[0016] First put the artificial leather garment into the dryer, then heat and dry for 10 minutes at 55°C, then spray the additive solution evenly on the leather garment with a high-pressure water gun to make the leather garment wet, then close the dryer door and dry Dry for 10 minutes, then stop drying, and then use cold air for 10 minutes.
[0017] The dryer is a tumble dryer.
[0018] The auxiliary agent is three-element block silicone oil SRS. , the solubility is 25%. The spray amount of auxiliary agent solution is 5% of leather clothing weight.
Embodiment 2
[0020] First put the artificial leather garment into the dryer, then heat and dry for 20 minutes at 50°C, then spray the additive solution evenly on the leather garment with a high-pressure water gun to make the leather garment wet, then close the dryer door and dry Dry for 20 minutes, then stop drying, and then use cold air for 30 minutes.
[0021] The dryer is a tumble dryer.
[0022] The auxiliary agent is three-element block silicone oil SRS. The spray amount of auxiliary agent solution is 5% of leather clothing weight.
Embodiment 3
[0024] First put the artificial leather garment into the dryer, then heat and dry for 15 minutes at a temperature of 53°C, then spray the additive solution evenly on the leather garment with a high-pressure water gun to make the leather garment wet, then close the dryer door and dry Dry for 15 minutes, then stop drying, and then use cold air for 20 minutes.
[0025] The dryer is a tumble dryer.
[0026] The auxiliary agent is three-element block silicone oil SRS. The spray amount of auxiliary agent solution is 5% of leather clothing weight.
[0027] Existing methods: the appearance is too bright, like artificial leather, only limited to making sofas and home textiles, and is rarely used as clothing fabrics. Because there is no matte treatment and the surface is hard, the surface fold and damage rate is 7-10% during drying.
[0028] The method of the present invention: the matt finish has the same luster, appearance and feel as real leather, and the sales volume increases by ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com