Water-based paint for phoebe zhennan furniture

A water-based technology of golden nanmu, applied in the direction of coating, etc., can solve the problems of reducing the aesthetics of golden nanmu, human hazards, etc., and achieve the effect of excellent color retention, good chemical resistance and high hardness

Inactive Publication Date: 2019-01-01
阜南佳利工艺品股份有限公司
View PDF6 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] After the existing golden nanmu furniture is finished, it is often sprayed on its surface to increase the comprehensive performance of the golden nanmu furniture, but the existing paint often covers the texture pattern of the golden nanmu furniture, reducing the quality of the golden nanmu furniture. In addition, the current paint contains a lot of volatile solvents, which will cause certain harm to the human body. Because water-based paint uses water instead of organic solvents, all that evaporates when forming a film is water, and it will not harm the human body. hurt

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Water-based paint for phoebe zhennan furniture

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0021] A water-based paint for golden nanmu furniture, which consists of the following components in parts by weight: 60 parts of water-soluble resin, 20 parts of acrylic acid, 18 parts of polyethylene glycol, 23 parts of modified nano-silica, and 20 parts of modified plateau soil , 5 parts of nano zinc oxide, 9 parts of lanthanum carbonate, 8 parts of sodium carbonate, 6 parts of cerium nitrate, 5 parts of phenylethyl alcohol oleate, 3 parts of polyoxypropylene glyceryl ether, 10 parts of sodium alginate, 40 parts of sterile water.

[0022] Further, the preparation of the modified nano silicon dioxide comprises the following steps:

[0023] 1) Put the nano-silica and the modified solution A in the reactor at a weight ratio of 1:5, control the temperature in the reactor to 300°C, control the pressure in the reactor to 10MPa, and stir for 40 minutes;

[0024] 2) When the temperature in the reaction kettle in operation 1) drops to room temperature, take out the nano-silica and p...

Embodiment 2

[0032] A water-based paint for golden nanmu furniture, which consists of the following components in parts by weight: 65 parts of water-soluble resin, 22 parts of acrylic acid, 19 parts of polyethylene glycol, 24 parts of modified nano-silica, and 23 parts of modified plateau soil , 5.5 parts of nano-zinc oxide, 11 parts of lanthanum carbonate, 10 parts of sodium carbonate, 8 parts of cerium nitrate, 7 parts of phenylethyl alcohol oleate, 4 parts of polyoxypropylene glyceryl ether, 13 parts of sodium alginate, and 45 parts of sterile water.

[0033] Further, the preparation of the modified nano silicon dioxide comprises the following steps:

[0034] 1) Put the nano-silica and the modified liquid A together in the reactor according to the weight ratio of 1:5.5. The temperature in the reactor is controlled at 350°C, the pressure in the reactor is controlled at 15MPa, and the stirring process is carried out for 45 minutes;

[0035] 2) When the temperature in the reaction kettle i...

Embodiment 3

[0043] A water-based paint for golden nanmu furniture, which is composed of the following components in parts by weight: 70 parts of water-soluble resin, 24 parts of acrylic acid, 20 parts of polyethylene glycol, 25 parts of modified nano-silica, and 26 parts of modified plateau soil , 6 parts of nano zinc oxide, 13 parts of lanthanum carbonate, 12 parts of sodium carbonate, 10 parts of cerium nitrate, 9 parts of phenylethyl alcohol oleate, 5 parts of polyoxypropylene glyceryl ether, 16 parts of sodium alginate, and 50 parts of sterile water.

[0044] Further, the preparation of the modified nano silicon dioxide comprises the following steps:

[0045] 1) Put the nano-silica and the modified solution A in the reactor at a weight ratio of 1:6, control the temperature in the reactor to 400°C, control the pressure in the reactor to 20MPa, and stir for 50 minutes;

[0046] 2) When the temperature in the reaction kettle in operation 1) drops to room temperature, take out the nano-si...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses water-based paint for phoebe zhennan furniture, and belongs to the technical field of water-based paint. The water-based paint is prepared from the following ingredients in parts by weight: 60 to 70 parts of water-soluble resin, 20 to 24 parts of acrylic acid, 18 to 20 parts of polyethyleneglycol, 23 to 25 parts of modified nano-SiO2, 20 to 26 parts of modified upland soil,5 to 6 parts of nano-zinc oxide, 9 to 13 parts of lanthanum carbonate, 8 to 12 parts of sodium carbonate, 6 to 10 parts of cerium nitrate, 5 to 9 parts of phenylethanol oleate, 3 to 5 parts of polyoxypropylene glycerol ether, 10 to 16 parts of sodium alginate and 40 to 50 parts of sterile water. The raw materials are reasonably matched; the finally prepared water-based paint has the advantages ofhigh adhesion capability, good dispersion performance, ultrahigh transparency, high light resistant performance, good film forming performance, cracking difficulty, almost no volatile solvents, highsafety and good market popularization values.

Description

technical field [0001] The invention belongs to the technical field of water-based paint, and in particular relates to a water-based paint for golden nanmu furniture. Background technique [0002] Jinsinan is a general term for some nanmu (including frame nan, purple nan, Fujian nan, runnan, etc.) that have gold silk and satin-like luster in their materials. Nan. The wood has aroma, straight texture and fine structure, not easy to deform and crack, and is an excellent wood for construction and high-end furniture. Historically, golden nanmu was dedicated to the buildings and furniture of royal palaces and a few temples. The crystals in golden nanmu are obviously more than ordinary nanmu. The surface of the wood is golden in the sun, with golden threads emerging, and it has an elegant and delicate fragrance. The texture of Jinsinnan is rich and changeable, plus its unique moving and changing shadows (the wood is divided into Yin and Yang sides, different colors at different...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D4/02C09D4/06C09D7/61C09D7/62C09D7/65C09D7/63
CPCC09D4/06C09D7/61C09D7/62C09D7/63C09D7/65
Inventor 徐学进
Owner 阜南佳利工艺品股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products