludge with a thickness of 1...
Embodiment 3
[0044] This embodiment provides a method for reconfiguring the mine soil system, including the following steps:
[0045] (1) Use a rotary tiller to plow the hardened soil on the surface of the mine to a depth of 20cm, and collect the hardened soil, which needs to be collected after passing through a 2mm sieve to remove large-size gravel;
[0046] (2) Mix municipal sludge, straw, and biochar with a water content of 80% according to the material mass ratio of 100:20:9, and the fermentation period is 45 days to obtain stabilized sludge;
[0047] (3) The step of covering the mine with a thickness of 25cm after cleaning the hardened soil (2) Stabilizing sludge;
[0048] (3) On the basis of covering the stabilized sludge, cover the loam with a thickness of 20cm;
[0049] (4) On the basis of covering loam, cover the hardened soil collected in step (1) with a thickness of 15cm;
[0050] (5) On the basis of covering the hardened soil, cover the stabilized sludge with a thickness of 1...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com